Abstract Coseismic temperature rise activates fault dynamic weakening that promotes earthquake rupture propagation. The spatial scales over which peak temperatures vary on slip surfaces are challenging to identify in the rock record. We present microstructural observations and electron backscatter diffraction data from three small‐displacement hematite‐coated fault mirrors (FMs) in the Wasatch fault damage zone, Utah, to evaluate relations between fault properties, strain localization, temperature rise, and weakening mechanisms during FM development. Millimeter‐ to cm‐thick, matrix‐supported, hematite‐cemented breccia is cut by ∼25–200 μm‐thick, texturally heterogeneous veins that form the hematite FM volume (FMV). Grain morphologies and textures vary with FMV thickness over μm to mm lengthscales. Cataclasite grades to ultracataclasite where FMV thickness is greatest. Thinner FMVs and geometric asperities are characterized by particles with subgrains, serrated grain boundaries, and(or) low‐strain polygonal grains that increase in size with proximity to the FM surface. Comparison to prior hematite deformation experiments suggests FM temperatures broadly range from ≥400°C to ≥800–1100°C, compatible with observed coeval brittle and plastic deformation mechanisms, over sub‐mm scales on individual slip surfaces during seismic slip. We present a model of FM development by episodic hematite precipitation, fault reactivation, and strain localization, where the thickness of hematite veins controls the width of the deforming zones during subsequent fault slip, facilitating temperature rise and thermally activated weakening. Our data document intrasample coseismic temperatures, resultant deformation and dynamic weakening mechanisms, and the length scales over which these vary on slip surfaces.
more »
« less
High resolution dataset of plastic deformation at cryogenic temperatures in a nickel-based superalloy
A nickel-based superalloy is examined during monotonic deformation at cryogenic temperatures, reaching as low as liquid helium temperature. A detailed multimodal analysis of the microstructure and plasticity is conducted to discern changes in deformation mechanisms and plastic deformation localization under cryogenic conditions. This study employs high-resolution digital image correlation to identify the deformation mechanisms and understand their influence on plastic deformation localization as the temperature varies. At cryogenic temperatures, unusual plastic deformation localization processes are observed, attributed to the competing activation of a range of deformation processes. Furthermore, a mechanism of slip delocalization, i.e., local plastic deformation homogenization through closely spaced slip, is noted at these extreme temperatures. Ultimately, the impact of the microstructure is identified across the temperature range, from room to cryogenic temperatures.
more »
« less
- Award ID(s):
- 2234892
- PAR ID:
- 10577385
- Publisher / Repository:
- Dryad
- Date Published:
- Subject(s) / Keyword(s):
- FOS: Materials engineering FOS: Materials engineering High Resolution Digital Image Correlation Cryogenic Temperatures Nickel-based Superalloy Plastic Deformation Delocalization
- Format(s):
- Medium: X Size: 9103591504 bytes
- Size(s):
- 9103591504 bytes
- Right(s):
- Creative Commons Zero v1.0 Universal
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
Sinnott, Susan (Ed.)Single crystalline sapphire (-) possesses superior mechanical, thermal, chemical, and optical properties over a wide range of temperatures and pressure conditions, allowing it for a broad spectrum of industrial applications. For the past few decades, research has aimed at comprehensive understanding of its plastic deformation mechanisms under mechanical loading. In this study, we have employed molecular dynamics (MD) simulations to study rhombohedral twinning of sapphire, which is of critical importance in understanding the plastic deformation of sapphire as one of most commonly observed deformation modes. Since the critical resolved shear stress (CRSS) plays a pivotal role in describing the activation of slip systems, it is adopted in this study as the key parameter for analysis. The CRSS is calculated during the uniaxial compression test of a cubic sapphire crystal, oriented to exclusively activate rhombohedral twinning deformation, under simulation conditions such as temperature, strain rate, and system size. Furthermore, a theoretical model of CRSS is constructed based on theories of thermal activation processes, then empirically fitted to CRSS data gathered from the MD simulations. This model accurately captures the relationships between CRSS and external parameters including temperature, strain rate, and system size and shows excellent agreements with the simulation results.more » « less
-
