<?xml-model href='http://www.tei-c.org/release/xml/tei/custom/schema/relaxng/tei_all.rng' schematypens='http://relaxng.org/ns/structure/1.0'?><TEI xmlns="http://www.tei-c.org/ns/1.0">
	<teiHeader>
		<fileDesc>
			<titleStmt><title level='a'>Photothermoelectric effect in cadmium arsenide thin films for unbiased, mid-infrared photodetection</title></titleStmt>
			<publicationStmt>
				<publisher>American Institute of Physics</publisher>
				<date>05/05/2025</date>
			</publicationStmt>
			<sourceDesc>
				<bibl> 
					<idno type="par_id">10646583</idno>
					<idno type="doi">10.1063/5.0272453</idno>
					<title level='j'>Applied Physics Letters</title>
<idno>0003-6951</idno>
<biblScope unit="volume">126</biblScope>
<biblScope unit="issue">18</biblScope>					

					<author>Jacob Brady</author><author>Arman Rashidi</author><author>Sina Ahadi</author><author>Susanne Stemmer</author>
				</bibl>
			</sourceDesc>
		</fileDesc>
		<profileDesc>
			<abstract><ab><![CDATA[<p>Mid-infrared photodetectors that can operate at room temperature are of great interest for a wide range of applications. Here, we demonstrate unbiased, mid-infrared (10.4μm) photodetection in epitaxial thin films of the three-dimensional Dirac semimetal cadmium arsenide (Cd3As2), which are grown on a III–V heterostructure. We show that the photocurrent response of planar metal–Cd3As2–metal devices is consistent with the photothermoelectric effect, which is due to a temperature gradient that develops under asymmetric illumination of the device. We show that the photoresponsivity of Cd3As2 channel devices is an order of magnitude greater than devices with a III–V semiconductor channel, attesting to the excellent thermoelectric properties of Cd3As2 and promising efficient unbiased, room-temperature mid-infrared photodetection.</p>]]></ab></abstract>
		</profileDesc>
	</teiHeader>
	<text><body xmlns="http://www.tei-c.org/ns/1.0" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:xlink="http://www.w3.org/1999/xlink">
<div xmlns="http://www.tei-c.org/ns/1.0"><p>Published under an exclusive license by AIP Publishing. <ref type="url">https://doi.org/10.1063/5.0272453</ref> </p><p>Photodetectors that can efficiently detect photons with energies in the mid-to far-infrared (IR) regime of the electromagnetic spectrum and that can operate at room temperature without any cooling or externally applied bias have attracted interest due to a wide range of applications. Of particular interest is the atmospherically transparent window, corresponding to wavelengths between 8 and 12 lm. Many different detection principles, materials, and device architectures have been considered for operation at these wavelengths. <ref type="bibr">[1]</ref><ref type="bibr">[2]</ref><ref type="bibr">[3]</ref><ref type="bibr">[4]</ref><ref type="bibr">[5]</ref><ref type="bibr">[6]</ref><ref type="bibr">[7]</ref> Photovoltaic detectors, such as those based on III-V antimonides or HgCdTe heterostructures, typically require active cooling. Detectors based on the photo-bolometric effect have a spectrally broad response but require an external bias and suffer from low speeds. <ref type="bibr">8</ref> For these reasons, detectors that utilize the photothermoelectric effect (PTE) have attracted interest. <ref type="bibr">3,</ref><ref type="bibr">9</ref> PTE-based detectors rely on the incident IR light to locally heat a thermoelectric material. The resulting thermal gradient generates a thermoelectric voltage or current via the Seebeck effect. PTE-based detectors allow for unbiased photodetection from visible to terahertz wavelengths at room temperature. The best candidates for PTE-based detectors are low-resistivity materials with large Seebeck coefficients that also exhibit strong absorption at the wavelengths of interest.</p><p>These requirements suggest that the topological semimetal cadmium arsenide (Cd 3 As 2 ) would be great a candidate for PTE detectors.</p><p>Reported room-temperature values for the Seebeck coefficient of Cd 3 As 2 range from 60 lV/K up to a remarkable 600 lV/K, <ref type="bibr">[10]</ref><ref type="bibr">[11]</ref><ref type="bibr">[12]</ref><ref type="bibr">[13]</ref> which, combined with its broadband absorption of light across mid-infrared wavelengths, <ref type="bibr">14,</ref><ref type="bibr">15</ref> high room-temperature charge carrier mobility, <ref type="bibr">16</ref> and low thermal conductivity, <ref type="bibr">12,</ref><ref type="bibr">17</ref> indicate its potential for midinfrared photodetectors based on the PTE. A Cd 3 As 2 -based PTE detector for operation in the near-IR (1.064 lm) has previously been