<?xml-model href='http://www.tei-c.org/release/xml/tei/custom/schema/relaxng/tei_all.rng' schematypens='http://relaxng.org/ns/structure/1.0'?><TEI xmlns="http://www.tei-c.org/ns/1.0">
	<teiHeader>
		<fileDesc>
			<titleStmt><title level='a'>Perovskite Catalysts for Pure-Water-Fed Anion-Exchange-Membrane Electrolyzer Anodes: Co-design of Electrically Conductive Nanoparticle Cores and Active Surfaces</title></titleStmt>
			<publicationStmt>
				<publisher>American Chemical Society</publisher>
				<date>04/24/2025</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10594482</idno>
					<idno type="doi">10.1021/jacs.5c01621</idno>
					<title level='j'>Journal of the American Chemical Society</title>
<idno>0002-7863</idno>
<biblScope unit="volume">147</biblScope>
<biblScope unit="issue">18</biblScope>					

					<author>Tingting Zhai</author><author>Hao Wang</author><author>Sarah R Beaudoin</author><author>Ran Zhang</author><author>Minkyoung Kwak</author><author>Shujin Hou</author><author>Zhengxiao Guo</author><author>Shannon W Boettcher</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[Anion-exchange-membrane water electrolyzers (AEMWEs) are a possible low-capital expense, efficient, and scalable hydrogen-production technology with inexpensive hardware, earth-abundant catalysts, and pure-water. However, pure-water-fed AEMWEs are still at an early stage of development and suffer from inferior performance compared to proton-exchange-membrane water electrolyzers (PEMWEs). One key challenge is to develop effective non-platinum group metal (non-PGM) anode catalysts and electrodes in pure-water-fed AEMWEs. We show how LaNiO3-based perovskite oxides can be tuned by co-substitution on both A-and B-sites to simultaneously maintain high metallic electrical conductivity along with self-limiting surface reconstruction to expose stable Co-based active catalyst. The optimized perovskite, Sr0.1La0.9Co0.5Ni0.5O3, yielded pure-water AEMWEs operating at 1.97 V at 2 A cm -2 at 70 o C with pure-water feed, thus illustrating the utility of the catalyst design principles.]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><head>INTRODUCTION</head><p>There are several relevant low-temperature electrolysis technologies <ref type="bibr">1,</ref><ref type="bibr">2</ref> possibly suited to produce inexpensive H2 taking advantage of variable renewable electricity production. <ref type="bibr">[3]</ref><ref type="bibr">[4]</ref><ref type="bibr">[5]</ref> Alkaline water electrolyzers (AWEs) are well established and typically use ~30 wt. % KOH electrolyte that is at ~80 o C with the two electrodes being non-platinum-group metal (non-PGM) catalysts separated by a porous diaphragm. AWEs have historically suffered from limited current density (&lt; 500 mA cm -2 ) due to the higher internal resistance of the thick diaphragm and mass-transfer resistance from accumulated bubbles on the electrodes, although advanced systems are working to overcome these limitations. <ref type="bibr">6</ref> Gas crossover through the porous separator further limits the ability to operate at differential pressure as well as the output H2 purity. <ref type="bibr">7</ref> To address these limitations, proton-exchange-membrane water electrolyzers (PEMWEs) were developed. Modern PEMWEs operate at high current density of 2-4 A cm -2 and differential pressure (200-400 psi) with a low degradation rate of &lt; 20 &#956;V h -1 . <ref type="bibr">8</ref> However, the locally acidic and corrosive environment due to the acidic perfluorinated polymeric membrane requires expensive acid-resistant catalysts (IrO2 and Pt), which does limit scalability. <ref type="bibr">2,</ref><ref type="bibr">9</ref> Less-expensive components for the cell hardware and substantially reduced use of PGM catalysts are needed to achieve the cost and scale targets for H2 production.</p><p>Combining advantages of AWEs and PEMWEs, the anion-exchange-membrane water electrolyzers (AEMWEs) enable a zero-gap configuration and differential pressure operation, with pure water or supporting-electrolyte feed. <ref type="bibr">[10]</ref><ref type="bibr">[11]</ref><ref type="bibr">[12]</ref> AEMWEs may also be able to better tolerate less-pure water sources compared to PEMWEs, which could decrease system complexity, operational costs, and robustness. <ref type="bibr">13</ref> The alkaline environment permits the use of inexpensive hardware components and earth-abundant catalysts. <ref type="bibr">14</ref> However, current pure-water-fed AEMWEs yield far lower performance as PEMWEs in terms of efficiency (~ 65 kWh/kgH2) and durability (typically &gt;1 mV h -1 performance loss in the AEMWE). <ref type="bibr">15</ref> To compensate for the drawbacks of membranes/ionomers and anode catalysts, supporting electrolytes, such as aq. KOH or K2CO3, are commonly fed to AEMWEs to reduce the ionic resistance of membrane and catalyst layer and increase durability. An example AEMWE fed with 1.0 M KOH electrolyte has demonstrated ~ 2 A cm -2 at ~ 1.8 V, which approaches the performance of PEMWEs. <ref type="bibr">16</ref> The use of corrosive alkaline electrolytes, however, is a drawback to the membrane electrolyzer system, which can lead to shunt currents and hardware corrosion issues at the system level. The ultimate target for AEMWEs is to realize comparable performance of PEMWEs with the electrolyte-free (nominally pure water) feed but non-PGM catalysts and non-fluorocarbon membranes.