<?xml-model href='http://www.tei-c.org/release/xml/tei/custom/schema/relaxng/tei_all.rng' schematypens='http://relaxng.org/ns/structure/1.0'?><TEI xmlns="http://www.tei-c.org/ns/1.0">
	<teiHeader>
		<fileDesc>
			<titleStmt><title level='a'>Green Synthesis of Thermoplastic Composites from a Terpenoid-Cellulose Ester</title></titleStmt>
			<publicationStmt>
				<publisher></publisher>
				<date>09/11/2020</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10199251</idno>
					<idno type="doi">10.1021/acsapm.0c00803</idno>
					<title level='j'>ACS Applied Polymer Materials</title>
<idno>2637-6105</idno>
<biblScope unit="volume">2</biblScope>
<biblScope unit="issue">9</biblScope>					

					<author>Moira K. Lauer</author><author>Andrew G. Tennyson</author><author>Rhett C. Smith</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[Herein we report a green route to thermoplastics from cellulose, the terpenoid geraniol, and fossil fuel byproduct sulfur with an overall atom economy of 90% over three steps. The only stoichiometric byproducts are NaCl and water. The process involves (1) oxidation of cellulose, (2) amino acid-catalyzed esterification, and (3) cross-linking of olefins with sulfur to give GCS x (x = wt % sulfur, varied from 80-90%). The thermoplastics exhibit flexural strengths and moduli competitive with some commercial materials and are recyclable without loss of strength. The method delineated herein should be applicable to many combinations of saccharide and terpenoid precursors to facilitate similarly green routes to a range of sustainably sourced materials.]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><p>T he search for polymers that can be made by applying the principles of green chemistry 1 is central to modern polymer science. Some of the most attractive strategies in this regard employ plant-derived precursors like cellulose, <ref type="bibr">[2]</ref><ref type="bibr">[3]</ref><ref type="bibr">[4]</ref> lignin, <ref type="bibr">[5]</ref><ref type="bibr">[6]</ref><ref type="bibr">[7]</ref> triglycerides/fatty acids, <ref type="bibr">[8]</ref><ref type="bibr">[9]</ref><ref type="bibr">[10]</ref><ref type="bibr">[11]</ref> or terpenoids. <ref type="bibr">[12]</ref><ref type="bibr">[13]</ref><ref type="bibr">[14]</ref> One drawback facing efforts in this vein is that synthetic manipulation of sustainably sourced precursors to convert them to appropriate monomers can require multistep processes employing nongreen solvents, driving up cost and lowering the atom economy.</p><p>Cellulose, as the most prevalent biopolymer in nature and the primary constituent of agricultural waste biomass, is an attractive target for polymer synthesis. Unfortunately, cellulose itself cannot be thermally processed, and its derivatization is often challenging. <ref type="bibr">15</ref> Herein we report a green route to thermoplastics from cellulose, a terpenoid alcohol, and sulfur (Figure <ref type="figure">1</ref>). The only stoichiometric side products of the process are environmentally innocuous NaCl and H 2 O, and the process has very high atom economy. The first step was partial oxidation of cellulose by a green variation of classic aqueous NaOCl oxidation of primary alcohols <ref type="bibr">16</ref> to give oxidized cellulose OC (Scheme 1). Infrared spectroscopy confirmed successful oxidation, while potentiometric titration of OC revealed a degree of substitution (DS, # per anhydroglucose unit) of 0.28 (Figures <ref type="figure">S1-S3</ref>, Equation S1). <ref type="bibr">17</ref> Oxidation had an atom economy of 91%, and the only stoichiometric byproduct was NaCl.</p><p>The carboxylic acid moieties in OC can be esterified with any number of alcohols. In the current case, geraniol was selected as the alcohol because geraniol is a naturally occurring monoterpenoid: it is the primary constituent of rose oil and can be efficiently extracted from a variety of other grasses and flowers. Esterification of OC to give GC employed the amino acid leucine as a catalyst and geraniol as the solvent (Scheme Letter pubs.acs.org/acsapm 1). <ref type="bibr">18</ref> Water is the only stoichiometric byproduct of esterification by this protocol. Because geraniol was used as the solvent for esterification, it was present in a large excess that was easily, quantitatively recovered by filtration. Recovered geraniol was found to be &#8805;98% pure by gas chromatographic analysis and so could be used in subsequent esterification reactions. Esterification was quantified by iodometric titration of GC, <ref type="bibr">19</ref> which revealed that esterification at approximately half of the carboxylic acid sites had taken place such that ester DS = 0.128 &#177; 0.010 in GC. The atom economy of esterification was thus 99%. As anticipated, modifications of microcrystalline cellulose led to decreased decomposition temperatures (T d = 305, 226, and 213 &#176;C for microcrystalline cellulose, OC, and GC, respectively) as well as slight changes in glass transition temperatures (T g = 87, 79, and 74 &#176;C for microcrystalline cellulose, OC, and GC, respectively) while the crystallinity remained unchanged (Figures <ref type="figure">S4-S6</ref>).