			<titleStmt><title level='a'>Shape-transformation of polymersomes from glassy and crosslinkable ABA triblock copolymers</title></titleStmt>
			<publicationStmt>
				<publisher></publisher>
				<date>10/07/2020</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10220780</idno>
					<idno type="doi">10.1039/D0TB01643H</idno>
					<title level='j'>Journal of Materials Chemistry B</title>
<idno>2050-750X</idno>
<biblScope unit="volume">8</biblScope>
<biblScope unit="issue">38</biblScope>					

					<author>Tamuka Chidanguro</author><author>Elina Ghimire</author><author>Yoan C. Simon</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[Recent developments in the field of polymer vesicles,              i.e.              polymersomes, have demonstrated that disrupting the equilibrium conditions of the milieu could lead to shape transformation into stable non-spherical morphologies, bringing on-demand shape control to reality and bearing great promise for cell mimicry and a variety of biomedical applications. Here, we studied the self-assembly behavior of glassy amphiphilic triblock copolymers, poly(ethylene glycol)-              block              -polystyrene-              stat              -poly(coumarin methacrylate)-              block              -poly(ethylene glycol) (PEG-              b              -P(S-              stat              -CMA)-              b              -PEG), and their response to various stimuli. By changing the respective molecular weights of both the hydrophobic P(S-              stat              -CMA) and the hydrophilic PEG blocks, we varied the hydrophobic volume fraction thereby accessing a range of morphologies from spherical and worm-like micelles, as well as polymersomes. For the latter, we observed that slow osmotic pressure changes induced by dialysis led to a decrease in size while rapid osmotic pressure changes by addition of a PEG fusogen led to morphological transformations into rod-like and tubular polymersomes. We also found out that chemically crosslinking the vesicles before inducing osmotic pressure changes led to the vesicles exhibiting hypotonic shock, atypical for glassy polymersomes. We believe that this approach combining the robustness of triblock copolymers and light-based transformations will help expand the toolbox to design ever more complex biomimetic constructs.]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><p>and light-based transformations will help expand the toolbox to design ever more complex biomimetic constructs.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="1.">Introduction</head><p>Since the late 1990s, the self-assembly of amphiphilic block copolymers has expanded the toolkit to design complex biomimetic architectures at the nanoscale from the bottom up. <ref type="bibr">1,</ref><ref type="bibr">2</ref> Polymersomes (also known as polymer vesicles) have especially garnered much interest because of their unique cell-like structure, whereby amphiphilic macromolecules form a membrane separating the inside (or lumen) of the polymersome from its outside. As a result, they can encapsulate both hydrophilic cargo in their lumen and/or carry hydrophobic molecules within their membrane. <ref type="bibr">3</ref> Their tunable permeability can even allow them to function as nanoreactors, <ref type="bibr">4</ref> akin to organelles in the body. For instance, trypsin displayed increased activity towards a BZiPAR (Rhodamine 110, bis-(N-CBZ-L-isoleucyl-L-prolyl-L-arginine amide), dihydrochloride) substrate when encapsulated in poly(2-methyloxazoline)-block-poly(dimethylsiloxane)-block-poly(2methyloxazoline) vesicles. <ref type="bibr">5,</ref><ref type="bibr">6</ref> As a result, polymer vesicles are highly desirable in diverse areas of research ranging from catalysis, <ref type="bibr">7</ref> cellular modelling, <ref type="bibr">8,</ref><ref type="bibr">9</ref> drug delivery, <ref type="bibr">10</ref> to bioimaging and diagnostics. <ref type="bibr">11,</ref><ref type="bibr">12</ref> Since polymersomes are becoming increasingly useful, their shape control is now proving to be the next frontier. Cellular organelles, bacteria, and viral capsids exist in a plethora of morphologies that allow them to efficiently carry out their functions. As we aspire to replicate these complex, compartmentalized, biological architectures, it becomes essential to diverge from simple spherical morphologies to access a broad array of shapes and structures that will enable new functionalities. <ref type="bibr">13,</ref><ref type="bibr">14</ref> In drug delivery, tubular and rod-like structures offer higher loading efficiencies compared to their spherical analogs. Additionally, their large surface area enhances cellular uptake, <ref type="bibr">[15]</ref><ref type="bibr">[16]</ref><ref type="bibr">[17]</ref> and, in the bloodstream, particle geometry affects the hemodynamic (drag) and buoyancy forces which govern the particle trajectory. <ref type="bibr">[18]</ref><ref type="bibr">[19]</ref><ref type="bibr">[20]</ref> Various groups have recently explored the ability of polymersomes to achieve nonspherical morphologies, such as stomatocytes, tubular and nested polymersomes. <ref type="bibr">17,</ref><ref type="bibr">21,</ref><ref type="bibr">22</ref> For instance, the groups of van Hest and Wilson demonstrated that the addition of water-miscible organic solvents plasticized the membrane of polymersomes made from block copolymers containing glassy hydrophobic segments, such as polystyrene-block-poly(ethylene glycol) (PS-b-PEG) and poly(D,L-lactide)-block-poly(ethylene glycol) (PDLLA-b-PEG), and enabled their shape manipulation. <ref type="bibr">21</ref> They could kinetically freeze or quench these non-spherical morphologies by adding them into water thereby vitrifying the PS and PDLLA blocks and exploited these structures in applications, such as drug delivery or nanomotors. <ref type="bibr">23</ref> Due to their very nature, ABA triblock copolymers possess the ability to span the vesicular membrane bridging the inside and outside of the polymersome. <ref type="bibr">24,</ref><ref type="bibr">25</ref> This unique characteristic significantly enhances their stability and ability to withstand changes in osmotic pressure. For copolymers consisting of a hydrophilic PEG block and a soft hydrophobic poly(dimethylsiloxane) block, Salva et al compared the responses of polymersomes made from diblock and triblock copolymers to hypertonic salt solutions by cryogenically freezing the otherwise unstable intermediates. <ref type="bibr">26</ref> They found that the diblock-based polymersomes transformed beyond stomatocytes into nested polymersomes upon fusion of the membrane. Comparatively, while they could manipulate triblock-based vesicles to form stomatocytes, the ABA architecture precluded membrane fusion and the formation of nested structures.