Ga-containing oxides are selective catalysts for high-temperature hydrocarbon oxidations such as alkane dehydrogenation. The active sites are proposed to have an oxidation state of either +1 or +3 and bear a combination of hydride and alkyl ligands, in addition to oxygen-donor ligands associated with the support. Activating Ga/-Al2O3 or Ga/ZSM5 in H2 at or above 473 K causes the Ga K-edge to (1) shift decisively to lower energy, and (2) increase significantly in its white line intensity. Taken together, these behaviors are shown to be signatures for Ga(III) reduction. The extent of Ga(I) formation, assessed by quantitative XANES analysis, varies with temperature, H2 pressure, and the nature of the support. In addition, H2 causes strong suppression of the EXAFS amplitude. The origin of the latter phenomenon was investigated by analyzing Ga(I) EXAFS signatures in two well-defined model compounds: mixed-valent Ga2Cl4 and Ga(I)-β´´-Al2O3. Theoretical simulations show the EXAFS “invisibility” of Ga(I) at non-cryogenic temperatures is a direct result of anomalously large vibrational amplitudes. Due to its valence electron configuration and largely unhybridized 4p orbitals, Ga(I) forms very long, labile bonds whose mean-squared relative displacements (σ2) are an order of magnitude higher compared to the shorter, stronger bonds of Ga(III). Consequently, EXAFS signals for materials containing a mixture of Ga oxidation states are virtually devoid of structural information about the Ga(I) sites, being dominated instead by scattering paths involving residual Ga(III) sites. At reaction temperatures in the H2-activated catalysts, hydrides are at best minority species, accompanying the majority Ga(I) sites. These insights set the stage for quantitative analysis of Ga speciation during alkane dehydrogenation, and elucidation of the structure(s) of the active sites. Furthermore, they have broad implications for the use of X-ray spectroscopy to extract structure-property relations for catalysts and other materials containing Ga(I) or other weakly-bonded and highly dynamic metal ions.
more »
« less
This content will become publicly available on September 1, 2027
Rapid Migration of Oxide-Supported Ga(I) Ions, and Consequences for Catalytic Propane Dehydrogenation
Ga-containing oxides have been widely investigated as catalysts for acceptorless propane dehydrogenation. During catalyst activation by H2 at elevated temperatures, Ga can migrate. Nevertheless, the PDH active sites have not typically been considered mobile under reaction conditions. Evidence for mobility during activation is indirect and consists largely of changes in the hydroxyl population, observed using IR spectroscopy. In this study, Magic-Angle Spinning NMR and IR spectroscopies, STEM-EDS, and conventional kinetic measurements are enhanced by analysis of the in situ XANES. They establish that Ga(I) is the highly mobile species, and that it can interconvert with active sites. Since the XANES signatures differ significantly for Ga(I)/SiO2 vs Ga(I)/ZSM-5, it was possible using linear combination fitting to monitor and quantify the dynamic redistribution of Ga species in physical mixtures of SiO2 and HZSM-5. Under H2, Ga(III) is reduced to Ga(I), which then diffuses rapidly between SiO2 and ZSM-5 particles whose diameters are ca. 200 μm. This migration can occur in both directions, and is significantly faster than Ga(III) reduction. As a result, a mixture of weakly active Ga/SiO2 and HZSM-5 shows a PDH activity approaching that of highly active Ga/ZSM-5. Thermodynamic analysis of the equilibrium populations on both supports suggests an enthalpic preference for Ga(III) and an entropic preference for Ga(I). Ga ions in both oxidation states are enthalpically more stable on HZSM-5, while Ga association with SiO2 is likely entropically favored. These thermodynamic preferences, in combination with long-range Ga(I) mobility, predict and explain the temperature-dependent redistribution of Ga species between oxidation states, across supports, and even onto catalyst bed diluents under reducing conditions. The high mobility of Ga(I) during catalyst activation and under reaction conditions enables Ga to sample a large range of environments, challenging long-standing assumptions about the ability to precisely synthesize single-site Ga catalysts for alkane dehydrogenation.
