Title: Efficient Cobalt-Catalyzed Coupling of Amines and Siloxanes to Prepare Ceramics and Polymers
The phosphine-substituted aryl diimine cobalt catalyst, (Ph2PPrADI)Co, has been found to mediate the dehydrocoupling of diamines or polyamines to poly(methylhydrosiloxane) (PMHS) to generate hydrogen and crosslinked solids in an atom-efficient fashion. The resulting siloxane diamine and siloxane polyamine networks persist in the presence of air or water at room temperature and can tolerate temperatures of up to 1,600 °C. Upon lowering the catalyst loading to 0.01 mol%, (Ph2PPrADI)Co was found to catalyze the dehydrocoupling of 1,3-propanediamine and PMHS (m = 35) to generate a siloxane diamine foam with a turnover frequency of 157 s-1 relative to diamine consumption, the highest activity ever reported for Si‒N dehydrocoupling. Furthermore, upon systematically reducing the number of potential branch points, the (Ph2PPrADI)Co catalyzed dehydrocoupling of diamines with hydride-terminated poly(dimethylsiloxane) (PDMS) was found to yield linear siloxane diamine polymers with molecular weights of up to 47,300 g/mol.  more » « less
Award ID(s):
2154359
PAR ID:
10508495
Author(s) / Creator(s):
; ; ;
Publisher / Repository:
American Chemical Society
Date Published:
Journal Name:
ACS Sustainable Chemistry & Engineering
Volume:
11
Issue:
30
ISSN:
2168-0485
Page Range / eLocation ID:
11172 to 11180
Subject(s) / Keyword(s):
Sponsoring Org:
National Science Foundation
More Like this
  1. Although silane diamine copolymers have captured the attention of the catalysis community, the optimization of their synthesis and end uses have yet to be explored. In this study, a well-defined Earth-abundant metal catalyst, [(2,6-iPr2PhBDI)Mn(µ-H)]2, has been found to couple organosilanes to diamines to prepare networks that feature varied silane substitution and diamine chain lengths. By performing dehydrocoupling in the absence of solvent with 0.01 mol% catalyst loading, substrate utilisation turnover frequencies of up to 300 s-1 have been achieved at early reaction times, the highest Si–N dehydrocoupling activity ever observed. These networks have been employed as absorbents for common organic solvents, a property that had not been studied for this class of materials. By incorporating a long-chain hydrophobic linker, one network has been found to absorb 7.7× its orginal mass in THF and recycling has been demonstrated upon solvent removal. Controlling the degree of dehydrocoupling also offered an opportunity to deposit coatings from freshly-prepared silane diamine polymer solutions and monitor their integrity upon curing in air. While uniform and persistent coatings have been obtained from 1,6-hexanediamine derived polymers, the need to prepare dilute solutions that have a short shelf-life and the tackiness associated with extended dry times have been identified as potential limitations. 
    more » « less
  2. The halogen-free synthesis of oligosilazanes has been observed upon dehydrocoupling silanes with ammonia at 25 °C using [(2,6-iPr2PhBDI)Mn(µ-H)]2. Extending this methodology to polymethyl-hydrosiloxanes afforded thermally robust polysiloxazane solids, and the dehydrocoupling of 1,3,5,7-tetramethylcyclotetrasiloxane with ammonia afforded a polysiloxazane having a weight-average molecular weight of 4300 g/mol. A representative oligosilazane has been applied to a copper surface and found to afford a 20 μm thick coating that resists corrosion after 24 h under water. Addition of ammonia to [(2,6-iPr2PhBDI)Mn(µ-H)]2 allowed for characterization of the catalyst resting state, [(2,6-iPr2PhBDI)Mn(µ-NH2)]2, which has been found to mediate Si‒N dehydrocoupling. 
