<?xml-model href='http://www.tei-c.org/release/xml/tei/custom/schema/relaxng/tei_all.rng' schematypens='http://relaxng.org/ns/structure/1.0'?><TEI xmlns="http://www.tei-c.org/ns/1.0">
	<teiHeader>
		<fileDesc>
			<titleStmt><title level='a'>Reversible Electrochemical Anionic Redox in Rechargeable Multivalent-Ion Batteries</title></titleStmt>
			<publicationStmt>
				<publisher>American Chemical Society</publisher>
				<date>07/13/2023</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10495759</idno>
					<idno type="doi">10.1021/jacs.3c02542</idno>
					<title level='j'>Journal of the American Chemical Society</title>
<idno>0002-7863</idno>
<biblScope unit="volume">145</biblScope>
<biblScope unit="issue">29</biblScope>					

					<author>Ankur L. Jadhav</author><author>Taylor R. Juran</author><author>Matthew A. Kim</author><author>Andrea M. Bruck</author><author>Brendan E. Hawkins</author><author>Joshua W. Gallaway</author><author>Manuel Smeu</author><author>Robert J. Messinger</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[Rechargeable multivalent-ion batteries are of significant interest due to the high specific capacities and earth abundance of their metal anodes, though few cathode materials permit multivalent ions to electrochemically intercalate within them. The crystalline chevrel phases are among the few cathode materials known to reversibly intercalate multivalent cations. However, to date, no multivalent-ion intercalation electrodes can match their reversibility and stability, in part due to the lack of design rules that guide how ion intercalation and electron charge transfer are coupled up from the atomic scale. Here, we elucidate the electronic charge storage mechanism that occurs in chevrel phase (Mo 6 Se 8 , Mo 6 S 8 ) electrodes upon the electrochemical intercalation of multivalent cations (Al 3+ , Zn 2+ ), using solid-state nuclear magnetic resonance spectroscopy, synchrotron X-ray absorption near edge structure measurements, operando synchrotron diffraction, and density functional theory calculations. Upon cation intercalation, electrons are transferred selectively to the anionic chalcogen framework, while the transition metal octahedra are redox inactive. This reversible electrochemical anionic redox, which occurs without breaking or forming chemical bonds, is a fundamentally different charge storage mechanism than that occurring in most transition metal-containing intercalation electrodes using anionic redox to enhance energy density. The results suggest material design principles aimed at realizing new intercalation electrodes that enable the facile electrochemical intercalation of multivalent cations.]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; INTRODUCTION</head><p>Lithium-ion batteries revolutionized portable electronics, but critical improvements are required in energy density, cycle life, safety, and cost to electrify transportation and integrate renewable energy sources into the electric grid on a global scale. <ref type="bibr">[1]</ref><ref type="bibr">[2]</ref><ref type="bibr">[3]</ref> Batteries that use multivalent cations (e.g., Mg 2+ , Ca 2+ , Zn <ref type="bibr">2+</ref> , and Al 3+ ) as the electroactive species transfer multiple electrons per ion, resulting in high specific capacities. <ref type="bibr">3,</ref><ref type="bibr">4</ref> Their corresponding metal anodes (Mg, Ca, Zn, and Al) are earth-abundant, low-cost, energy-dense metals, some of which are intrinsically safe (Zn, Al). <ref type="bibr">5</ref> Unlike lithium cations, the electrodeposition of multivalent cations is often relatively uniform, mitigating dendrite formation. <ref type="bibr">2,</ref><ref type="bibr">6</ref> Due to their smaller size compared to monovalent ions, multivalention intercalation into crystalline compounds results in minimal volume expansion, a key factor in long-cycle life batteries. <ref type="bibr">7</ref> However, reversible multivalent-ion intercalation into crystalline electrode materials is challenging due to high ionic charge densities, resulting in slow solid-state ionic diffusion within the host crystal structure. <ref type="bibr">[8]</ref><ref type="bibr">[9]</ref><ref type="bibr">[10]</ref><ref type="bibr">[11]</ref><ref type="bibr">[12]</ref> Furthermore, desolvation of these highly charged ions adds higher energetic penalties at the electrode-electrolyte interface, requiring unique ion-solvent coordination structures that have thus far limited the number of compatible electrolytes for multivalent-ion battery systems. <ref type="bibr">3,</ref><ref type="bibr">5</ref> Widespread use of multivalent battery chemistry has remained elusive, in part due to limited understanding and control of the complex electronic, chemical, and structural changes that the electrodes and their interfaces undergo upon ion intercalation.</p><p>The chevrel phases Mo 6 X 8 (X = S, Se, or Te) are among the few materials known to electrochemically intercalate divalent (e.g., Mg 2+ , Zn 2+ , etc.) <ref type="bibr">6,</ref><ref type="bibr">12</ref> and trivalent (Al 3+ ) cations. <ref type="bibr">8,</ref><ref type="bibr">[13]</ref><ref type="bibr">[14]</ref><ref type="bibr">[15]</ref> Discovered by Chevrel in 1971 <ref type="bibr">16</ref> and introduced by Aurbach et al. <ref type="bibr">6</ref> in 2000 as a positive electrode material for magnesium batteries, chevrel Mo 6 S 8 has since acted as the quintessential Mg-ion intercalation electrode. The remarkable chevrel unit cell is composed of a Mo 6 octahedron caged within an X 8 chalcogen cube, which crystallizes into a structure with large cavities and an electronically polarizable framework that enables fast ion diffusion. <ref type="bibr">17,</ref><ref type="bibr">18</ref> Other unique chalcogen clusters have been reported that can electrochemically intercalate cations; for example, organometallic rhenium(III) chalcogenide