</p><p>One challenge for AEMWE technology is the difficulty in designing non-noble-metal OER catalysts specifically for pure-water-fed AEMWEs with nearly all OER-catalyst development having been done in liquid alkali environments. <ref type="bibr">17</ref> Still, the most common anode catalysts for AEMWEs are Ir-based catalysts as they are electrically conductive, largely insoluble under OER conditions, and have modest OER activity in basic media. <ref type="bibr">18,</ref><ref type="bibr">19</ref> In liquid-electrolyte-fed AEMWEs, Ni-Fe (oxy)hydroxide, and related, catalysts show excellent OER activity, as they do in liquid-alkaline media. These oxyhydroxides, however, tend to have poor performance and durability in pure-water-fed AEMWEs, probably due to the lower electrical conductivity of hydroxides (10 -5 mS cm -1 ), which fail to fully oxidize to more-conductive oxyhydroxides without liquid electrolyte, along with the possible dissolution and loss of soluble Fe species. <ref type="bibr">17,</ref><ref type="bibr">20,</ref><ref type="bibr">21</ref> Metal-oxide nanoparticles with higher electrical conductivity have tended to exhibit better performance. For example, Co3O4 (~ 0.2 mS cm -1 ) anode catalysts had nearly the performance to IrO2 despite having the electrical conductivity (all reported conductivities are measured for the samples here, see below) almost a million times lower than that of the IrO2 (1.4 &#177; 0.1 &#215; 10 5 mS cm -1 ). <ref type="bibr">18</ref> The conductivity of Co3O4, however, remains far from optimal.</p><p>While most non-noble-metal oxides are electrical insulators or semiconductors, some classes of perovskite oxides exhibit high metallic conductivities. <ref type="bibr">22,</ref><ref type="bibr">23</ref> LaNiO3, in the family of ABO3 perovskites, exhibits metallic behaviour with electrical conductivity of 4.3 &#177; 0.1 &#215; 10 5 mS cm -1 . <ref type="bibr">24</ref> However, LaNiO3 alone is a very poor catalyst for the OER in alkaline conditions and is only activated for OER by absorption of Fe-impurities and through the formation of NiFeOOH surface species. <ref type="bibr">25</ref> The catalytic, electrochemical, and electrical properties of LaNiO3 can be, however, systematically controlled by cation substitution at both A and B sites. One underlying challenge is the high-temperature synthesis of LaNiO3 (usually &gt; 700 o C), leading to the large particle size and low density of active sites.</p><p>In this work, we leverage the high electrical conductivity of crystalline LaNiO3 and illustrate how strategic cation substitution can be used to simultaneously control and optimize over the i) electrical conductivity, ii) surface reconstruction, and iii) activesurface-phase composition. We show that the electrical conductivity and degree of reconstruction can be controlled and tuned by substitution of Co onto the Ni sites in LaNiO3.</p><p>While the pure LaCoO3 compound is a semiconductor with low electrical conductivity, the LaCoxNi1-xO3 series shows orders of magnitude higher electrical conductivities (2.3 &#177; 0.1 &#215; 10 5 mS cm -1 to 1.1 &#177; 0.1 &#215; 10 5 mS cm -1 ) for a broad range of x values from 0.3 up to 0.7.</p><p>The addition of Co also suppresses the degree of surface structure reconstruction, leading to more morphologically stable catalyst nanoparticles.</p><p>We found that A-site substitution of La with Sr reduced the particle sizes, roughly doubling the BET surface area. Sr, being also much more soluble as Sr(OH)2 than La as La(OH)3 in basic media, enables further tuning of the degree of surface amorphization. Thus, through systematic understanding and design, we report Sr0.1La0.9Co0.5Ni0.5O3 anode catalyst powders which have the state-of-the-art performance in pure-water-fed AEMWEs at 70 o C, achieving cell voltage of 1.81 V at 1 A cm -2 and 1.97 V at 2 A cm -2 . These results are among the best reported for pure-water-fed AEMWEs, closing in on those of the alkalineelectrolyte-fed AEMWE (~ 1.8 V at ~ 2 A cm -2 ), <ref type="bibr">19,</ref><ref type="bibr">[26]</ref><ref type="bibr">[27]</ref><ref type="bibr">[28]</ref> although still somewhat higher than established PEMWE technologies with PGM catalysts (~ 1.7 V at ~ 2 A cm -2 ). <ref type="bibr">[29]</ref><ref type="bibr">[30]</ref><ref type="bibr">[31]</ref> This work thus establishes key design rules for crystalline metallic-conductive non-precious metal-oxide OER catalysts where the electrical conductivity, surface reactivity/restructuring, and catalytic surface composition are together co-designed through systematic manipulation of the solid-state chemistry.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>RESULTS AND DISCUSSION</head></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>Structure characterization, electrical conductivity and morphology of perovskites.