Atomic Layer Deposition of Cu Electrocatalysts on Gas Diffusion Electrodes for CO 2 Reduction
- Award ID(s):
- 2131709
- PAR ID:
- 10532739
- Publisher / Repository:
- American Chemical Society
- Date Published:
- Journal Name:
- Nano Letters
- Volume:
- 23
- Issue:
- 23
- ISSN:
- 1530-6984
- Page Range / eLocation ID:
- 10779 to 10787
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
An official website of the United States government