more »
« less
- PAR ID:
- 10713631
- Publisher / Repository:
- American Chemical Society
- Date Published:
- Journal Name:
- ACS Catalysis
- ISSN:
- 2155-5435
- Subject(s) / Keyword(s):
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
Ethane dehydroaromatization (EDA) is a potentially attractive process for converting ethane to valuable aromatics such as benzene, toluene, and xylene (BTX). In this study, a Pt3Mn/SiO2 + ZSM-5 bifunctional catalyst was used to investigate the effect of dehydrogenation and the Brønsted acid catalyst ratio, hydrogen partial pressure, and reaction temperature on the product distributions for EDA. Pt3Mn/SiO2 + ZSM-5 with a 1/1 weight ratio showed the highest ethane conversion rate and BTX formation rate. Ethylene is initially formed by dehydrogenation by the Pt3Mn catalyst, which undergoes secondary reactions on ZSM-5, forming C3+ reaction intermediates. The latter form final products of CH4 and BTX. At conversions from 15 to 30%, the BTX selectivities are 82–90%. For all bifunctional catalysts, the ethane conversion significantly exceeds the ethane–ethylene equilibrium conversion due to reaction to secondary products. Low H2 partial pressures did not significantly alter the product selectivity or conversion. However, higher H2 partial pressures resulted in increased methane and decreased BTX selectivity. The excess hydrogen saturated the olefin intermediates to form alkanes, which produced methane by monomolecular cracking on ZSM-5. With an increasing reaction temperature from 550 °C to 650 °C, the benzene selectivity increased, while the highest BTX selectivity was obtained at 600 to 650 °C.more » « less
-
Methane activation remains a grand challenge in catalysis science and reaction engineering. Under nonoxidative conditions, this is likely not due to the intrinsic inertness of CH4 molecules, but because activity must be balanced with selectivity and long-term stability of catalysts. We clarify that the C–H bond dissociation enthalpy (BDE) of methane, while large, is a poor metric for the catalytic reactivity of methane: BDE is a gas-phase quantity that neither dictates the reaction free energy nor the site-specific activation free energy relevant to reaction pathways. Guided by thermodynamic analysis of non-oxidative coupling of methane (NOCM) and kinetic evidence on Pt-based catalysts, we show that rapid deactivation via deep dehydrogenation and coking dominates catalytic performance limits. We advance selective passivized catalysis (SPC) as a differentiated catalyst design strategy in which a fraction of overly active sites is deliberately shielded, ex situ (e.g., alloying, support modification, geometric confinement) or in situ (reaction-induced passivation), to suppress undesired pathways while preserving sites that promote desired products. SPC reconciles activity with stability and has delivered sustained NOCM performance with C2 selectivities >90% on Pt–Bi/ZSM-5 and stable operation using Pt nanolayers on Mo2TiC2Tx MXene. We outline mechanistic scenarios for solely heterogeneous NOCM and highlight operando characterization (EPR, MBMS) to resolve radical vs. surface-mediated routes. In this Feature Article, we review that selective passivized catalysis provides a rational blueprint to stabilize methane activation and bring NOCM closer to practical relevance.more » « less
-
Recently, stable non-oxidative conversion of methane (NOCM) for up to 8 h with a C 2 selectivity greater than 90% has been reported over Pt–Bi/ZSM-5 at moderate temperatures (600–700 °C). In this study, we show that the structure of the bimetallic nanoparticles on Pt–Bi/ZSM-5 catalyst is similar to Pt–Bi/SiO 2 . EXAFS indicates the formation of Pt-rich bimetallic Pt–Bi nanoparticles with Pt–Bi bond distance of 2.80 Å. The XRD spectra (on SiO 2 ) are consistent with cubic, intermetallic surface Pt 3 Bi phase on a Pt core. The Pt 3 Bi structure is not known in the thermodynamic phase diagram. In all catalysts, only a small fraction of Bi alloys with Pt. At high Bi loadings, excess Bi reduces at high temperature, covering the catalytic surface leading to a loss in activity. At lower Bi loadings with little excess Bi, the Pt 3 Bi surface is effective for non-oxidative coupling of CH 4 (on ZSM-5) and propane dehydrogenation (on SiO 2 ).more » « less
-
null (Ed.)Nonoxidative alkane dehydrogenation is a promising route to produce olefins, commonly used as building blocks in the chemical industry. Metal oxides, including γ-Al 2 O 3 and β-Ga 2 O 3 , are attractive dehydrogenation catalysts due to their surface Lewis acid–base properties. In this work, we use density functional theory (DFT) to investigate nonoxidative dehydrogenation of ethane, propane, and isobutane on the Ga-doped and undoped (100) γ-Al 2 O 3 via the concerted and stepwise mechanisms. We revealed that doping (100) γ-Al 2 O 3 with Ga atoms has significant improvement in the dehydrogenation activity by decreasing the C–H activation barriers of the kinetically favored concerted mechanism and increasing the overall dehydrogenation turnover frequencies. We identified the dissociated H 2 binding energy as an activity descriptor for alkane dehydrogenation, accounting for the strength of the Lewis acidity and basicity of the active sites. We demonstrate linear correlations between the dissociated H 2 binding energy and the activation barriers of the rate determining steps for both the concerted and stepwise mechanisms. We further found the carbenium ion stability to be a quantitative reactant-type descriptor, correlating with the C–H activation barriers of the different alkanes. Importantly, we developed an alkane dehydrogenation model that captures the effect of catalyst acid–base surface properties (through dissociated H 2 binding energy) and reactant substitution (through carbenium ion stability). Additionally, we show that the dissociated H 2 binding energy can be used to predict the overall dehydrogenation turnover frequencies. Taken together, our developed methodology facilitates the screening and discovery of alkane dehydrogenation catalysts and demonstrates doping as an effective route to enhance catalytic activity.more » « less