Title: Plasma-enhanced atomic layer deposition of SiO 2 film using capacitively coupled Ar/O 2 plasmas: A computational investigation
Award ID(s):
2009219
PAR ID:
10337198
Author(s) / Creator(s):
; ; ;
Date Published:
Journal Name:
Journal of Vacuum Science & Technology A
Volume:
39
Issue:
5
ISSN:
0734-2101
Page Range / eLocation ID:
052403
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. null (Ed.)
    HN(CH 2 CH 2 PR 2 ) 2 -ligated copper borohydride complexes, ( R PN H P)Cu(BH 4 ) (R = i Pr, Cy, t Bu), which can be prepared from ( R PN H P)CuBr and NaBH 4 , are capable of catalyzing the hydrogenation of aldehydes in an alcoholic solvent. More active hydrogenation catalysts are ( R PN H P)CuBr mixed with KO t Bu, allowing various aldehydes and ketones to be efficiently reduced to alcohols except those bearing a nitro, N -unprotected pyrrole, pyridine, or an ester group, or those prone to aldol condensation ( e.g. , 1-heptanal). Modifying the catalyst structure by replacing the NH group in ( i Pr PN H P)CuBr with an NMe group results in an inferior catalyst but preserves some catalytic activity. The hexanuclear copper hydride cluster, ( i Pr PN H P) 3 Cu 6 H 6 , is also competent in catalyzing the hydrogenation of aldehydes such as benzaldehyde and N -methyl-2-pyrrolecarboxaldehyde, albeit accompanied by decomposition pathways. The catalytic performance can be enhanced through the addition of a strong base or i Pr PN H P. The three catalytic systems likely share the same catalytically active species, which is proposed to be a mononuclear copper hydride ( R PN H P)CuH with the NH group bound to copper. 
    more » « less
  2. Abstract Organofunctionalized tetranuclear clusters [(MIICl)2(VIVO)2{((HOCH2CH2)(H)N(CH2CH2O))(HN(CH2CH2O)2)}2] (1, M=Co,2: M=Zn) containing an unprecedented oxometallacyclic {M2V2Cl2N4O8} (M=Co, Zn) framework have been prepared by solvothermal reactions. The new oxo‐alkoxide compounds were fully characterized by spectroscopic methods, magnetic susceptibility measurement, DFT and ab initio computational methods, and complete single‐crystal X‐ray diffraction structure analysis. The isostructural clusters are formed of edge‐sharing octahedral {VO5N} and trigonal bipyramidal {MO3NCl} units. Diethanolamine ligates the bimetallic lacunary double cubane core of1and2in an unusual two‐mode fashion, unobserved previously. In the crystalline state, the clusters of1and2are joined by hydrogen bonds to form a three‐dimensional network structure. Magnetic susceptibility data indicate weakly antiferromagnetic interactions between the vanadium centers [Jiso(VIV−VIV)=−5.4(1); −3.9(2) cm−1], and inequivalent antiferromagnetic interactions between the cobalt and vanadium centers [Jiso(VIV−CoII)=−12.6 and −7.5 cm−1] contained in1. 
    more » « less
  3. High-resolution X-ray diffraction experiments, theoretical calculations and atom-specific X-ray absorption experiments were used to investigate two nickel complexes, (MePh 3 P) 2 [Ni II (bdtCl 2 ) 2 ]·2(CH 3 ) 2 SO [complex (1)] and (MePh 3 P)[Ni III (bdtCl 2 ) 2 ] [complex (2)]. Combining the techniques of nickel K - and sulfur K -edge X-ray absorption spectroscopy with high-resolution X-ray charge density modeling, together with theoretical calculations, the actual oxidation states of the central Ni atoms in these two complexes are investigated. Ni ions in two complexes are clearly in different oxidation states: the Ni ion of complex (1) is formally Ni II ; that of complex (2) should be formally Ni III , yet it is best described as a combination of Ni 2+ and Ni 3+ , due to the involvement of the non-innocent ligand in the Ni— L bond. A detailed description of Ni—S bond character (σ,π) is presented. 
    more » « less