<?xml-model href='http://www.tei-c.org/release/xml/tei/custom/schema/relaxng/tei_all.rng' schematypens='http://relaxng.org/ns/structure/1.0'?><TEI xmlns="http://www.tei-c.org/ns/1.0">
	<teiHeader>
		<fileDesc>
			<titleStmt><title level='a'>Block Copolymer Pressure-Sensitive Adhesives Derived from Fatty Acids and Triacetic Acid Lactone</title></titleStmt>
			<publicationStmt>
				<publisher></publisher>
				<date>2020 June</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10161265</idno>
					<idno type="doi">10.1021/acsapm.0c00317</idno>
					<title level='j'>ACS Applied Polymer Materials</title>
<idno>2637-6105</idno>
<biblScope unit="volume"></biblScope>
<biblScope unit="issue"></biblScope>					

					<author>Hussnain Sajjad</author><author>William B. Tolman</author><author>Theresa M. Reineke</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[A method for the development of ABA triblock copolymers for high-performance pressure-sensitive adhesives from the biorenewable chemicals lauryl acrylate and triacetic acid lactone (TAL) is presented. Lauryl acrylate, readily derived from vegetable oils, was polymerized via a reversible additionfragmentation chain-transfer process to yield high-molecularweight telechelic polymers. The synthesis of triblock copolymers was accomplished by subsequent chain extension with TAL, which is available from carbohydrates via the action of genetically modified yeast. The resulting triblock copolymers were found to exhibit excellent adhesion, with tunable peel forces up to 8 N cm -1 when a rosin ester-based tackifier was used. Tack forces up to 7 N cm -1 and no shear failure up to 100 h demonstrate the competitive performance of the potentially sustainable adhesives with commercial commodity products.]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; INTRODUCTION</head><p>Thermoplastic elastomers (TPEs) comprise an important class of reprocessable materials that have found use in a wide range of applications including pressure-sensitive adhesives (PSAs), footwear, electronics, and medical devices. <ref type="bibr">1,</ref><ref type="bibr">2</ref> Petroleum-based triblock copolymers with an ABA architecture, such as poly(styrene-butadiene-styrene) (SBS) or poly(styrene-isoprene-styrene), have been traditionally used as TPEs. The ABA-type architecture, employing a "rubbery" midblock (B) and flanking "glassy" blocks (A), allows for molecular variation in composition, which influences the nanoscale structure of the material and ultimately dictates its application and use. <ref type="bibr">3,</ref><ref type="bibr">4</ref> For example, immiscibility of the high T g poly(styrene) domains with the low T g poly(butadiene) domains in SBS triblock copolymers leads to phase-segregated nanostructures, which enhance the mechanical properties of the material. <ref type="bibr">3</ref> The use of finite, petroleum-based platform chemicals for the manufacturing of TPEs, however, is concerning from a sustainability and environmental viewpoint. Consequently, the development of soft materials from alternative, more sustainable sources is a major contemporary societal demand, <ref type="bibr">[5]</ref><ref type="bibr">[6]</ref><ref type="bibr">[7]</ref> and researchers have maintained a focused effort into replacing the outer (A) and/or inner (B) blocks with biorenewable feedstocks. For example, poly(lactide) (PLA) has been used as a glassy component in TPEs with various lactones, alkenes, glycols, menthide, or ricinoleic acid serving as the rubbery component. <ref type="bibr">[8]</ref><ref type="bibr">[9]</ref><ref type="bibr">[10]</ref><ref type="bibr">[11]</ref><ref type="bibr">[12]</ref><ref type="bibr">[13]</ref><ref type="bibr">[14]</ref><ref type="bibr">[15]</ref><ref type="bibr">[16]</ref><ref type="bibr">[17]</ref><ref type="bibr">[18]</ref><ref type="bibr">[19]</ref><ref type="bibr">[20]</ref><ref type="bibr">[21]</ref><ref type="bibr">[22]</ref> Although PLA is used as the glassy component, its relatively low glass-transition temperature (T g ) limits its utility in TPEs. Acrylic block copolymers, however, offer functional versatility (such as tunable T g values) because of the ability to vary the pendant ester group. Notable examples in recent years have employed renewable terpene derivatives as replacements for the rubbery and glassy blocks in triblock copolymers for PSAs and elastomers. <ref type="bibr">23,</ref><ref type="bibr">24</ref> In a similar fashion, we previously reported on the production of TPEs employing acrylic derivatives of glucose and isosorbide as replacements for the glassy, styrene-based endblocks in traditional TPEs. <ref type="bibr">[25]</ref><ref type="bibr">[26]</ref><ref type="bibr">[27]</ref><ref type="bibr">[28]</ref> Using reversible addition-fragmentation chain-transfer (RAFT) polymerization as a controlled polymerization technique, <ref type="bibr">29,</ref><ref type="bibr">30</ref> n-butyl acrylate (nBA) was copolymerized with the acrylate-functionalized sugar derivatives to create triblock copolymers with an ABA-type architecture. Poly nBA has a low glass-transition temperature (-47 &#176;C) and an entanglement molecular weight of 28 kDa <ref type="bibr">31,</ref><ref type="bibr">32</ref> and is often used as a rubbery midblock in ABA-type polymers for PSA applications. Because the elastic modulus of an elastomer is related to the average molecular weight between entanglements, polymers with larger M e values are favorable for PSAs owing to their inherently lower elastic modulus compared to traditional butadiene-or isoprene-based elastomers. <ref type="bibr">33</ref> The adhesive and mechanical properties of the resultant ABA-triblock materials were comprehensively evaluated and shown to exhibit promising properties that depended on block identity, molecular weight, and tackifier presence. Another notable example similarly used RAFT polymerization to copolymerize nBA with acrylic derivatives of phenolic compounds obtained from the depolymerization of lignocellulosic biomass to create PSAs. <ref type="bibr">34</ref> While these studies substituted the glassy component of acrylic-based TPEs, sustainability is difficult to attain because of the use of p(nBA) as the rubbery midblock.