</p><p>To the best of our knowledge, and despite the advantageous mechanical properties of triblock copolymers, all of the reports to date on the shape-transformation of glassy polymersomes have focused on diblock copolymers. We have therefore designed an amphiphilic triblock copolymer poly(ethylene glycol)-block-poly(styrene-stat-(coumarin methacrylate))-blockpoly(ethylene glycol) (PEG-b-P(S-stat-CMA)-b-PEG). We hypothesized that slow and rapid osmotic pressure changes, respectively via dialysis and the use of a PEG fusogen, would lead to an area-mismatch between the vesicle membrane interior and exterior, and to shape transformation. We originally posited that UV-induced [2+2] cycloaddition dimerization of the coumarin moiety would enable easy crosslinking of the polymersomes, lower their permeability to water and thereby facilitate their shape transformation. As demonstrated in the following paragraphs, this assumption turned out to be erroneous and crosslinking resulted in a presumed increase in permeability. Most importantly, we expected that the glassy nature of the vesicle hydrophobic membrane would allow us to isolate stable non-spherical polymersomes.</p><p>Interestingly, osmotic pressure changes via dialysis and rapid changes using a PEG fusogen led to markedly different responses for the vesicles, demonstrating the delicate nature of these out-ofequilibrium shape-changes.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.">Results and Discussion</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.1">Synthesis of amphiphilic block copolymers</head><p>Scheme 1. (Top) Synthesis of the difunctional chain-transfer agent (diCEP) via Steglich esterification. (Bottom) Synthesis of amphiphilic triblock copolymers via RAFT copolymerization of styrene (S) and coumarin methacrylate (CMA) followed by one-pot aminolysis and thia-Michael addition of methoxy poly(ethylene glycol) acrylate (mPEGA). Note that, for the simplicity of the representation of the copolymers, the central diCEP subunit is omitted. As a result, the bonds connecting the trithiocarbonate and thioether moieties to the P(S-stat-CMA) block on the left-hand side are not representative of the actual regiochemistry and therefore simply depicted as a purple line.</p><p>To synthesize the amphiphilic triblock copolymers, we designed a difunctional chaintransfer agent (CTA), whose structure allows divergent reversible addition-fragmentation chaintransfer (RAFT). This approach enables the easy post-polymerization functionalization of the thiocarbonylthio end groups flanking the telechelic hydrophobic core. <ref type="bibr">27,</ref><ref type="bibr">28</ref> To this end, we first synthesized cyano-4-(ethylsulfanylthiocarbonylsulfanyl)pentanoic acid (CEP) using a known procedure, <ref type="bibr">29</ref> followed by a Steglich esterification with ethylene glycol (Scheme 1) to yield the subsequent difunctional CTA (diCEP). The shift of the ethylene glycol methylene proton peaks at 3.76 ppm to 4.33 ppm and the disappearance of the OH peak at 3.17 ppm confirmed the success of the esterification reaction (Figure <ref type="figure">S2-3</ref>).</p><p>While S and CMA have been copolymerized before, <ref type="bibr">30</ref> we wanted to establish whether the coumarin moiety would be randomly distributed throughout the membrane. We carried out the diCEP-mediated RAFT copolymerization in DMF at 75 &#176;C with a 1:4 molar ratio of CMA:S and took out aliquots at five time points between 4 and 20 hours (Scheme S1). After precipitating the aliquots in methanol and drying them overnight under vacuum, we then used 1 H NMR spectroscopy to compare the ratio of the alkene proton at 6.13 ppm characteristic of the coumarin to the aromatic region between 6.33 ppm and 7.55 ppm comprising the aromatic signals of both styrene and coumarin (Figure <ref type="figure">S4</ref>). For all time-points, we observed a ratio of 14.1-17.8 between the alkene and aromatic regions, indicating that the final polymers had a final CMA:S ratio between 1:2.23 and 1:2.95 (Table <ref type="table">S1</ref>). These results suggest that the polymers contained a slightly higher CMA content compared to the initial monomer mixture. However, the fluctuation in this ratio throughout the polymerization suggested that the monomer addition largely followed a random incorporation.