</head><p>The SryLa1-yCoxNi1-xO3 series (x = 0, 0.3, 0.5, 0.7, 1; y = 0, 0.1, 0.2, 0.3) were synthesized via a citric-acid sol-gel method from nitrate salts followed by decomposition of the organic species and nitrates at 700 &#8451; in air. The crystalline structures of Sr-doped LaCoxNi1-xO3 (x = 0, 0.3, 0.5, 0.7, 1) were investigated by powder X-ray diffraction (XRD) analysis (Figures <ref type="figure">1a</ref>, <ref type="figure">S1-S3</ref> and Table <ref type="table">S1</ref>). The results show that all synthesized powders adopt a rhombohedral perovskite structure (space group: R-3m), comprising eight tilted cornersharing BO6 octahedra (where B = Ni, Co) with a central cavity accommodating La 3+ /Sr 2+ ions. <ref type="bibr">32</ref> Rietveld refinement of the representative Sr0.1La0.9Co0.5Ni0.5O3 sample (Figure <ref type="figure">1a</ref>) confirms this structure, yielding lattice parameters a = 5.46 &#197; and c = 13.17 &#197; with low residuals (Rwp = 6.73%, Rp = 7.98%, Table <ref type="table">S1</ref>). Full XRD patterns for all samples (Figures <ref type="figure">S1-S5</ref>) exhibit consistent rhombohedral symmetry, with minor peak shifts attributed to ionic radius differences between dopants. No impurities were detected in any of the asprepared samples. For the LaCoxNi1-xO3 series (Figure <ref type="figure">S2</ref>), the characteristic diffraction peaks (e.g., strongest peak near 2&#952; = 33 &#176;) shifted incrementally towards higher angles with increasing Co 3+ /Ni 3+ ratios. This shift is attributed to the smaller ionic radius of Co 3+ (0.54 &#197;) relative to Ni 3+ (0.56 &#197;). In contrast, when Sr 2+ is introduced into the SryLa1-yCo0.5Ni0.5O3 structure (y = 0.1, 0.2, 0.3), the lattice constant increases relative to LaCo0.5Ni0.5O3 (Figure <ref type="figure">S3</ref>), due to the larger ionic radius of Sr 2+ (1.18 &#197;) compared to La 3+ (1.03 &#197;). XRD patterns of Fe-doped SryLa1-yCo0.5Ni0.5O3 also show no detectable impurity phases (Figures <ref type="figure">S4-S5</ref>).</p><p>The electrical conductivities of LaCoxNi1-xO3 (x = 0, 0.3, 0.5, 0.7, 1) and Sr/Fe doped LaCoxNi1-xO3 perovskites were measured at room temperature using a four-probe method (Figure <ref type="figure">1b</ref>). The through-plane conductivity of commercial Co3O4 (30-50 nm) powder was determined by two electrode polarization curves due to its high electrical resistance. <ref type="bibr">20</ref> LaNiO3 exhibited a high electrical conductivity of 4.3 &#177; 0.1 &#215; 10 5 mS cm -1 , consistent with the metallic behavior, <ref type="bibr">22</ref> and significantly higher than that of LaCoO3 (1.2 &#177; 0.2 &#215; 10 2 mS cm -1 ) and commercial Co3O4 (30-50 nm, 2.0 &#177; 0.8 &#215; 10 -1 mS cm -1 ) as in Figure <ref type="figure">1b</ref>.</p><p>Although Co substitution at the Ni site in LaNiO3 reduces the electrical conductivity, LaCo0.5Ni0.5O3 retains a high electrical conductivity of 1.9 &#177; 0.1 &#215; 10 5 mS cm -1 . Sr doping to yield Sr0.1La0.9Co0.5Ni0.5O3 leads to a small decrease in electrical conductivity (1.6 &#177; 0.1 &#215; 10 5 mS cm -1 ), but is still comparable to commercial IrO2 (1.4 &#177; 0.1 &#215; 10 5 mS cm -1 ). The morphologies and microstructures of the as-prepared samples were characterized using scanning electron microscopy (SEM) and transmission electron microscopy (TEM) (Figures <ref type="figure">1c-f</ref> and <ref type="figure">S6-S9</ref>). LaNiO3 and LaCoO3 had sizes of 98 &#177; 26 nm and 109 &#177; 35 nm, respectively, with the distribution of sizes spanning 50 to 200 nm. LaCo0.5Ni0.5O3 had more-uniform distribution and smaller particle size, 78 nm &#177; 20 nm. Substitution with Sr led to a decrease in particle size, with Sr0.1La0.9Co0.5Ni0.5O3 at 56 nm &#177; 11 nm (Figures <ref type="figure">S6-S9</ref>). The Brunauer-Emmett-Teller (BET) specific surface area of the perovskites, commercial Co3O4, and IrO2 were fitted by N2 adsorption-desorption isotherms (Table <ref type="table">S2</ref>).</p><p>LaCo0.5Ni0.5O3 (8.9 &#177; 0.2 m 2 g -1 ) and Sr0.1La0.9Co0.5Ni0.5O3 (13.6 &#177; 0.1 m 2 g -1 ) exhibited higher surface area than LaNiO3 (8.8 &#177; 0.2 m 2 g -1 ) and LaCoO3 (7.7 &#177; 0.1 m 2 g -1 ), consistent with the SEM observations. High-angle annular dark-field STEM (HAADF-STEM) images and corresponding energy-dispersive X-ray spectroscopy (EDS) elemental mapping showed uniform distribution of all elements (Figure <ref type="figure">1f</ref>). The stoichiometric ratio of metal elements in key samples were verified by inductively coupled plasma-mass spectroscopy (ICP-MS) (Table <ref type="table">S3</ref>) and were consistent with the intended synthesis ratios.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>Electrocatalytic performance and relation to materials and interface properties. The electrocatalytic performance and durability of the as-prepared perovskites, commercial</head><p>Co3O4 and IrO2 were evaluated in AEMWEs at 70 o C with electrolyte-free water feed (see details in supporting information). Catalyst powder and ionomer were dispersed in isopropyl alcohol and water and sprayed on porous-transport layers (PTLs) with the catalyst mass loading of 3.0 &#177; 0.2 mg cm -2 . The membrane-electrode assemblies (MEAs) were constructed using various anode catalysts on stainless-steel woven mesh, a 40 &#956;m TP-85 membrane and a Pt black cathode catalyst on Toray-090 carbon paper with a high mass loading of 3.0 &#177; 0.2 mg cm -2 . Pt black was selected for its high HER activity, reproducibility, and stability under pure-water operation, compared to commercial Pt/C (40 wt%) (Figure <ref type="figure">S10</ref>), which is critical for our studies focused on the anode. The above components were compressed together under 55 in-lb by applying a torque wrench to ensure uniform contact of the assembly. MEA configurations remained consistent across all AEMWE measurements, with only the anode catalyst varying between samples.