</p><p>Although it is feasible to derive nBA from bio-sourced nbutanol, <ref type="bibr">35</ref> an arguably more attractive choice for the midblock in the context of this work is lauryl acrylate (LauAc). Lauryl alcohol can be directly obtained from the fatty acids of vegetable oils and is a major component of coconut and palm kernel oils. <ref type="bibr">36,</ref><ref type="bibr">37</ref> In illustrative applications, lauryl acrylate and stearyl acrylate were copolymerized with styrene via RAFT polymerization to create elastomers with an ABA-type architecture. <ref type="bibr">37,</ref><ref type="bibr">38</ref> As a consequence of the high entanglement molecular weights (M e ) of longer-chain alkyl acrylates, the resultant elastomers were weaker than the traditional SBS elastomers (i.e., exhibited lower stress and strain at break). PSAs of this architecture, however, benefit from the use of a base elastomer with a high entanglement molecular weight. We postulated that the higher M e of p(LauAc) should yield an elastomer that exhibits a lower elastic modulus in comparison to p(nBa), a property that is desirable for instantaneous bonding of an adhesive to a substrate.</p><p>In addition to exploring alternatives for the midblock in ABA copolymers, we also sought to replace styrene with renewable feedstocks for use in synthesizing the glassy component in TPEs. We chose 4-hydroxy-6-methyl-2-pyrone [denoted as triacetic acid lactone (TAL)], which can be obtained synthetically from acetic acid <ref type="bibr">[39]</ref><ref type="bibr">[40]</ref><ref type="bibr">[41]</ref> or through biological pathways in select microbes, which synthesize the compound as a secondary metabolite of glucose and other sugars. <ref type="bibr">[42]</ref><ref type="bibr">[43]</ref><ref type="bibr">[44]</ref> Notably, ongoing research into the genetic bioengineering of Escherichia coli and Saccharomyces cerevisiae suggests that biologically synthesized TAL may be a viable feedstock. <ref type="bibr">[45]</ref><ref type="bibr">[46]</ref><ref type="bibr">[47]</ref><ref type="bibr">[48]</ref><ref type="bibr">[49]</ref><ref type="bibr">[50]</ref> Although TAL and its numerous derivatives have been studied for their efficacy as food preservatives, antimicrobials, pharmaceuticals, and so forth, its use as a renewable feedstock for polymer synthesis has yet to be explored in detail. <ref type="bibr">41,</ref><ref type="bibr">49,</ref><ref type="bibr">51</ref> In a recent study, partial substitution of p(epichlorohydrin) with TAL via postpolymerization modification resulted in an apparent increase in the T g of the material from -30 &#176;C up to 70 &#176;C depending on the degree of substitution. <ref type="bibr">49</ref> We hypothesized that TAL and its hydrogenated derivative could be readily substituted with acrylic groups and polymerized via controlled methods, resulting in a material with properties suitable for use as a glassy component in biosourced multiblock copolymer TPEs for PSA applications. In addition, we postulated that renewable rubbery blocks derived from vegetable oils can replace p(nBA) as the base elastomer. Herein, we report functionalization of TAL directly with acryloyl chloride, as well as the synthesis of a similarly substituted variant derived from hydrogenating TAL. Block copolymerization with lauryl acrylate as the rubbery midblock was performed to create a series of well-defined, high-molar-mass ABA acrylic triblock copolymers. Adhesion performance studies (peel adhesion, loop tack, and shear failure) revealed functional properties comparable to commercial PSAs. This work demonstrates a new strategy for the preparation of functional block copolymer PSAs from renewably sourced building blocks.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; EXPERIMENTAL SECTION</head><p>Materials. 4-Hydroxy-6-methyl-2-pyrone ("TAL" "pyrone") was purchased from Oakwood Chemical and used without further purification. Pd/C (10 wt % loading) was purchased from Sigma-Aldrich and dried under vacuum prior to use. Acryloyl chloride, nBA, and lauryl acrylate were purchased from Sigma-Aldrich, passed through basic alumina to remove inhibitors, and stored at -30 &#176;C until further use. The RAFT chain-transfer agent (CTA) [(3,5-bis(2dodecylthiocarbonothioylthio-1-oxopropoxy)benzoic acid (BTCBA)] and 2,2&#8242;-azobis(2-methylpropionitrile) (AIBN) were purchased from Sigma-Aldrich and used as-received. The rosin ester tackifier (SYLVALITE RE-80HP) was from Arizona Chemical and used asreceived.