demonstrated. <ref type="bibr">18</ref> It was also suggested that the PTE played a role in reports of broadband (532 nm to 10.6 lm) photoresponses of Cd 3 As 2 nanowires and platelets. <ref type="bibr">19</ref> Despite these promising results, challenges remain in realizing practical Cd 3 As 2 -based photodetectors at midinfrared wavelengths. For example, Cd 3 As 2 -based nanostructures are difficult to scale into practical devices. Furthermore, Pauli blocking can reduce light absorption in Cd 3 As 2 at longer infrared wavelengths, <ref type="bibr">14,</ref><ref type="bibr">15</ref> potentially limiting the responsivity of a PTE detector. Such limitations could be overcome by improving our understanding of PTEs in epitaxial heterostructures of Cd 3 As 2 , which is the focus of this study.</p><p>In this study, we demonstrate mid-IR photodetection in planar, unbiased metal-Cd 3 As 2 -metal devices on a III-V heterostructure. We characterize photocurrents and device responsivity under illumination with a 10.4-lm-wavelength laser at room temperature. We show that the direction of the photocurrent depends on which end of the channel is illuminated, consistent with the development of a thermal gradient and the PTE. We also discuss the role of plasmon excitations and losses in the gold contacts in the detection of mid-infrared radiation in these devices.</p><p>A 400-nm-thick (001) Cd 3 As 2 film was grown by molecular beam epitaxy (MBE) on a (001) Al 0.47 In 0.53 Sb buffer layer/(001) GaSb substrate heterostructure, as reported elsewhere. <ref type="bibr">20</ref> The buffer layer is lattice-matched to the Cd 3 As 2 film. Van der Pauw room-temperature Hall and sheet resistance measurements (see supplementary material Fig. <ref type="figure">S1</ref>) yielded a resistivity of 2.7 &#194; 10 &#192;4 X cm, an n-type carrier density of 2.3 &#194; 10 18 cm &#192;3 , and a mobility of 10,000 cm 2 /V s. The photodetectors were patterned using photolithography and electron beam evaporation techniques. The devices consisted of pairs of 100 lmwide, rectangular Ti/Pt/Au (25 nm/25 nm/250 nm) metal strips deposited on the surface of the Cd 3 As 2 film with variable channel spacings between the strips. 200 lm &#194; 200 lm pads were used for wire bonding. Figure <ref type="figure">1</ref> shows a schematic of the device and heterostructure, while Photocurrent measurements were performed at normal incidence by connecting the devices in series with an Ithaco model1211 current preamplifier or a 1.00 X shunt resistor and focusing the output of a collimated 10.40 6 0.02 lm wavelength quantum cascade laser onto the devices. The approximate beam spot diameter was 100 lm. The preamplifier (shunt resistor) converted the short-circuit photocurrent to a voltage (voltage drop), which was recorded with an oscilloscope. In the case of the shunt resistor, the voltage drop was amplified with an SR560 voltage preamplifier with a 10 kHz low-pass filter. This method avoided the unintentional bias (of approximately 1-10 lV) applied by the Ithaco model1211 current preamplifier. All photocurrent measurements were performed in the dark and at room temperature. Devices were not externally biased, unless stated otherwise. Figure <ref type="figure">2</ref>(b) shows the photocurrent response of the 250 lm device depicted in Fig. <ref type="figure">2</ref>(a) at an incident beam power of 69.4 mW, measured with the 1.00 X shunt resistor. When the beam position is moved from one contact toward the other, the direction of the photocurrent reverses, while the magnitude of the photocurrent remains nearly the same. When the beam is centered between the two contacts [orange curve in Fig. <ref type="figure">2(b)</ref>], the photocurrent vanishes. The photocurrent responses of the devices with l c &#188; 25 lm and l c &#188; 1000 lm behave similarly (see supplementary material Figs. <ref type="figure">S3</ref> and <ref type="figure">S4</ref>).