- NSF-PAR ID:
- 10052917
- Publisher / Repository:
- American Institute of Physics
- Date Published:
- Journal Name:
- The Journal of Chemical Physics
- Volume:
- 146
- Issue:
- 5
- ISSN:
- 0021-9606
- Page Range / eLocation ID:
- 052817
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
Abstract An along‐isobath current in stratified waters leads to a bottom boundary layer. In models with no alongshore variation, cross‐isobath density transport in this bottom boundary layer reduce the velocity in the bottom boundary layer via thermal wind, and thus the bottom friction experienced by the current above the boundary layer—this is bottom‐boundary‐layer arrest. If, however, alongshore variation of the flow is allowed, the bottom boundary layer is baroclinically unstable. We show with high resolution numerical models that these instabilities reduce this arrest and allow bottom friction to decelerate the flow above the bottom boundary layer when the flow is in the Kelvin wave direction (so that the bottom Ekman transport is downwelling). Both the arrest of the bottom boundary layer and the release from this arrest are asymmetric; the friction experienced by flows in the direction of Kelvin‐wave propagation (downwave) is much greater than flows in the opposite direction. The strength of the near bottom currents, and thus the magnitude of bottom friction, is found to be governed by the destruction of potential vorticity near the bottom balanced by the offshore along‐isopycnal transport of this anomalous potential vorticity. A simple model of this process is created and used to quantify the magnitude of this effect and the resulting reduction of arrest of the bottom boundary layer.
-
Abstract Two-dimensional (2D) transition metal dichalcogenide (2D TMD) layers present an unusually ideal combination of excellent opto-electrical properties and mechanical tolerance projecting high promise for a wide range of emerging applications, particularly in flexible and stretchable devices. The prerequisite for realizing such opportunities is to reliably integrate large-area 2D TMDs of well-defined dimensions on mechanically pliable materials with targeted functionalities by transferring them from rigid growth substrates. Conventional approaches to overcome this challenge have been limited as they often suffer from the non-scalable integration of 2D TMDs whose structural and chemical integrity are altered through toxic chemicals-involved processes. Herein, we report a generic and reliable strategy to achieve the layer-by-layer integration of large-area 2D TMDs and their heterostructure variations onto a variety of unconventional substrates. This new 2D layer integration method employs water only without involving any other chemicals, thus renders distinguishable advantages over conventional approaches in terms of material property preservation and integration size scalability. We have demonstrated the generality of this method by integrating a variety of 2D TMDs and their heterogeneously-assembled vertical layers on exotic substrates such as plastics and papers. Moreover, we have verified its technological versatility by demonstrating centimeter-scale 2D TMDs-based flexible photodetectors and pressure sensors which are difficult to fabricate with conventional approaches. Fundamental principles for the water-assisted spontaneous separation of 2D TMD layers are also discussed.