</p><p>Characterization. All reported 1 H NMR spectra were collected on a Bruker AVANCE III HD 500 MHz spectrometer in deuterated chloroform (CDCl 3 ), and chemical shifts are referenced to tetramethylsilane at 0.00 ppm. The spectra of all small molecules were collected at 22 &#176;C with D1 = 1 s (16 scans), and the spectra of all polymers were collected at 22 &#176;C with D1 = 10 s (64 scans). Highresolution mass spectrometry (HRMS) was performed using a Bruker BioTOF II in positive mode. Tetrahydrofuran (THF) size exclusion chromatography (SEC) was performed in uninhibited THF utilizing a Waters Styragel guard column and three consecutive Waters Styragel columns at a flow rate of 1 mL min -1 at 22 &#176;C. The instrument was equipped with an Agilent 1260 Infinity liquid chromatograph coupled with a Wyatt Dawn Heleos II multiangle light scattering detector (18 angles from 10 to 160&#176;and a 662.6 nm laser) and a Wyatt Optilab T-rEX refractive index detector. Dimethylformamide (DMF) SEC was performed in DMF with 0.05 M LiBr at a flow rate of 1.0 mL min -1 at 50 &#176;C. The instrument was equipped with a Wyatt Dawn Heleos II multiangle light scattering detector (18 angles from 10 to 160&#176;and a 662.6 nm laser) and a Wyatt Optilab T-rEx refractive index detector. The reported dn/dc values were calculated from the RI signal using a known sample concentration and assuming 100% mass recovery from the column and used for molar mass determination. Thermogravimetric analysis (TGA) was performed on a TA Instruments Q500 series at a heating rate of 10 &#176;C min -1 under 60/40 nitrogen/oxygen flow. Differential scanning calorimetry (DSC) experiments were conducted with a TA Instruments Discovery DSC, using samples hermetically sealed in aluminum pans, at a heating/cooling rate of 10 &#176;C min -1 . The reported T g /T c /T m values were from the second heating/cooling ramps. Adhesion and tensile testing was performed on a Shimadzu AGS-X tensile tester.</p><p>Hydrogenation of 4-Hydroxy-6-methyl-2-pyrone (TAL). Uninhibited THF was stirred over activated 3 &#197; molecular sieves for 24 h and filtered through a bed of Celite prior to use. A 300 mL high-pressure reactor vessel was charged with TAL (12.0 g, 95.1 mmol), Pd/C (1.2 g, 10% by mass), and 200 mL of THF. The reactor was sealed, first pressurized and depressurized with argon (3&#215;) to remove O 2 , then pressurized with gaseous H 2 to 100 psi, heated to 50 &#176;C, and then pressurized to 500 psi. Over the next 48 h, the reactor vessel was periodically repressurized to 500 psi, after which time the vessel was cooled to room temperature and purged with argon to remove H 2 . The reaction mixture was then filtered through a bed of Celite to remove the Pd/C. THF was removed under vacuum to afford 4-hydroxy-6-methyl-2-lactone ("lactone") (11.7 g, 95% isolated yield). <ref type="bibr">1</ref>  Synthesis of 4-Acrylate-6-methyl-2-pyrone (Acrylated-pyrone, AcPy). TAL (4-hydroxy-6-methyl-2-pyrone) (10.0 g, 79.3 mmol), acryloyl chloride (7.18 g, 79.3 mmol), and 100 mL of anhydrous CH 2 Cl 2 were sequentially added to a dry 200 mL roundbottom flask. The flask was sealed with a rubber septum and submerged in an ice bath, and then, NEt 3 (10.1 mL, 7.29 g, 72.1 mmol) was added dropwise to the stirring solution. After 4 h, the precipitated NEt 3 HCl salt was removed by filtration, and the filtrate was washed with 100 mL of a saturated sodium bicarbonate solution (&#215;3) and once with 100 mL of brine. The organic layer was dried over magnesium sulfate, filtered, and concentrated under vacuum to yield a yellow liquid. The yellow liquid was loaded onto a silica column (2&#8243; diameter &#215; 1.5&#8242; length), and a mixture of diethyl ether/ hexanes (4:1) was used as the eluent. The desired compound elutes first from the column. The solvents were then removed under vacuum to afford AcPy (6.2 g, 43.6% isolated yield). <ref type="bibr">1</ref> H NMR (500 MHz, chloroform-d): &#948; 6.62 (d, J = 17.2 Hz, 1H), 6.24 (dd, J = 17.2, 10.5 Hz, 1H), 6.11 (d, J = 10.1 Hz, 2H), 6.02 (d, J = 1.8 Hz, 1H), 2.28 (s, 3H). <ref type="bibr">13</ref>  Synthesis of 4-Acrylate-6-methyl-2-lactone (Acrylated-lactone, AcLa). Lactone (11.7 g, 89.9 mmol), acryloyl chloride (8.97 g, 99.1 mmol), and 100 mL of anhydrous CH 2 Cl 2 were sequentially added to a dry 200 mL round-bottom flask. The flask was sealed with a rubber septum and submerged in an ice bath, and then, N,Ndiisopropylethylamine (17.3 mL, 12.8 g, 99.1 mmol) was added dropwise to the stirring solution. After 2 h, CH 2 Cl 2 was removed under vacuum to yield a dark orange oil. The oil was diluted with 5 mL of CH 2 Cl 2 and loaded onto a silica column (5&#8243; diameter &#215; 1&#8242; length), and neat diethyl ether was used as the eluent (note: excess acryloyl chloride elutes first and then the desired product. R f = 0.35). The solvent was removed under vacuum to afford AcLa (11.0 g, 66.4% isolated yield). <ref type="bibr">1</ref> H NMR (400 MHz, chloroform-d): &#948; 6.43 (dd, J = 17.3, 1.3 Hz, 1H), 6.10 (dd, J = 17.3, 10.5 Hz, 1H), 5.89 (dd, J = 10.4, 1.3 Hz, 1H), 5.29 (m, 1H), 4.47-4.37 (m, 1H), 2.96 (ddd, J = 17.2, 6.4, 1.0 Hz, 1H), 2.62 (dd, J = 17.3, 6.6 Hz, 1H), 2.43 (dddd, J = 14.0, 6.2, 2.9, 1.0 Hz, 1H), 1.67 (ddd, J = 14.1, 11.6, 8.6 Hz, 1H), 1.43 (d, J = 6.3 Hz, 3H). <ref type="bibr">13</ref>  Synthesis of Poly(acrylated-lactone) (p(AcLa)) via Free Radical Polymerization. Acrylated-lactone (0.200 g, 1.09 mmol), AIBN (1.78 mg, 10.8 &#956;mol) (from a dilute stock solution), and 5 mL of acetonitrile were added to a vacuum flask. The flask was sealed and degassed by four consecutive freeze-pump-thaw cycles and then submerged in a preheated oil bath at 70 &#176;C. After stirring vigorously for 18 h, the flask was immediately submerged in liquid nitrogen until frozen and opened to the atmosphere. After thawing the solution at room temperature, the polymer was precipitated in cold H 2 O and washed repeatedly with methanol until pure (monitored via 1 H NMR). The polymer was then dried in a vacuum oven at 60 &#176;C for 24 h (50% conversion via 1 H NMR spectroscopy, 0.100 g, 50% isolated yield). <ref type="bibr">1</ref> H NMR (400 MHz, chloroform-d): &#948; 5.26 (s, 1H), 4.45 (s, 1H), 2.28 (s, 1H), 2.61 (s, 1H), 2.42 (s, 1H), 2.30 (s, 1H), 1.86 (s, 2H), 1.69 (s, 1H), 1.45 (s, 3H). M n (p(AcLa)) = 30 kg mol -1 , &#272; = 1.60.