Title: Elucidating the Impact of Mg Substitution on the Properties of NASICON‐Na 3+ y V 2− y Mg y (PO 4 ) 3 Cathodes
Abstract

Vanadium multiredox‐based NASICON‐NazV2−yMy(PO4)3(3 ≤z ≤ 4; M = Al3+, Cr3+, and Mn2+) cathodes are particularly attractive for Na‐ion battery applications due to their high Na insertion voltage (>3.5 V vs Na+/Na0), reversible storage capacity (≈150 mA h g−1), and rate performance. However, their practical application is hindered by rapid capacity fade due to bulk structural rearrangements at high potentials involving complex redox and local structural changes. To decouple these factors, a series of Mg2+‐substituted Na3+yV2−yMgy(PO4)3(0 ≤y ≤ 1) cathodes is studied for which the only redox‐active species is vanadium. While X‐ray diffraction (XRD) confirms the formation of solid solutions between they = 0 and 1 end members, X‐ray absorption spectroscopy and solid‐state nuclear magnetic resonance reveal a complex evolution of the local structure upon progressive Mg2+substitution for V3+. Concurrently, the intercalation voltage rises from 3.35 to 3.45 V, due to increasingly more ionic VO bonds, and the sodium (de)intercalation mechanism transitions from a two‐phase fory ≤ 0.5 to a solid solution process fory ≥ 0.5, as confirmed by in operando XRD, while Na‐ion diffusion kinetics follow a nonlinear trend across the compositional series.

 
more » « less
NSF-PAR ID:
10448210
Author(s) / Creator(s):
 ;  ;  ;  ;  ;  ;  ;  ;  ;  
Publisher / Repository:
Wiley Blackwell (John Wiley & Sons)
Date Published:
Journal Name:
Advanced Functional Materials
Volume:
31
Issue:
48
ISSN:
1616-301X
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. Abstract

    All‐solid‐state rechargeable sodium (Na)‐ion batteries are promising for inexpensive and high‐energy‐density large‐scale energy storage. In this contribution, new Na solid electrolytes, Na3−yPS4−xClx, are synthesized with a strategic approach, which allows maximum substitution of Cl for S (x= 0.2) without significant compromise of structural integrity or Na deficiency. A maximum conductivity of 1.96 mS cm−1at 25 °C is achieved for Na3.0PS3.8Cl0.2, which is two orders of magnitude higher compared with that of tetragonal Na3PS4(t‐Na3PS4). The activation energy (Ea) is determined to be 0.19 eV. Ab initio molecular dynamics simulations shed light on the merit of maximizing Cl‐doping while maintaining low Na deficiency in enhanced Na‐ion conduction. Solid‐state nuclear magnetic resonance (NMR) characterizations confirm the successful substitution of Cl for S and the resulting change of P oxidation state from 5+ to 4+, which is also verified by spin moment analysis. Ion transport pathways are determined with a tracer‐exchange NMR method. The functional detects that promote Na ‐ion transport are maximized for further improvement in ionic conductivity. Full‐cell performance is demonstrated using Na/Na3.0PS3.8Cl0.2/Na3V2(PO4)3with a reversible capacity of ≈100 mAh g‐1at room temperature.

     
    more » « less
  2. Abstract

    Deep sodium extraction/insertion of sodium cathodes usually causes undesired Jahn–Teller distortion and phase transition, both of which will reduce structural stability and lead to poor long‐cycle reliability. Here we report a zero‐strain P2‐ Na2/3Li1/6Co1/6Mn2/3O2cathode, in which the lithium/cobalt substitution contributes to reinforcing the host structure by reducing the Mn3+/Mn4+redox, mitigating the Jahn–Teller distortion, and minimizing the lattice change. 94.5 % of Na+in the unit structure can be reversibly cycled with a charge cut‐off voltage of 4.5 V (vs. Na+/Na). Impressively, a solid‐solution reaction without phase transitions is realized upon deep sodium (de)intercalation, which poses a minimal volume deviation of 0.53 %. It attains a high discharge capacity of 178 mAh g−1, a high energy density of 534 Wh kg−1, and excellent capacity retention of 95.8 % at 1 C after 250 cycles.

     
    more » « less
  3. Abstract

    Deep sodium extraction/insertion of sodium cathodes usually causes undesired Jahn–Teller distortion and phase transition, both of which will reduce structural stability and lead to poor long‐cycle reliability. Here we report a zero‐strain P2‐ Na2/3Li1/6Co1/6Mn2/3O2cathode, in which the lithium/cobalt substitution contributes to reinforcing the host structure by reducing the Mn3+/Mn4+redox, mitigating the Jahn–Teller distortion, and minimizing the lattice change. 94.5 % of Na+in the unit structure can be reversibly cycled with a charge cut‐off voltage of 4.5 V (vs. Na+/Na). Impressively, a solid‐solution reaction without phase transitions is realized upon deep sodium (de)intercalation, which poses a minimal volume deviation of 0.53 %. It attains a high discharge capacity of 178 mAh g−1, a high energy density of 534 Wh kg−1, and excellent capacity retention of 95.8 % at 1 C after 250 cycles.

     
    more » « less
  4. Abstract

    Aqueous zinc‐ion batteries are receiving increasing attention; however, the development of high‐voltage cathodes is limited by the narrow voltage window of conventional aqueous electrolytes. Herein, it is reported that Na3V2(PO4)2O1.6F1.4exhibits the excellent performance, optimal to date, among polyanion cathode materials in a novel neutral water‐in‐bisalts electrolyte of 25 m ZnCl2+ 5 m NH4Cl. It delivers a reversible capacity of 155 mAh g−1at 50 mA g−1, a high average operating potential of ≈1.46 V, and stable cyclability of 7000 cycles at 2 A g−1.

     
    more » « less
  5. Abstract

    A thin solid electrolyte with a high Li+conductivity is used to separate the metallic lithium anode and the cathode in an all‐solid‐state Li‐metal battery. However, most solid Li‐ion electrolytes have a small electrochemical stability window, large interfacial resistance, and cannot block lithium‐dendrite growth when lithium is plated on charging of the cell. Mg2+stabilizes a rhombohedral NASICON‐structured solid electrolyte of the formula Li1.2Mg0.1Zr1.9(PO4)3(LMZP). This solid electrolyte has Li‐ion conductivity two orders of magnitude higher at 25 °C than that of the triclinic LiZr2(PO4)3.7Li and6Li NMR confirm the Li‐ions in two different crystallographic sites of the NASICON framework with 85% of the Li‐ions having a relatively higher mobility than the other 15%. The anode–electrolyte interface is further investigated with symmetric Li/LMZP/Li cell testing, while the cathode–electrolyte interface is explored with an all‐solid‐state Li/LMZP/LiFePO4cell. The enhanced performance of these cells enabled by the Li1.2Mg0.1Zr1.9(PO4)3solid electrolyte is stable upon repeated charge/discharge cycling.

     
    more » « less