clusters [Re 6 Q 8 (Q = S, Se)] have also been synthesized and have successfully shown lithium cation insertion. <ref type="bibr">19,</ref><ref type="bibr">20</ref> While numerous studies have investigated ion intercalation mechanisms into chevrel-phase electrodes and their structural ramifications over the last two decades, particularly for Mg 2+ cations, the electron charge transfer process is not well understood. The few studies investigating the electron charge transfer mechanism in Mg-Mo 6 S 8 batteries have reported conflicting results. Using X-ray photoelectron spectroscopy, Richard et al. <ref type="bibr">21</ref> reported that the additional electronic charge upon Mg 2+ cation intercalation is distributed over both the Mo 6 clusters and S 8 (i.e., chalcogen) cubes in a two-step charge transfer process. On the contrary, Thole et al. <ref type="bibr">22</ref> and Wan et al. <ref type="bibr">23</ref> studied the charge transfer process theoretically and using ex situ X-ray absorption near edge structure (XANES) measurements, indicating that only the sulfur framework takes part in the electron charge transfer upon Mg 2+ insertion. <ref type="bibr">19,</ref><ref type="bibr">20</ref> A decisive understanding of the electron charge transfer and storage mechanism is a missing link, one that could help researchers better understand why the chevrel phase remains the dominant intercalation electrode for multivalent ions batteries while leading to material design principles aimed at new multivalent intercalation electrodes with improved electrochemical properties. Furthermore, regarding the ion charge storage mechanism, it has been shown that multivalent ions intercalate into chevrel Mo 6 S 8 differently depending on their charge density, as shown for Mg 2+ ions <ref type="bibr">15,</ref><ref type="bibr">24,</ref><ref type="bibr">25</ref> and Al 3+ ions, <ref type="bibr">15,</ref><ref type="bibr">24,</ref><ref type="bibr">25</ref> though the consequences on the electron charge storage mechanism remain unclear.</p><p>In parallel, researchers have been striving to increase the energy density of Li-ion battery cathodes by leveraging anionic redox, particularly in lithium-rich transition metal oxides and chalcogenides. In most traditional Li-ion batteries using transition metal oxides (e.g., NMC) as electrode materials, the electrons are stored and distributed over the d-orbitals of the transition metals, which are redox active. <ref type="bibr">26</ref> However, oxygen anionic redox has been the subject of intense investigation, which has been observed at higher potentials in Li or Na-rich transition metal oxides such as Li-rich NMC (Li 1+x Ni y Co z Mn (1-x-y-z) O 2 ) and Ru-containing layered oxide compounds (Li 2 Ru 1-y Sn y O 3 ). <ref type="bibr">[27]</ref><ref type="bibr">[28]</ref><ref type="bibr">[29]</ref><ref type="bibr">[30]</ref> This electrochemical anionic redox enhances the energy density due to additional specific capacity at higher voltage; however, oxygen anionic redox typically leads to structural instabilities and side reactions that result in capacity fade. Interestingly, anionic redox has been demonstrated in lithium-rich chalcogenides, including lithium-rich titanium sulfides (LiTiS 2 -Li 2 TiS 3 family), <ref type="bibr">31</ref> lithium-rich iron sulfides Li 2 FeS 2 and LiNaFeS 2 , <ref type="bibr">32</ref> and the solid solution Li 2 FeS 2-y Se y . <ref type="bibr">33</ref> These electrode systems function by coupling the cationic redox of the transition metals with the anionic redox of the chalcogen atoms. Notably, all of the above materials contain an excess of lithium, where transition metal redox activity alone is not sufficient to charge balance the excess Li inserted. Thus, researchers have been searching for unique electron storage mechanisms, including anionic redox processes, that can be used in rechargeable battery electrodes to enhance energy density without affecting electrode stability and electrochemical reversibility.</p><p>Here, we elucidate that chevrel-phase electrodes undergo reversible electrochemical anionic redox upon the intercalation of multivalent cations, which occurs without breaking or forming chemical bonds. While the chalcogen framework is redox active, the transition metal octahedra are redox inactive. We study trivalent Al 3+ cation intercalation into chevrel Mo 6 Se 8 for the first time using electrochemical, spectroscopic, diffraction, and computational methods, comparing its electrochemical, structural, and electronic properties to chevrel Mo 6 S 8 . The anionic electron charge transfer mechanism is shown to be general, occurring also for divalent Zn 2+ cation intercalation into chevrel Mo 6 Se 8 . The results suggest that anionic redox may be incorporated as a molecular-level material design principles aimed at realizing new multivalention battery intercalation electrodes with enhanced ion intercalation and diffusion properties.  <ref type="bibr">34</ref> In a typical synthesis, 1.2 g of molybdenum powder (Mo, Alfa Aesar, 99.9%), 0.8 g of copper sulfide or 1.18 g of copper selenide (CuS/CuSe, Alfa Aesar, 99.9%), and 2.0 g of molybdenum disulfide or 3.17 g of molybdenum diselenide (MoS 2 / MoSe 2 , Alfa Aesar, 99.9%) were ball-milled for 3 h. The solid mixture was then placed in a tube furnace at 1000 &#176;C for 7 h under an ultrahigh purity argon atmosphere to form crystalline Cu 2 Mo 6 X 8 (X = Se, Se). The solid powder of Cu 2 Mo 6 X 8 was then mixed with a 6 M HCl solution for 8 h at room temperature under constant air bubbling, which leaches the copper into solution, forming crystalline Mo 6 S 8 or Mo 6 Se 8 . The resulting precipitate was filtered from the solution, rinsed twice with ethanol and once with water, and then dried under vacuum at 90 &#176;C overnight.