<?xml-model href='http://www.tei-c.org/release/xml/tei/custom/schema/relaxng/tei_all.rng' schematypens='http://relaxng.org/ns/structure/1.0'?><TEI xmlns="http://www.tei-c.org/ns/1.0">
	<teiHeader>
		<fileDesc>
			<titleStmt><title level='a'>Visible emission properties of melt-gown Dy-doped CsPbCl3 and KPb2Cl5 crystals,</title></titleStmt>
			<publicationStmt>
				<publisher></publisher>
				<date>2020 Summer</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10231467</idno>
					<idno type="doi"></idno>
					<title level='j'>Optical materials express</title>
<idno>2159-3930</idno>
<biblScope unit="volume">10</biblScope>
<biblScope unit="issue"></biblScope>					

					<author>S. Uba U. Hommerich</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[We report results of the optical properties of Dy-doped CsPbCl3 and KPb2Cl5 bulkcrystals for potential applications in yellow solid-state laser development. The crystals weresynthesized from purified starting materials and melt-grown by vertical Bridgman technique.Optical transmission measurements revealed characteristic absorption bands from intra-4ftransitions of Dy3+ ions. Direct optical excitation at 455 nm (6H15/2 -> 4I15/2) resulted indominant yellow emission bands at 575 nm from the 4F9/2 excited state of Dy3+ ions. Inaddition, both crystals exhibited weaker emission lines in the blue (483 nm) and red (670 nm)regions. The peak emission-cross sections for the yellow transition (4F9/2 -> 6H13/2) weredetermined to be 0.22 x 10^20 cm2 for Dy: CsPbCl3 (lpeak = 576.5 nm) and 0.59 x 10^20 cm2 for Dy: KPb2Cl5 (lpeak = 574.5 nm). The spectral properties and decay dynamics of the 4F9/2 excited state were evaluated within the Judd-Ofelt theory to predict total radiative decay rates, branching ratios, and emission quantum efficiencies.]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="1.">Introduction</head><p>The visible emission properties of Dy 3+ doped solids continue to be of current interest for applications in white light source development and yellow solid-state lasers <ref type="bibr">[1]</ref><ref type="bibr">[2]</ref><ref type="bibr">[3]</ref><ref type="bibr">[4]</ref><ref type="bibr">[5]</ref><ref type="bibr">[6]</ref><ref type="bibr">[7]</ref>. Laser action based on the yellow Dy 3+ transition 4 F 9/2 &#8594; 6 H 13/2 was first reported at cryogenic temperature for Dy: KY(WO 4 ) 2 and Dy: KGd(WO 4 ) 2 under flashlamp pumping <ref type="bibr">[4]</ref>. More recently, blue laser diode pumped Dy 3+ solid-state lasers were reported for Dy: YAG <ref type="bibr">[6]</ref> and Dy,Tb: LiLuF 4 <ref type="bibr">[7]</ref> operating at room temperature. Ternary lead halides including halide perovskites with composition CsPbX 3 (X = Br, Cl) have emerged as promising photonic materials for applications in photovoltaics, optoelectronics, and nuclear radiation detection <ref type="bibr">[8]</ref><ref type="bibr">[9]</ref><ref type="bibr">[10]</ref><ref type="bibr">[11]</ref>. The low-phonon energy of lead halide based materials has also been of interest for rare earth (RE) doping in solid-state laser applications at IR wavelengths <ref type="bibr">[12]</ref><ref type="bibr">[13]</ref><ref type="bibr">[14]</ref><ref type="bibr">[15]</ref><ref type="bibr">[16]</ref>. For example, Nd doped KPb 2 Br 5 and RbPb 2 Cl 5 crystals have shown lasing at several near-IR wavelengths <ref type="bibr">[13]</ref>, whereas Dy doped RbPb 2 Cl 5 has shown mid-IR lasing at 5.5 &#181;m <ref type="bibr">[15]</ref>. The low-phonon energies of lead halide based crystals promises also efficient visible emission from RE ions with only weak non-radiative decay. Furthermore, the relatively broad spectral features observed from RE doped ternary lead halides reduces requirements for wavelength stabilization in diode laser pumping and suggests possible yellow laser tuning. In this paper, we present results of the material preparation and visible emission properties of Dy doped CsPbCl 3 and KPb 2 Cl 5 crystals melt-grown by vertical Bridgman technique. The visible emission properties were studied and important spectroscopic parameters were derived for applications in yellow laser development.