</p><p>The current-voltage polarization curves for different catalysts were recorded over a current range of 10-2000 mA cm -2 (without iR-compensation) to assess their catalytic activities in AEMWEs (Figure <ref type="figure">2a</ref>). All perovskite oxides had higher performance than commercial Co3O4 and IrO2. The cell voltage measured at low current is related to the catalytic activity of the anode, as ohmic and mass-transport loss are negligible in this region. <ref type="bibr">10,</ref><ref type="bibr">18</ref> At 10 mA cm -2 , the cell voltages for perovskite oxides were 100-150 mV lower than that of commercial Co3O4. The voltage difference between the cells with the perovskite oxides and the commercial Co3O4 widens as the current density increases, likely due to the reduced voltage drop in the porous electrode due to the superior electrical conductivities of perovskite oxides.</p><p>Among the tested perovskites, Sr0.1La0.9Ni0.5Co0.5O3 yielded the best cell performance with 1.81 and 1.97 V at current densities of 1 and 2 A cm -2 , respectively, outperforming commercial Co3O4 (2.13 V at 1 A cm -2 and 2.36 V at 2 A cm -2 ) and IrO2 (1.99 V at 1 A cm -2 and 2.19 V at 2 A cm -2 ). Sr0.1La0.9Ni0.5Co0.5O3 also exhibited the smallest potential at the small current of 0.025 mA cm -2 BET, highlighting its superior intrinsic OER activity (see BET-normalized currents in Figure <ref type="figure">S11</ref>). LaNi0.5Co0.5O3 also exhibited good performance (2.07 V at 2 A cm -2 ), relative to pristine perovskite oxides, LaNiO3 (2.12 V at 2 A cm -2 ) and LaCoO3 (2.10 V at 2 A cm -2 ). The AEMWE performance of LaCoxNi1-xO3 (x = 0, 0.3, 0.5, 0.7 and 1), SryLa1-yCo0.5Ni0.5O3 (y = 0, 0.1 and 0.2), LaFezCo0.5-z/2Ni0.5-z/2O3 (z = 0, 0.1 and 0.2) and Sr0.1La0.9FezCo0.5-z/2Ni0.5-z/2O3 (z = 0, 0.05, 0.1 and 0.2) are compared in</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>Figures S12-S15.</head><p>To deconvolute the cell equivalent resistances, galvanostatic electrochemical impedance spectroscopy (GEIS) was conducted at 50 mA cm -2 . The mass-transfer resistance was assumed to be negligible at this low current density. The Nyquist plots and fitted results are shown in Figure <ref type="figure">2b-c</ref>, with the equivalent circuit model. The equivalent circuit includes an ohmic resistance Rohm in the high-frequency region and two additional circuits in low-frequency region (each comprising a resistor and constant phase element in parallel -Rct,1, Rct,2 with CPE1 and CPE2). The total charge-transfer resistance is determined using the equation: Rct = Rct,1 + Rct,2. Rohm reflects the total ionic resistance of membrane, and the electrical resistance at all MEA contact interfaces and is largely independent of the applied voltage.</p><p>All tested perovskite oxides exhibited similar Rohm (0.10-0.12 &#937; cm 2 ), slightly lower than that of commercial Co3O4 (0.143 &#177; 0.015 &#937; cm 2 ), likely attributed to better electrical contact from the higher-conductivity perovskite catalysts. LaNiO3 and IrO2 demonstrated the lowest ohmic resistance (0.101 &#177; 0.003 &#937; cm 2 and 0.096 &#177; 0.003 &#937; cm 2 ), also consistent with their high electrical conductivity (measured to be 4.3 &#177; 0.1 &#215; 10 5 mS cm -1 and 1.4 &#177; 0.1 &#215; 10 5 mS cm -1 , respectively, using the methods described herein). LaCoO3 exhibited a higher ohmic resistance (0.124 &#177; 0.006 &#937; cm 2 ), probably due to its lower electrical conductivity (here measured to be 1.2 &#177; 0.2 &#215; 10 2 mS cm -1 ) relative to the other perovskites.</p><p>Even with 10% Sr and 50% Co substitution at La site and Ni site of LaNiO3, respectively, Sr0.1La0.9Co0.5Ni0.5O3 maintained a low ohmic resistance of 0.11 &#177; 0.01 &#937; cm 2 .</p><p>At 2 A cm -2 , the difference between the catalysts with the lowest Rohm of ~0.10 &#937; cm 2 and those with the highest of ~0.14 &#937; cm 2 would lead to a cell voltage difference of ~80 mV.</p><p>The difference in cell performance, however, between the best conductive perovskite catalysts and the baseline Co3O4 at 2 A cm -2 is ~400 mV. This can be explained by the observed trend in apparent Rct. The electrode kinetics are a function of potential. To assess the relative effect of kinetics, we plot Rct = Rct,1 + Rct,2 from the impedance analysis at 50 mA cm -2 where kinetic resistances are expected to be substantial. Sr0.1La0.9Co0.5Ni0.5O3 exhibited a Rct of 1.03 &#177; 0.02 &#937; cm 2 , lower than that of baseline Co3O4 (1.46 &#177; 0.06 &#937; cm 2 ). This lower apparently Rct is likely due to a combination of faster OER kinetics from the active surfaces, and higher electrical conductivity which improves the electrical transport within the ionomer-filled porous electrode structure and thus effective surface area. The value of Rct generally tracked the measured total cell voltage (Figure <ref type="figure">2c</ref>).