</p><p>We then synthesized seven hydrophobic blocks with molecular weights ranging from 8 500 g/mol to 32 000 g/mol targeting 50% monomer conversion (Table <ref type="table">1</ref>) and using a 1:4 molar ratio of CMA:S. We used a low diCEP:initiator ratio of 1:0.2 (1:0.1 ratio for each CTA functionality) to ensure that the polymers would have more than 90% living chains. <ref type="bibr">31</ref> We found that the CMA:S ratio was comprised between 1:2.03 and 1:3.0 (Figure <ref type="figure">S5</ref> and Table <ref type="table">S2</ref>). The use of acetone-d6 ensured that the solvent peaks would not coincide with polymer signals. Overall, the target and experimentally measured molecular weights by size-exclusion chromatography (SEC) agreed (Table <ref type="table">1</ref> and Figure <ref type="figure">S6</ref>, black SEC traces). Satisfyingly, all chromatograms showed a narrow monomodal molecular weight distribution with &#208; = 1.11 -1.23. We then performed a one-pot aminolysis of the trithiocarbonate end groups and thia-Michael coupling reaction with methoxy poly(ethylene glycol) acrylate (mPEGA) to yield the ABA triblock copolymers. While soft amphiphilic block copolymers typically self-assemble into vesicular morphologies at 0.25 &#8804; f &#8804; 0.45, where f is defined as the hydrophilic fraction, glassy diblock copolymers often require a much lower f. <ref type="bibr">32</ref> We therefore utilized two PEG acrylate blocks with molecular weights of 1 000 g/mol (PEG22) and 2 000 g/mol (PEG45) to synthesize seven triblock copolymers in order to access vesicle morphologies. Conveniently, the disappearance of the characteristic yellow color of the CTA during the reaction was a good visual indicator of the successful aminolysis. The shift towards lower retention times (Figure <ref type="figure">S6</ref>, red SEC traces) further confirmed the efficiency of the thia-Michael addition. Fortunately, the shape of the SEC traces also remained unchanged (except for PEG22-b-P(S-stat-CMA)136-b-PEG22 where a small low-molecular weight shoulder appeared), confirming the completion of the reaction. This clean shift is particularly apparent for PEG45-b-(S-stat-CMA)70-b-PEG45 (Figure <ref type="figure">S6d</ref>) and overall, the dispersity remained low (&#208; = 1.09 -1.20).</p><p>Nevertheless, due to inconsistencies in the refractive index increment values obtained by SEC assuming 100% mass recovery (Table <ref type="table">S4</ref>), we relied on 1 H NMR spectroscopic data to accurately evaluate the molecular weight of the triblocks.</p><p>The appearance of the characteristic PEG peak at 3.64 ppm and the absence of any signal between 5.65 and 5.95 ppm further corroborated the achievement of the thia-Michael addition (Figure <ref type="figure">S7</ref>). Based on the P(S-stat-CMA) molecular weight obtained by SEC and the CMA content previously determined by <ref type="bibr">1</ref> H NMR spectroscopy, we used the integration ratio of the PEG protons to the characteristic coumarin alkene protons to determine the Mn of the corresponding PEG-b-P(S-stat-CMA)-b-PEG triblocks (Tables <ref type="table">1</ref> and<ref type="table">S3</ref>, Figure <ref type="figure">S8</ref> and subsequent explanation in ESI).</p><p>For the PEG22 series, the experimental Mn line up remarkably well with the values expected at full completion of the thia-Michael coupling reaction. We note however that the experimental Mn values appear to be ever so slightly below for the larger PEG45 which could potentially stem from a less quantitative though efficient coupling for the larger PEG blocks. The integration ratios of the PEG protons to the alkene protons also enabled the determination of f for each triblock, with 0.08 &#8804; f &#8804; 0.24. and Table <ref type="table">S2</ref>). e Determined via <ref type="bibr">1</ref> H NMR (see Figure <ref type="figure">S8</ref> and Table <ref type="table">S3</ref>).</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.2">Self-assembly of the amphiphilic triblocks</head><p>We first focused our attention on determining the conditions and volume fraction that would enable the fabrication of polymersomes using PEG-b-P(S-stat-CMA)-b-PEG. For soft block copolymers, the self-assembly can be conducted by directly hydrating the polymers with an aqueous solution. <ref type="bibr">26,</ref><ref type="bibr">33</ref> However, we resorted to a solvent injection method for the self-assembly of PEG-b-P(S-stat-CMA)-b-PEG, since the glassiness of the P(S-stat-CMA) center block makes it extremely hydrophobic and therefore requires plasticization with an organic solvent. <ref type="bibr">34</ref> Dioxane:THF 1:1 (v/v) <ref type="bibr">35</ref> was used as the organic solvent mixture for it dissolved the PEG-b-P(Sstat-CMA)-b-PEG at all compositions. Upon dissolution, we slowly added deionized (DI) water via a syringe pump until we reached 50% by volume. Notably, the mixture turned cloudy around 20% by volume, suggesting that the self-assembly process had already begun at or before this composition. After the water addition was complete, an aliquot was then extracted and subsequently quenched in vigorously stirring water, thus vitrifying the hydrophobic block and freezing the morphologies that formed.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.2.1">Self-assembly behavior of PEG22 triblock copolymers</head><p>Using the aforementioned self-assembly procedure, yielded a mixture of large compound micelles and vesicles (Figure <ref type="figure">1d</ref>), suggesting that under these conditions, the value of f was approaching a threshold where vesicles were no longer the most stable morphology. These results showed that vesicles started forming at f close to 20% in the PEG45 systems just like observations made using the shorter PEG22 block. Membrane thickness is dependent on the polymer molecular weight. <ref type="bibr">25,</ref><ref type="bibr">36</ref> As expected, dry and cryo-TEM results (Figure <ref type="figure">1e-g</ref> </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.3.">Effect of osmotic pressure changes induced by dialysis</head><p>The default shape for most vesicles is spherical for it constitutes the thermodynamically most stable morphology, which minimizes the surface-to-volume ratio. However, like their lipidbased counterparts, polymersomes can transform into different shapes in response to changes in their milieu. Giant unilamellar vesicles and even smaller unilamellar vesicles adopt oblate, prolate, spherocylindrical and other shapes as a response to factors such as mechanical force and osmotic pressure changes. <ref type="bibr">37</ref> The area-difference elasticity (ADE) theory asserts that volume changes of the inner compartment of the vesicles drive their shape transformations. Osmotic pressure differences and concentration gradients between the vesicle interior and their surroundings will therefore cause an area mismatch which leads to shape transformation. <ref type="bibr">38</ref> After successfully identifying their fabrication conditions, we turned our attention to vesicles made from PEG45-b-P(S-stat-CMA)206-b-PEG45 and probed their ability to shapetransform. In comparison to other reported systems, <ref type="bibr">35,</ref><ref type="bibr">39</ref> we hypothesized that the vesicle membrane thickness (~21 nm) would be enough to sustain the planned shape-transformation. To characterize the size changes, we used dynamic light scattering (DLS) at multiple angles to evaluate the angular dependence of the diffusion coefficient with the square of the scattering vector, q 2 . We then compared this effective hydrodynamic diameter (Dh) to the Dh values obtained at each angle via CONTIN (Figure <ref type="figure">S9</ref> and Table <ref type="table">S5</ref>). <ref type="bibr">40,</ref><ref type="bibr">41</ref> In view of this observation, the size data discussed here will be based on the effective Dh calculations from the angle-dependent DLS, while for visual purposes, the size distributions are displayed for a given indicated angle.</p><p>First, we investigated the response of the polymer vesicles to osmotic pressure differences induced by dialysis. When the polymersome suspension was dialyzed against DI water for two days, we observed a decrease in Dh from 450 nm to 410 nm, without a significant change in the polydispersity of the assemblies, suggesting that the initial polymersomes were still intact (Figure <ref type="figure">2a-b</ref>). Note that for the sake of simplicity, we are using the average value of Dh for the rest of the discussion. Kim et al reported a similar decrease in size for the transformation of glassy polymersomes into stomatocytes for PS-b-PEG. <ref type="bibr">35</ref> Upon removal of the organic solvent by dialysis, the glassy nature of the hydrophobic block at room temperature limits permeability of the water molecules, resulting in a decrease in hydrodynamic radius since the water could not replace the organic solvent. Surprisingly, we did not observe any transformation of polymersomes into stomatocytes or any other non-spherical morphologies (Figure <ref type="figure">2a</ref>, inset AD). For successful longlived transformation, the polymersome membrane needs to be flexible enough to allow for a shape change but rigid enough maintain the newly formed morphology and prevent water inflow. <ref type="bibr">39</ref> These results suggested that the vesicles satisfied the former but not the latter, hence the retention of the spherical morphologies.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.4.">Effect of UV crosslinking in the polymersome shape transformation.</head><p>Chemical modification of the polymersome membrane can also induce non-equilibrium conditions that foster the shape transformation of vesicles. For example, van Oers et al fabricated polymersomes with an azide-functionalized styrenic hydrophobic block, poly(ethylene glycol)-bpoly(styrene-co-4-vinylbenzyl azide). <ref type="bibr">42</ref> When they added an external alkyne crosslinker to the vesicle suspension, the resulting alkyne-azide cycloaddition led to their transformation into tubular polymersomes. The crosslinker could not uniformly permeate the vesicle membrane, thereby creating a crosslinker gradient which led to an asymmetry of the bilayer membrane. We chose the coumarin-based derivative because of its biocompatibility and the rapid nature of the [2+2] cycloaddition dimerization reaction. <ref type="bibr">43</ref> Furthermore, the facile crosslinking uses long wavelength UV light, does not require any external chemicals and the reaction can be performed at room temperature, thereby minimizing other changes in the vesicle environment which might inadvertently affect the vesicle properties under investigation. <ref type="bibr">44</ref> When we irradiated PEG45-b-P(Sstat-CMA)206-b-PEG45-based vesicles, the Dh of the vesicles slightly decreased from 450 nm to 443 nm presumably due to crosslinking-induced shrinking (Figures <ref type="figure">2c-d</ref>). Note that despite the proximity of the two average values, each sequence saw a decrease in Dh, which further confirms that shrinking behavior upon crosslinking. The decrease of the characteristic absorbance peak at 319 nm further confirmed coumarin dimerization (Figure <ref type="figure">S10</ref>). Interestingly, the cryo-TEM images indicated membrane wrinkling (Figure <ref type="figure">2c</ref>, inset AI). We also observed this wrinkling in the form of jagged edges on the membrane upon analysis by dry TEM (Figure <ref type="figure">S11b</ref>). We however did not observe any tubular morphologies like van Oers et al. <ref type="bibr">42</ref> We suspect that the UV irradiation ensured uniform crosslinking of the membrane, maintaining its equilibrium conditions. </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.4.">Effect of combining UV crosslinking and dialysis</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.4.1.">Effect of crosslinking dialyzed vesicles</head><p>When we irradiated the vesicles after dialysis, we did not observe any significant changes in the polymersome size (Figure <ref type="figure">2a-b</ref>). The TEM images of the vesicles from this combination did not show any significant changes in the vesicle shape as the spherical morphology was retained (Figure <ref type="figure">2a</ref>, inset ADI). This absence of morphological changes upon irradiation of the dialyzed vesicles is also observed in the dry TEM (Figure <ref type="figure">S12c</ref>).</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.4.2.">Dialysis of crosslinked polymersomes</head><p>We then reversed the order of these processes by dialyzing the crosslinked polymersomes against DI water over two days. We expected that crosslinking would lower the permeability of the polymer vesicles and therefore even lead to a larger decrease in the vesicle size upon dialysis.</p><p>However, after the initial slight decrease in size upon crosslinking, the hydrodynamic size of the vesicles increased upon dialysis to sizes larger than the initial assemblies (Figure <ref type="figure">2c-d</ref>).</p><p>Interestingly, the majority of these larger vesicles exhibited ellipsoidal morphologies via cryo-TEM (Figure <ref type="figure">2c</ref>, inset AID). We also observed the same behavior when we carried out the same procedure on polymersomes from the self-assembly of PEG45-b-P(S-stat-CMA)170-b-PEG45</p><p>(Figure <ref type="figure">S13</ref>). Since swelling could only be observed in the AID samples and not in ADI samples (Figures <ref type="figure">2c-d</ref>), we posit that local shrinking upon crosslinking facilitated the formation of pores within the membrane of the polymersomes thereby eliciting their rapid swelling upon dialysis. We are currently investigating avenues to probe this phenomenon in greater depth.</p><p>To confirm that crosslinking played a role in this hypotonic response to dialysis, we synthesized a control triblock copolymer consisting a CMA-free center block flanked by two PEG blocks (PEG45-b-PS403-b-PEG45) (Figure <ref type="figure">S14</ref>, SEC and 1 H NMR spectroscopy). After assembling into vesicles following the aforementioned procedure, we irradiated the polymersomes with UVlight and did not observe any significant size changes presumably on account of the absence of crosslinking (Figure <ref type="figure">3</ref>). As anticipated and contrary to the coumarin-containing triblocks, the dialysis against DI water for two days led to a decrease in size. This result confirms that the crosslinking is directly responsible for the hypotonic behavior observed for PEG45-b-P(S-stat-CMA)206-b-PEG45. Interestingly, upon dialysis, the polymersomes AID appear to undergo membrane fusion and to have a double-walled morphology (Figure <ref type="figure">3e</ref>). This observation warrants further investigation that goes beyond the scope of the present study but was worth pointing out nonetheless. Interestingly, we also investigated the effect of crosslinking on the polymersomes in hypertonic conditions by dialyzing vesicles assembled from PEG45-b-P(S-stat-CMA)170-b-PEG45 against two different concentrations of a NaCl solution (25 mM and 50 mM). We again observed a decrease in the size of the uncrosslinked polymersomes after dialysis at both salt concentrations (Figures <ref type="figure">S16a</ref> and<ref type="figure">S17a</ref>), while the crosslinked vesicles showed a slight increase in size and aggregated in solution. The dry TEM images also suggested that the polymersomes still retained their shape under these hypertonic conditions (Figures <ref type="figure">S16b-d</ref> and<ref type="figure">S17b-d</ref>). </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.5.">Shape-transformation via PEG-induced rapid osmotic pressure changes</head><p>We then adapted a method recently demonstrated by Men et al to induce faster shape transformation using a low concentration of PEG as an additive. <ref type="bibr">39,</ref><ref type="bibr">45</ref> PEG is a known fusogen with a dehydration effect on the membrane and a single ethylene oxide unit can bind up to three water molecules, creating an osmotic gradient. <ref type="bibr">38</ref> In contrast to the osmotic pressure changes that rely on dialysis, this method results in immediate shape change of polymersomes, with these transformations observed in less than a minute. Men et al observed that the PEG-induced osmotic gradient could be increased by either increasing the concentration or the molecular weight of the PEG additive. We carried out the rapid osmotic change investigations using three different concentrations of a solution of 2 000 g/mol PEG, namely 0.5 mg/mL, 1 mg/mL and 5 mg/mL. In a typical procedure, we dissolved PEG45-b-P(S-stat-CMA)206-b-PEG45 in THF:dioxane 1:1 (v/v) and slowly added water at a rate of 1 mL/h until the aqueous composition reached 20% by volume (unlike the 50% by volume in the previously described procedure). We chose a high organic solvent composition to elicit shape change in view of the seemingly high flexibility of the polymersome membranes (cf. absence of transformation upon dialysis demonstrated in section 2.3). We subsequently transferred an aliquot of the suspension to a vial, added the PEG solution, centrifuged the mixture and quenched it in water. As a control, we performed similar experiment in the absence of PEG additive and without centrifugation.</p><p>With increasing fusogen concentration, the vesicle morphology transformed from spheres, to ellipsoids, to tubes and eventually to a mixture of tubes and folded stomatocyte-like structures (Figure <ref type="figure">4</ref>). Men et al. described a similar trajectory for PSn-b-PEG45 diblock copolymers. <ref type="bibr">45</ref> However, they could not observe any sustainable shape change for PS160-b-PEG45 (&#119891; = 10.7) with a hydrophobic block of 16 700 g/mol. Compellingly, PEG45-b-P(S-stat-CMA)206-b-PEG45 triblocks could sustain the deformation and deviation from spherical morphology at &#119891; = 10%, i.e.</p><p>for a center block of 32 000 g/mol (&lt; 33 400 g/mol = 2 x 16 700 g/mol). Although the hydrophobic blocks are different, this result points towards the anticipated enhanced sturdiness of the triblock copolymers compared to their diblock analogs and their consequent ability to promote shape transformation. It is interesting to observe that no permanent shape transformation occurred upon slow dialysis conditions while the rapid fusogen methods led to more stable non-spherical assemblies signifying the importance of kinetics in the shape transformation process. After confirming that the triblock-based system could lead to successful shapetransformation of polymer vesicles, we were still curious about investigating the role of crosslinking in altering the polymersome membrane. To carry out this investigation, we first crosslinked the polymersomes before exposing them to osmotic pressure changes via PEG. Unlike the uncrosslinked polymersomes, no shape-transformation took place, suggesting that the crosslinking does affect the membrane makeup in such a way that affects its response to osmotic pressure changes. The polymersomes showed some wrinkling upon crosslinking, but there were no apparent morphological changes (Figure <ref type="figure">5</ref>). The absence of shape transformation is even clearer on the more concentrated sample with 5 mg/mL PEG concentration (Figure <ref type="figure">5c</ref>). In the future, we also intend to investigate whether inducing coumarin dimerization after the shape transformation would also lead to further morphological changes.