<?xml-model href='http://www.tei-c.org/release/xml/tei/custom/schema/relaxng/tei_all.rng' schematypens='http://relaxng.org/ns/structure/1.0'?><TEI xmlns="http://www.tei-c.org/ns/1.0">
	<teiHeader>
		<fileDesc>
			<titleStmt><title level='a'>Polyethylene-BN nanosheets nanocomposites with enhanced thermal and mechanical properties</title></titleStmt>
			<publicationStmt>
				<publisher></publisher>
				<date>03/01/2021</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10251958</idno>
					<idno type="doi">10.1016/j.compscitech.2020.108631</idno>
					<title level='j'>Composites Science and Technology</title>
<idno>0266-3538</idno>
<biblScope unit="volume">204</biblScope>
<biblScope unit="issue">C</biblScope>					

					<author>Md Golam Rasul</author><author>Alper Kiziltas</author><author>Christos D. Malliakas</author><author>Ramin Rojaee</author><author>Soroosh Sharifi-Asl</author><author>Tara Foroozan</author><author>Reza Shahbazian-Yassar</author><author>Babak Arfaei</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[Polyethylene (PE) are in demand for electrical insulation and thermal management applications; however, their low mechanical and thermal properties pose major challenges. Herein, we report on novel properties of PE-boron nitride (BN) nanocomposites prepared by melt compounding followed by injection molding. The thermal and mechanical properties of silane-functionalized (sBN) and non-functionalized (pBN) PE-BN nanocomposites were studied in order to assess the role of silane functional groups at the interface of BN nanosheets and PE matrix. In comparison with PE materials, addition of 5 wt % BN nanosheets increases tensile modulus of elasticity by 37 and 42%, flexural modulus of elasticity by 24 and 30%, tensile strength by 15 and 27%, and storage modulus by 80 and 91% for pBN and sBN nanocomposites, respectively. Besides mechanical reinforcement, thermal and thermomechanical properties were evaluated for PE-BN nanocomposites. While thermal stability of PE-pBN and PE-sBN nanocomposites was comparable, coefficient of thermal expansion was decreased by 12 and 20% at 5 wt % pBN and sBN nanosheets, respectively. These polymer nanocomposites with enhanced mechanical and thermal properties can be an excellent choice for application in insulation materials, including thermal interface layers in electronic devices.]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="1.">Introduction</head><p>Recent advances in electronic devices have led to more demand in polymer materials like polyethylene (PE) for insulation and thermal management purposes <ref type="bibr">[1]</ref><ref type="bibr">[2]</ref><ref type="bibr">[3]</ref>. Because of low permittivity and high electrical breakdown strength, PE is widely used as an insulation material <ref type="bibr">[4,</ref><ref type="bibr">5]</ref>. However, low mechanical and thermal properties of PE polymer result in early mechanical failure during long term service <ref type="bibr">[6,</ref><ref type="bibr">7]</ref>. Boron nitride (BN) nanomaterials with outstanding mechanical properties (Young's modulus ~1 TPa), flexibility, high thermal stability (~800 &#8226; C in air), low dielectric constant (~4), high band gap (~5.4 eV), high voltage breakdown strength (~12 MV/cm), and chemical inertness are promising fillers to tune the mechanical and thermal properties of PE materials <ref type="bibr">[8]</ref>. BN nanosheets have been used in polymer nanocomposite materials where thermal management, electrical resistivity, and dielectric properties are important.</p><p>In spite of the potential reinforcement effects of BN nanosheets in polymers, the incompatibility of inorganic BN nanosheets with organic polymer materials can cause the degradation in mechanical and thermal properties of such nanocomposites <ref type="bibr">[9,</ref><ref type="bibr">10]</ref>. For example, Wang et al. <ref type="bibr">[11]</ref> reported degradation in mechanical properties of epoxy-BN nanosheets nanocomposites, where tensile strength and elastic modulus were reduced by 80 and 20% compared to the base epoxy polymer. Therefore, it is important to improve the compatibility by functionalizing BN nanosheets with appropriate coupling agents and enhance polymer-BN nanosheets interfacial interactions <ref type="bibr">[12]</ref>. Organic polymer molecules such as PE and inorganic BN nanosheets have limited