</p><p>The polarization curves for the different anode catalysts were then decomposed into i) the thermodynamic potential for water electrolysis (1.19 V at 70 o C), ii) the ohmic overpotential &#951;ohm = iRohm where Rohm taken from the high-frequency impedance in the fit above, iii) the kinetic overpotential (&#951;kin), which includes overall contributions from both the oxygen evolution reaction (OER) at the anode and the hydrogen evolution reaction (HER) at the cathode, calculated using the Tafel model from ohmic-loss-free cell voltages at current densities below 100 mA cm -2 (and extrapolated to all currents), and iv) the residual overpotential (&#951;res) that is unexplained by i) -iii), which will be discussed below (Figure <ref type="figure">2d-e</ref>). <ref type="bibr">33,</ref><ref type="bibr">34</ref> This analysis shows that &#951;kin is the predominant voltage loss across all catalysts. Sr0.1La0.9Ni0.5Co0.5O3 achieved an &#951;kin as low as 0.48 V at 2 A cm -2 , which is 250 mV and 110 mV lower than that of the commercial Co3O4 (0.73 V) and commercial IrO2 (0.59 V) (Figure <ref type="figure">2e</ref>), respectively. This analysis is thus consistent with the lower Rct from GEIS results. The calculated &#951;ohm increases with current density, representing 20-30% of the total cell voltage loss for these devices at 2 A cm -2 . Both LaNiO3-based perovskites and commercial IrO2 catalysts had 60-80 mV lower &#951;ohm at 2 A cm -2 than Co3O4, likely due to lower electrical resistance at the catalyst-PTL interface. We note that the PiperION membrane has a hydroxide ion conductivity of 0.1-0.2 S cm -1 at 70 &#8451; leading to an expected contribution solely from the 40-&#181;m membrane only 0.02-0.04 &#937;.</p><p>We also note that the large variations in electrical conductivity across catalysts did not produce equally significant differences in &#951;ohm. This is because the electrical resistivity of the catalyst layer is not measured by the high frequency impedance that is used to find Rohm; <ref type="bibr">35</ref> the porous electrode has parallel ionic and electrical conduction pathways resulting in the catalyst layer's ionic and electrical resistances being lumped into the equivalent impedance of associated with Rct,1, Rct,2, CPE1, and CPE2.</p><p>At lower current density (e.g., 100 mA cm -2 ), residual overpotentials (&#951;res) were negligible across all catalysts (&lt;1%). However, as the current density increased from 100 mA cm -2 to 2 A cm -2 , the &#951;res contribution increased to 10-20% of the total voltage loss. These observations suggest that a least a portion of &#951;res can be ascribed to mass-transfer-related losses, perhaps in combination with increasing overpotentials due to ion and electron transport through the resistive porous electrode's catalyst layer.</p><p>The double-layer capacitance (Cdl), estimated from the non-faradaic charging measured between 0.6 V to 1.0 V in the two-electrode electrolyzer configuration, was used to calculate the electrochemically active surface area (ECSA) for the catalysts (Figure <ref type="figure">2f</ref>). <ref type="bibr">36</ref> In this two-electrode configuration the measured capacitance is determined by the smaller of the anode or cathode. Because of the large loading of Pt on porous carbon at the cathode, we expect measured capacitances to by roughly equal to that of the anode (i.e. Ctot = Canode Ccathode/(Canode + Ccathode) &#8776; Canode, when Canode &lt;&lt; Ccathode). This assumption was further confirmed that the Cdl of Pt black in a three-electrode system (0.1 M Fe-free KOH) was 65 times larger than that of Sr0.1La0.9Co0.5Ni0.5O3 (Figure <ref type="figure">S16</ref>). The cell capacitances for LaNiO3, LaCoO3 and LaCo0.5Ni0.5O3 systems were 5.0, 4.0 and 5.5 mF cm -2 , respectively, all lower than that of commercial Co3O4 (7.2 mF cm -2 ) (Figure <ref type="figure">S17</ref>). This difference is in part attributed to the larger particle size for the perovskites after high-temperature annealing (700 &#8451;). However, Sr0.1La0.9Ni0.5Co0.5O3 and IrO2 possess high Cdl of 27.3 and 11.2 mF cm -2 , respectively, although they have smaller BET surface areas of 13.6 &#177; 0.1 and 6.3 &#177; 0.1 m 2 g -1 , respectively, compared to commercial Co3O4 (91.3 &#177; 0.2 m 2 g -1 ). Sr0.1La0.9Ni0.5Co0.5O3 and IrO2 therefore have more available surface redox-active species per unit BET surface area providing pseudocapacitive charging response.</p><p>The Cdl per gram was divided by BET surface area (area per gram) was used quantify the average surface redox/capacitance per internal microscopic surface area of catalyst (mF cm -2 micro). All metallic catalysts, including LaNiO3-based perovskites and IrO2, had higher Cdl/BET than non-metallic Co3O4 (Figure <ref type="figure">2g</ref>). The Co3O4 had the smallest Cdl/BET of 0.0026 mF cm -2 micro, consistent with the low electrical conductivity (2.0 &#177; 0.8 mS cm -1 ), meaning that only small portion of the Co3O4 near the metal current collector is likely electrochemically active, especially under high-current conditions for ohmic drops through electrode would lead to significant current heterogeneity. LaNiO3, LaCoO3 and LaNi0.5Co0.5O3 had much higher Cdl/BET of 0.017-0.021 mF cm -2 micro, compared to Co3O4, ascribed to the enhanced electrical conductivity. Notably, Sr0.1La0.9Ni0.5Co0.5O3 had Cdl/BET of 0.067 mF cm -2 micro, 25 times higher than Co3O4, and four times higher than metallic LaNiO3. Sr leaching during electrolysis likely facilitates surface restructuring to form a thin layer of electrolyte-permeated oxyhydroxide phase with higher apparent capacitance per internal area due to Ni/Co redox.