</p><p>Synthesis of Poly(n-butyl acrylate) via RAFT (CTA-p(nBA)-CTA). The synthesis of the macro-CTA was performed following literature procedures. <ref type="bibr">[24]</ref><ref type="bibr">[25]</ref><ref type="bibr">[26]</ref> AIBN (5.12 mg, 0.031 mmol), BTCBA (128 mg, 0.156 mmol), and nBA (10.0 g, 78.0 mmol) were added to a dry 50 mL vacuum flask. The flask was sealed and degassed by four freeze-pump-thaw cycles and then submerged in a preheated oil bath at 70 &#176;C. After stirring vigorously for 2 h, the flask was immediately submerged in liquid nitrogen and opened to the atmosphere. CH 2 Cl 2 (10 mL) was added to the flask, and the polymer was precipitated in 200 mL of cold methanol. After allowing the contents to settle for 1 h, methanol was decanted, and 200 mL of additional cold methanol was added. The process was repeated twice, and then the purified CTA-p(nBA)-CTA polymer was dried in a vacuum oven at 60 &#176;C for 18 h (84% conversion via 1 H NMR spectroscopy, 8.14 g, 81.0% isolated yield). <ref type="bibr">1</ref> H NMR (500 MHz, chloroform-d): &#948; 4.04 (dq, J = 18.6, 10.1 Hz, 2H), 2.40-2.22 (m, 1H), 1.93 (m, 2H), 1.63 (m, 2H), 1.39 (m, 2H), 0.95 (t, J = 7.5 Hz, 3H). M n (CTA-p(nBA)-CTA) = 55 kg mol -1 , &#272; = 1.05, dn/dc = 0.066.</p><p>Synthesis of CTA-p(AcLa)-p(nBA)-p(AcLa)-CTA. An illustrative example is provided. CTA-p(nBA)-CTA (1.0 g, 0.018 mmol), acrylated-lactone (AcLa) (0.335 g, 1.81 mmol), AIBN (0.299 mg, 1.82 &#956;mol) (from a dilute stock solution), and 10 mL of DMF were added to a vacuum flask. The flask was sealed and degassed by four consecutive freeze-pump-thaw cycles and then submerged in a preheated oil bath at 70 &#176;C. After stirring vigorously for 24 h, the flask was immediately submerged in liquid nitrogen and opened to the atmosphere. The polymer was precipitated in cold H 2 O and washed repeatedly with methanol until DMF and the unreacted monomer were removed (monitored via 1 H NMR). The precipitates were then dried in a vacuum oven at 60 &#176;C for 24 h. <ref type="bibr">1</ref>  Synthesis of Poly(lauryl acrylate) via RAFT (CTA-p(LauAc)-CTA). The synthesis of macro-CTA was performed following modified literature procedures. <ref type="bibr">[24]</ref><ref type="bibr">[25]</ref><ref type="bibr">[26]</ref> AIBN (0.27 mg, 1.64 &#956;mol from stock solution), BTCBA (6.8 mg, 8.36 &#956;mol), and lauryl acrylate (2.0 g, 8.32 mmol) were added to a dry 50 mL vacuum flask. The flask was sealed and degassed by four freeze-pump-thaw cycles and then submerged in a preheated oil bath at 70 &#176;C. After stirring vigorously for 3 h, the flask was immediately submerged in liquid nitrogen and opened to the atmosphere. CHCl 3 (10 mL) was added to the flask, and the polymer was precipitated in 200 mL of cold methanol. After allowing the contents to settle for 1 h, methanol was decanted, and 200 mL of additional cold methanol was added. The process was repeated twice and then the purified CTA-p(LauAc)-CTA polymer was dried in a vacuum oven at 60 &#176;C for 18 h (88% conversion via 1 H NMR spectroscopy, 1.60 g, 80.0% isolated yield). <ref type="bibr">1</ref>  Synthesis of CTA-p(AcLa)-p(LauAc)-p(AcLa)-CTA. An illustrative example is provided. CTA-p(LauAc)-CTA (0.5 g, 2.17 &#956;mol), acrylated-lactone (AcLa) (0.12 g, 0.65 mmol), AIBN (71.4 &#956;g, 0.43 &#956;mol) (from a dilute stock solution), and 5 mL of CHCl 3 were added to a vacuum flask. The flask was sealed and degassed by four consecutive freeze-pump-thaw cycles and then submerged in a preheated oil bath at 70 &#176;C. After stirring vigorously for 24 h, the flask was immediately submerged in liquid nitrogen and opened to the atmosphere. The polymer was precipitated in cold methanol and washed repeatedly with methanol until the unreacted monomer was removed (monitored via 1 H NMR). The precipitates were then dried in a vacuum oven at 60 &#176;C for 24 h. <ref type="bibr">1</ref>  Dynamic Mechanical Analysis. Dynamic mechanical analysis (DMA) of poly(LauAc) (M n = 300 kDa) was performed at 5 &#176;C within the linear viscoelastic regime. An oscillatory stress was applied to sample between two 25 mm steel plates, and the sinusoidal stress response was measured. The resultant complex modulus was decoupled into the in-phase/elastic (G&#8242;) and out-of-phase/viscous (G&#8243;) moduli. The loss tangent (tan &#948;), which is the ratio of the viscous modulus G&#8243; to the elastic modulus G&#8242;, was also calculated. The plateau in the storage modulus versus angular frequency curve (26,460 Pa), corresponding to a minimum in tan &#948;, was used to calculate the entanglement molecular weight (M e ) of poly(LauAc) as 66 kDa.</p><p>Adhesion Testing. Samples for PSA evaluations were prepared by dissolving the polymer or polymer/tackifier blend in THF or CHCl 3 to produce 30% solid content solution (example: 100 mg of polymer or 70 mg of polymer/30 mg of tackifier in 265 &#956;L THF). The solution was then solvent-cast onto a 50 &#956;m thick sheet of polyethylene terephthalate (PET) films using a standard laboratory drawdown rod to target a coat weight of 25 gsm. The films were allowed to dry under ambient conditions for 24 h and then cut into 1 cm wide strips for adhesion testing.</p><p>180&#176;Peel Adhesion (PSTC-101 Adhesion Test Method). A 1 cm wide strip of the polymer-coated PET film was adhered, using a 500 g roller, to a dry stainless steel plate that was cleaned with acetone prior to the test. The PET film was then peeled from the stainless steel plate using a Shimadzu AGX-X tensile tester at a peel rate of 305 mm min -1 . The peel force was recorded as the maximum force measured during the test, and the reported average and standard deviation values were acquired from five replicates.