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; METHODS</head><p>Composite Electrode Preparation. To prepare the chevrelphase composite electrode, chevrel (80 wt. % of the composite electrode) and carbon black (10 wt. %) (Super P, Alfa Aesar, 99%) were ball-milled in the glovebox for 1 h. In a glass vial, polyvinylidene fluoride (PVDF, Sigma-Aldrich, average molecular weight 534,000 g/ mol) binder (10 wt. %) was dissolved in N-methyl-2-pyrrolidone (NMP), and the ball-milled chevrel-carbon mixture was added to the solution. The mixture was ultra-sonicated for 30 s and mixed well to form an electrode slurry, which was then cast on Mo foil (Alfa Aesar, 99.95%, 0.025-mm thick, used for Al-chevrel cells) or stainless-steel foil (McMaster-Carr, 0.1-mm thick, used for Zn-chevrel cells) using an MTI film coater and doctor blade. The casted sheet was dried in a vacuum oven at 120 &#176;C overnight to evaporate the NMP solvent. The final electrode thickness was ca. 120 &#956;m.</p><p>Electrochemical Cell Assembly. Rechargeable Al-chevrel cells were constructed in an argon-filled glovebox (&lt;1 ppm O 2 and H 2 O). Polytetrafluorethylene (PTFE) Swagelok unions with a diameter of either 1/4-in or 1/2-in were used to assemble airtight cells. Molybdenum rods were used as current collectors for both electrodes. Aluminum foil (MTI, 99.99%, 0.1-mm thick) was used as an anode. Circular electrodes of 6-mm or 11-mm diameter were used in 1/4-in or 1/2-in Swagelok cells, respectively. A glass microfiber filter (GF/D, Whatman) was used as a separator. Aluminum chloride:1-ethyl-3methylimidazolium chloride (Iolitec, AlCl 3 :[EMIm]Cl, molar ratio 1.5:1) ionic liquid was used as an electrolyte (40 &#956;L or 120 &#956;L for 1/ 4-in or 1/2-in Swagelok cells, respectively). The electrodes, separator, and electrolyte were compressed by the current collector rods on both sides. Rechargeable Zn-chevrel cells were assembled using a similar process, except: (i) zinc foil (Alfa-Aesar, 99.98%, 0.25-mm thick) was used as the anode, (ii) 1 M aqueous Zn(SO 4 ) 2 solution was used as the electrolyte, (iii) the composite chevrel electrodes were cast on stainless steel, while stainless steel current collector rods were used with PTFE Swagelok unions.</p><p>Electrochemical Measurements. Galvanostatic cycling and cyclic voltammetry (CV) were performed on an Arbin LBT battery tester and Metrohm Autolab potentiostat (PGSTAT302N), respectively. The higher temperature (50 &#176;C) electrochemical measure-ments were performed in a Thermo Scientific Heratherm Oven. For Al-Mo 6 Se 8 and Zn-Mo 6 Se 8 batteries, the upper cut-off potentials were 1.20 and 0.80 V, respectively, while the lower cut-off potentials were 0.05 and 0.30 V. For CV experiments, a scan rate of 20 &#956;V/s or 50 &#956;V/s was used for Al-chevrel or Zn-chevrel cells, respectively.</p><p>Sample Preparation for NMR Spectroscopy. All Al-chevrel cells were disassembled inside an argon-filled glovebox (&lt;1 ppm O 2 and H 2 O). The Al-chevrel electrodes were rinsed three times in anhydrous methanol and dried in the glovebox. The samples were then stripped from the current collector foil, crushed using a mortar and pestle, and packed into a 1.6-mm diameter zirconia rotor inside the glovebox. All Zn-chevrel cells were disassembled under ambient conditions. The Zn chevrel electrodes were rinsed three times with deionized water, dried under vacuum at 60 &#176;C, and then packed within the 1.6-mm zirconia rotors.</p><p>Solid-State NMR Spectroscopy. Solid-state <ref type="bibr">77</ref> Se, <ref type="bibr">95</ref> Mo, and <ref type="bibr">27</ref> Al nuclear magnetic resonance (NMR) spectra were acquired on a Bruker AVANCE III HD 600 MHz NMR spectrometer with a 14.1 T narrow-bore superconducting magnet operating at 114.45, 39.11, and 156.39 MHz, respectively. A PhoenixNMR 1.6-mm HXY magic-anglespinning (MAS) probehead was used, where samples were rotated at MAS rates of 20 kHz. For 95 Mo measurements, a separate low-gamma accessory was used to tune to the 95 Mo frequency. Air at a temperature of 293.2 K was pumped through the probehead at 600 L/ h to mitigate sample heating due to MAS. <ref type="bibr">77</ref> Se, <ref type="bibr">95</ref> Mo, and <ref type="bibr">27</ref> Al shifts were referenced to selenous acid (H 2 SeO 3 , Alfa Aesar, 97%) at 1290 ppm, 2 M aqueous Na 2 MoO 4 (Sigma-Aldrich, 99%) at 0 ppm, and 1 M aqueous Al(NO 3 ) 3 (Sigma-Aldrich, 99.997%) at 0 ppm, respectively.</p><p>For solid-state <ref type="bibr">77</ref> Se and 95 Mo NMR spectra, spin-echo experiments were acquired to minimize acoustic ring-down effects. Solid-state <ref type="bibr">77</ref> Se spin-echo experiments were acquired using an initial short rf pulse of 1.2 &#956;s with a 52.1 kHz rf field strength to excite the broad <ref type="bibr">77</ref> Se spectral range of Mo 6 Se 8 . Solid-state 95 Mo spin-echo NMR experiments were conducted with a &#960;/2 pulse of 5 &#956;s, calibrated with respect to 2 M aqueous Na 2 MoO 4 (&#960;/2 pulse of 5 &#956;s, 50 kHz rf field strength). Solid-state <ref type="bibr">27</ref> Al single-pulse experiments were conducted using a short &#960;/12 pulse of 0.31 &#956;s, calibrated with respect to 1 M aqueous Al(NO 3 ) 3 (&#960;/2 pulse of 1.9 &#956;s, 125 kHz rf field strength). Recycle delays of 0.05, 0.01, and 0.01 s were used for <ref type="bibr">77</ref> Se, <ref type="bibr">95</ref> Mo, and 27 Al NMR experiments, during which all spins relaxed to thermal equilibrium (d 1 &gt; 5*T 1 ). Spectra were deconvoluted using the DMFit program. <ref type="bibr">35</ref> DFT Calculations. Density functional theory (DFT) calculations were carried out with the Vienna Ab initio Simulation Package (VASP), <ref type="bibr">[36]</ref><ref type="bibr">[37]</ref><ref type="bibr">[38]</ref> utilizing the projector-augmented-wave (PAW) method <ref type="bibr">39</ref> and the SCAN functional. <ref type="bibr">40</ref> The energy sufficiently