The thin film phase behavior of ternary blends consisting of symmetric poly(styrene) (PS)‐
Ternary block copolymer (BCP)‐homopolymer (HP) blends offer a simple method for tuning nanostructure sizes to meet application‐specific demands. Comprehensive dissipative particle dynamic (DPD) simulations were performed to study the impact of polymer interactions, molecular weight, and HP volume fraction (
- Award ID(s):
- 1752611
- PAR ID:
- 10461552
- Publisher / Repository:
- Wiley Blackwell (John Wiley & Sons)
- Date Published:
- Journal Name:
- Journal of Polymer Science Part B: Polymer Physics
- Volume:
- 57
- Issue:
- 12
- ISSN:
- 0887-6266
- Page Range / eLocation ID:
- p. 794-803
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
ABSTRACT b ‐poly(dimethylsiloxane)(PDMS), PS, and PDMS was investigated using X‐ray reflectivity (XRR) and atomic force microscopy (AFM). This system is strongly segregated, and the homopolymers are approximately the same length as the corresponding blocks of the copolymer. The XRR and AFM data are used to quantify changes in domain spacing (L ) and morphology evolution with increasing homopolymer content (ΦH ). In 100 nm thick films, from ΦH = 0 to 0.20, the system maintains a perfect parallel lamellar structure and domains swell as predicted based on theory; however, from ΦH = 0.30 to 0.50, a morphology transition to a “dot pattern” morphology (tentatively identified as perforated lamellae) and mixed morphologies were observed before macrophase separation. In thicker films, dot patterns were observed for a broad range of ΦH before macrophase separation. The absence of the bicontinuous microemulsion phase reported for bulk blends and thin films of perpendicular lamellae and the presence of dot patterns/perforated lamellae are attributed to preferential migration of the PDMS homopolymer to the wetting layers located at the substrate and free air interfaces, which leads to an asymmetric composition within the film and morphology transition. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys.2018 ,56 , 1443–1451 -
ABSTRACT The ever‐growing catalog of monomers being incorporated into block polymers affords exceptional control over phase behavior and nanoscale structure. The segregation strength, χ
N , is the fundamental link between the molecular‐level detail and the thermodynamics. However, predicting phase behavior mandates at least one experimental measurement of χN for each pair of blocks. This typically requires access to the disordered state. We describe a method for estimating χN from small‐angle X‐ray scattering measurements of the interfacial width between lamellar microdomains,t x , in the microphase‐separated melt. The segregation strength is determined by comparingt x to self‐consistent field theory calculations of the intrinsic interfacial width,t i , as a function of the mean‐field χN . The method is validated using a series of independent experimental measurements oft x and χN , measured via the order–disorder transition temperature,T ODT. The average absolute relative difference between χN calculated fromt x and the value calculated fromT ODTis a modest 11%. Corrections for nonplanarity of the interfaces are investigated but do not improve the agreement between the experiments and theory. Published 2019. This article is a U.S. Government work and is in the public domain in the USA. J. Polym. Sci., Part B: Polym. Phys. 2019 © 2019 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys.2019 ,57 , 932–940 -
ABSTRACT We report the structure and thermal properties of blends comprising poly(vinylidene fluoride) (PVDF) and a random fluorinated copolymer (FCP) of poly(methyl methacrylate)‐
random ‐1H,1H,2H,2H‐perfluorodecyl methacrylate, promising membrane materials for oil–water separation. The roles of processing method and copolymer content on structure and properties were studied for fibrous membranes and films with varying compositions. Bead‐free, nonwoven fibrous membranes were obtained by electrospinning. Fiber diameters ranged from 0.4 to 1.9 μm, and thinner fibers were obtained for PVDF content >80%. As copolymer content increased, degree of crystallinity and onset of degradation for each blend decreased. Processing conditions have a greater impact on the crystallographic phase of PVDF than copolymer content. Fibers have polar beta phase; solution‐cast films contain gamma and beta phase; and melt crystallized films form alpha phase. Kwei's model was used to model the glass transition temperatures of the blends. Addition of FCP increases hydrophobicity of the electrospun membranes. © 2019 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys.2019 ,57 , 312–322 -
ABSTRACT The compatibilization effect of linear low‐density polyethylene‐grafted maleic anhydride (LLDPEgMA) and high‐density polyethylene‐grafted maleic anhydride (HDPEgMA) on high‐density polyethylene (HDPE)/polyamide 6 (Nylon 6) blend system is investigated. The morphology of 45 wt %/55 wt % polyethylene/Nylon 6 blends with three compatibilizer compositions (5 wt %, 10 wt %, and 15 wt %) are characterized by atomic force microscopic (AFM) phase imaging. The blend with 5 wt % LLDPEgMA demonstrates a Nylon 6 continuous, HDPE dispersed morphology. Increased amount of LLDPEgMA leads to sharp transition in morphology to HDPE continuous, Nylon 6 dispersed morphology. Whereas, increasing HDPEgMA concentration in the same blends results in gradual morphology transition from Nylon 6 continuous to co‐continuous morphology. The mechanical properties, oxygen permeability, and water vapor permeability are measured on the blends which confirm the morphology and indicate that HDPEgMA is a better compatibilizer than LLDPEgMA for the HDPE/Nylon 6 blend system. © 2019 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys.
2019 ,57 , 281–290