</p><p>Loop Tack (PSTC-16 Adhesion Test Method). A 1 cm wide strip of the polymer-coated PET film was formed into a tear-drop-shaped loop and mounted onto the upper grip of the tensile tester. The loop was then lowered onto a dry stainless steel plate that was cleaned with acetone prior to the test to give a contact area of 1 cm &#215; 1 cm. The tack force was recorded as the maximum force measured while raising the upper grip at a rate of 305 mm min -1 , and the reported average and standard deviation values were acquired from five replicates.</p><p>Shear Adhesion (PSTC-107 Adhesion Test Method). A 2.54 cm &#215; 2.54 cm strip of the polymer-coated PET film was adhered, using a 500 g roller, to a dry stainless steel plate that was cleaned with acetone prior to the test. The steel plate was held at a 2&#176;angle relative to a vertical plane, and a 1 kg weight was suspended from the test strip. The time to adhesive failure was recorded for three samples.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; RESULTS AND DISCUSSION</head><p>Initial efforts focused on targeting high-molecular-weight poly(lauryl acrylate) (p(LauAc)) for testing as a suitable midblock in an ABA triblock copolymer. Despite the advantage of using an elastomer with a high M e as discussed above, appreciable peel adhesion values for triblock-based PSAs are only obtainable if the molecular weight of the rubbery midblock is at least 2-3 times the entanglement molecular weight of the polymer (i.e., the elastomer is "loosely" entangled). <ref type="bibr">52</ref> RAFT polymerization of nBA using a bifunctional CTA was previously introduced by our group as a means to synthesize a living, chain-extendable rubbery midblock for an acrylic-based system. <ref type="bibr">[26]</ref><ref type="bibr">[27]</ref><ref type="bibr">[28]</ref> Using a similar RAFT polymerization method with a commercially available difunctional CTA (BTCBA), we synthesized high-molecular-weight p-(LauAc) with narrow dispersities (M n = 300 kDa, &#272; = 1.19) while retaining the living nature of the polymer chain for chain extension with a glassy block (Scheme 1, see Figure <ref type="figure">S1</ref> for 1 H NMR spectrum). The TGA analysis of the p(LauAc) macro-CTA showed good thermal stability with 5% weight loss occurring at &#8764;330 &#176;C (Figure <ref type="figure">S2</ref>). The DSC thermogram displays T m = 2 &#176;C, T c = -5 &#176;C, and no discernible T g feature (Figure <ref type="figure">S3</ref>). The thermal features seen in the thermogram of p(LauAc) correspond to the crystallization and melting events of the pendant alkyl chains. <ref type="bibr">[53]</ref><ref type="bibr">[54]</ref><ref type="bibr">[55]</ref> To validate that p(LauAc) is minimally entangled at the synthesized molecular weights, DMA was performed to calculate M e , which had not been reported to date. The entanglement molecular weight was calculated using the moduli versus frequency plot shown in Figure <ref type="figure">1</ref>  </p><p>where G N 0 is the plateau modulus determined from oscillatory shear experiments, &#961; is the density of the polymer (taken as 0.94 g/mL at 21 &#176;C from the literature), <ref type="bibr">37</ref> R is the gas constant, and T is the temperature at which the rheological experiments were conducted (5 &#176;C). We note that although the reference temperature differs from the temperature at which the density measurement was performed, the difference in density of p(LauAc) between the two temperatures is expected to be negligible. Using the minimum of tan &#948;, a ratio of the loss to elastic moduli, as a reference point, the plateau modulus was determined to be 26,500 Pa, and the M e of p(LauAc) was calculated to be 70 kDa. Therefore, polymers above approximately 210 kDa (i.e., &#8764;3 &#215; M e ) are expected to be minimally entangled. A M e value for poly-(laurylmethacrylate) was reported to be 225 kDa based on rheological measurements on a sample with M n = 82 kDa. <ref type="bibr">57</ref> However, it is uncertain if the tested sample was suitably entangled in order to gather meaningful data for an accurate calculation.</p><p>We then sought to design efficient methods to create acrylic variants of TAL through two routes for polymerization into block polymer architectures (Scheme 2). Catalytic hydrogenation of TAL using Pd/C afforded the reduced lactone derivative (Figure <ref type="figure">S4</ref>). <ref type="bibr">51</ref> The transformation approached nearquantitative yields under the given conditions after 2-3 days, depending on the scale. The lengthy reaction time toward complete hydrogenation is attributed to an internal keto-enol tautomerism, largely in favor of the keto-form, which is established following partial reduction of the pyrone ring (Scheme S1, Figure <ref type="figure">S5</ref>). Esterification of the hydroxyl substituents on both the pyrone and lactone rings with acryloyl chloride yielded 4-acrylate-6-methyl-2-pyrone (AcPy, Scheme 1. Synthesis of p(Lauryl acrylate) via RAFT Polymerization Figures <ref type="figure">S6</ref> and<ref type="figure">S7</ref>) and 4-acrylate-6-methyl-2-lactone (AcLa, Figures <ref type="figure">S8</ref> and<ref type="figure">S9</ref>), respectively.