converged to &lt;1 meV/atom for the AlMo 6 X 8 unit cell, where X = S, Se, when setting the kinetic energy cutoff to 650 eV and the &#915;-centered k-mesh to 5 &#215; 5 &#215; 5. For computational efficiency, this criterion was reduced for the 2 &#215; 2 &#215; 2 supercells; an energy cutoff of 450 eV and &#915;centered k-mesh of 1 &#215; 1 &#215; 1 was determined to be adequate. Spin polarization was not included in our calculations, as it was determined to not be necessary in our previous DFT study of chevrel Mo 6 S 8 electrodes. <ref type="bibr">14</ref> Full structural and ionic relaxations were performed for bulk Al metal and Al M Mo 6 X 8&#8242; , where X = S, Se and M = 0 to 4/3. All chevrel phase structures are based on the MgMo 6 Se 8 as studied by Levi et al., <ref type="bibr">17,</ref><ref type="bibr">41</ref> changing only the type of chalcogen or intercalant, not the position. For a battery consisting of a pure Al metal anode and a chevrel-phase cathode, the full cell electrochemical reaction is described by</p><p>From the electronic structure calculations, the voltage can be calculated as the difference in total energies between the products and the reactants, normalized by the number of electrons transferred, according to</p><p>where E(AlMo 6 X 8 ) is the energy of the intercalated chevrel-phase cathode, E(Mo 6 X 8 ) is the energy of the empty chevrel-phase cathode, E(Al) is the energy per atom of the Al metal anode, and N electrons is the number of electrons transferred with the cation. <ref type="bibr">42</ref> Note that the voltage calculated by eq 2 is an approximation. The exact voltage calculation is dependent upon the Gibbs free energy rather than the change in internal energy. However, including changes in volume and entropy would result in a less than 0.1 V correction from the approach used here; therefore, the impact of doing so is negligible. <ref type="bibr">43</ref> Voltage profiles were calculated by expanding the unit cell to a 2 &#215; 2 &#215; 2 supercell. We performed a full ionic and structural relaxation for each of the possible Al M Mo 6 X 8 configurations; the lowest energy structure was taken as the preferred configuration. Voltages were calculated according to eq 2, though here we compare the energy of the structure to the energy of the relaxed structure with one less intercalated Al ion [e.g., with n ions vs (n -1) Al ions].</p><p>EDXRD. Operando synchrotron energy dispersive X-ray diffraction (EDXRD) measurements were performed at beamline 6-BM-A at the Advanced Photon Source (APS) at Argonne National Laboratory. Diffraction data were collected on hermetically sealed gold-plated stainless-steel CR2032 coin cells without transparent windows or other modifications. This setup was possible because the incident white beam had an energy range from approximately 20-200 keV, sufficient to penetrate the cell. For this reason, there was no opportunity for oxidation or contamination of the chevrel electrode during extraction from the cell. Crystallographic data for Al-ion and Zn-ion batteries with both Mo 6 S 8 and Mo 6 Se 8 electrodes were collected as the cells were discharged on a low-profile hotplate at 60 &#176;C. A MACCOR battery cycler was used to cycle the batteries at C/ 10.7 (12 mA/g) during EDXRD measurements at a constant angle of 2&#952; = 3&#176;. The diffracted beam intensity was measured using a highresolution germanium detector, while calibration from the detector channel to photon energy was performed using an &#945;-Al 2 O 3 standard. The diffraction gauge volume was 40 &#956;m tall. The chevrel electrodes were profiled spatially; however, no inhomogeneity in the electrochemical intercalation reaction was observed in any cell. Thus, the data were taken from the centers of the electrode, which was representative of the cell. The data collection time per diffraction pattern was 60 s. EDXRD data are reported as a function of photon energy in keV, which can be converted to d-spacing by Bragg's law</p><p>where E is photon energy, &#952; EDXRD is the diffraction angle, h is Planck's constant, and c is the speed of light. XANES. Synchrotron XANES measurements were performed at NSLS-II beamline 7-BM (QAS). All measurements were performed in fluorescence mode, scanning the Mo K-edge.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; RESULTS AND DISCUSSION</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>Electrochemical Al 3+ Ion Intercalation into Chevrel</head><p>Phase Electrodes. To experimentally measure the electron charge transfer to chevrel phase frameworks, we first electrochemically intercalated trivalent Al 3+ cations into chevrel Mo 6 Se 8 . The selenium chalcogen frameworks enable solid-state <ref type="bibr">77</ref> Se NMR measurements, which are highly sensitive to the local electronic environments of the Se 8 cubes. Note that solid-state <ref type="bibr">33</ref> S NMR is challenging due to the very low natural abundance (0.76%), low gyromagnetic ratio (Larmor frequency of 46.08 MHz at 14.1 T), and quadrupolar nature (spin = 3/2) of 33 S nuclear spins. Solid-state <ref type="bibr">77</ref> Se is more sensitive due to its higher natural abundance (7.63%), higher gyromagnetic ratio (Larmor frequency of 114.48 MHz at 14.1 T), and non-quadrupolar nature (spin = 1/2).