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>Electrocatalytic durability of perovskite anodes in AEMWEs with pure-water feed.</head><p>The anode in the AEMWEs undergoes more-severe degradation than the cathode. <ref type="bibr">17,</ref><ref type="bibr">37</ref> Previous studies have identified ionomer within the ionomer-catalyst porous anode structure as the primary factor limiting durability when pure water is used. <ref type="bibr">38</ref> To understand how conductivity influences stability in pure-water-fed AEMWEs, we conducted 20-h durability tests at 70 &#176;C under pure-water-fed conditions at 500 mA cm -2 using as-prepared perovskite oxides, IrO2 and Co3O4 as anodes, a duration capturing substantial degradation (2.7-13.4 mV h -1 ) across all samples due to rapid ionomer degradation (Figures <ref type="figure">S18-S20</ref>).</p><p>The cell voltage with Sr0.1La0.9Ni0.5Co0.5O3 increased from 1.71 V to 1.83 V over 20 h (a degradation rate of 5.0 mV h -1 , see also Figure <ref type="figure">S19</ref> for polarization curves before and after testing). The degradation rate of Sr0.1La0.9Ni0.5Co0.5O3 is comparable to that of IrO2 (5.1 mV h -1 ), but inferior to commercial Co3O4 (2.7 mV h -1 ). The faster degradation observed for Sr0.1La0.9Ni0.5Co0.5O3 and IrO2 compared to that of commercial Co3O4, is consistent with the higher electrical conductivity, which would accelerate ionomer degradation throughout the entire conductive-catalyst porous electrode <ref type="bibr">18</ref> </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>compared to commercial</head><p>Co3O4 where the oxidation is limited to the interfacial region near the current collector. We note, however, the lack of anode catalyst's electrical conductivity is not a useful mechanism to stabilize AEMWE ionomer because of the performance loss -metallic catalysts are essential for achieving high active catalyst loading and hence the best cell performance. Indeed, Sr0.1La0.9Ni0.5Co0.5O3 maintained a lower cell voltage than commercial Co3O4 after the 20-h test, despite a higher degradation rate. LaNiO3-based devices degraded the fastest (13.4 mV h -1 over 20 h), likely due to combination of high electrical conductivity and poor catalytic activity compared to Sr0.1La0.9Ni0.5Co0.5O3 leading to higher initial voltages (Figure <ref type="figure">S20</ref>). To further substantiate the critical role of ionomer degradation in stability loss, we highlight that introducing an HfOx protective layer via atomic-layer deposition following our prior report <ref type="bibr">39</ref> significantly enhanced stability in pure-water AEMWE configurations (Figure <ref type="figure">2h</ref>). This direct correlation between ionomer preservation and operational durability offers one pathway to decouple stability from conductivity constraints, but requires more development. </p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>Postmortem analysis of the ionomer degradation and catalyst reconstruction.</head><p>To investigate the degradation mechanism(s), the AEMWE cell was disassembled for postmortem analysis. After operation, the anode was soaked in 3 M aq. NaCl to exchange OH -with Cl -and prevent further degradation from OH -nucleophilic attack upon drying.</p><p>Surface and cross-sectional SEM analysis were performed on Sr0.1La0.9Co0.5Ni0.5O3 to reveal morphological and microstructural changes (Figure <ref type="figure">3b-c</ref> and <ref type="figure">3e-f</ref>). After the stability test, significant ionomer degradation was observed on the surface of the catalyst layer (Figure <ref type="figure">3c</ref>). This near-complete ionomer degradation within the catalyst layer was further substantiated by mapping analysis (Figure <ref type="figure">S21</ref>), which demonstrated a significant reduction in C and N content (elemental markers of the ionomer) after operation.</p><p>Cross-sectional SEM images revealed only perovskite nanoparticles comprising the postmortem porous electrode, with higher-magnification views (Figure <ref type="figure">3e-f</ref>  <ref type="figure">S23</ref>). This localized failure stems from aggressive ionomer oxidation at the PTL interface, which disrupts catalyst adhesion and leads to catastrophic mechanical degradation. X-ray photoelectron spectra of PiperION ionomer before and after testing with Sr0.1La0.9Co0.5Ni0.5O3 catalyst also show the chemical signature of degradation (Figure <ref type="figure">S24</ref>). In the C 1s spectra, a new high-binding-energy C-O peak and a reduced-intensity C-N peak was observed, indicating oxidation of the phenyl group and a loss of C-N content in the ionomer after operation. For the N 1s and F 1s spectra, a new N 1s peak emerged around 400 eV, and the intensities of both the nitrogen cation peak and the fluorine peak decreased post-operation, further confirming anode-ionomer decomposition during the electrochemical tests. <ref type="bibr">38,</ref><ref type="bibr">39</ref> Moreover, 1 H NMR and ATR-FTIR were conducted to further analyze the ionomer (PiperION) pre-and post-operation. The 1 H NMR spectrum post-test reveals new