</p><p>Prior to block copolymerization with p(LauAc), attempts toward the free radical and RAFT polymerizations of AcPy were carried out with azobis(isobutyronitrile) (AIBN) and various CTAs at 70 &#176;C in DMF to establish reactivity and kinetics. Aliquots taken from the reaction mixture over time were analyzed by 1 H NMR spectroscopy, and the results indicated that no appreciable polymerization had occurred. In contrast, the free radical polymerization of AcLa under similar reaction conditions yielded p(AcLa) (Figure <ref type="figure">S10</ref>), reaching equilibrium at 88% conversion ( 1 H NMR spectroscopy). We speculate that the observed difference in reactivity between AcPy and AcLa toward radical polymerizations may be attributed to the alkene bonds of the pyrone ring, which can react with propagating radicals and lead to chain termination events.</p><p>The purified p(AcLa) homopolymer was analyzed by SEC in DMF with multiangle laser light scattering (SEC-MALLS) to determine a number-average molar mass (M n ) of 30 kg mol -1 and a dispersity (&#272;) of 1.60 (Figure <ref type="figure">S11</ref>). TGA showed a thermal degradation temperature (T d , 5 wt % loss) of 197 &#176;C (Figure <ref type="figure">S12</ref>). Because degradation of polyacrylic backbones typically occurs at &#8764;300-350 &#176;C following a random chain scission mechanism, the relatively lower observed T d of p(AcLa) is likely due to the decomposition of the pendant lactone rings. <ref type="bibr">58,</ref><ref type="bibr">59</ref> DSC analysis of the homopolymer, scanning to a maximum temperature limit of 170 &#176;C, initially indicated a T g of 84 &#176;C (Figure <ref type="figure">2</ref>). This relatively high T g of p(AcLa) suggests that it can be used as a "glassy" component in a triblock copolymer system. Intriguingly, the DSC thermogram exhibited an exothermic feature beginning at 125 &#176;C during the first temperature sweep; the second heating ramp in the experiment then showed a shift of the T g value of the homopolymer to lower temperatures (&#8764;23 &#176;C in Figure <ref type="figure">2</ref>). Both the exothermic feature and the observed shift in T g between consecutive heating ramps were not observed if the DSC experiment was conducted to a maximum temperature limit of 110 &#176;C (Figure <ref type="figure">S13</ref>). The soluble fraction of a sample of p(AcLa) subjected to temperatures above 125 &#176;C was analyzed via 1 H NMR spectroscopy. The results indicated the presence of an unsaturated derivative of TAL (Figure <ref type="figure">S14</ref>), which is presumably ejected from the polymer backbone at elevated temperatures. <ref type="bibr">51,</ref><ref type="bibr">60</ref> A change in the polymer sequence (i.e., interspersed acrylic acid moieties along the backbone of the polymer) and the presence of a small molecule within the polymer matrix are likely responsible for the observed shift in T g shown in Figure <ref type="figure">2</ref>. Nevertheless, because the formulated adhesives in this work are stable up to 125 &#176;C, and only change chemically upon exposure to higher temperatures, processing temperatures of &#8764;100 &#176;C (i.e., above the T g of both blocks) would be unlikely to interfere with treatment. Additionally, because most of the commodity PSAs are typically used at room temperature (tape, sticky notes, etc.), the chemical change observed at elevated temperatures will not limit userend applicability.</p><p>We then used a controlled radical polymerization strategy to prepare a family of triblock copolymers (Scheme 3). <ref type="bibr">[61]</ref><ref type="bibr">[62]</ref><ref type="bibr">[63]</ref> In addition to testing p(LauAc) as the base elastomer, nBA was also polymerized in accordance with previous methods. <ref type="bibr">26,</ref><ref type="bibr">27,</ref><ref type="bibr">34</ref> A molecular weight of 55 kDa for the p(nBA) midblock was targeted to allow for direct comparisons among the various PSAs, which have used p(nBA) of the same molecular weight as that of the base elastomer and different acrylic derivatives as the glassy endblocks. RAFT polymerization of nBA was performed in the bulk with AIBN and BTCBA at 70 &#176;C to afford the living macro-CTA (see Figure <ref type="figure">S15</ref> for 1 H NMR). The number-average molar mass, analyzed via THF SEC-MALLS, and the measured thermal data (T d and T g ) of this rubbery midblock were in agreement with the values previously reported for this synthetic procedure (Table <ref type="table">1</ref>, Figures <ref type="figure">S16</ref> and<ref type="figure">S17</ref>). <ref type="bibr">26,</ref><ref type="bibr">27</ref> Lauryl acrylate was polymerized to target molecular weights such that the elastomer is minimally entangled (&#8764;3 &#215; M e ) and therefore has a low elastic modulus, which is desirable for bonding of the adhesive to a given substrate. The molecular weights of the glassy p(AcLa) endblocks were varied to examine the effect of higher hard block weight percentages on the adhesive performance of the PSAs.</p><p>Subsequent chain extension of the p(nBA) and p(LauAc) macro-CTAs with AcLa afforded the desired triblock copolymers. Successful chain extension was validated by observation of peaks corresponding to p(AcLa) in the 1 H NMR spectra (Figures <ref type="figure">S18</ref> and<ref type="figure">S19</ref>) accompanied by a clear shift of the SEC traces to lower retention times when compared to the macro-CTAs (Figures <ref type="figure">S20-S22</ref>). The Scheme 2. Syntheses of Acrylated-Pyrone (AcPy) and Acrylated-Lactone (AcLa) Figure <ref type="figure">2</ref>. DSC thermograms of p(AcLa) from -50 to 170 &#176;C taken on the first and second ramps of heating at 10&#176;C min -1 . The synthetic scheme shown depicts the chemical change of the polymer at temperatures above 125 &#176;C. The 1 H NMR spectrum of the ejected small molecule can be found in the Supporting Information (Figure <ref type="figure">S9</ref>). presence of a shoulder in the SEC traces at lower retention times is likely due to the formation of multiblock