non-covalent interactions (e.g., van der Waals) due to their bond structure. As a result, chemically modifying BN nanosheets with appropriate functional groups are essential to enhance these non-covalent interactions <ref type="bibr">[13]</ref>. Functionalization may also introduce new molecular interactions (e.g., hydrogen bonding, hydrophobic, and &#960;-&#960; interactions) and increase the degree of miscibility into polymer matrices that can contribute to the improvement of mechanical and thermal properties. Yu et al. <ref type="bibr">[14]</ref> functionalized BN nanoplates with covalent, i.e., hyperbranched aromatic polyamide (HBP) and noncovalent, i.e., octadecylamine (ODA) ways to fabricate epoxy-BN nanoplates nanocomposites. This work reported 12.8 and 12.3% increase in storage modulus by the covalent and non-covalent functionalized BN nanoplates while the same property in the pristine BN nanoplates nanocomposites increased only by 7% at 5 wt % BN nanoplates, respectively. This improvement is believed to be originating from the enhanced interactions between epoxy and functionalized BN nanoplates. Depending on the compatibility of BN nanosheets with different polymer materials, nanocomposites were fabricated with wide range of BN functionalities, including -OH, -NH 2 , -C 4 H 9 , -F, -CH 3 (CH 2 ) 17 NH 2 , -C 9 H 23 N 2 O 3 Si <ref type="bibr">[15]</ref><ref type="bibr">[16]</ref><ref type="bibr">[17]</ref>. Huang and co-workers <ref type="bibr">[18]</ref> reduced the interfacial thermal resistance of epoxy-BN nanocomposites by modifying BN with polyhedral oligosilsesquioxane molecules. The 29% decrease in coefficient of thermal expansion (CTE) and 1360% increase in thermal conductivity were achieved at 30 wt % BN mass loading by the effective BN surface modification.</p><p>Silane functionalization is an attractive choice for modifying BN nanosheets due to the functional groups that can bond and interact with both organic and inorganic compounds <ref type="bibr">[19]</ref>. Silane functionals have organic alkyl molecules (-R), which are very compatible with polyethylene molecules due to nonpolar chemical structure. Additionally, silane contains oxygen molecules which are electronegative and may create Hydrogen-bond between polymer materials and BN nanosheets; these increase molecular interactions and enhance nanocomposite performances <ref type="bibr">[20]</ref><ref type="bibr">[21]</ref><ref type="bibr">[22]</ref>. In spite of few reports on the reduction of interfacial thermal resistance for PE-BN nanocomposites <ref type="bibr">[20,</ref><ref type="bibr">23]</ref>, these studies lack detailed analyses of thermal stability, thermomechanical and mechanical performances. The objective of this work is to investigate the effects of silane functionalization (3-aminopropyltriethoxy silane) on mechanical and thermal properties for PE-BN nanocomposites. The PE-BN nanocomposites were fabricated via melt compounding method utilizing industrially available PE polymer materials. Their mechanical and thermal properties were thoroughly evaluated in terms of tensile modulus of elasticity (TMOE), flexural modulus of elasticity (FMOE), tensile strength, storage modulus, coefficient of thermal expansion (CTE), and thermal stability using tensile and flexural, DMA, DSC, and TGA tests.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.">Experimental</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.1.">Materials</head><p>PE polymers were kindly received from an industrial supplier, which were used to fabricate PE nanocomposites. This PE is usually used for cable insulation material for automotive applications. The detailed characterization of the as-received PE samples is shown in Supplementary Information (Fig. <ref type="figure">S1, S2,</ref> and<ref type="figure">S3</ref>). The scanning electron microscopy (SEM) image (Fig. <ref type="figure">S1</ref>) and thermogravimetric analysis (TGA) (Fig. <ref type="figure">S2</ref>) indicate that the as-received PE material contains ~37 wt % inorganic residues. The SEM-EDS mapping (Fig. <ref type="figure">S3</ref>) suggests that most of these residues are likely to be aluminium oxide (Al 2 O 3 ) and zinc oxide (ZnO). In this study, the pristine BN (pBN) and silane-modified BN (sBN) nanosheets were used to fabricate polymer nanocomposites. These BN nanosheets were purchased from US Research Nanomaterials Inc. and added to the PE during nanocomposite compounding. Both pristine and silane-modified BN nanosheets are hexagonal crystal structure, and the average lateral sizes are 100-200 nm. Silane modified BN nanosheets were modified by functionalizing with 1-3 wt % silane coupling agent (KH-550) using 3-aminopropyltriethoxysilane (C 9 H 23 N 2 O 3 Si, CAS: 919-30-2). Both pristine and silane-modified BN nanosheets were 99.8% pure. The polymer and BN nanosheets were dried in air at 80 &#8226; C for 6-8 h before melt compounding.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="2.2.">Fabrication of polymer nanocomposites</head><p>An appropriate amount of dried PE pellets and BN nanosheets were fed into the K-Tron (Coperion, Stuttgart, Germany) gravimetric feeders separately to compound the master batch of 5 wt % PE-BN nanocomposites. In order to fabricate a homogenous mixture of nanocomposites, the speed of the gravimetric feeder was optimized. Twin-screw extruder (ThermoHaake Rheomex Model PTW25, St. Louis, MO, USA) was used to compound the master batch of 5 wt % PE-BN nanocomposites. Extruded melt compounded product streams were cooled down through a room temperature water bath and granulated using a Nelmor lab-scale grinder (AEC, New Berlin, WI, USA). The grinded master batch nanocomposites were dried in an oven at 60 &#8226; C for at least 12 h before further processing. The rest of the nanocomposites were prepared by mixing appropriate amount of master batch nanocomposites (5 wt % PE-BN) and PE polymer utilizing twin-screw extruder. Extrusion was carried out with a barrel temperature range of 185-200 &#8226; C at 120 rpm screw speed. The maximum pressure in barrel was set to 70 MPa for compounding nanocomposites. Later, an injection molding machine (Boy Machines, Model 80 M, Exton, PA, USA) was used to prepare specimens for mechanical and thermal characterizations. The barrel temperature for injection molding was in the range of 205-215 &#8226; C. The cooling time was 30 s, with a mold temperature of 50 &#8226; C. Base PE materials (without BN nanosheets) were prepared following the same procedures to have the similar thermal and processing history. The PE nanocomposites are labeled in the format of PEweight percentage of BN nanosheets, type of BN nanosheets (pBN or sBN). For example, PE-5.0 wt % pBN indicates that this nanocomposite is composed of polyethylene polymer and 5 wt % pristine BN nanosheets. Simply PE-BN indicates that the PE-BN nanocomposite is prepared with PE and BN nanosheets (i.e., either pBN or sBN nanosheets).</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.">Results and discussion</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.1.">BN nanosheets characterization</head><p>Fig. <ref type="figure">1a-c</ref> shows the morphology and structure of BN nanosheets before addition into PE polymer matrix. The average lateral sizes of the BN nanosheets are in the range of 100-200 nm. Atomic resolution lowangle annular dark field (LAADF) image (Fig. <ref type="figure">1b</ref>) depicts the crystalline nature of BN nanosheet with a six-fold symmetry in the indexed fast Fourier transform (FFT) image (inset in Fig. <ref type="figure">1b</ref>), confirming the hexagonal crystalline structure of BN nanosheets with a lattice spacing of 0.246 nm. Height profile was also obtained from atomic force microscope (AFM) data, and the average thickness of BN nanosheets is 50 nm (Fig. <ref type="figure">1c</ref>). These morphological characteristics (i.e., higher surface area) are essential for interacting with polymer chains and, thus, desirable for polymer nanocomposite applications.</p><p>Chemical bonding and molecular interactions for pBN and sBN nanosheets were compared to better understand the silane functionalization. The high-intensity Fourier transform infrared (FTIR) spectra at 1384 and 808 cm -1 (Fig. <ref type="figure">1d</ref>) for both pBN and sBN nanosheets are attributed to in-plane B-N stretching and out of plane B-N-B bending vibration <ref type="bibr">[21]</ref>. The peak at 3427 cm -1 indicates the -OH group, and the peak at 1616 cm -1 (inset in Fig. <ref type="figure">1d</ref>) is attributed to N-H + vibration mode <ref type="bibr">[21]</ref>. The Si-O stretching bond information is shown at 1100 cm -1 for sBN nanosheets. This weak intensity of the peak at 1100 cm -1 is possibly due to the intensive characteristics of BN nanosheets. A slight shift of IR spectra (1384-1396 cm -1 ) at in-plane B-N stretching is assumed to be originating from the new covalent bond formation due to silane grafting on BN nanosheets <ref type="bibr">[21]</ref>. Further, time-of-flight secondary ion mass spectra (ToF-SIMS) analysis was conducted to confirm the presence of elemental molecules on BN nanosheets. Both the positive and negative ion spectra were collected to identify the chemical states of the functionalization. Fig. <ref type="figure">1e</ref> exhibits the presence of Si molecules on sBN nanosheets. X-ray photoelectron spectroscopy (XPS) analysis was performed to further confirm the silane functionalization. Silane molecules react with BN nanosheets and form covalent bonds with boron molecules. The binding energy is measured by XPS and demonstrated in Fig. <ref type="figure">1f-h</ref>. Fig. <ref type="figure">1f</ref> indicates B 1s spectrum of pBN nanosheets while B 1s spectrum of sBN nanosheets can be fitted into B-N and B-O bonding (Fig. <ref type="figure">1g</ref>). Because of the covalent bond of silane molecules with B atoms, these two B-N and B-O bonds are appeared on sBN nanosheets. To further illustrate the silane bonding with BN nanosheets, Fig. <ref type="figure">1h</ref> demonstrates Si 2p spectrum for sBN nanosheets. The deconvoluted peaks (Si-O-Si, Si-O-B, and Si-CH 2 bonding) reiterate the successful grafting of silane molecules on BN nanosheets. In addition, survey spectrums of both pBN and sBN nanosheets show the presence of B, N, C, and O (Fig. <ref type="figure">S4</ref>) molecules. Owing to the chemical structure of silane functionalized BN nanosheets, the peak intensities of C 1s and O 1s are higher for sBN compared to pBN nanosheets. These observations confirm that the silane was successfully grafted onto the BN nanosheets. Besides, the morphology and lattice structure of BN nanosheets have been tested before and after functionalization using SEM, TEM, and X-ray diffraction (XRD). The SEM images of pBN and sBN nanosheets confirm that the functionalization does not affect the size of BN nanosheets (Fig. <ref type="figure">S5</ref>). In addition, AC-STEM images (Fig. <ref type="figure">S6</ref>) and XRD peak analysis (Fig. <ref type="figure">S7</ref> in Supporting Information provides details of XRD peak analysis) confirm that the silane functionalization does not change the lattice integrity of BNnanosheets. Also, there is no change in d-spacing of BN nanosheets after functionalization, indicating that the silane functional molecules are attached on the surface of BN nanosheets.</p><p>Quantitative analysis of silane functionalization was performed to assess the amount of silane grafting on BN nanosheets. TGA graph (Fig. <ref type="figure">1i</ref>) indicates thermal stability of both pBN and sBN nanosheets. Because of the presence of hydroxyl molecules, surface-functionalized BN nanosheets exhibit a weight loss starting at 100 &#8226; C. Fig. <ref type="figure">1i</ref> indicates that sBN nanosheets start to lose mass at ~250 &#8226; C and continue up to 600 &#8226; C, at which point approximately 2 wt% of the initial mass is lost. Whereas pBN nanosheets exhibit nearly no change in the weight loss up to 800 &#8226; C where 99.68% of initial weight is retained. This indicates that the silane functionalization is estimated to be ~1.7 wt %, which is very low and complies with weak spectra reported in both FTIR and ToF-SIMS analysis. The electronic structure of BN nanosheets is the possible reason behind this low grafting of silane. Since weak organicinorganic interaction of polymer-BN nanosheets plays an unfavorable role in boosting mechanical and thermal properties of bulk nanocomposites <ref type="bibr">[24]</ref>. In this work, this challenge was overcome by utilizing silane functionalized BN nanosheets. A schematic illustration of BN nanosheets modification is shown in Fig. <ref type="figure">2a</ref>. Functionalization of BN nanosheets (Fig. <ref type="figure">2a</ref>) indicates the presence of organic molecules on inorganic BN nanosheets, which increase the miscibility and enhance interactions with various organic solvents. As seen in Fig. <ref type="figure">S8</ref>, the surface-functionalized sBN nanosheets disperse into organic solvents such as tetrahydrofuran (THF) uniformly compared to pBN nanosheets due to polar-polar interactions, indicating increased dispersibility of sBN nanosheets <ref type="bibr">[18]</ref>.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.2.">Mechanical characterization</head><p>The non-linear mechanical reinforcement of pBN and sBN nanosheets was analyzed to show the effect of silane functionalization on PE matrix chain mobility. Because of the molecular chain structure, the base PE matrix has very low TMOE (~316 MPa), FMOE (~292 MPa), and tensile strength (~11 MPa). This means that the molecular chains within the polymer face little difficulty to move or relax under an applied load <ref type="bibr">[25]</ref>. The stress-strain curves for PE-BN nanocomposites are shown in Fig. <ref type="figure">3a</ref>. Fig. <ref type="figure">3a</ref> indicates that the mechanical properties of PE-BN nanocomposites are increased with an expense of ductility. While FMOE was calculated from a 3-point bending test and plotted in Fig. <ref type="figure">3b</ref>, TMOE and tensile strengths are calculated from stress-strain curves (Fig. <ref type="figure">3a</ref>) and plotted in Fig. <ref type="figure">3c-d</ref>. Once pBN nanosheets are added into the base PE matrix, it is demonstrated that the FMOE (Fig. <ref type="figure">3b</ref>) and TMOE (Fig. <ref type="figure">3c</ref>) are reported an increment of 37% and 24% compared to the base PE matrix, respectively. Similarly, tensile strength is also increased by 15% (Fig. <ref type="figure">3d</ref>), and all of these improvements are realized at 5 wt % pBN nanosheets. Differential scanning calorimetry (DSC) and XRD analysis of PE and PE-BN nanocomposites were conducted to evaluate the effect of the percentage of crystal regions and crystallite sizes (details of calculations and results are provided in Supplementary Information). As shown in Table <ref type="table">S1</ref>,there is little change in the percentage of crystal regions and crystallite sizes between PE and PE-BN nanocomposites. Therefore, the reinforcement of BN nanosheets is not likely originating from either the percentage of crystal region or crystallite size, as reported in <ref type="bibr">[26]</ref>. This means that the entanglement of pBN nanosheets into PE chains creates obstacles for the movement of the chains under applied tensile load. Polymer chain entanglement originating from weak interactions between pBN nanosheets and PE matrix explains this increase in mechanical properties of nanocomposites <ref type="bibr">[27]</ref>. Interestingly, the silane-modified BN nanosheets enhance these mechanical properties of nanocomposites even further compared to pBN nanosheets (Fig. <ref type="figure">3a-d</ref>). For example, FMOE and TMOE of PE-5.0 wt % sBN nanocomposites are increased by 30 and 42% and tensile strength is increased by 27% compared to the base PE matrix, respectively. Thus, sBN nanocomposites show 5.5% increase in FMOE, 3.7% increase in TMOE, and 11% increase in tensile strength in comparison to pBN nanocomposites at 5.0 wt % BN nanosheets.</p><p>The fractography of the PE, PE-5.0 wt % pBN, and PE-5.0 wt % sBN nanocomposites were investigated to uncover the polymer chain deformation during tensile fracture using SEM micrographs (Fig. <ref type="figure">4a-h</ref>). The surface morphology of the fractured PE-BN (PE-5.0 wt % pBN and PE-5.0 wt % sBN) nanocomposites indicates a limited plastic  deformation, which implies a brittle behavior of fracture. In sharp contrast, the base PE specimen shows a fibrous morphology, indicating an extensive deformation before the fracture. In addition, a close examination of the fractured surfaces reveals that the plastic flow characteristics are more noticeable for PE-5.0 wt % pBN when compared to PE-5.0 wt % sBN nanocomposites. The mechanical interlocking characteristic of pBN nanosheets reduces the matrix mobility within nanocomposites, thus reducing its ductility when compared to PE. However, if the adhesion between fillers and matrix is not sufficient, extensive delamination will usually occur between the polymer matrix and fillers <ref type="bibr">[28]</ref>. Whereas PE-sBN nanocomposites show the least plastic deformation among all nanocomposites (PE, PE-pBN, and PE-sBN nanocomposites), indicating an enhanced interfacial adhesion between PE matrix and sBN nanosheets. Moreover, the XRD peak analysis of the PE and PE-BN nanocomposites were conducted to observe the PE polymer chain organization because of BN nanosheets addition (details of the XRD analysis and results are shown in Supplementary Information). As shown in Fig. <ref type="figure">S10</ref>, the addition of pBN and sBN nanosheets into PE materials results in no new peak because of three possible reasons: (i) overlapping with the peaks of ZnO and Al 2 O 3 , (ii) exfoliated dispersion state of BN nanosheets, and (iii) low content of BN nanosheets <ref type="bibr">[29]</ref>. The reduction of the peak intensity at the 2&#952; value of 26.81 &#8226; could be attributed to the possible exfoliation of the sBN nanosheets compared to pBN into PE materials <ref type="bibr">[30]</ref>. In addition, the peak intensity reduction  of PE crystalline structure (2&#952; value of 21.3 &#8226; and 23.4 &#8226; ) could be the result of the better compatibility of silane-modified BN nanosheets with PE matrix <ref type="bibr">[31]</ref>. Such compatibility is likely resulting from the molecular interactions between PE matrix and sBN nanosheets, as also reported for other nanocomposite systems <ref type="bibr">[31,</ref><ref type="bibr">32]</ref>. As a result, a higher TMOE, tensile strength, and FMOE are obtained for the PE-sBN when compared to the PE-pBN nanocomposites, which is in agreement with reported observations for other polymer nanocomposite systems <ref type="bibr">[33]</ref>.</p><p>To reveal the load transfer efficiency and polymer chain interactions with BN nanosheets, thermomechanical properties (i.e., storage modulus and loss modulus) were investigated <ref type="bibr">[34]</ref>. Since storage and loss modulus require measuring stored elastic and dissipated energy during straining, molecular orientation and relaxation processes information can reveal chain mobility during transition periods. The changes in storage modulus (Fig. <ref type="figure">5a</ref>) and loss modulus (Fig. <ref type="figure">5b</ref>) for silane-modified BN nanosheets compared to pristine BN nanosheets nanocomposites are significant. In the rubbery state at 25 &#8226; C, the storage modulus of sBN nanocomposites is increased by 36% (218-296 MPa) at 1 wt % BN nanosheets loading level compared to pBN nanosheets. More significant changes are observed at below -40 &#8226; C, where friction between polymer chains is more prominent, and higher storage modulus is observed. Besides entanglements, the higher noncovalent interaction may increase the storage modulus in sBN compared to pBN nanocomposites due to efficient stress transfer from sBN nanosheets to polymer matrix <ref type="bibr">[14]</ref>. Hence, the storage modulus of PE-sBN is higher compared to PE-pBN nanocomposites. Besides, loss tangent (tan&#948;) was calculated from the ratio of loss modulus to storage modulus and reported in Fig. <ref type="figure">S11</ref>. The tan&#948; could provide glass transition temperature (T g ) of a material where T g is determined from the peak temperature of the curves, as reported in many reports <ref type="bibr">[21]</ref>. Although Fig. <ref type="figure">S11</ref> shows tan&#948; of PE and PE-BN composites with the increasing temperature from -80 to 100 &#8226; C; however, this graph does not show any peak in the glassy-rubbery region of the samples. It is likely that the test temperature of the tan&#948; curve (-80 to 100 &#8226; C) was not sufficient to elucidate the glass transition temperature of the PE and PE-BN nanocomposites, since T g of the polyethylene matrix usually occurs at around -115 &#8226; C <ref type="bibr">[35]</ref>. The slightly decreased tan&#948; value of sBN nanocomposites compared to pBN indicates increased molecular interactions between PE and sBN nanosheets <ref type="bibr">[21]</ref>. The silane molecule contains organic and inorganic functional groups, which act as a coupling agent and are likely to increase molecular interactions between organic PE polymer matrix and inorganic BN nanosheets <ref type="bibr">[24]</ref>. The gap between PE and BN nanosheets is reduced due to these increased molecular interactions and leads to create an immobile phase (interphase) at the PE-sBN interface <ref type="bibr">[36]</ref>. Thus, an efficient stress transfer could be originated at the interphase, and nanocomposites show reinforced mechanical properties with reduced chain mobility within nanocomposites. The reduced chain mobility will also lead to decrease CTEs <ref type="bibr">[37]</ref>. Since BN nanosheets have very high specific surface area (~2600 m 2 /g) and silane functionalization leads to the formation of an immobilized phase at the interface in comparison to PE-pBN case <ref type="bibr">[38]</ref>. The higher molecular interactions at the PE and sBN nanosheets interface can effectively restrain polymer chain dynamics.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="3.3.">Thermal characterization</head><p>The coefficient of thermal expansion was investigated to further understand the effects of BN nanosheets and their functionalization on thermomechanical stability of nanocomposites. CTE is an important parameter of polymer material that gives not only fundamental information about chain dynamics, but also important dimensional stability associated with heat. As shown in Fig. <ref type="figure">5c</ref>, the changes in length for PE and nanocomposites are reported over the temperature range from 30 to 75 &#8226; C. The linear region of Fig. <ref type="figure">5c</ref> (35-65 &#8226; C) was fitted, and CTEs were calculated from their slopes. As it can be observed (Fig. <ref type="figure">5d</ref>), the CTE of base PE is 607 &#215; 10 -6 K -1 . By adding BN nanosheets, CTE decreases monotonically down to 484 &#215; 10 -6 K -1 . Similar to what was observed in mechanical properties, sBN outperformed pBN nanocomposites in decreasing CTEs of PE nanocomposites at each of the concentrations of BN nanosheets (Fig. <ref type="figure">5d</ref>). With 5.00 wt % BN nanosheets, pBN nanocomposites demonstrate CTE as 536 &#215; 10 -6 K -1 while sBN nanocomposites exhibit 484 &#215; 10 -6 K -1 . This is 12 and 20% decrease in CTE of pBN and sBN nanocomposites in comparison to base PE. The physical entanglement of polymer chains induced by BN nanosheets and increased molecular interactions of silane functional groups with the PE matrix (Fig. <ref type="figure">2b</ref>) could explain this significant reduction in CTE compared to the pBN nanocomposites <ref type="bibr">[39]</ref>.</p><p>Thermal degradation was explored to further understand the thermal stability of polymer materials and the role of silane grafting. Analyzing the thermal decomposition of pBN and sBN nanocomposites (Fig. <ref type="figure">6a</ref>), it is evident that the degradation is a two-stage process, and the mechanism is not affected due to BN nanosheets addition. The addition of BN nanosheets increases the thermal stability of PE nanocomposites structures irrespective of functionalization. For example, the first onset temperature (T onset ) is shown in Fig. <ref type="figure">6c</ref>, where T onset indicates the starting of the 1st stage degradation of the materials. The result indicates that the decomposition process is delayed by adding BN nanosheets. T onset of base PE matrix exhibits 268 &#8226; C. By the addition of 1 wt % pBN nanosheets, T onset is increased by 12 &#8226; C. Further addition of pBN nanosheets (e.g., 5 wt %) does not enhance the thermal stability beyond PE-1.0 wt % pBN nanocomposites. This observation can be explained knowing that BN nanosheets can act as gas barriers and play a crucial role in increasing the thermal stability of nanocomposites <ref type="bibr">[40]</ref>. A well tortuous path created by BN nanosheets into PE matrix enhances thermal stability by delaying the escape of decomposed volatile gases <ref type="bibr">[41]</ref>. At the beginning of the degradation process (i.e., onset degradation), barrier nature of BN nanosheets obstructs volatile gas flow within the polymer matrix and results in delayed decomposition.</p><p>Likewise, the second onset temperature (T 20% ) (i.e., 20% weight loss temperature) where the materials start to degrade of its 2nd stage is also analyzed (Fig. <ref type="figure">6d</ref>). Interestingly, higher improvement (thermal degradation temperature) is achieved for thermal stability at 20% weight loss compared to T onset . For instance, the addition of 1 wt % pBN nanosheets increase T onset of nanocomposites by 12 &#8226; C while T 20% is improved by 18 &#8226; C. This may be explained by the formation of chars (Fig. <ref type="figure">6a</ref>), which likely act as volatile gas barriers <ref type="bibr">[40,</ref><ref type="bibr">42]</ref>. Thus, BN nanosheets, along with chars, delay the escaping of volatile gases and reduce the decomposition of PE matrix at T 20% . Interestingly, the PE-sBN nanocomposites do not show improvement in thermal weight loss over PE-pBN nanocomposites. Both T onset and T 20% show almost similar behavior and increment of 16 and 18 &#8226; C for T 20% for both sBN and pBN nanocomposites. This slight early degradation of sBN compared to pBN nanocomposites can be explained by the thermal degradation behavior of silane molecules. The thermal stability of sBN nanosheets (Fig. <ref type="figure">1i</ref>) indicates that the degradation of silane starts at ~250 &#8226; C <ref type="bibr">[43]</ref>. This early degradation of silane alters the polymer-BN nanosheets interface and triggers the degradation of sBN nanocomposites at a slightly lower temperature compared to pBN nanocomposites. Similar results were also reported by Xie et al. <ref type="bibr">[44,</ref><ref type="bibr">45]</ref> for thermal decomposition of long carbon-chain alkyl quaternary ammonium ions modified montmorillonite (MMT). The authors found that the weakly bonded water molecules were decomposed in the temperature region below 200 &#8226; C, which is the possible reason for the early degradation of the polymer nanocomposite materials. Although the thermal stability of sBN nanocomposites is comparable to pBN nanocomposites. Yet, both pBN and sBN nanosheets show a moderate improvement in thermal stability performance. Besides the fact that the mass barrier property of BN nanosheets plays a crucial role in reducing thermal degradation, high thermal stability, and nanostructured morphology of BN nanosheets are also believed to be the other important reasons for enhanced thermal stability.</p><p>Overall, the addition of BN nanosheets into PE polymers enables nanocomposites with enhanced mechanical, thermomechanical, and thermal properties. However, the extent of improvement closely depends on PE-BN nanosheets interfacial molecular interaction. In this work, silane functionalized BN nanosheets were used to enhance this interaction. We obtained higher mechanical properties (TMOE, FMOE, and tensile strengths), thermomechanical properties (storage modulus), and lower CTE compared to PE-pBN nanocomposites. Unlike other 2D materials, BN nanosheets and their polymer nanocomposites are electrically insulative <ref type="bibr">[1,</ref><ref type="bibr">[46]</ref><ref type="bibr">[47]</ref><ref type="bibr">[48]</ref>. These mechanically strong, thermally, and dimensionally stable nanocomposite materials are promising in applications ranging from insulation materials (e.g., cable insulation), thermal management (e.g., heat transfer equipment) to electronic devices (e. g., thermal interface materials) <ref type="bibr">[49]</ref><ref type="bibr">[50]</ref><ref type="bibr">[51]</ref>. While this study provides adequate insight on the role of silane functionalization groups, it would be interesting to study the effects of BN nanosheets over a broader range of BN nanosheets mass fraction to fully elucidate the silane functionalization effect on the properties of PE-BN nanocomposites.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head n="4.">Conclusions</head><p>In this work, the mechanical, thermomechanical, and thermal properties of PE polymer nanocomposites reinforced with silane functionalized and pristine boron nitrides were studied. Substantial improvements in the mechanical properties of PE-BN nanocomposites were achieved. In nanocomposites with 5 wt % pBN and sBN nanosheets, TMOE increased by 37, 42%, FMOE improved by 24, 30%, and tensile strength increased by 15, 27%, respectively. While thermal stability improvements are nominal (e.g., T 20% increased by 18, 16 &#8226; C for 1 wt % pBN and sBN nanosheets, respectively), the reductions in nanocomposites' CTE are compelling (e.g., pBN and sBN nanosheets reduce CTE by 12% and 20%, respectively). The chain mobility is also reduced because of the BN nanosheets addition, as evidenced from the increased storage modulus of pBN and sBN nanocomposites compared to PE. These enhancements in mechanical and thermal properties are likely originated not only from the outstanding mechanical, physical, thermal, and chemical properties of BN nanosheets, but also from the molecular interaction of silane modified BN nanosheets with base PE matrix.</p></div></body>
		</text>
</TEI>