We report the effects of screening capacity, surface roughness, and interfacial epitaxy of the bottom electrodes on the polarization switching, domain wall (DW) roughness, and ferroelectric Curie temperature (TC) of PbZr0.2Ti0.8O3 (PZT)-based free-standing membranes. Singe crystalline 10−50 nm (001) PZT and PZT/La0.67Sr0.33MnO3 (LSMO) membranes are prepared on Au, correlated oxide LSMO, and two-dimensional (2D) semiconductor MoS2 base layers. Switching the polarization of PZT yields nonvolatile current modulation in the MoS2 channel at room temperature, with an on/off ratio of up to 2 × 105 and no apparent decay for more than 3 days. Piezoresponse force microscopy studies show that the coercive field Ec for the PZT membranes varies from 0.75 to 3.0 MV cm-1 on different base layers and exhibits strong polarization asymmetry. The PZT/LSMO membranes exhibit significantly smaller Ec, with the samples transferred on LSMO showing symmetric Ec of about −0.26/+0.28 MV cm-1, smaller than that of epitaxial PZT films. The DW roughness exponent ζ points to 2D random bond disorder dominated DW roughening (ζ = 0.31) at room temperature. Upon thermal quench at progressively higher temperatures, ζ values for PZT membranes on Au and LSMO approach the theoretical value for 1D random bond disorder (ζ = 2/3), while samples on MoS2 exhibits thermal roughening (ζ = 1/2). The PZT membranes on Au, LSMO, and MoS2 show TC of about 763 ± 12, 725 ± 25, and 588 ± 12 °C, respectively, well exceeding the bulk value. Our study reveals the complex interplay between the electrostatic and mechanical boundary conditions in determining ferroelectricity in free-standing PZT membranes, providing important material parameters for the functional design of PZT-based flexible nanoelectronics.
more »
« less
Low-temperature grapho-epitaxial La-substituted BiFeO3 on metallic perovskite
Abstract Bismuth ferrite has garnered considerable attention as a promising candidate for magnetoelectric spin-orbit coupled logic-in-memory. As model systems, epitaxial BiFeO3thin films have typically been deposited at relatively high temperatures (650–800 °C), higher than allowed for direct integration with silicon-CMOS platforms. Here, we circumvent this problem by growing lanthanum-substituted BiFeO3at 450 °C (which is reasonably compatible with silicon-CMOS integration) on epitaxial BaPb0.75Bi0.25O3electrodes. Notwithstanding the large lattice mismatch between the La-BiFeO3, BaPb0.75Bi0.25O3, and SrTiO3(001) substrates, all the layers in the heterostructures are well ordered with a [001] texture. Polarization mapping using atomic resolution STEM imaging and vector mapping established the short-range polarization ordering in the low temperature grown La-BiFeO3. Current-voltage, pulsed-switching, fatigue, and retention measurements follow the characteristic behavior of high-temperature grown La-BiFeO3, where SrRuO3typically serves as the metallic electrode. These results provide a possible route for realizing epitaxial multiferroics on complex-oxide buffer layers at low temperatures and opens the door for potential silicon-CMOS integration.
