All‐solid‐state sodium batteries, using solid electrolyte and abundant sodium resources, show great promise for safe, low‐cost, and large‐scale energy storage applications. The exploration of novel solid electrolytes is critical for the room temperature operation of all‐solid‐state Na batteries. An ideal solid electrolyte must have high ionic conductivity, hold outstanding chemical and electrochemical stability, and employ low‐cost synthetic methods. Achieving the combination of these properties is a grand challenge for the synthesis of sulfide‐based solid electrolytes. Design of the solid electrolyte Na3SbS4is described, realizing excellent air stability and an economic synthesis based on hard and soft acid and base (HSAB) theory. This new solid electrolyte also exhibits a remarkably high ionic conductivity of 1 mS cm−1at 25 °C and ideal compatibility with a metallic sodium anode.
- Award ID(s):
- 1825470
- PAR ID:
- 10346251
- Date Published:
- Journal Name:
- Journal of The Electrochemical Society
- Volume:
- 168
- Issue:
- 11
- ISSN:
- 0013-4651
- Page Range / eLocation ID:
- 110533
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
Abstract -
Synthesis of high-purity Li 2 S nanocrystals via metathesis for solid-state electrolyte applicationsLi 2 S is the key precursor for synthesizing thio-LISICON electrolytes employed in solid state batteries. However, conventional synthesis techniques such as carbothermal reduction of Li 2 SO 4 aren't suitable for the generation of low-cost, high-purity Li 2 S. Metathesis, in which LiCl is reacted with Na 2 S in ethanol, is a scalable synthesis method conducted at ambient conditions. The NaCl byproduct is separated from the resulting Li 2 S solution, and the solvent is removed by evaporation and thermal annealing. However, the annealing process reveals the presence of oxygenated impurities in metathesis Li 2 S that are not usually observed when recovering Li 2 S from ethanol. In this work we investigate the underlying mechanism of impurity formation, finding that they likely derive from the decomposition of alkoxide species that originate from the alcoholysis of the Na 2 S reagent. With this mechanism in mind, several strategies to improve Li 2 S purity are explored. In particular, drying the metathesis Li 2 S under H 2 S at low temperature was most effective, resulting in high-purity Li 2 S while retaining a beneficial nanocrystal morphology (∼10 nm). Argyrodite electrolytes synthesized from this material exhibited essentially identical phase purity, ionic conductivity (3.1 mS cm −1 ), activation energy (0.19 eV), and electronic conductivity (6.4 × 10 −6 mS cm −1 ) as that synthesized from commercially available battery-grade Li 2 S.more » « less
-
Abstract All‐solid‐state sodium‐ion batteries are highly promising for next generation grid energy storage with improved safety. Among the known sodium superionic conductors, the Na3PnS4family and the recently discovered Na11Sn2PnS12(Pn = P, Sb) have garnered major interest due to their extremely high ionic conductivities. In this work, comprehensive investigation of the Na3PnS4‐Na4TtS4(Pn = P/As/Sb, Tt = Si/Ge/Sn) phase space of superionic conductors using density functional theory calculations, as well as AIMD simulations on the promising new Na11Sn2PnS12(Pn=P/As/Sb) structures are presented. Crucial design rules on the effect of cation mixing are extracted on relative phase stability, electrochemical stability, moisture stability, and ionic conductivity. In particular, it is shown that while larger cations can substantially improve the ionic conductivity and moisture stability in these structures, there is an inherent trade‐off in terms of electrochemical stability. Na11Sn2AsS12is also identified as a hitherto unexplored stable sodium superionic conductor with higher Na+conductivity and better moisture stability than the Na11Sn2PS12and Na11Sn2SbS12phases already reported experimentally.
-
Abstract All‐solid‐state potassium batteries emerge as promising alternatives to lithium batteries, leveraging their high natural abundance and cost‐effectiveness. Developing potassium solid electrolytes (SEs) with high room‐temperature ionic conductivity is critical for realizing efficient potassium batteries. In this study, we present the synthesis of K2.98Sb0.91S3.53Cl0.47, showcasing a room‐temperature ionic conductivity of 0.32 mS/cm and a low activation energy of 0.26 eV. This represents an increase of over two orders of magnitude compared to the parent compound K3SbS4, marking the highest reported ionic conductivity for non‐oxide potassium SEs. Solid‐state39K magic‐angle‐spinning nuclear magnetic resonance on K2.98Sb0.91S3.53Cl0.47reveals an increased population of mobile K+ions with fast dynamics. Ab initio molecular dynamics (AIMD) simulations further confirm a delocalized K+density and significantly enhanced K+diffusion. This work demonstrates diversification of the anion sublattice as an effective approach to enhance ion transport and highlights K2.98Sb0.91S3.53Cl0.47as a promising SE for all‐solid‐state potassium batteries.
-
Abstract NASICON‐type sodium vanadium phosphate (Na3V2(PO4)3, or NVP) cathode materials have great potential for fast charging and long cycling sodium‐ion batteries (SIBs) similar to lithium iron phosphate (LiFePO4, or LFP) cathode materials used in lithium‐ion batteries (LIBs). However, the cycle life and energy density in the full cell using NVP materials need to be significantly improved. This paper investigates the degradation mechanisms of NVP‐based SIBs and identifies the Na loss from the cathode to the anode solid electrolyte interphase (SEI) reactions as the main cause of capacity degradation. A new Na‐rich NVP cathode (e.g., Na4V2(PO4)3, or Na4VP) is developed to address the Na loss problem. Conventional NVP can be easily transformed into the Na4VP by a facile and fast chemical solution treatment (30 s). Na‐free‐anode Na4VP and hard carbon‐Na4VP full cells are assembled to evaluate the electrochemical properties of the Na‐rich NVP cathode. The Na4VP cathode provides excess Na to compensate for the Na loss, resulting much longer cycle life in the full cells (>400 cycles) and a high specific energy and power density. Good low‐temperature performance is also observed.