</p><p>Olefinic ester GC was then cross-linked by inverse vulcanization with sulfur at 180 &#176;C to yield GC-sulfur composites (GCS x , where x = wt % sulfur, varied from 80-90%). Although not observed in the current case (as deduced by elemental analysis), heating elemental sulfur with organics can result in the formation of toxic H 2 S gas, so caution should be exercised in such manipulations. Inverse vulcanization <ref type="bibr">20,</ref><ref type="bibr">21</ref> is a 100% atom-economical process in which olefins react with thermally generated sulfur radicals analogous to the reaction of sulfur radicals and olefins in the thiol-ene click reaction. Like thiol-ene click reactions, inverse vulcanization is quite functional group tolerant, so a wide range of sustainable olefins can be polymerized by inverse vulcanization with many promising applications. <ref type="bibr">14,</ref><ref type="bibr">[22]</ref><ref type="bibr">[23]</ref><ref type="bibr">[24]</ref><ref type="bibr">[25]</ref> Elemental sulfur is also an underutilized byproduct of fossil fuel refining prior to combustion (Figure <ref type="figure">1</ref>). The three-step process to GCS x employing geraniol, cellulose, and sulfur showed an impressive 90% atom economy.</p><p>GCS x composites were remeltable and range in color from gray to black solids (Figure <ref type="figure">2</ref>) that can be remelted and reshaped over many cycles by simply melting them and pouring the liquid into molds at temperatures above 130 &#176;C. Composites prepared by inverse vulcanization are generally composed of a highly cross-linked network in which some free sulfur is trapped. Free sulfur, meaning sulfur that is not covalently attached to the organic network as cross-links, is quite soluble in CS 2 , whereas the cross-linked cellulose-sulfur network is completely insoluble in CS 2 (confirmed by elemental microanalysis). Extractable sulfur was thus readily quantified by recursive washing of GCS x with CS 2 , and elemental analysis of the CS 2 -soluble fraction revealed that sulfur was indeed the only element present. Elemental analysis GCS x paired with quantitation of the relative amount of soluble and insoluble fractions confirmed retention of covalently bound sulfur in the network solid (for raw data and calculation information, see Figure <ref type="figure">S14</ref>, Table <ref type="table">S2</ref>, and Equation S2). Considering that the alkene functionalities had been completely consumed based on IR spectroscopic data and the quantity of covalently bound sulfur, the sulfur rank (average number of S atoms in each cross-link between cellulose chains) was calculated to be 8-22 sulfur atoms (Table <ref type="table">1</ref>). These values are larger than the average cross-link length of 4-5 sulfur atoms reported for highly cross-linked composites of sulfur with polystyrene <ref type="bibr">26</ref> or xylenol <ref type="bibr">27</ref> derivatives but on par with those reported for cellulose derivative PCS 80 (22, structure provided in Figure <ref type="figure">3</ref>), <ref type="bibr">4</ref> allyl lignin (48-103 sulfur atoms), <ref type="bibr">7</ref> and chlorolignin (12-31 sulfur atoms). <ref type="bibr">6</ref> Regardless of the olefin-bearing comonomer used in inverse vulcanization, the average cross-link length correlates expectedly with the ratio of sulfur to cross-linkable olefin sites in the monomer feed.</p><p>Although not observable by IR spectroscopy (Figure <ref type="figure">S5</ref>), Raman spectroscopy provided additional evidence that sulfur in GCS x exists primarily as small rings or chains, as the peak characteristic of polymeric sulfur domains was not observed (Figure <ref type="figure">S6</ref>). Integration of the orthorhombic sulfur melt peak from differential scanning calorimetry (DSC) measurements of GCS x likewise confirmed that both free and covalently bound sulfur are present in GCS x (Figure <ref type="figure">S9</ref>). Because of the confinement of orthorhombic sulfur in the sulfur-cross-linked cellulose network, GCS 85 and GCS 80 exhibited a depressed melting endotherm in the second and later heating cycles by DSC (Figures <ref type="figure">S10-S13</ref>; DSC for precursors OC and GC are in Figure <ref type="figure">S5</ref> for comparison).</p><p>Thermogravimetric analysis (TGA) of GCS x reveals that thermal decomposition of the sulfur component occurs at a lower temperature than does decomposition of the cross-linked network. The decomposition temperatures (T d ) for GCS 80-90 thus range from 234-243 &#176;C, quite similar to that of elemental sulfur (&#8764;240 &#176;C). The char yield (at 800 &#176;C) scales expectedly with the amount of organic comonomer present (Figure <ref type="figure">S8</ref>; TGA data for precursors OC and GC are in Figure <ref type="figure">S4</ref> for comparison).</p><p>The data from CS 2 fractionation studies, elemental analysis, IR spectroscopy, Raman spectroscopy, TGA, and DSC are consistent with the formulation of GCS x as a network of covalently cross-linked cellulose chains wherein each cross-link is composed of short chains of 8-22 sulfur atoms on average. The remaining sulfur is present in the composite but is not covalently attached to the organic component of the network.