</p><p>We thus prepared rechargeable Al-Mo 6 Se 8 cells for the first time, analyzed their electrochemical properties, and compared them to Al-Mo 6 S 8 cells (Figures <ref type="figure">1</ref> and<ref type="figure">S1</ref>). Galvanostatic cycling shows two distinct discharge plateaus where theoretical capacities of 88 and 128 mA h/g were achieved upon the second discharge for Mo 6 Se 8 and Mo 6 S 8 electrodes, respectively, corresponding to four electron transfers per Mo 6 X 8 unit (Figure <ref type="figure">1a</ref>). Additional capacities observed during the first cycles are associated with decomposition of the ionic liquid electrolyte and the formation of a surface layer upon desolvation of Al 3+ from the chloroaluminate anions. <ref type="bibr">8,</ref><ref type="bibr">13,</ref><ref type="bibr">15</ref> Al 3+ cations electrochemically intercalate into Mo 6 Se 8 at lower potentials compared to Mo 6 S 8 , consistent with our DFT calculations described below, as well as Levi and Aurbach's work on Mg 2+ cation intercalation into Mo 6 Se 8 and Mo 6 S 8 electrodes. <ref type="bibr">18,</ref><ref type="bibr">44</ref> CV reveals two distinct reduction peaks (0.34 and 0.25 V) for Mo 6 Se 8 as opposed to three peaks for Mo 6 S 8 (0.48, 0.38, and 0.33 V) (Figure <ref type="figure">1b</ref>), all of which are due to Al 3+ intercalation into the chevrel electrode.</p><p>Using quantitative solid-state <ref type="bibr">27</ref> Al NMR measurements, we previously established that Al 3+ cations intercalate "simultaneously" into cavities 1 and 2 of chevrel Mo 6 S 8 , <ref type="bibr">15</ref> as opposed to sequentially as observed for Mg 2+ cations, <ref type="bibr">25</ref> consistent with XRD analyses of Geng et al. <ref type="bibr">24</ref> Al 3+ cations intercalate into cavity 1, but due to strong Coulombic repulsions among them, the ions "hop" into cavity 2 before cavity 1 is filled. This movement of ions is due to strong cation-cation repulsion and results in an additional CV peak with reduced overpotential, as discussed previously. <ref type="bibr">15</ref> However, in chevrel Mo 6 Se 8 , only two CV reduction peaks are observed, while the length of the first galvanostatic discharge plateau is &#8764;75% of the total specific capacity, suggesting that Al 3+ cations intercalate sequentially into cavities 1 and 2 during the first and second discharge plateaus, respectively. This Al-ion intercalation mechanism is consistent with reduced cation-cation repulsions among intercalated Al 3+ cations, which are screened by the larger Se atoms, as well as the more facile diffusion of Al 3+ cations within the chevrel Mo 6 Se 8 . In addition, the potential differences &#916;E between the first CV reduction peak (0.34 V) and its corresponding coupled oxidation peak (0.47 V) are much less in Mo 6 Se 8 (0.13 V) compared to Mo 6 S 8 (0.22 V), further suggesting a lower activation barrier for ion diffusion.</p><p>To measure the solid-state diffusion of Al 3+ cations within the chevrel frameworks and the equilibrium potentials at which intercalation occurs, galvanostatic intermittent titration technique (GITT) measurements were performed on Al-Mo 6 Se 8 and Al-Mo 6 S 8 cells (Figure <ref type="figure">1c</ref>). Al 3+ cation diffusion coefficients during the first discharge plateau, which occurs at an equlibrium potential of 0.60 V for Mo 6 S 8 and 0.40 V for Mo 6 Se 8 , were on the order of 10 -19 and 10 -17 cm 2 /s, respectively (Text S1, Supporting Information). Al 3+ cation diffusion within Mo 6 Se 8 is approximately two orders-ofmagnitude faster compared to Mo 6 S 8 during the first discharge voltage plateau. Faster cation diffusion is attributed to (i) the higher electronic polarizability of the anionic selenium framework <ref type="bibr">18</ref> and (ii) the larger size of Se, which reduces cation-cation interactions between intercalated Al 3+ and the Mo 6 octahedra, resulting in lower activation energies for ion hopping between cavities. Note that a similar trend has also been observed in other transition metal chalcogenides, such as the magnesium spinels MgX 2 Z 4 (Z = S, Se; X = In, Y, Sc) <ref type="bibr">45</ref> and the rare earth spinels MgLn 2 X 4 (Ln = lanthanide; X = S, Se), <ref type="bibr">46</ref> where the higher electronic polarizability of the chalcogen network reduces the activation energy for cation migration. <ref type="bibr">47</ref> The thermodynamic intercalation potentials computed using strongly constrained and appropriately normed semilocal (SCAN) density functionals <ref type="bibr">40</ref> (Figure <ref type="figure">1c</ref>) match well with the experimental potentials. Note that the DFT-predicted voltage represents the average potentials for Al intercalation, resulting in the step-like nature of the calculated voltage curve.</p><p>Electron Charge Transfer Mechanism. Solid-state NMR spectroscopy is highly sensitive to electronic environments at the atomic scale; thus, the electrochemical reduction of the chevrel framework, i.e., the addition of electrons required to charge balance Al 3+ cation insertion, is expected to result in observable NMR shifts. To measure changes in the electronic structure of the chevrel framework, solid-state <ref type="bibr">77</ref> Se and 95 Mo NMR spectra were acquired on pristine Mo 6 Se 8 and electrochemically discharged Al 4/3 Mo 6 Se 8 electrodes. Solidstate <ref type="bibr">77</ref> Se MAS NMR measurements performed on pristine Mo 6 Se 8 revealed two Knight-shifted <ref type="bibr">48,</ref><ref type="bibr">49</ref>  <ref type="bibr">77</ref> Se signals with isotropic shifts of 3565 and 2739 ppm and broad spinningside-band manifolds (Figure <ref type="figure">2a</ref>). Spectral deconvolutions of both the <ref type="bibr">77</ref> Se MAS and static NMR spectra (Figure <ref type="figure">2b</ref>) enabled the relative populations of selenium atoms in each site to be quantified and their <ref type="bibr">77</ref> Se NMR parameters to be determined, including isotropic shifts and shift anisotropy tensorial parameters associated with the atomic-level electronic environment (Table <ref type="table">S1</ref>), enabling <ref type="bibr">77</ref> Se signal assignments. The 77 Se signal with an isotropic shift of 3565 ppm is attributed to selenium atoms in the six "peripheral" 4-coordinated Se 1 crystallographic sites, consistent with their 75% relative population and anisotropy (asymmetry parameter &#951; of 0.75). The <ref type="bibr">77</ref> Se signal with an isotropic shift at 2739 ppm corresponds to selenium atoms in the two "axial" 3coordinated Se 2 crystallographic sites, consistent with their 25% population and axial asymmetry (&#951; of 0). <ref type="bibr">50,</ref><ref type="bibr">51</ref> The large 77 Se NMR shifts and anisotropies are dominated by NMR Knight shift effects, which are observed due to the metallic nature of the chevrel phase <ref type="bibr">44,</ref><ref type="bibr">48,</ref><ref type="bibr">50</ref> and arise from hyperfine couplings between electron spins in the conduction band and nuclear spins. The Knight shift K is described by</p><p>where &#967; p is the Pauli spin susceptibility per atom and P F is the average value of the s-electron probability density at the Fermi energy E F . <ref type="bibr">48,</ref><ref type="bibr">50</ref> Nuclear spins are thus indirect probes of electron spin density within the conduction band. <ref type="bibr">50</ref> Consequently, the addition of electrons upon electrochemical reduction is expected to result in an increase in the NMR Knight shift and hence the NMR frequency. Note that the Knight shift is a larger interaction than the chemical shift, which is a diamagnetic effect wherein additional electron density increases nuclear shielding and thus decreases the chemical shift and NMR frequency.</p><p>Solid-state <ref type="bibr">77</ref> Se MAS NMR measurements were performed on pristine Mo 6 Se 8 and discharged Al 4/3 Mo 6 Se 8 electrodes to measure electronic changes upon electrochemical Al-ion intercalation (Figure <ref type="figure">2b</ref>). Notably, the isotropic <ref type="bibr">77</ref> Se shift associated with Se 1 sites increased by 46 ppm upon Al 3+ intercalation and concomitant reduction of the chevrel framework, a result of an enhanced Knight shift due to To measure changes in the electronic structure of the transition metal Mo 6 clusters upon Al-ion intercalation, both solid-state <ref type="bibr">95</ref> Mo MAS NMR and synchrotron Mo K-edge XANES measurements were performed on Mo 6 Se 8 and discharged Al 4/3 Mo 6 Se 8 electrodes. The solid-state singlepulse <ref type="bibr">95</ref> Mo NMR spectra establish one Knight-shifted signal with an isotropic 95 Mo shift of 1859 ppm associated with the Mo 6 octahedral clusters, which notably do not shift upon Al 3+ cation intercalation (Figure <ref type="figure">2c</ref>). Note that <ref type="bibr">95</ref> Mo is an insensitive nucleus due to its low gyromagnetic ratio and quadrupolar nature (spin = 5/2). Synchrotron Mo K-edge XANES measurements at pristine and discharged states were essentially identical, further establishing no change in the oxidation state of the Mo 6 clusters upon Al 3+ intercalation into chevrel phase Mo 6 Se 8 (Figure <ref type="figure">2d</ref>). Remarkably, the solid-state NMR and XANES measurements establish that the Mo 6 clusters remain relatively electronically isolated upon Al 3+ cation intercalation. Thus, upon electrochemical Al 3+ intercalation, electrons are transferred directly to the redox active chalcogen frameworks, while the transition metal clusters are redox inactive, establishing that the chevrel phases store charge by reversible electrochemical anionic redox.</p><p>To investigate the Al-ion intercalation mechanism, solidstate <ref type="bibr">27</ref> Al single-pulse MAS NMR measurements were acquired under quantitative conditions on the fully intercalated chevrel phase Al 4/3 Mo 6 Se 8 and compared with Al 4/3 Mo 6 S 8 , revealing inherent differences in their structural and electronic properties (Figure <ref type="figure">2e</ref>). In Al 4/3 Mo 6 Se 8 , two <ref type="bibr">27</ref> Al signals with shifts of 38 ppm and -10 ppm are associated Al ions within cavities 1 and 2, respectively. The relative populations of Al in cavities 1 and 2, determined by the relative integrated signal intensities, are 74 and 26%, respectively, consistent with the expected compositions. In Al 4/3 Mo 6 S 8 , the <ref type="bibr">27</ref> Al shifts of 62 and 38 ppm, associated with tetrahedral aluminum environments, exhibit relative populations of 78 and 22% for cavity 1 and cavity 2, respectively. However, in Al 4/3 Mo 6 Se 8 , the <ref type="bibr">27</ref> Al NMR shift of -10 ppm indicates that the intercalated Al 3+ cation in cavity 2 is in an octahedral environment, as opposed to the tetrahedral environments observed for cavity 1 or for both cavities in Mo 6 S 8 , which was proposed as a possible intercalation site for Mg 2+ by Levi and Aurbach. <ref type="bibr">18</ref> Also, the The Al 3+ ions "hop" between the six energetically crystallographic sites within each cavity of the chevrel phases, resulting in fast electric quadrupolar relaxation (5 times T 2 * &lt;400 &#956;s). Circular ion hopping within a cavity is expected to be faster for Mo 6 Se 8 compared to Mo 6 S 8 , based on the GITT diffusion measurements above. Such faster motions would manifest themselves in faster transverse NMR relaxation times and hence broader <ref type="bibr">27</ref> Al linewidths, as measured here. In addition, solid-state <ref type="bibr">27</ref> Al NMR measurements on the charged Mo 6 Se 8 electrode revealed the majority of the aluminum is removed upon de-intercalation with minimal Al-ion trapping (&lt;4%, compared with &lt;7% for Mo 6 S 8 ), <ref type="bibr">15</ref> highlighting the reversibility of Al-ion intercalation into chevrel Mo 6 Se 8 .