Engineering oxygen vacancy-rich CeOx overcoating onto Ni/Al2O3 by atomic layer deposition for bi-reforming of methane
- Award ID(s):
- 2306177
- PAR ID:
- 10442487
- Date Published:
- Journal Name:
- Chemical Engineering Journal
- Volume:
- 459
- Issue:
- C
- ISSN:
- 1385-8947
- Page Range / eLocation ID:
- 141611
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation