Title: Annealing post-drawn polycaprolactone (PCL) nanofibers optimizes crystallinity and molecular alignment and enhances mechanical properties and drug release profiles
Post-drawn PCL nanofibers can be molecularly tuned to have a variety of mechanical properties and drug release profiles depending on the temperature and time of annealing, which has implications for regenerative medicine and drug delivery applications. Post-drawing polycaprolactone (PCL) nanofibers has previously been demonstrated to drastically increase their mechanical properties. Here the effects of annealing on post-drawn PCL nanofibers are characterized. It is shown that room temperature storage and in vivo temperatures increase crystallinity significantly on the order of weeks, and that high temperature annealing near melt significantly increases crystallinity and molecular orientation on the order of minutes. The kinetics of crystallization were assessed using an anneal and quench approach. High temperature annealing also increased the ultimate tensile strength and toughness of the fibers and changed the release profile of a model drug absorbed in PCL nanofibers from first-order to zero-order kinetics.  more » « less
Award ID(s):
1653329
PAR ID:
10333435
Author(s) / Creator(s):
; ; ; ;
Date Published:
Journal Name:
Materials Advances
Volume:
3
Issue:
7
ISSN:
2633-5409
Page Range / eLocation ID:
3303 to 3315
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. Abstract Forcespinning technique was used to fabricate sub-micron size polycaprolactone (PCL) fibers. Forcespinning method uses centrifugal forces for the generation of fibers unlike the electrospinning method which uses electrostatic force. PCL has been extensively used as scaffolds for cell regeneration, substrates for tissue engineering and in drug delivery systems. The aim of this study is to qualitatively analyze the force spun fiber mats and investigate the effect of the spinneret rotational speed on the fiber morphology, thermal and mechanical properties. The extracted fibers were characterized by scanning electron microscopy differential scanning calorimetry, tensile testing and dynamic mechanical analysis. The results showed that higher rotational speeds produced uniform fibers with less number of beads. The crystallinity of the fibers decreased with increase in rotational speeds. The Young’s modulus of the forcespun fibers was found to be in the range of 3.5 to 6 MPa. Storage and loss moduli decreased with the increase in the fiber diameter. The fibers collected at farther distance from spinneret exhibited optimal mechanical properties compared to the fibers collected at shorter distances. This study will aid in extracting fibers with uniform geometries and lower beads to achieve the desired nanofiber drug release properties. 
    more » « less
  2. null (Ed.)
    Purpose The purpose of this study is to understand how printing parameters and subsequent annealing impacts porosity and crystallinity of 3D printed polylactic acid (PLA) and how these structural characteristics impact the printed material’s tensile strength in various build directions. Design/methodology/approach Two experimental studies were used, and samples with a flat vs upright print orientation were compared. The first experiment investigates a scan of printing parameters and annealing times and temperatures above the cold crystallization temperature ( T cc ) for PLA. The second experiment investigates annealing above and below T cc at multiple points over 12 h. Findings Annealing above T cc does not significantly impact the porosity but it does increase crystallinity. The increase in crystallinity does not contribute to an increase in strength, suggesting that co-crystallization across the weld does not occur. Atomic force microscopy (AFM) images show that weld interfaces between printed fibers are still visible after annealing above T cc , confirming the lack of co-crystallization. Annealing below T cc does not significantly impact porosity or crystallinity. However, there is an increase in tensile strength. AFM images show that annealing below T cc reduces thermal stresses that form at the interfaces during printing and slightly “heals” the as-printed interface resulting in an increase in tensile strength. Originality/value While annealing has been explored in the literature, it is unclear how it affects porosity, crystallinity and thermal stresses in fused filament fabrication PLA and how those factors contribute to mechanical properties. This study explains how co-crystallization across weld interfaces is necessary for crystallinity to increase strength and uses AFM as a technique to observe morphology at the weld. 
    more » « less
  3. Abstract Poly(ε-caprolactone) (PCL) is one of the leading biocompatible and biodegradable polymers. However, the mechanical property of PCL is relatively poor as compared with that of polyolefins, which has limited the active applications of PCL as an industrial material. In this study, to enhance the mechanical property of PCL, cellulose nanofibers (C-NF) with high mechanical property, were employed as reinforcement materials for PCL. The C-NF were fabricated via the electrospinning of cellulose acetate (CA) followed by the subsequent saponification of the CA nanofibers. For the enhancement of the mechanical property of the PCL composite, the compatibility of C-NF and PCL was investigated: the surface modification of the C-NF was introduced by the ring-opening polymerization of the ε-caprolactone on the C-NF surface (C-NF-g-PCL). The polymerization was confirmed by the Fourier transform infrared (FTIR) spectroscopy. Tensile testing was performed to examine the mechanical properties of the C-NF/PCL and the C-NF-g-PCL/PCL. At the fiber concentration of 10 wt%, the Young’s modulus of PCL compounded with neat C-NF increased by 85% as compared with that of pure PCL, while, compounded with C-NF-g-PCL, the increase was 114%. The fracture surface of the composites was analyzed by scanning electron microscopy (SEM). From the SEM images, it was confirmed that the interfacial compatibility between PCL and C-NF was improved by the surface modification. The results demonstrated that the effective surface modification of C-NF contributed to the enhancement of the mechanical property of PCL. 
    more » « less
  4. The study delves into the kinetics of non-isothermal crystallization of Poly (ɛ-caprolactone) (PCL) and MgO-incorporated PCL nanofibers with varying cooling rates. Differential Scanning Calorimetry (DSC-3) was used to acquire crystallization information and investigate the kinetics behavior of the two types of nanofibers under different cooling rates ranging from 0.5–5 K/min. The results show that the crystallization rate decreases at higher crystallization temperatures. Furthermore, the parameters of non-isothermal crystallization kinetics were investigated via several mathematical models, including Jeziorny and Mo’s models. Mo’s approach was suitable to describe the nanofibers’ overall non-isothermal crystallization process. In addition, the Kissinger and Friedman methods were used to calculate the activation energy of bulk-PCL, PCL, and MgO-PCL nanofibers. The result showed that the activation energy of bulk-PCL was comparatively lower than that of nanofibers. The investigation of the kinetics of crystallization plays a crucial role in optimizing manufacturing processes and enhancing the overall performance of nanofibers. 
    more » « less
  5. This paper reports the molecular organization and mechanical properties of electrospun, post-drawn polyacrylonitrile (PAN) nanofibers. Without post-drawing, the polymer chain was kinked and oriented in hexagonal crystalline structures. Immediate post-drawing in the semi-solid state disrupted the crystal structures and chain kink at maximum draw ratio. Structural re-orientation at maximum draw resulted in a 500% increase in Young's modulus and a 100% increase in ultimate tensile strength. By applying post-drawing to electrospinning it may be possible to obtain PAN fibers and PAN-derived carbon fibers with enhanced mechanical properties compared to available fabrication technologies. 