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.">Materials and experimental details</head><p>CsPbCl 3 (CPC) is a direct semiconductor with a bandgap of &#8764; 3.0 eV. It has a density of 4.21 g/cm 3 and a melting point of &#8764; 600 &#176;C <ref type="bibr">[16]</ref>. CPC crystallizes in a close to cubic perovskite structure. CPC has a low moisture sensitivity and can be handled under ambient conditions. The refractive index was derived from published data to be n&#8764;1.75 at visible to near-IR wavelengths <ref type="bibr">[17]</ref>. KPb 2 Cl 5 (KPC) is a monoclinic crystal with a band gap of &#8764;3.77 eV <ref type="bibr">[18]</ref>. KPC has a density of 4.629 g/cm 3 and a melting point of 434 &#176;C <ref type="bibr">[18]</ref>. KPC is considered non-hygroscopic and has a refractive index of n&#8764;2 <ref type="bibr">[12]</ref>. Dy: CPC and Dy: KPC crystals were grown by a vertical Bridgman technique employing a two-zone furnace <ref type="bibr">[14]</ref>. Beads of PbCl 2 (99.999%) were mixed in a stoichiometric ratio with CsCl (99.999%) or KCl (99.999%) to synthesize CPC or KPC, respectively. DyCl 3 was added as dopant to the mix at 1-2 wt%. The combined material was loaded into a pre-cleaned quartz ampoule inside an argon-filled glovebox and heated at &#8764;110 &#176;C under a dynamic vacuum for 2 days. After sealing under vacuum (&#8764;10 -6 torr) the growth ampoule was positioned inside the hot zone of a two-zone crystal growth furnace. The temperature of the hot zone was kept at &#8764;30 &#176;C above the melting point. The ampoule was then lowered at a growth speed of 1-3 mm/h. After the crystal growth was completed, the furnace temperature was slowly reduced to room-temperature over a time period of four days. Single crystalline grains in the size range of 5 to 10 mm could be mined out from each boule. It was observed that Dy: KPC was colorless and stable under ambient conditions without any change in overall transmission. In contrast, the Dy: CPC crystal exhibited a slight yellowish coloration and became milky with reduced transmission after a few hours of exposure to air. The crystal structure of CPC and KPC was confirmed by XRD measurements. The dopant concentration for Dy: CPC was measured to be 1.1 &#215; 10 20 cm -3 using inductively coupled plasma optical emission spectroscopy (ICP-OES). The Dy concentration for Dy: KPC was determined to be 5 &#215; 10 19 cm -3 by comparison to published absorption cross-section data <ref type="bibr">[12]</ref>. Samples of good optical quality with dimensions of &#8764;5 &#215; 5&#215;3 mm 3 were selected and polished for spectroscopic studies. Transmission spectra were measured using a Shimadzu UV-3600 spectrophotometer. Emission spectra, excitation spectra, and lifetimes were recorded employing an Edinburgh Instruments FLS 980 fluorescence spectrometer.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.">Results and discussion</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.1.">Transmission, absorption, and Judd-Ofelt analysis</head><p>The optical transmission and absorption spectra of Dy: CPC and Dy: KPC crystals are shown in Figs. <ref type="figure">1</ref> and<ref type="figure">2</ref>. For both crystals the transmission in the IR region was over 50%, but decreased significantly at visible wavelengths due to background absorption losses.</p><p>Characteristic intra-4f absorption bands of Dy 3+ ions were identified in the IR region peaking at &#8764;0.76, &#8764;0.81, &#8764;0.91, &#8764;1.10, &#8764;1.29, &#8764;1.67, and &#8764;2.9 &#181;m corresponding to transitions from the 6 H 15/2 ground state to the 6 </p><p>, and 6 H 13/2 states, respectively. In addition, weaker UV-visible absorption bands were observed for Dy: KPC at 354 nm ( 6 P 7/2 ), 366 nm ( 6 P 5/2 ), 388 nm ( 4 I 13/2 ), 427 nm ( 4 G 11/2 ), 454 nm ( 4 I 15/2 ), and 476 nm ( 4 F 9/2 ), respectively <ref type="bibr">[19,</ref><ref type="bibr">20]</ref>. Dy: CPC did not reveal any visible Dy 3+ absorption bands most likely due to overlapping defects and the onset of near bandedge absorption <ref type="bibr">[16]</ref>. Using five IR Dy 3+ absorption bands a Judd-Ofelt (JO) analysis was performed for Dy: CPC. The 2.9 &#181;m absorption band was not included because of possible overlap with OH absorption <ref type="bibr">[14]</ref>. The reduced matrix elements were taken from Kaminskii <ref type="bibr">[19]</ref> and yielded the following intensity parameters: &#8486; 2 = 4.05 &#215; 10 -20 cm 2 , &#8486; 4 = 0.06 &#215; 10 -20 cm 2 , and &#8486; 6 = 0.39 &#215; 10 -20 cm 2 . Table <ref type="table">1</ref> summarizes the relevant data and calculated oscillator strengths for Dy: CPC. For Dy: KPC a JO analysis was reported by Nostrand et al. <ref type="bibr">[12]</ref> yielding the intensity parameters: &#8486; 2 = 5.41 &#215; 10 -20 cm 2 , &#8486; 4 = 0.99 &#215; 10 -20 , &#8486; 6 = 2.96 &#215; 10 -20 cm 2 .      <ref type="table">2</ref>.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.2.">Visible emission studies and emission cross-sections</head><p>The excitation spectra for Dy: CPC and Dy: KPC for a monitor wavelength of &#8764;575 nm are shown in Fig. <ref type="figure">4</ref>. It can be seen that intra-4f excitation at &#8764;455 nm ( 6 H 15/2 &#8594; 4 I 15/2 ) is the most efficient pump wavelength for achieving yellow emission from both crystals. The excitation spectra also reveal that carrier-mediated excitation using above gap energies does not efficiently excite Dy 3+ ions in both hosts. The room temperature 4 F 9/2 emission decay transients monitored at &#8764;575 nm for Dy: CPC and Dy: KPC are shown in Fig. <ref type="figure">5</ref>. For lifetime studies low-concentration samples (&#8764;0.5 wt%) were employed to avoid possible cross-relaxation processes <ref type="bibr">[3]</ref>. Following an initial fast decaying component, the emission lifetime of Dy: CPC was single exponential with a value of &#8764;1.0 ms. The initial fast decaying component is attributed to residual broad background emission from the CPC host. Since the decay time for Dy: KPC was slightly non-exponential, the average lifetime was determined according to the following equation:</p><p>where I (t) is the emission intensity as a function of time. The average lifetime for Dy: KPC yielded a value of 0.37 ms. Based on the existing emission data, the peak emission cross-sections were calculated using the Fuchtbauer-Ladenburg expression <ref type="bibr">[5]</ref>: where &#955; peak is the peak emission wavelength, &#946; is the branching ratio, &#964; rad is the radiative lifetime, and &#8710;&#955; eff is the emission bandwidth. The derived peak emission cross-sections for Dy: CPC and Dy: KPC were determined to be 0.22 &#215; 10 -20 cm 2 (&#955; peak = 576.5 nm) and 0.59 &#215; 10 -20 cm 2 (&#955; peak = 574.5 nm), respectively. The cross-section spectra for both crystals are shown in Fig. <ref type="figure">6</ref> and the emission properties are summarized in Table <ref type="table">2</ref>. It can be noted, that the calculated and experimental emission lifetimes are similar for Dy: KPC, which suggest a quantum efficiency of &#8764;82%. Since KPC has a small maximum phonon energy of only h&#969; max &#8764;200 cm -1 and due to the large energy-separation of &#8764;7200 cm -1 between the 4 F 9/2 and the next lower 4 F 1/2 level, non-radiative decay through multi-phonon relaxation is expected to be weak <ref type="bibr">[5,</ref><ref type="bibr">19]</ref>. For Dy: CPC measured and calculated lifetimes are significantly different, which indicates the existence of non-radiative decay despite the narrow phonon spectrum (h&#969; max &#8764;375 cm -1 ) of the host. Non-radiative losses in Dy: CPC are most likely due to residual defects as indicated by the significant background absorption and OH related multi-phonon quenching <ref type="bibr">[16,</ref><ref type="bibr">21]</ref>. Further studies on the relation between decay dynamics and material purification are in progress. The main laser relevant spectroscopic parameters for the investigated Dy: CPC and Dy: KPC in comparison to other Dy doped crystals are shown in Table <ref type="table">3</ref>. It can be noted that Dy: KPC compares well with Dy: YAG and Dy: LiLuF 4 laser materials and exhibits higher emission cross-section and quantum efficiency. Furthermore, the broad absorption and emission features with bandwidth of several nanometers offer advantages for diode laser pumping and yellow laser tunability. Careful studies on possible quenching effects for higher Dy 3+ concentrations, however, are still needed to fully explore Dy: KPC as a novel yellow laser material. For Dy: CPC the strong background absorption losses due to intrinsic defects severely limits its potential for laser applications. </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.">Conclusions</head><p>Results of the material preparation and optical spectroscopy for Dy: CsPbCl 3 and Dy: KPb 2 Cl 5 were presented. High purity starting materials were employed for the synthesis of both compounds and crystal growth experiments were carried out using vertical Bridgman technique. Under resonant excitation into an intra-4f absorption band, Dy: CPC and Dy: KPC exhibited bright yellow emission peaking in the &#8764;575-577 nm range from the 4 F 9/2 &#8594; 6 H 13/2 transition of Dy 3+ ions. Based on a Judd-Ofelt analysis, it was determined that the yellow emission exhibited high branching ratios (65-78%) with an emission quantum efficiency of &#8764;82% for Dy: KPC. In addition, Dy: KPC also exhibited a slightly higher peak emission cross-section for the 4 F 9/2 &#8594; 6 H 13/2 transition compared to other yellow laser crystals <ref type="bibr">[6,</ref><ref type="bibr">7]</ref>, which indicates the potential of Dy: KPC for solid-state gain media applications. On the contrary, Dy: CPC exhibited non-radiative losses due to unknown defects and possible OH multi-phonon relaxation. Dy: CPC also suffered from intrinsic transmission losses which make this material less attractive for visible laser applications. Future studies on these crystals will focus on additional purification experiments in an effort to reduce background absorption losses and to improve overall crystal quality.</p></div></body>
		</text>
</TEI>