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.">Conclusion</head><p>In this work, we have shown that polymersomes from the self-assembly of glassy amphiphilic ABA triblock copolymers can be transformed into stable non-spherical morphologies. In addition to the membrane rigidity, the speed of the shape transformation also plays an important role in determining whether metastable morphologies can form. While slower osmotic pressure changes through dialysis only resulted in size decreases, the faster PEG-induced osmotic pressure changes led to morphological transformations of these polymersomes. We also demonstrated that chemically altering the membranes through crosslinking led to the vesicles demonstrating hypotonic shock, deviating from the typical behavior of the glassy polymers, suggesting that rearrangement of the membrane during crosslinking increases the permeability of the membranes.</p><p>We believe that this phenomenon is very interesting to create triggered response of polymersomes in a variety of systems. Furthermore, we triggered this shape transformation of polymersomes with membranes whose diblock analogs are usually too short to sustain stable non-spherical shapes.</p><p>This work demonstrates the complexities associated with membrane flexibility and dynamics in glassy polymersomes. Moreover, these results discussed highlight opportunities for utilizing facile and easily accessible chemical modifications which can play an important role in enhancing the use of these polymersomes as both cellular or organelle mimics and as delivery agents. In addition to designing a phase diagram of the morphologies that can be obtained from our polymersomes via rapid osmotic pressure changes, we also intend to do a comparative study of the diblock-based systems and triblock-based systems from our polymer system.</p><p>Cellulose Dialysis Tubing (Fisherbrand, MWCO 12-14kDa) was soaked in DI water for 1 hour and washed with at DI water (1 L) before use.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.">Methods</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.1.">Nuclear magnetic resonance spectroscopy (NMR)</head><p>1 H NMR spectra were recorded on a Varian MERCURY 300 MHz and 600 MHz Bruker AVANCE III spectrometers. <ref type="bibr">13</ref> C NMR spectra were recorded at 150 MHz on the Bruker AVANCE III spectrometer. All chemical peaks were referenced to TMS at 0 ppm for 1 H NMR and <ref type="bibr">13</ref> C NMR spectra were recorded at 298 K.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.2">Flash Chromatography</head><p>Column chromatography was done using a Biotage Isolera One flash purification system with a 200-400 nm variable detector, using pre-packed Snap Ultra 10 g or 25 g cartridges (Biotage).</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.3.">Size-exclusion chromatography (SEC)</head><p>SEC was performed using a Wyatt GPC consisting of a Waters Alliance 2695 separations module and an interferometric refractometer (refractive index detector, Optilab TrEX, Wyatt Technology Inc.) (operating at 35 &#176;C and 685 nm), an on-line multi-angle laser light scattering (MALLS)</p><p>detector fitted with a gallium arsenide laser (power: 20 mW) operating at 658 nm (miniDAWN TREOS, Wyatt Technology Inc.), and two PLgel (Polymer Laboratories Inc.) mixed 3E columns (3 &#181;m bead size, pore size range 50-103&#197;,). Freshly distilled THF was used as the mobile phase at a flow rate of 1.0 mL/min and sample volume of 100 &#181;L was injected for each run. All the detector signals were recorded and analyzed using ASTRA 6 software (Wyatt Technology Inc).</p><p>The refractive index increments values were calculated from the refractive index detector response assuming 100% mass recovery for use with MALLS to determine the absolute molecular weights.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.4.">UV-vis spectrometry</head><p>All UV-vis absorbance spectra were measured on a Lambda 35 UV-vis Spectrophotometer (Perkin Elmer) equipped with a deuterium (UV light source) and halogen (Visible light source) lamp.</p><p>Measurements were performed at a scan speed of 480 nm/min and a lamp change occurred at 326 nm. Samples were prepared by diluting 50 &#181;L of the polymersome suspension with 2.95 mL of dry THF before transferring them to a 3 mL-quartz cuvette (Hellma 111-QS) with a 10 mm x 10 mm light path.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.5.">Dynamic light scattering (DLS)</head><p>DLS measurements were collected using incident light at 633 nm from a Research Electro Optics</p><p>HeNe laser operating at 40 mW. The time-averaged scattering intensity (over two min) was measured from a Brookhaven Instruments BI-200SM goniometer with an avalanche photodiode detector and TurboCorr correlator.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.6.">UV-crosslinking</head><p>UV irradiation was conducted using a H&#246;nle Bluepoint 4 UV light source (320-390 nm).