</p><p>The PTE effect can give rise to a photocurrent in the absence of an external bias, via the generation of a net temperature gradient in the Cd 3 As 2 channel through localized heating. In a short-circuit configuration, such as used in our experiments, the magnitude of the photocurrent in the device is approximately given by </p><p>where S is the Seebeck coefficient, DT is the temperature difference, and R d is the resistance of the device, which includes the channel resistance and the shunt resistance (1.00 X). Moving the beam from one end of the device to the other reverses the direction of the thermal gradient, leading to the sign reversal of the photocurrent, consistent with our observations. In contrast, when the beam is centered in the middle of the channel, the majority charge carriers diffuse in opposite directions, from the hot center to the cold contacts on either side of the device, resulting in net-zero photocurrent. Based on the direction of the photocurrent and how the voltage preamplifier is connected to the shunt resistor and contacts, S is negative, in agreement with thick Cd 3 As 2 films being n-type, 20 similar to bulk Cd 3 As 2 . <ref type="bibr">21,</ref><ref type="bibr">22</ref> Figure <ref type="figure">2</ref>(c) shows the photocurrent, measured using a lock-in amplifier, as a function of incident laser power (P) and device channel length with the beam positioned on the left side [yellow circle in Fig. <ref type="figure">2(a)</ref>]. For comparison, measurements from the Al 0.47 In 0.53 Sb channel reference devices are also shown. The lines are power-law fits, I &#188; bP a , where a and b are fit parameters. Here, a % 0.96-1.00 for all devices, indicating a nearly linear response over the full range of incident powers. The 250 lm device has a larger responsivity than both the 1000 and 25 lm devices. For large l c (1000 lm), it is likely that the increased channel resistance reduces the photocurrent, see Eq. (1) and Fig. <ref type="figure">1(b)</ref>. The large beam size (100 lm) limited the thermal gradient [DT In Eq. ( <ref type="formula">1</ref>)] that could be established in the shorter devices (l c &#188; 25 lm), leading to a reduced response. Notably, the photocurrent measured in the Al 0.47 In 0.53 Sb channel devices was more than an order of magnitude smaller than in the Cd 3 As 2 channel devices, due to their larger channel resistance and smaller Seebeck coefficient. The responsivity is given by R &#188; I/P and was approximately 0.17 mA/W for the 250 lm device, comparable to Cd 3 As 2 nanoplate PTE detectors operating at 1.064 lm (0.27 mA/W 18 ) and at 10.6 lm (0.22 mA/W <ref type="bibr">19</ref> ), respectively. The photocurrent rise time (from 10% to 90% of its saturated value) ranges from 70 to 90 ms. For comparison (see Fig. <ref type="figure">3</ref>), we also fabricated a bolometric photodetector having a similar device geometry and heterostructure, by depositing a continuous Au strip on Cd 3 As 2 . When biased, the bolometric device shows a response time that is almost an order of magnitude larger ($500 ms), consistent with the response being governed by heating of the lattice, which is intrinsically slow. This comparison indicates that there are faster mechanisms involved in the PTE-based photodetection, which may potentially be exploited to improve the response times.</p><p>To optimize the Cd 3 As 2 thin film photodetectors, a comprehensive understanding of the processes involved in the PTE in our devices is required. This includes the role of absorption by the Au contacts, which may result in indirect heating of the Cd 3 As 2 film. While Au is 99% reflective at a wavelength of 10.4 lm, <ref type="bibr">23</ref> plasmon excitations and their losses have previously been used for local heating of PTE-based photodetectors. <ref type="bibr">9,</ref><ref type="bibr">24</ref> Heating via surface or interface plasmon losses can occur on picosecond timescales via the generation of hot charge carriers. <ref type="bibr">25</ref> Time-resolved photocurrent measurements would, thus, help elucidating the different mechanisms that result in the PTE in the devices. Such measurements are challenging in the mid-infrared, but several approaches have been reported in the literature. <ref type="bibr">26,</ref><ref type="bibr">27</ref> To summarize, we have shown that the PTE is responsible for photocurrent generation in planar metal-Cd 3 As 2 -metal photodetectors operating in the mid-infrared (10.4 lm). The photodetectors, which require no external bias to operate and are simple to fabricate, promise opportunities for optimization and miniaturization for enhanced room-temperature mid-infrared photodetection.</p><p>See the supplementary material for additional figures showing results from van der Pauw measurements, I-V data of the reference sample, photoresponses of devices with different channel lengths, and the photocurrent as a function of incident beam power for a different position of the incident beam.</p></div><note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_0"><p>Published under an exclusive license by AIP Publishing</p></note>
			<note xmlns="http://www.tei-c.org/ns/1.0" place="foot" xml:id="foot_1"><p>Appl. Phys. Lett. 126, 181102 (2025); doi: 10.1063/5.0272453</p></note>
		</body>
		</text>
</TEI>