Grain size effects on the early plastic strain localization and slip transfer at grain boundaries were investigated for the Alloy 718 Ni-based superalloy at 650C. Three microstructures with different grain sizes underwent monotonic tensile tests at 650C, both in air and under vacuum, until rupture. All the microstructure variants exhibit fully intragranular fracture under vacuum and partially intergranular fracture in air. In this latter case, predominant intergranular fracture mode was found in the fine-grain microstructures. Interrupted tensile tests were also conducted under vacuum with ex-situ SEM high-resolution digital image correlation (HR-DIC) measurements to assess in-plane kinematics fields at the microstructure scale. Out-of-plane displacement jumps were obtained using laser scanning confocal microscopy. Both crystallographic slip within grains and near twin boundaries (TBs) and morphological sliding happening at grain boundaries (GBs) were documented. Statistical analysis of all plastic events aimed at quantifying strain localization distribution as a function of the microstructure. The fine-grain microstructure was found to have extensive strain localization at grain boundaries, while the coarse-grain microstructure is more prone to intragranular slip development and slip localization near TBs. Different scenarios of slip band/grain boundary interactions were evidenced.more » « less
-
A study was conducted to investigate the temperature dependence of thermomechanical coupling in Inconel 718 (IN718). IN718 was selected as a model material due to deformation being predominantly accommodated by planar slip. Split-Hopkinson (or Kolsky) tension bar experiments were conducted at a nominal strain rate of 750 s^-1 at room temperature and 450 ^o C, representing homologous temperatures (T_H=T/T_melt) of T_H = 0.2 and T_H = 0.5, respectively. During deformation, specimen gauge sections were imaged with a high-speed infrared camera. Using one-dimensional wave analysis, the transient heat conduction equation, and temperature- dependent specific heat capacity values, the temperature rise as a function of plastic strain was used to calculate plastic work, thermal work, and the plastic work to heat conversion efficiency, commonly known as the Taylor–Quinney coefficient (TQC). As expected, a significant reduction in plastic work was observed during testing at elevated temperatures. The temperature rise due to plastic deformation was observed to be lower at room temperature compared to elevated temperature experiments. It is reported here for the first time that the TQC is a temperature-sensitive quantity. At T_H = 0.5, a nearly complete conversion of plastic work to heat was observed (TQC = 1.0). Under ambient conditions of T_H = 0.2, a much lower efficiency TQC = 0.4 was observed.more » « less
-
Abstract The deformation behavior of Ti-6Al-4V titanium alloy is significantly influenced by slip localized within crystallographic slip bands. Experimental observations reveal that intense slip bands in Ti-6Al-4V form at strains well below the macroscopic yield strain and may serially propagate across grain boundaries, resulting in long-range localization that percolates through the microstructure. These connected, localized slip bands serve as potential sites for crack initiation. Although slip localization in Ti-6Al-4V is known to be influenced by various factors, an investigation of optimal microstructures that limit localization remains lacking. In this work, we develop a novel strategy that integrates an explicit slip band crystal plasticity technique, graph networks, and neural network models to identify Ti-6Al-4V microstructures that reduce the propensity for strain localization. Simulations are conducted on a dataset of 3D polycrystals, each represented as a graph to account for grain neighborhood and connectivity. The results are then used to train neural network surrogate models that accurately predict localization-based properties of a polycrystal, given its microstructure. These properties include the ratio of slip accumulated in the band to that in the matrix, fraction of total applied strain accommodated by slip bands, and spatial connectivity of slip bands throughout the microstructure. The initial dataset is enriched by synthetic data generated by the surrogate models, and a grid search optimization is subsequently performed to find optimal microstructures. Describing a 3D polycrystal with only a few features and a combination of graph and neural network models offer robustness compared to the alternative approaches without compromising accuracy. We show that while each material property is optimized through a unique microstructure solution, elongated grain shape emerges as a recurring feature among all optimal microstructures. This finding suggests that designing microstructures with elongated grains could potentially mitigate strain localization without compromising strength.more » « less