</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.7.">Transmission Electron Microscope (TEM)</head><p>Cryogenic-TEM (cryo-TEM) images were collected using a FEI G2 F30 Tecnai TEM instrument operated at 200 kV. Samples were prepared by placing a drop (5 &#181;L) of the polymersome suspension on a carbon-coated TEM grid (Electron Microscopy Sciences). Using an automated Vitrobot (FEI) system at 100% humidity, the film was blotted for 5 s with a Whatman filter paper and then vitrified in liquid ethane cooled by liquid nitrogen. The sample was then transferred onto a single-tilt cryo-specimen holder for imaging. The specimens were maintained below -175 &#176;C during imaging. Membrane thicknesses for PEG22-b-P(S-stat-CMA)118-b-PEG22 and PEG45-b-P(S-stat-CMA)206-b-PEG45 were measured using ImageJ software and an average thickness of 10 different areas of the membrane was calculated.</p><p>Dry TEM was performed using a JEM-1400 TEM microscope at an acceleration of 60 kV. The samples were prepared by placing a drop (5 &#181;L) of the polymersome suspension on a fresh carboncoated TEM grid (Electron Microscopy Sciences). The specimen was allowed to dry in air for at least 30 minutes before imaging.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.2.8.">Data processing and presentation</head><p>All graphs were plotted using Origin Pro 2016 software (Origin Lab) and Microsoft Excel (Office 365, Microsoft), and figures were assembled using Adobe Illustrator software. Membrane thickness was obtained using ImageJ software (National Institutes of Health, Bethesda, MD) by calculating the average thickness from 10 measurements at different areas of the membrane.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.3.">Synthetic procedures</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.3.1.">Synthesis of 7-(2-methacryloyloxyethoxy)-4-methylcoumarin (CMA)</head><p>The synthesis of 7-(2-hydroxyethoxy)-4-methylcoumarin was conducted following a previously reported procedure. <ref type="bibr">46</ref> The product was collected as an off-white powder with a yield of 85% and used without further purification. The CMA was adapted from a previously reported procedure. <ref type="bibr">30</ref> In a one-neck 250 mL Schlenk flask mounted with a stir bar and equipped with a PTFE stopcock, 7-(2-hydroxyethoxy)-4methylcoumarin (8.00 g, 36.3 mmol, 1.0 equiv.) were dissolved in chloroform (100 mL) under a nitrogen atmosphere. Following the addition of triethylamine (10.13 mL, 72.65 mmol, 2.0 equiv.), the mixture was stirred at 0 &#176;C for 15 minutes. Then, methacryloyl chloride (7.097 mL, 72.65 mmol, 2.0 equiv.) was added dropwise to the mixture at 0 &#176;C, which was stirred for 16 hours under a nitrogen atmosphere. After 16 hours, the reaction mixture was treated with DCM and the organic layer was washed with brine (2 x 100 mL). The organic layer was then dried over MgSO4 and the solvent was removed under reduced pressure via rotary evaporation. The crude product was further purified by recrystallization in ethanol to obtain white powdery crystals with a yield of 65%. </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.3.2.">Synthesis of diCEP</head><p>CEP was synthesized based on a previously reported procedure. <ref type="bibr">47</ref> In a 500-mL two-neck round-bottom flask, a suspension of (95%) NaH (2.11 g, 83.5 mmol, 1.0 equiv.) in anhydrous diethyl ether (150 mL) and was cooled to 0 &#176;C in an ice/water bath. Ethane thiol (5.73 g, 92.3 mmol, 1.1 equiv.) was then added over 15 min accompanied by vigorous evolution of hydrogen gas. The reaction was stirred for an additional 15 min at 0 &#176;C. Then, carbon disulfide (7.03 g, 92.3 mmol, 1.1 equiv.) was added dropwise over 5 min at 0 &#176;C. The ice bath was then removed and the reaction was stirred for 60 min and allowed to warm back up to room temperature. Upon addition of pentane (100 mL), a yellow precipitate formed. The precipitate was then vacuum filtered with a B&#252;chner funnel and dried in vacuo to yield sodium ethyl trithiocarbonate as a yellow powder. In a 500-mL two-neck round-bottom flask, a portion of the sodium ethyl trithiocarbonate (9.89 g, 61.7 mmol, 1.0 equiv.) was then suspended in diethyl ether (200 mL) at room temperature and solid I2 (8.63 g, 34.0 mmol, 0.55 equiv.) was slowly added to the suspension. The reaction was stirred at room temperature for 60 min and a precipitate of NaI salts formed. The precipitate was then removed by vacuum filtration over a B&#252;chner funnel and washed with diethyl ether (50 mL).</p><p>The filtrate was then collected and transferred to a separatory funnel where it was washed with 5% sodium thiosulfate (2 x 150 mL), H2O (1 x 150 mL), and brine (1 x 150 mL). The organic layer was then dried over magnesium sulfate and the solvent was removed under reduced pressure via rotary evaporation. A yellow powder was obtained and dried in a vacuum oven at room temperature to obtain bis(ethyl) trithiocarbonate as a yellow solid. In a 500 mL 3-necked roundbottom flask equipped with stir bar and condenser, bis-ethyltrithiocarbonate (5.00g, 18.2 mmol, 1.0 equiv.) and V-501 (7.66 g, 27.3 mmol, 1.5 equiv.) were dissolved in EtOAc (250 mL). The solution was purged with N2 for 45 mins and then heated to reflux for 18 hours. The reaction was quenched via exposure by opening the reaction vessel to air and cooling to room temperature. A yellow powder was obtained under reduced pressure via rotary evaporation under vacuum, and then purified via flash column chromatography hexanes/EtOAc/Acetic acid (60/35/5, v/v, Rf = 0.4). The column fractions containing CEP were transferred into a separatory funnel and washing with 0.05 N HCl (2 x 150 mL), and brine (1 x 150 mL). The organic layer was dried over MgSO4, and the solvent was removed under reduced pressure via rotary evaporation followed by drying in a in a vacuum oven overnight at room temperature to yield CEP as a yellow solid. Yield: 7.10 g (74%); ) was then added to the flask followed by the addition of DCM (30 mL). The reaction vessel was then immersed in an ice and water bath. Separately, DCC (1.56 g, 7.60 mmol, 2.10 equiv.)</p><p>and DMAP (0.09g, 0.76 mmol, 0.21 equiv.) were dissolved in DCM (5 mL) in a scintillation vial.