</p><p>Dynamic mechanical analysis (DMA) of GCS x was undertaken to assess mechanical properties. Because of the high viscosity of molten GCS 80 and the difficulty of preparing reproducible samples, DMA was only performed on GCS 90 and GCS 85 , which exhibited very similar mechanical properties to one another (Figure <ref type="figure">4</ref> and Table <ref type="table">1</ref>). Temperature scans (Figure <ref type="figure">4A</ref>) revealed that the materials were considerably stronger as they exhibited storage moduli approximately 80% larger in magnitude than in cellulose derivative PCS 80 (Figure <ref type="figure">3</ref>) over the measured temperature range of -60 to +80 &#176;C. <ref type="bibr">4</ref> Although GCS 90 and PCS 80 have a nearly identical cross-link density and sulfur rank, the drastic difference in storage moduli can be attributed to the retention of crystallinity upon modification observed in GC whereas PC became amorphous upon modification, as assessed by powder X-ray diffraction (Figure <ref type="figure">S16</ref>). Stress-strain experiments revealed that the GCS x materials have flexural moduli of &#8764;1000 MPa, similar to the low end of the range for high impact ABS (acrylonitrile butadiene styrene, 1000-2500 MPa) with low loss moduli and tan delta values indicating their inability to dissipate stress </p><p>Storage modulus value at -40 &#176;C when each material is below T g . b Value at T g , except for Portland cement, which did not exhibit a T g in the range -100 to 100 &#176;C. c As measured by the maximum of the tan &#948; curve. d Sample could not be measured beyond this level due to instrumental limitations. e Data refer to Portland cement that was sifted, mixed with water (1:2, water/cement), and cured very gradually before being dried in an oven. f Data not available/applicable. g Material exhibited no apparent maximum value in the range -100 to 100 &#176;C. h Value was outside of measured range. i Ref 28. j Cellulose acetate butyrate was plasticized with tributyl citrate, and values were estimated from the provided curves for a 2 mm thick sample. k Estimated from loss modulus plot. l Average reported value. n Azdel SuperLite SL550600-100. (Figure <ref type="figure">S15</ref>). As a result of their high flexural moduli and relatively low elastic limits (0.4 and 0.7 MPa for GCS 90 and GCS 85 , respectively), GCS x materials exhibited considerably smaller moduli of resilience relative to PCS 80 but were on par with the moduli of resilience of Portland cement. The flexural strengths of GCS 90 and GCS 85 (&gt;4.9 and &gt;5.2 MPa, respectively) are higher than the flexural strength exhibited by Portland cement but lower than that exhibited by some other commercial cellulose-based polymers like cellulose acetate butyrate, a material used commercially for applications such as tool handles. <ref type="bibr">28</ref> Both the flexural strength and modulus of GCS x are comparable to glass fiber-polypropylene composites like Azdel SuperLite that are used commercially in nonstructural automotive door panels. <ref type="bibr">29</ref> It is also notable that GCS x materials can be thermally processed over many cycles. This property is a result of the thermal reversibility of S-S bond formation and is a notable advantage over some traditional polymers that cannot be repeatedly processed by remelting and recasting. <ref type="bibr">30</ref> A potential industrial application that has been demonstrated for other high sulfur-content materials is as a coating to protect typical mineral cement products from acid corrosion. <ref type="bibr">4,</ref><ref type="bibr">11</ref> To evaluate the utility of GCS 90 for this application, a block of Portland cement was impregnated by pressure treatment with molten GCS 90 following a reported protocol. <ref type="bibr">4</ref> The block took up 7 wt % GCS 90 to give a material with a density of 1.6 g/cm <ref type="bibr">3</ref> . Despite the small weight percentage of GCS 90 in the GCS 90 -impregnated Portland cement block, the mechanical properties were altered drastically. The flexural modulus of GCS 90 -impregnated Portland cement was found to be 67% greater than that of untreated Portland cement. Additionally, the GCS 90 -impregnated Portland cement block exhibited significantly improved acid-resistance. Whereas a Portland cement block submerged in 0.5 M H 2 SO 4 loses its structural integrity and shape within 30 min, the GCS 90impregnated Portland cement block retained its shape and modulus after acid challenge (Figure <ref type="figure">5</ref>). The acid-challenged GCS 90 -impregnated sample exhibited a negligible change in flexural modulus relative to the material before soaking. The significant benefits to acid resistance and modulus resulting from a relatively small infusion of GCS 90 into Portland cement make GCS 90 an especially intriguing material as a cement additive while additionally ensuring that the density of the material is not too high for commercial applications.</p><p>In conclusion, we report a three-step green route to thermoplastics from cellulose, terpenoid, and waste sulfur with overall 90% atom economy. The mechanical properties of the resultant polymers display mechanical properties that are competitive with commercially viable materials, and a potential industrial application to improve acid corrosion resistance of cement products was also demonstrated. Perhaps most importantly, the synthetic method delineated herein should be applicable to many combinations of saccharide and terpenoid precursors to facilitate similarly green routes to a range of sustainably sourced materials. Several additional polysaccharide-terpenoid composite formulations are currently being pursued.   </p></div><note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_0"><p>https://dx.doi.org/10.1021/acsapm.0c00803 ACS Appl. Polym. Mater. XXXX, XXX, XXX-XXX D</p></note>
		</body>
		</text>
</TEI>