polymers stemming from termination-by-combination events. By adjusting the molar ratio of macro-CTA to AcLa in the reaction mixture, variable weight percentages of hard block content within the resultant triblock copolymers were attained (Table <ref type="table">1</ref>). The TGA profiles of the triblock copolymers (P1-P7) show two distinct features at 190 and 350 &#176;C, corresponding to the decomposition of the pendant lactone rings and the acrylate backbone, respectively (Figures <ref type="figure">S23-S29</ref>). While the glass-transition temperature of the p(nBA) midblock can be clearly seen in the DSC thermograms of P1-P4 (Figure <ref type="figure">3</ref>), the T g feature of the p(AcLa) blocks is only well defined in P3 and P4, which have longer endblock lengths. The DSC thermograms of P5-P7 (Figures <ref type="figure">S30-S32</ref>, respectively) show the T m and T c features of the dodecyl alkyl chains, but a discernable T g peak for the p(AcLa) segments is only seen in P6, which also contains the highest weight fraction of the hard blocks. This observation has been reported for other triblock copolymers with a relatively low hard block content and is likely a result of the shorter p(AcLa) segments, <ref type="bibr">26,</ref><ref type="bibr">27,</ref><ref type="bibr">34</ref> which ultimately translates to imperceptible heat exchange in the calorimetry experiment. Furthermore, a match of both the p(nBA) and p(AcLa) T g values in the triblock copolymers to those of their homopolymers suggests that the two blocks are immiscible. <ref type="bibr">64</ref> To evaluate the materials as PSAs and understand how the ratio of glassy block affects their properties, samples for adhesion testing were prepared by casting solutions of the polymers onto a sheet of PET film (see the Supporting Information for details). The adhesive capabilities of thin films of the triblock copolymers with and without added ester-based tackifier were evaluated by pressure-sensitive tape council (PSTC) standard methods. The samples of triblock copolymers were mixed with an appropriate amount of tackifier, and the adhesive properties of the polymer and polymer/tackifier blends were evaluated and compared by a 180&#176;peel test (PSTC-101) to assess adherence, a loop tack bonding test (PSTC-16) to measure tackiness (instantaneous bonding capability), and a static shear strength test (PSTC-107) to measure resistance to shear failure under an applied force. Another important factor in evaluating these PSAs is the mode of failure, which is qualitatively reported as "cohesive" or "adhesive". Cohesive failure is a result of failure within the adhesive layer, which leaves behind residue on the surface, while adhesive failure occurs at the interfacial boundary. Either mode may be acceptable depending on the desired application of the adhesive, with cohesive failure being more favorable for Scheme 3. Synthesis of p(AcLa)-p(nBA)-p(AcLa) and p(AcLa)-p(LauAc)-p(AcLa)   permanent PSAs and adhesive failure sought for removable PSAs. <ref type="bibr">16,</ref><ref type="bibr">26,</ref><ref type="bibr">33,</ref><ref type="bibr">65,</ref><ref type="bibr">66</ref> Blending of an appropriate tackifier was carried out in order to dilute entanglements of the midblock and effectively lower the elastic modulus of the material, allowing for tunable adhesive values under controlled test conditions. <ref type="bibr">33,</ref><ref type="bibr">67</ref> DSC measurements of P1 and P2 with added SYLVALITE 80HP rosin ester (a renewable resin manufactured by Arizona Chemicals) showed an increase in the T g of the p(nBA) midblock relative to the homopolymer (from -48 to -26 &#176;C, Figures <ref type="figure">S33</ref> and<ref type="figure">S34</ref>), suggesting successful integration of the tackifier within the midblock. <ref type="bibr">68</ref> A similar experiment with the p(LauAc)-based triblock copolymers did not produce a discernable T g feature in the DSC thermograms. Maximum values of peel adhesion were obtained with 30 wt % of tackifier added to the nBA-based polymers and 40 wt % of tackifier added to the LauAc-based polymers. Incorporation of greater amounts of tackifier (e.g., 60 wt %) led to a reduction in tack. This observation has similarly been seen with other block copolymers <ref type="bibr">22,</ref><ref type="bibr">68,</ref><ref type="bibr">69</ref> and is explained by the apparent increase in the T g of the midblock with increasing tackifier content, ultimately diminishing the tackiness. The results of the adhesion tests for the triblock copolymers are summarized in Figure <ref type="figure">4</ref> and Table <ref type="table">2</ref>.</p><p>By varying the tackifier content, the peel adhesion values of the p(nBA)-based polymers can be tuned in the range of 2-6 N cm -1 , which are comparable to commercial commodity products such as Duct tape, Scotch tape, and so forth. <ref type="bibr">28,</ref><ref type="bibr">34</ref> Cohesive failure was observed during the peel adhesion test of P1, while adhesive failure was observed for P2. The difference in the failure modes between P1 and P2 likely stems from the degree of endblock length, whereby longer lengths of the hard blocks translate to stronger intermolecular interactions within the glassy domains. These interactions result in stronger cohesive forces within the adhesive layer, which leads to adhesive failure. Measured loop tack forces were in the range of 3-6 N cm -1 , also comparable to commercial products. Notably, the adhesives demonstrated excellent shear resistance under an applied static load. All formulations examined for adhesion, regardless of the hard block weight percentage or tackifier content, did