    more » « less
  3. Water-lean absorbents can increase gravimetric CO2 capacity but often exhibit significant viscosity increases upon CO2 loading. In this study, five single-component alkoxy-functionalized diamines with a common tetraoxa backbone were synthesized with systematic variation in N-substitution and amine functionality ([M, N, N, M] to [M, DN, DN, M]). CO2 uptake at 298.15 K and 0.1 MPa reached 1.20–1.81 mol/mol (22.33–28.67 wt%), exceeding chemisorption-only predictions for several solvents, consistent with additional physical CO2 dissolution in the ether-rich matrix. CO2 absorption caused pronounced, structure-dependent increases in viscosity. At 313.15 K, CO2-loaded viscosities spanned 12.56–529.40 cP, with [M, BN, BN, M] providing the most favorable balance between high uptake and low rich-phase viscosity (1.80 mol/mol and 12.56 cP). Molecular simulations provided molecular-level insight into the observed viscosity differences, showing that rich-phase transport behavior is governed by architecture-dependent intermolecular associations and their relaxation dynamics following CO2 uptake. FTIR and 13C NMR confirm predominant ammonium carbamate formation, and the carbamate carbonyl persists with 10 wt% water. ReactIR monitoring shows rapid disappearance of carbamate-associated bands during heating at 393.15 K, indicating reversible CO2 release. Across ten absorption–desorption cycles, [M, BN, BN, M] maintained CO2 uptake within 22.33–23.67 wt% (1.77–1.87 mol/mol), demonstrating reproducible short-term cyclic performance. The primary amine functionality of [M, N, N, M] was further demonstrated as a monomer for polyamide and polyurea synthesis, illustrating the potential of this compound class to serve dual roles as CO₂ capture solvents and polymer building blocks. Overall, these combined experimental and molecular simulation results establish molecular architecture as a key design variable governing the balance between CO2 capture capacity and rich-phase transport behavior in ether-rich diamine absorbents. 
    more » « less
  4. Abstract Herein, we report a selective photooxidation of commodity postconsumer polyolefins to produce polymers with in‐chain ketones. The reaction does not involve the use of catalyst, metals, or expensive oxidants, and selectively introduces ketone functional groups. Under mild and operationally simple conditions, yields up to 1.23 mol % of in‐chain ketones were achieved. Installation of in‐chain ketones resulted in materials with improved adhesion of the materials and miscibility of mixed plastics relative to the unfunctionalized plastics. The introduction of ketone groups into the polymer backbone allows these materials to react with diamines, forming dynamic covalent polyolefin networks. This strategy allows for the upcycling of mixed plastic waste into reprocessable materials with enhanced performance properties compared to polyolefin blends. Mechanistic studies support the involvement of photoexcited nitroaromatics in consecutive hydrogen and oxygen atom transfer reactions. 
    more » « less
  5. The binding of linear diamine counterions with different methylene chain lengths to the amino-acid-based surfactants undecanoic L-isoleucine (und-IL) and undecanoic L-norleucine (und-NL) was investigated with NMR spectroscopy. The counterions studied were 1,2-ethylenediamine, 1,3-diaminopropane, 1,4-diaminobutane, 1,5-diaminopentane, and 1,6-diaminohexane. These counterions were all linear diamines with varying spacer chain lengths between the two amine functional groups. The sodium counterion was studied as well. Results showed that when the length of the counterion methylene chain was increased, the surfactants’ critical micelle concentrations (CMC) decreased. This decrease was attributed to diamines with longer methylene chains binding to multiple surfactant monomers below the CMC and thus acting as templating agents for the formation of micelles. The entropic hydrophobic effect and differences in diamine counterion charge also contributed to the size of the micelles and the surfactants’ CMCs in the solution. NMR diffusion measurements showed that the micelles formed by both surfactants were largest when 1,4-diaminobutane counterions were present in the solution. This amine also had the largest mole fraction of micelle-bound counterions. Finally, the und-NL micelles were larger than the und-IL micelles when 1,4-diaminobutane counterions were bound to the micelle surface. A model was proposed in which this surfactant formed non-spherical aggregates with both the surfactant molecules’ hydrocarbon chains and n-butyl amino acid side chains pointing toward the micelle core. The und-IL micelles, in contrast, were smaller and likely spherically shaped. 
    more » « less