signals at 4.8, 5.3, and 6.5 ppm (Figure <ref type="figure">S25</ref>), suggesting the Hofmann ringopening elimination, which is due to hydroxide nucleophilic attack. <ref type="bibr">40,</ref><ref type="bibr">41</ref> In addition, a reduction in the intensity of the methyl proton peak attached to the quaternary ammonium group at 3.1 ppm further supports the degradation of the quaternary ammonium charged groups. ATR-FTIR shows evidence of oxidation: the pristine C=C stretching band at 1616 cm -1 transforms into multiple peaks in the region of 1667 -1540 cm -1 , likely due to the formation of new C=C or C=O bonds resulting from phenyl oxidation. <ref type="bibr">42</ref> Furthermore, the C-N stretching vibration (1221 cm -1 ) weakens and shifts, while a new C-O bond signal emerges at 1079 cm -1 (Figure <ref type="figure">S26</ref>). <ref type="bibr">43</ref>   region outlined by yellow dashed lines (region 1), while the catalyst particles are visible as the bright areas (region 1-2)). XPS spectra of (d) O 1s, (g) Sr 3d, (h) Co 2p, and (i) Ni 2p in pristine and post-mortem PTLs after 20 h stability test at 0.5 A cm -2 with pure water feed in AEMWEs for Sr0.1La0.9Co0.5Ni0.5O3 sample.</p><p>XRD measurements of Sr0.1La0.9Co0.5Ni0.5O3 were also carried out before and after the stability test (Figure <ref type="figure">3a</ref>). The post-test XRD data revealed no additional peaks, indicating that the bulk crystalline structure remained intact, although this data does not preclude significant surface reconstructions. XPS collected for Sr0.1La0.9Co0.5Ni0.5O3 showed the Sr 3d peak nearly vanished (from 2.25 atom % in the pristine sample to 0.14 atom % after 20h operation at 0.5 A cm -2 ), confirming Sr leaching (Figure <ref type="figure">3g</ref>). To distinguish leaching from surface-masking effects, Sr signals were normalized against La, Co, and Ni. The Sr/La, Sr/Co, and Sr/Ni atomic ratios decreased from 0.30, 0.88, and 0.17 (pristine) to 0.17, 0.29, and 0.10 (post-test), respectively. While absolute XPS quantification can be confounded by surface adsorbates, this data across elemental references is strong evidence of Sr leaching during operation. In the O 1s spectra, the characteristic peak at ~528 eV associated with lattice oxygen lost intensity due to the formation of metal hydroxides on the perovskite surface (Figure <ref type="figure">3d</ref>). Co 2p spectra changed less after the stability test, while the fitted intensity of a possible Ni 2+ 2p3/2 peak in the Ni 2p spectra increased (Figure <ref type="figure">3hi</ref>). Co 2+ /Ni 2+ is originated from the existence of oxygen vacancies on the surface of perovskite oxides, which induces charge compensation by reducing adjacent Co 3+ /Ni 3+ ions to Co 2+ /Ni 2+ . <ref type="bibr">44,</ref><ref type="bibr">45</ref> Together, these results indicate that Sr0.1La0.9Co0.5Ni0.5O3 underwent surface reconstruction, probably yielding a Ni-rich Ni/Co (oxy)hydroxide on the surface that hosts the active catalyst after Sr leaching, while the core retained its crystalline perovskite structure that is electrically conductive. For the Sr0.1La0.9Co0.5Ni0.5O3 after 20-h operation in the AEMWE cell, TEM analysis showed only a thin disordered layer (~ 2 nm) on the surface, with the core crystalline structure retained (Figure <ref type="figure">4a-b</ref>). The average compositions of the particles before and after testing were calculated from the entire image (Figures <ref type="figure">1f</ref> and <ref type="figure">4c-d</ref>). All the elements are similar, except for Sr, which changed from 2.6 &#177; 0.2 atom % to 0.4 &#177; 0.1 atom % after testing. This finding is consistent with XPS results; Sr leaches from Sr0.1La0.9Co0.5Ni0.5O3 during the AEMWE operation. The reconstructed layer hypothesized from Sr-loss and XPS analysis was not visible in HR-TEM analysis. This result illustrates the difficulty in directly imaging electrochemically active disordered surface layers in these catalyst structures, despite their almost-certain presence based on the electrochemical and surface analyses.</p><p>Surface reconstruction of perovskite catalysts in Fe-free KOH electrolyte. To investigate the surface reconstruction of perovskite catalysts during water oxidation, cyclic voltammetry (CV) tests were conducted on the prepared perovskite catalysts with 10 wt% PiperION ionomers on Pt/Ti quartz-crystal electrodes in 1.0 M rigorously Fe-free KOH electrolyte <ref type="bibr">46</ref> using a standard three-electrode cell. This setup aims to simplify the analysis compared to the complexity of AEMWE system, although due to the use of liquid versus solid-ionomer electrolytes. The current densities were normalized by the BET specific surface areas to evaluate the intrinsic OER activities. Sr0.1La0.9Ni0.5Co0.5O3 exhibited the highest OER activity among all prepared perovskites whereas LaNiO3 showed the worst performance, consistent with need for Fe-impurity activation for Ni-based OER catalysts (Figure <ref type="figure">5a</ref>). The addition of Co at the Ni site in LaNi0.5Co0.5O3 improved activity compared to LaNiO3. For Sr0.1La0.9Ni0.5Co0.5O3, the emergence of a redox wave at ~ 1.34 V vs. RHE in the pre-OER region is indicative of the generation of (oxy)hydroxide species induced by the surface reconstruction (inset of Figure <ref type="figure">5b</ref>). This redox peak increased in intensity with cycling, becoming prominent after 25 cycles. Ni-containing perovskite catalysts developed redox peaks at ~1.43 V vs. RHE for LaNiO3 and ~1.39 V vs. RHE for LaCo0.5Ni0.5O3 (inset of Figure <ref type="figure">5c</ref>). In contrast, LaCoO3 did not exhibit observable redox peaks even after extended cycling, consistent with previous results that LaNiO3 is prone to surface reconstruction while LaCoO3 maintains greater structural stability. <ref type="bibr">25</ref> The observed redox reaction preceding the OER for LaNiO3-based perovskites corresponds to the reversible transition of Ni(OH)2 to NiOOH. The number of redox-active Ni(OH)2 can be estimated by integrating the Ni oxidation peak, <ref type="bibr">21,</ref><ref type="bibr">47</ref> with the monolayer equivalents (MLE) of the reconstructed nickel hydroxide layer calculated using an average of 1.7 nmol Ni cm -2 per MLE (verified using the lattice parameters of &#946;-Ni(OH)2: a = b = 3.126 &#197; and 1 Ni atom per unit cell). <ref type="bibr">21,</ref><ref type="bibr">25</ref> The MLE values of Ni(OH)2 generated after 100 cycles on the surface of LaNiO3, LaCo0.5Ni0.5O3 and Sr0.1La0.9Co0.5Ni0.5O3 were 0.08, 0.03 and 0.09, respectively (Figure <ref type="figure">5c</ref>). The lower MLE growth rate for LaCo0.5Ni0.5O3, compared to LaNiO3, is attributed to the introduction of more-stable Co-O bonds and active sites. Sr0.1La0.9Co0.5Ni0.5O3 had a higher growth rate of redox-active oxyhydroxide than LaCo0.5Ni0.5O3 likely due to Sr leaching during OER that facilitated the reconstruction of amorphous layer. <ref type="bibr">48</ref> Regardless, all the perovskites yielded a thin layer of redox-active Ni species on the surface while preserving the core perovskite structure, which we hypothesize is important for high performance in the liquid-electrolytefree AEMWE cells. The post-mortem HR-TEM images on the catalyst powders removed from EQCM electrodes after 100 cycles of CV cycling in 1 M Fe-free KOH and chronopotentiometric (CP) testing in 0.1 M Fe-free KOH (Figure <ref type="figure">S27</ref>) also demonstrated putative surface reconstruction under the supporting electrolyte environment, akin to observations in pure-water conditions (Figure <ref type="figure">S28</ref>). To investigate the influence of the generated redox-active metal (oxy)hydroxide species on charge transfer resistance (Rct), PEIS of Sr0.1La0.9Co0.5Ni0.5O3 was analyzed every 25 cycles at 1.7 V vs. RHE in the threeelectrode 1.0 M Fe-free KOH cell (Figure <ref type="figure">5d</ref>). The Rct values decreased with the increased cycles attributed to the higher intrinsic activity of the reconstructed redox-active Ni species, consistent with the observed increased activity after cycling (Figure <ref type="figure">5b</ref>).</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>CONCLUSIONS</head><p>We reported how to co-design mixed metal perovskite oxides for high electrical conductivity (metallic behaviour) along with surfaces that optimally reconstruct in a controlled way to form highly active sites for water oxidation catalysis. Starting with the parent LaNiO3, the substitution of Co on the Ni sites marginally reduces electrical conductivity, but provides higher catalytic activity for the oxygen-evolution in pure-water alkaline ionomer conditions (and without the need for Fe impurities that activate catalysts in KOH tests). <ref type="bibr">25</ref> The substitution of Sr on La sites both increases the degree of surface reconstruction due to the higher solubility of Sr 2+ and decreases the nanoparticle size to increase the effective surface area. The best Sr0.1La0.9Co0.5Ni0.5O3 catalyst provides exceptional activity in pure-water-fed AEMWE test platforms, with a total cell voltage of 1.97 &#177; 0.02 V at 2.0 A cm -2 ; at least 200 mV lower than the IrO2 baseline (at the same mass loading of 3.0 mg cm -2 ) and better than reported pure-water electrolyzer devices. <ref type="bibr">15,</ref><ref type="bibr">18</ref> The advanced cell performance is the result of solid-state chemical design of catalyst in the anode resulting in high electrical conductivity that leads to large effective surface areas in the porous anode for water oxidation, while controlled surface reconstruction by tuned 10% Sr incorporation and leaching facilitates formation of the optimal thickness of the surfaceactive phase. Optimized Co substitution stabilizes the bulk lattice, confining reconstruction to a self-limiting ~2 nm amorphous surface layer and retaining metallic conductivity. The same high electrical conductivity and porous electrode architecture, however, also accelerates ionomer degradation at the catalyst/ionomer interface, known to be the durability limiting process in AEMWEs. This challenge remains to be fully solved, for example by interface engineering and passivation. <ref type="bibr">39</ref> This work thus provides key insight for solid state chemical design of conductive perovskite anode catalysts in pure-water-fed AEMWEs thus contributing both to the science of electrocatalysis and practical goals of enabling efficient and cost-effective alkaline membrane electrolysis systems.</p></div>
<div xmlns="http://www.tei-c.org/ns/1.0"><head>ASSOCIATED CONTENT</head></div></body>
		</text>
</TEI>