not fail for the duration of the testing period (100 h at room temperature). A comparison of these results to previous studies which have also used p(nBA) as the rubbery component for triblock-based PSAs <ref type="bibr">26,</ref><ref type="bibr">27,</ref><ref type="bibr">34</ref> shows that peel adhesion forces are within the same 2-4 N cm -1 range (when the tackifier is disregarded), despite the fact that different acrylic derivatives were used as the glassy component in each study. These results suggest that the adhesive forces in triblock PSA systems are predominately influenced by the base elastomer. That is, if p(nBA) is "loosely" entangled and contributes 80-90% of the copolymer by weight, the measured adhesion forces will be similar regardless of the glassy component used. The materials obtained from P3 and P4, which incorporated greater amounts of the glassy component in the polymers, exhibited negligible tack and thus could not be tested for adhesion.</p><p>Samples of P5-P7 were also blended with the rosin ester tackifier, and the polymers and polymer/tackifier blends were evaluated as previously described. The results of the adhesion tests are summarized in Figure <ref type="figure">4</ref>. Peel adhesion values are tunable in the range of 2-8 N cm -1 depending on tackifier content. Adhesive failure mode was observed only for P6, which has the greatest hard block content in this series. The measured peel adhesion forces of the neat p(LauAc)-based polymers were in the same range as the neat p(nBA)-based polymers (2-4 N cm -1 ), proving that longer alkyl acrylates can effectively be used as the base elastomer for PSAs as long as the higher M e can be overcome. The measured loop tack forces were in the range of 5-8 N cm -1 , consistently greater than those measured for the PSAs which use p(nBA) as the rubbery midblock with similar hard block lengths. This observation is likely a consequence of the lower elastic modulus of p(LauAc) than that of p(nBA), resulting in a "tackier" material which adheres to the substrate more quickly. The shear test results indicated that the p(LauAc) series of polymers performed worse than the p(nBA) series. Only P6, which has the greatest hard block weight fraction, demonstrated resistance to shear failure on par with the p(nBA) series. Addition of tackifier to P5 and P7, which theoretically lowers the elastic modulus of the elastomer, resulted in greater peel adhesion and loop tack forces but led to a reduction in shear resistance. The spread of adhesion/tack forces and shear failure shows that the formulations of these sustainably sourced acrylic adhesives can be modified in a systematic manner to target a specific application (i.e., permanent vs removable PSAs) and are competitive in performance to commodity products on the market today. Additionally, in contrast to other biorenewable PSAs which use a polyester-based rubbery midblock, <ref type="bibr">11,</ref><ref type="bibr">12,</ref><ref type="bibr">16,</ref><ref type="bibr">22</ref> this acrylic-based system is shown to exhibit good adhesion both with and without tackifier additives because of the lower elastic modulus; however, polyester-based PSAs still maintain the distinct advantage of better degradability over their acrylic counterparts.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; CONCLUSIONS</head><p>In summary, we have reported the synthesis and study of new sustainable acrylic triblock copolymers for PSAs. Lauryl acrylate was employed as the rubbery midblock in place of commonly used nBA in an effort to improve upon the renewability aspect of the adhesives. Furthermore, TAL, an emerging platform chemical, was modified and subsequently copolymerized via RAFT polymerization to develop an acrylate-based system suitable for PSAs. The synthesized polymers were of high molecular weights and narrow dispersities, specific component ratios were targeted, and the adhesives demonstrated similar performance to commercial products. The intrinsically lower elastic modulus of p(LauAc) promoted excellent adhesion and tack capabilities of the resultant triblock copolymers. Use of high T g p(AcLa) as the glassy component in the triblock copolymers enhanced the physical properties of the adhesives (e.g., high shear forces and adhesive failure mode), albeit with limited thermal stability at temperatures above 125 &#176;C, which could be explored to trigger thermally responsive release properties. We demonstrate through this robust strategy that it is indeed possible to utilize renewable, long-chained alkyl-acrylates with high M e in conjunction with biologically accessible TAL to realize a fully sustainable system for high-performance PSA applications. </p></div><note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_0"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX B</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_1"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX C</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_2"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX D</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_3"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX E</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_4"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX F</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_5"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX H</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_6"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX I</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_7"><p>https://dx.doi.org/10.1021/acsapm.0c00317 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX J</p></note>
		</body>
		</text>