</p><p>Crystal Structure Evolution. Operando synchrotron EDXRD measurements were to measure how the chevrel Mo 6 Se 8 and Mo 6 S 8 crystalline structures evolved during electrochemical Al 3+ intercalation (Figure <ref type="figure">3</ref>). <ref type="bibr">53,</ref><ref type="bibr">54</ref> Diffraction data were collected using batteries constructed in hermetically sealed gold-plated CR2032 coin cells without transparent windows or other modifications. As previously reported, the electrochemically intercalated chevrel phases are very sensitive to air; 21 thus, operando characterization was performed to prevent undesired side reactions. In the EDXRD pattern of Al-Mo 6 S 8 cells (Figure <ref type="figure">3a</ref>), the 90 and 103 keV peaks, previously indexed to (-132) and (-240) reflections by Lee et al., <ref type="bibr">13</ref> shifted to lower energies during discharge, corresponding to larger d-spacings. Rather than a continuous change in d-spacing, the transition was discontinuous. This shift to lower energies reveals the expansion of the chevrel R3&#773; unit cell due to the electrochemical intercalation of Al 3+ cations. These results agreed with Lee et al., <ref type="bibr">13</ref> where there was no transformation in crystal structure as Mo 6 S 8 maintained its R3&#773; space group during Al 3+ cation insertion. Assuming a final intercalated (discharged) state of Al 4/3 Mo 6 S 8 , the final calculated discharge product corresponded to Al x Mo 6 S 8 with x = 1.43, indicating that electrolyte decomposition during the initial part of the galvanostatic discharge accounted for the remaining capacity (x = 0.1, indicated as an arrow on the discharge curve).</p><p>In contrast, the EDXRD pattern of Al-Mo 6 Se 8 cells (Figure <ref type="figure">3b</ref>) resulted in a triclinic distortion upon the electrochemical intercalation of Al 3+ cations and consequently an altered diffraction pattern. Levi et al. have shown that upon electrochemical insertion of Mg 2+ into Mo 6 Se 8 , the rhombohedral R3&#773; structure is distorted to triclinic P1&#773; . <ref type="bibr">17,</ref><ref type="bibr">18</ref> This result is supported by solid-state <ref type="bibr">27</ref> Al NMR measurements (Figure <ref type="figure">2e</ref>), wherein cavity 1 of Al 4/3 Mo 6 Se 8 is in an octahedral environment, while for Al 4/3 Mo 6 S 8 , Al 3+ cations in both cavities are tetrahedrally coordinated. For Al 4/3 Mo 6 Se 8 , the fully discharged diffraction pattern was not indexed but is similar to patterns reported for Mg x Mo 6 Se 8 (x = 1, 2) reported by Levi et al., <ref type="bibr">17</ref> which exhibit a series of prominent reflections from 110 to 120 keV. Interestingly, several prominent reflections in the discharged material form only in the final moments of discharge, whereupon the final intercalated (discharged) state of Al 4/3 Mo 6 Se 8 is obtained. Overall, the synchrotron diffraction results establish that the bonding structure and topology of the crystalline chevrel frameworks are preserved upon electrochemical cycling. Critically, the chevrel phase undergoes reversible anionic redox without the breaking or forming of chemical bonds, unlike some oxygen anionic redox processes that can occur in transition metal oxides, which explains its high electrochemical reversibility.</p><p>Calculated Electron Charge Distributions. The electron charge transfer mechanism was further investigated theoretically by DFT calculations (Figure <ref type="figure">4</ref>). Bader charge analysis (Figure <ref type="figure">4a</ref>) was performed on Mo 6 S 8 , Mo 6 Se 8 , AlMo 6 S 8 , and AlMo 6 Se 8 unit cell structures to evaluate the spatial distributions of electrons around each atom before and after Al 3+ cation intercalation (see Table <ref type="table">S2</ref> for average charge values for each type of atom). The charge differences between the intercalated and unintercalated chevrel phases establish that electrons are primarily transferred to the anionic chalcogen framework, as opposed to the transition metals. This result corroborates the anionic redox electron charge transfer mechanism measured experimentally by solid-state NMR spectroscopy and XANES. The DFT results show that two characteristic types of chalcogen atoms exist, consistent with the Se 1 and Se 2 measured by solid-state <ref type="bibr">77</ref> Se NMR (Figure <ref type="figure">2a</ref>). Crucially, the DFT results also indicate that the electron charge transfer mechanism observed experimentally for chevrel Mo 6 Se 8 also pertains to chevrel Mo 6 S 8 , which was challenging to characterize experimentally using analogous spectroscopic methods. Thus, the anionic redox mechanism observed in the chevrel phases does not appear to be dependent upon the type of chalcogen atom present within the anionic framework.</p><p>The total density of states (DOS) was also calculated for the chevrel systems (Figure <ref type="figure">4b</ref>, black; see Figure <ref type="figure">S2</ref> for overlayed spectra). The results indicate that all materials are metallic, based on their states being present at the Fermi level (E F ). Chevrel Mo 6 Se 8 systems maintained a larger bandgap than chevrel Mo 6 S 8 systems, independent of Al 3+ cation insertion. Additionally, the projected DOSs (PDOS) are shown for the Mo 4d orbitals (Figure <ref type="figure">4b</ref>, red) and the S or Se 3p orbitals (Figure <ref type="figure">4b</ref>, blue). The unoccupied states accept the electrons upon electrochemical reduction and Al 3+ cation intercalation, causing the PDOS spectra to shift to lower energies. This calculation is consistent with the change in Knight shift observed in solid-state <ref type="bibr">77</ref> Se NMR measurements (Figure <ref type="figure">2b</ref>), as well as the indirect observation of the change in conductivity of the chevrel samples upon Al 3+ intercalation, as discussed above.