Spider silk is biocompatible, biodegradable, and rivals some of the best synthetic materials in terms of strength and toughness. Despite extensive research, comprehensive experimental evidence of the formation and morphology of its internal structure is still limited and controversially discussed. Here, we report the complete mechanical decomposition of natural silk fibers from the golden silk orb-weaver Trichonephila clavipes into ≈10 nm-diameter nanofibrils, the material's apparent fundamental building blocks. Furthermore, we produced nanofibrils of virtually identical morphology by triggering an intrinsic self-assembly mechanism of the silk proteins. Independent physico-chemical fibrillation triggers were revealed, enabling fiber assembly from stored precursors “at-will”. This knowledge furthers the understanding of this exceptional material's fundamentals, and ultimately, leads toward the realization of silk-based high-performance materials.
more »
« less
Multi‐Point Nanoindentation Method to Determine Mechanical Anisotropy in Nanofibrillar Thin Films
Abstract Biomaterials with outstanding mechanical properties, including spider silk, wood, and cartilage, often feature an oriented nanofibrillar structure. The orientation of nanofibrils gives rise to a significant mechanical anisotropy, which is extremely challenging to characterize, especially for microscopically small or inhomogeneous samples. Here, a technique utilizing atomic force microscope indentation at multiple points combined with finite element analysis to sample the mechanical anisotropy of a thin film in a microscopically small area is reported. The system studied here is the tape‐like silk of the Chilean recluse spider, which entirely consists of strictly oriented nanofibrils giving rise to a large mechanical anisotropy. The most detailed directional nanoscale structure–property characterization of spider silk to date is presented, revealing the tensile and transverse elastic moduli as 9 and 1 GPa, respectively, and the binding strength between silk nanofibrils as 159±13 MPa. Furthermore, based on this binding strength, the nanofibrils’ surface energy is derived as 37 mJ m−2, and concludes that van der Waals forces play a decisive role in interfibrillar binding. Due to its versatility, this technique has many potential applications, including early disease diagnostics, as underlying pathological conditions can alter the local mechanical properties of tissues.
more »
« less
- PAR ID:
- 10369147
- Publisher / Repository:
- Wiley Blackwell (John Wiley & Sons)
- Date Published:
- Journal Name:
- Small
- Volume:
- 18
- Issue:
- 30
- ISSN:
- 1613-6810
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
Abstract Cribellate silks, produced by ancient spiders, are fascinating because they feature a highly sophisticated, 3D hierarchical structure consisting of filaments with different diameters and shapes. Here, the smallest and thinnest constituents of the cribellate silk are investigated: nanofibrils that form a dense mesh that is supported by larger fibers. Analysis of their structure via atomic force and transmission electron microscopies shows that they are flattened fibrils, only ≈5 nm thick — thinner than any other natural spider silk fibrils previously reported. In this work, the first mechanical tensile testing experiments on these fibrils are carried out, which reveals that the fibrils show an outstanding extensibility of at least 1100%, almost twice as much as the most stretchable spider silk previously reported. Based on these extraordinary findings, this work significantly expands the parameter space of materials properties attainable by spider silks and provides further insights into their nanomechanics.more » « less
-
null (Ed.)The spider major ampullate (MA) silk exhibits high tensile strength and extensibility and is typically a blend of MaSp1 and MaSp2 proteins with the latter comprising glycine–proline–glycine–glycine-X repeating motifs that promote extensibility and supercontraction. The MA silk from Darwin's bark spider ( Caerostris darwini ) is estimated to be two to three times tougher than the MA silk from other spider species. Previous research suggests that a unique MaSp4 protein incorporates proline into a novel glycine–proline–glycine–proline motif and may explain C. darwini MA silk's extraordinary toughness. However, no direct correlation has been made between the silk's molecular structure and its mechanical properties for C. darwini . Here, we correlate the relative protein secondary structure composition of MA silk from C. darwini and four other spider species with mechanical properties before and after supercontraction to understand the effect of the additional MaSp4 protein. Our results demonstrate that C. darwini MA silk possesses a unique protein composition with a lower ratio of helices (31%) and β-sheets (20%) than other species. Before supercontraction, toughness, modulus and tensile strength correlate with percentages of β-sheets, unordered or random coiled regions and β-turns. However, after supercontraction, only modulus and strain at break correlate with percentages of β-sheets and β-turns. Our study highlights that additional information including crystal size and crystal and chain orientation is necessary to build a complete structure–property correlation model.more » « less
-
Abstract Nanofibrils play a pivotal role in spider silk and are responsible for many of the impressive properties of this unique natural material. However, little is known about the internal structure of these protein fibrils. We carry out polarized Raman and polarized Fourier-transform infrared spectroscopies on native spider silk nanofibrils and determine the concentrations of six distinct protein secondary structures, including β-sheets, and two types of helical structures, for which we also determine orientation distributions. Our advancements in peak assignments are in full agreement with the published silk vibrational spectroscopy literature. We further corroborate our findings with X-ray diffraction and magic-angle spinning nuclear magnetic resonance experiments. Based on the latter and on polypeptide Raman spectra, we assess the role of key amino acids in different secondary structures. For the recluse spider we develop a highly detailed structural model, featuring seven levels of structural hierarchy. The approaches we develop are directly applicable to other proteinaceous materials.more » « less
-
Abstract Spider dragline silk is known for its exceptional strength and toughness; hence understanding the link between its primary sequence and mechanics is crucial. Here, we establish a deep-learning framework to clarify this link in dragline silk. The method utilizes sequence and mechanical property data of dragline spider silk as well as enriching descriptors such as residue-level mobility (B-factor) predictions. Our sequence representation captures the relative position, repetitiveness, as well as descriptors of amino acids that serve to physically enrich the model. We obtain high Pearson correlation coefficients (0.76–0.88) for strength, toughness, and other properties, which show that our B-factor based representation outperforms pure sequence-based models or models that use other descriptors. We prove the utility of our framework by identifying influential motifs and demonstrating how the B-factor serves to pinpoint potential mutations that improve strength and toughness, thereby establishing a validated, predictive, and interpretable sequence model for designing tailored biomaterials.more » « less