more »
« less
- Award ID(s):
- 2239545
- PAR ID:
- 10499530
- Publisher / Repository:
- Nature Communications
- Date Published:
- Journal Name:
- Nature Communications
- Volume:
- 15
- Issue:
- 1
- ISSN:
- 2041-1723
- Subject(s) / Keyword(s):
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
null (Ed.)Sm-doped BiFeO 3 (Bi 0.85 Sm 0.15 FeO 3 , or BSFO) thin films were fabricated on (001) SrTiO 3 (STO) substrates by pulsed laser deposition (PLD) over a range of deposition temperatures (600 °C, 640 °C and 670 °C). Detailed analysis of their microstructure via X-ray diffraction (XRD) and transmission electron microscopy (TEM) shows the deposition temperature dependence of ferroelectric (FE) and antiferroelectric (AFE) phase formation in BSFO. The Sm dopants are clearly detected by high-resolution scanning transmission electron microscopy (HR-STEM) and prove effective in controlling the ferroelectric properties of BSFO. The BSFO ( T dep = 670 °C) presents larger remnant polarization (Pr) than the other two BSFO ( T dep = 600 °C, 640 °C) and pure BiFeO 3 (BFO) thin films. This study paves a simple way for enhancing the ferroelectric properties of BSFO via deposition temperature and further promoting BFO practical applications.more » « less
-
Abstract Solid state lithium‐ion batteries have garnered increasing interest in recent years due to several potential advantages over liquid‐electrolyte based systems. The possibility of integrating the lithium garnet oxide, Li6.75La3Zr1.75Ta0.25O12(LLZTO), with the high voltage cathode, spinel LixMn2O4(LMO), is evaluated here. Thin film bilayer structures are prepared by pulsed laser deposition on MgO (001) substrates and characterized by x‐ray diffraction and transmission electron microscopy. The LLZTO is grown by an alternating layer‐by‐layer deposition of LLZTO and Li3N and subsequently annealed for several hours at 575 °C to promote crystallinity. Growth of crystalline LMO with a pristine interface to LLZTO is achieved by gentle heat treatment (500 °C) to remove surface carbonate from the electrolyte and by cathode growth at a low temperature of 250 °C. Higher temperature depositions (330 – 450 °C) result in reaction between the two materials and the appearance of Li2MnO3, which may be in part due to the presence of excess lithium in the electrolyte layer. Because fully lithiated LiMn2O4has a voltage of ≈3.7 V versus Li+/Li, the observation of a well‐defined interface, free of impurity phases and with no interdiffusion of elements, indicates LLZTO is stable to at least 3.7 V.more » « less
-
Abstract Spontaneous polarization and crystallographic orientations within ferroelectric domains are investigated using an epitaxially grown BiFeO3thin film under bi-axial tensile strain. Four dimensional-scanning transmission electron microscopy (4D-STEM) and atomic resolution STEM techniques revealed that the tensile strain applied is not enough to cause breakdown of equilibrium BiFeO3symmetry (rhombohedral with space group:R3c). 4D-STEM data exhibit two types of BiFeO3ferroelectric domains: one with projected polarization vector possessing out-of-plane component only, and the other with that consisting of both in-plane and out-of-plane components. For domains with only out-of-plane polarization, convergent beam electron diffraction (CBED) patterns exhibit “extra” Bragg’s reflections (compared to CBED of cubic-perovskite) that indicate rhombohedral symmetry. In addition, beam damage effects on ferroelectric property measurements were investigated by systematically changing electron energy from 60 to 300 keV.more » « less
-
Abstract The solid‐state synthesis of perovskite BiFeO3has been a topic of interest for decades. Many studies have reported challenges in the synthesis of BiFeO3from starting oxides of Bi2O3and Fe2O3, mainly associated with the development of persistent secondary phases such as Bi25FeO39(sillenite) and Bi2Fe4O9(mullite). These secondary phases are thought to be a consequence of unreacted Fe‐rich and Bi‐rich regions, that is, incomplete interdiffusion. In the present work, in situ high‐temperature X‐ray diffraction is used to demonstrate that Bi2O3first reacts with Fe2O3to form sillenite Bi25FeO39, which then reacts with the remaining Fe2O3to form BiFeO3. Therefore, the synthesis of perovskite BiFeO3is shown to occur via a two‐step reaction sequence with Bi25FeO39as an intermediate compound. Because Bi25FeO39and the γ‐Bi2O3phase are isostructural, it is difficult to discriminate them solely from X‐ray diffraction. Evidence is presented for the existence of the intermediate sillenite Bi25FeO39using quenching experiments, comparisons between Bi2O3behavior by itself and in the presence of Fe2O3, and crystal structure examination. With this new information, a proposed reaction pathway from the starting oxides to the product is presented.more » « less
An official website of the United States government