This content will become publicly available on March 15, 2027

Title: Evaluation of Hydrogen Embrittlement Susceptibility in Pipeline Steel Welds
Abstract Slow strain rate, fatigue crack growth rate, and fracture toughness (respectively SSRT, FCGR, and FT) tests in high pressure gaseous hydrogen are used in evaluating hydrogen embrittlement (HE) susceptibility of pipelines steels welds. The applicability of these tests to pipeline service conditions in stress-based design (below YS) or up to 5% strain in strain-based design is limited. SSRT demonstrates effects of HE at loading above UTS. FCGR and FT tests quantify resistance to propagation of existing cracks but cannot characterize susceptibility to HE crack nucleation. We present HE susceptibility results generated using the delayed hydrogen cracking test (DHCT), standardized as AMPP TM21453-2023. DHCT applies a constant tensile load below or slightly above the material YS on flat gauge section specimens subjected to electrolytic charging with hydrogen. HE susceptibility is quantified by the time to failure and the mechanical energy for crack nucleation and growth to critical size. The paper draws a parallel between the HE phenomena introduced by the SSRT, FCGR, FT tests and DHCT, in terms of hydrogen absorption and transportation effects on the crack nucleation and propagation mechanisms. The mechanical energy introduced by these tests and the resulting failure mechanisms are compared and discussed.  more » « less
Award ID(s):
2052747
PAR ID:
10685696
Author(s) / Creator(s):
;
Publisher / Repository:
AMPP
Date Published:
Page Range / eLocation ID:
1 to 13
Subject(s) / Keyword(s):
hydrogen embrittlement, delayed hydrogen cracking test
Format(s):
Size: 2.39 MB Other: pdf
Size(s):
2.39 MB
Location:
Houston, Texas
Sponsoring Org:
National Science Foundation
More Like this
  1. Abstract The objective of this study was to investigate the applicability of the delayed hydrogen cracking test (DHCT), standardized as AMPP TM21453, for evaluating hydrogen embrittlement (HE) susceptibility in pipeline steel welds. A comparative analysis of the HE mechanisms induced by the DHCT and the slow strain rate test (SSRT) was performed by quantifying the mechanical energy of crack nucleation and propagation in failures induced by these tests. The DHCT applies a static tensile load below the material yield strength (YS) in an electrochemically generated atomic hydrogen environment. Test results of X65 PSL2 steel welds demonstrated that the DHCT generates low-energy HE failures, associated with brittle QC and IG mechanisms, and can differentiate the effects of microstructure and weld profile-induced stress concentration on HE susceptibility. SSRT, performed in atomic hydrogen, induced brittle failures at plastic strains below 2%, showing potential application for evaluating HE susceptibility in pipeline welds for strain-based design service. Analysis of published results from SSRT in high-pressure gaseous hydrogen revealed that the related failure mechanism absorbs mechanical energy of up to three orders of magnitude higher than the DHCT. This was attributed to the large magnitude of plastic strain generated at loading above the material UTS, which is necessary for absorbing a sufficient amount of hydrogen to initiate HE failures. 
    more » « less
  2. null (Ed.)
    Abstract Articular cartilage heals poorly but experiences mechanically induced damage across a broad range of loading rates and matrix integrity. Because loading rates and matrix integrity affect cartilage mechanical responses due to poroviscoelastic relaxation mechanisms, their effects on cartilage failure are important for assessing and preventing failure. This paper investigated rate- and integrity-dependent crack nucleation in cartilage from pre- to post-relaxation timescales. Rate-dependent crack nucleation and relaxation responses were obtained as a function of matrix integrity through microindentation. Total work for crack nucleation increased with decreased matrix integrity, and with decreased loading rates. Critical energy release rate of intact cartilage was estimated as 2.39 ± 1.39 to 2.48 ± 1.26 kJ m −2 in a pre-relaxation timescale. These findings showed that crack nucleation is delayed when cartilage can accommodate localized loading through poroviscoelastic relaxation mechanisms before fracture at a given loading rate and integrity state. 
    more » « less
  3. Water ice Ih exhibits brittle behavior when rapidly loaded. Under tension, it fails via crack nucleation and propagation. Compressive failure is more complicated. Under low confinement, cracks slide and interact to form a frictional (Coulombic) fault. Under high confinement, frictional sliding is suppressed and adiabatic heating through crystallographic slip leads to the formation of a plastic fault. The coefficient of static friction increases with time under load, owing to creep of asperities in contact. The coefficient of kinetic (dynamic) friction, set by the ratio of asperity shear strength to hardness, increases with velocity at lower speeds and decreases at higher speeds as contacts melt through frictional heating. Microcracks, upon reaching a critical number density (which near the ductile-to-brittle transition is nearly constant above a certain strain rate), form a pathway for percolation. Additional work is needed on the effects of porosity and crack healing. ▪ An understanding of brittle failure is essential to better predict the integrity of the Arctic and Antarctic sea ice covers and the tectonic evolution of the icy crusts of Enceladus, Europa, and other extraterrestrial satellites. ▪ Fundamental to the brittle failure of ice is the initiation and propagation of microcracks, frictional sliding across crack faces, and localization of strain through both crack interaction and adiabatic heating. 
    more » « less
  4. This study investigates the effects of pores on the mechanical properties of metals produced by additive manufacturing, which can limit strength and ductility. This research aims to both measure and model the rate of crack growth emanating from these pores in additively manufactured Ti-6Al-4 V fabricated with laser powder bed fusion. Uniaxial tensile samples containing intentionally embedded penny-shaped pores were mechanically tested to failure, and loading was interrupted by a series of unload steps to measure the stiffness degradation with load. The factors contributing to reduction in stiffness, namely (1) elastic and plastic changes to geometry, (2) the effect of plastic deformation on modulus, and (3) crack growth, were deconvoluted through finite element modeling, and the crack size was estimated at each unloading step. The stiffness-based method was able to detect stable crack growth in samples with large pores (1.6% to 11% of the cross-sectional area). Crack growth as a function of strain was fit to a model where the crack driving force was based on equivalent strain and a model where the crack driving force was based on energy release rate. Significant crack growth occurred only after the onset of necking in samples containing small pores, while samples containing large pores experienced continuous crack growth with strain. 
    more » « less
  5. Abstract This work presents quantitative investigations into the relationships between lithium dendrite growth in the defects of Li6PS5Cl (LPSCl) solid electrolyte (SE), crack nucleation and propagation in the SE, and the associated mechanical forces driving these dendrites and cracks. Two different growth modes for lithium dendrites are identified by ex situ scanning electron microscopy (SEM) observation: longitudinal cracking inside pores in the SE and lateral penetration along boundaries of the SE particles. These in situ TEM tests reveal that concentrated Li plating in a nano‐sized defect on the LPSCl surface will lead to the nucleation and propagation of cracks into the LPSCl under a stress much smaller than the expected mechanical strength of the LPSCl material. This unexpected mechanical degradation is caused by a reduction in the mechanical strength of LPSCl during electrochemical charge/discharge cycling, resulting from a disorder in the crystal structure of LPSCl as revealed by DFT simulations. Due to this mechanical degradation of LPSCl, the threshold force necessary to initiate crack growth is much lower than the previously expected force to drive dendrite growth. 
    more » « less