</p><p>Generality of the Electron Charge Storage Mechanism. To further probe the generality of the electron charge storage mechanism, divalent Zn 2+ cations were electrochemically intercalated into Mo 6 Se 8 electrodes for the first time, and similar spectroscopic measurements were performed to elucidate changes in electronic structure (Figure <ref type="figure">5</ref>). Zinc metal was used as the anode and aqueous 1 M Zn(SO 4 ) was used as the electrolyte. Galvanostatic cycling (Figure <ref type="figure">5a</ref>) of the Zn-Mo 6 Se 8 cell, with Zn-Mo 6 S 8 cells shown for comparison, reveals two distinct discharge plateaus that achieve the theoretical capacities of 88 and 128 mA h/g upon full discharge, respectively, corresponding to Zn 2 Mo 6 Se 8 and Zn 2 Mo 6 S 8 . CV (Figure <ref type="figure">5b</ref>) reveals two distinct reduction peaks at 0.35 and 0.31 V for Mo 6 Se 8 and 0.49 and 0.31 V for Mo 6 S 8 . Synchrotron XANES measurements of the Mo K-edge of pristine Mo 6 Se 8 and discharged Zn 2 Mo 6 Se 8 states (Figure <ref type="figure">5c</ref>) were identical, indicating that the transition metal Mo 6 octahedra are redox inactive. Solid-state <ref type="bibr">77</ref> Se NMR experiments (Figure <ref type="figure">5d</ref>) reveal that the isotropic <ref type="bibr">77</ref> Se NMR signals shift to more positive frequencies upon electrochemical intercalation of Zn 2+ cations, consistent with increased electron density as per the Knight shift effect (eq 4). As upon Al 3+ intercalation, the majority of electrons are transferred specifically to the 4-coordinated Se 1 atoms ( 77 Se shift of 36 ppm) upon Zn 2+ intercalation, with a more modest quantity transferred to the 3-coordinated Se 2 atoms ( 77 Se shift of 7 ppm). Thus, an identical anionic redox electron charge transfer mechanism occurs when multivalent cations with different valences and coulombic charge densities (Al 3+ , Zn 2+ ) electrochemically intercalate within the chevrel Mo 6 Se 8 framework. In aggregate, these results are also consistent and build upon with the work of Thole et al. <ref type="bibr">22</ref> and Wan et al., <ref type="bibr">23</ref>   respectively, ending in distinct Zn 2 Mo 6 S 8 and Zn 2 Mo 6 Se 8 phases. The Zn-Mo 6 S 8 cell showed a well-defined transition from Mo 6 S 8 to a ZnMo 6 S 8 phase at Zn x Mo 6 S 8 with x = 0.98 (x &#8776; 1), where coexistence of both phases appeared over a range of x-values and an equivalence between the two phases occurred at x = 0.53. A similar conversion of the ZnMo 6 S 8 phase to the Zn 2 Mo 6 S 8 phase occurs with an equivalence between phases occurring at x = 1.66. A comparison of the operando synchrotron EDXRD patterns of the Zn-Mo 6 S 8 and Al-Mo 6 S 8 cells (Figure <ref type="figure">S4</ref>) highlights that the Zn x Mo 6 S 8 system has three distinct phases, compared to only two for the Al x Mo 6 S 8 system, a consequence of the different ion valences and quantities intercalated (2 for Zn 2+ vs 4/3 and Al 3+ ) per Mo 6 S 8 unit. Overall, as with Al 3+ cation intercalation, the bonding structure and topology of the crystalline chevrel frameworks were preserved upon Zn 2+ cation intercalation.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; CONCLUSIONS</head><p>Using the electrochemical intercalation of Al 3+ and Zn 2+ cations into chevrel Mo 6 Se 8 and Mo 6 S 8 electrodes as model battery systems, we elucidate experimentally and theoretically that the chevrel phase undergoes reversible electrochemical anionic redox as an electronic charge storage mechanism. The anionic redox occurs without breaking or forming chemical bonds, preserving the crystal structure and explaining the high degree of electrochemical reversibility. In contrast, the transition metal octahedra are redox inactive. This electronic charge storage mechanism is fundamentally different than that observed for the majority of intercalation battery electrodes, wherein the transition metals are redox active. In addition, the nature of the anionic redox phenomenon is different than that observed in lithium-rich transition metal oxides and chalcogenides, which couple cationic and anionic redox processes, are a result of excess lithium, and often result in electrode instabilities and capacity fade. The results also yield insights into how cation-framework and cation-cation interactions affect the intercalation mechanism of multivalent ions within chevrel-phase electrodes.</p><p>We propose that reversible electrochemical redox may be incorporated as a potential material design principle for future multivalent intercalation electrodes, which must not only electrochemically intercalate multivalent cations but also enable those high-charge-density cations to diffuse through their structures. With regards to ion diffusion, the chevrel phases not only have large 3D cavities, but also their electroactive and electronically polarizable anionic frameworks are in close molecular proximity to the intercalated cations and their diffusional transition states between cavities. While chevrel-phase electrodes cannot provide the energy densities necessary for demanding technological applications, computational materials discovery methods using similar anionic redox principles to those elucidated here are worth considering in the search for a multivalent intercalation electrode that is "beyond chevrel". Overall, we hope that this research provides new strategies into the molecular-level design of novel intercalation electrodes for rechargeable multivalent-ion batteries.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>&#9632; ASSOCIATED CONTENT</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>* s&#305; Supporting Information</head><p>The Supporting Information is available free of charge at <ref type="url">https://pubs.acs.org/doi/10.1021/jacs.3c02542</ref>. </p></div><note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_0"><p>https://doi.org/10.1021/jacs.3c02542 J. Am. Chem. Soc. 2023, 145, 15816-15826 Downloaded via CITY COLG OF NEW YORK on July 26, 2023 at 14:48:02 (UTC).See https://pubs.acs.org/sharingguidelines for options on how to legitimately share published articles.</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_1"><p>https://doi.org/10.1021/jacs.3c02542 J. Am. Chem. Soc. 2023, 145, 15816-15826</p></note>