</p><p>The solution was added to the cooled flask dropwise over 5 min and the mixture was stirred overnight. The reaction mixture was filtered to remove dicyclohexylurea and the salts were washed with DCM until white (ca. 10 mL). The filtrate was collected into an evaporating flask and the solvent was removed under reduced pressure in a rotary evaporator. </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.3.3.">Representative RAFT for the homopolymerization of styrene and copolymerizations of styrene and coumarin methacrylate</head><p>In general, desired ratio of monomers, chain-transfer agent, and initiator were dissolved in dry DMF and added to a 25-mL Schlenk tube equipped with a magnetic bar. For example, styrene (1.9 g, 18.26 mmol, 426 equiv.), CMA (1.3 g, 4.50 mmol, 105 equiv.), diCEP (0.025 g, 0.043 mmol, 1.0 equiv.), AIBN (1.4 mg, 9.0 &#181;mol, 0.2 equiv.) were dissolved in 3 mL of dry DMF and added to the Schlenk tube, which was then sealed and purged with argon gas for 30 minutes. After purging, an aliquot (0.2 mL) was taken, and the polymerization was started by plunging the reaction mixture into a pre-heated oil bath at 75 &#176;C under constant stirring. After 20 hours, the reaction was quenched by opening the reaction vessel to air and the tube was cooled in liquid nitrogen for approximately 1 min. An aliquot (0.2 mL) was taken, and the remaining reaction mixture was precipitated in cold methanol (45 mL). The mixture was centrifuged in 50-mL polypropylene tubes, the supernatant was decanted and the yellow precipitate was redissolved in DCM (5 mL). The solution was then precipitated in cold methanol (45 mL) and the centrifugation procedure was repeated twice. Note that for a few samples 1 H NMR spectroscopy indicated the presence of residual monomer, and additional precipitations in cold methanol were needed to completely remove the monomer. All polymers were characterized by SEC and 1 H NMR spectroscopy.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.3.4.">One-pot aminolysis and thia-Michael coupling</head><p>The hydrophobic block P(S-stat-CMA) underwent one-pot aminolysis and thia-Michael addition reaction, with either 1 000 g/mol or 2 000 g/mol PEG acrylate to obtain the triblock, PEG-b-P(Sstat-CMA)-b-PEG. For example, to a 100-mL round-bottom flask equipped with a stir bar under nitrogen, P(S-stat-CMA) (0.444 g, 0.014 &#181;mol, 1.0 equiv.) and PEG acrylate (2 000 g/mol) (0.278 g, 139 &#181;mol, 10 equiv.) were added. Using a syringe, dry THF (3 mL) was added to the flask to dissolve the polymers completely. Then, tributylphosphine (34.27 &#181;L, 139 &#181;mol, 10 equiv.) was added at once with a luer-lock gas-tight syringe (500 &#181;L) and the reaction was allowed to stir for 15 minutes. n-Hexylamine (18.25 &#181;L, 139 &#181;mol) was added at once with a luer-lock gas-tight syringe (100 &#181;L). After 18 hours, the solution was precipitated in a cold mixture of methanol:diethyl ether 10:1 (v/v) (16 mL). The mixture was centrifuged in 20-mL scintillation vial, the supernatant was decanted and the off-white precipitate was redissolved in THF (2 mL).</p><p>The solution was then precipitated in methanol:diethyl ether 10:1 (v/v) (16 mL) and the centrifugation procedure was repeated twice. After confirming the removal of unreacted PEG acrylate via NMR, the triblock polymer was dried in vacuum over for overnight. All polymers were characterized by SEC and 1 H NMR spectroscopy.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.4.">Self-assembly and shape-transformation procedures</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.4.1.">Procedure for the self-assembly process</head><p>The self-assembly procedure followed a previously published method. <ref type="bibr">35</ref> In a 20-mL reaction vial with a rubber septum, PEG45-b-P(S-stat-CMA)206-b-PEG45 triblock polymer (20 mg) was dissolved in THF:Dioxane 1:1 (v/v) (2 mL). Upon dissolution, DI water (2 mL) was added to the solution under constant stirring (700 rpm) at 1 mL/h via a syringe pump. An aliquot (75 &#181;L) of the cloudy suspension was then taken and quenched by addition to DI water (2 mL) under constant stirring (700 rpm). This sample was used for DLS measurements and TEM imaging.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.4.2.">Slow osmotic pressure changes via dialysis</head><p>The cloudy polymersome suspension was transferred to a dialysis bag (MWCO 12-14 kDa) which was then left in DI water (1 L) for 48 hours without any agitation. The DI water was changed every 12 hours. After dialysis, the polymersome suspension (75 &#181;L) was also quenched in DI water (2 mL) under constant stirring (700 rpm) and then analyzed by DLS and TEM imaging.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.4.3.">Vesicle crosslinking via UV irradiation</head><p>The polymersome suspension was transferred to a 1-dram vial equipped with a stir bar in air. The suspension was then irradiated for 120 seconds in a closed chamber before another aliquot (50 &#181;L)</p><p>was taken for UV-vis analysis. An aliquot (75 &#181;L) of the irradiated polymersome suspension was also quenched in DI water (2 mL) under constant stirring (700 nm) and then analyzed by DLS and TEM imaging.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.4.3.">Rapid osmotic pressure changes via PEG fusogen</head><p>The process was conducted following a previously reported procedure. <ref type="bibr">45</ref> In a 20-mL reaction vial with a rubber septum, PEG45-b-P(S-stat-CMA)206-b-PEG45 polymer (10 mg) was dissolved in THF:Dioxane 1:1 (v/v) (1 mL). DI water was then added at a rate of 1 mL/h until the aqueous composition reached 20% by volume. An aliquot (50 &#181;L) of the polymersome suspension was quenched by addition DI water (2 mL) under constant stirring. A portion (200 &#181;L) of the cloudy polymersome suspension was then transferred to a 2-dram vial before the PEG solution (15&#181;L of 0.5 mg/mL, 1 mg/mL or 5 mg/mL in DI water) was added. The PEG/polymersome mixture was centrifuged for one minute before an aliquot (50 &#181;L) was quenched in DI water (2 mL) under constant stirring and analyzed via TEM imaging.</p></div></body>
		</text>