Title: (Invited) Investigations into the Formation of Germanene Using Electrochemical Atomic Layer Deposition (E-ALD)
Award ID(s):
1410109
PAR ID:
10033438
Author(s) / Creator(s):
; ; ; ; ; ; ;
Date Published:
Journal Name:
ECS Transactions
Volume:
66
Issue:
6
ISSN:
1938-6737
Page Range / eLocation ID:
129 to 140
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation