Title: Effect of Precursor Purge Time on Plasma-Enhanced Atomic Layer Deposition-Prepared Ferroelectric Hf 0.5 Zr 0.5 O 2 Phase and Performance
Hafnium oxide-based thin films, in particular hafnium zirconium oxide (HZO), have potential for applications in nonvolatile memory and energy harvesting. Atomic layer deposition (ALD) is the most widely used method for HZO deposition due to its precise thickness control and ability to provide conformal coverage. Previous studies have shown the effects of different metal precursors, oxidizer precursors, and process temperatures on the ferroelectric properties of HZO. However, no mechanism has been identified to describe the different phase stabilities as the metal precursor purge time varies. This study investigates how varying the metal precursor purge time during plasma-enhanced ALD (PE-ALD) influences the phases and properties of the HZO thin films. Grazing incidence X-ray diffraction, Fourier transform infrared spectroscopy, and scanning transmission electron microscopy are used to study the changes in phase of HZO with variation of the metal precursor purge time during the PE-ALD process. The phases observed are correlated with polarization and relative permittivity responses under an electric field, including wake-up and endurance effects. The resulting phases and properties are linked to changes in composition, as measured using time-of-flight secondary ion mass spectrometry and X-ray photoelectron spectroscopy. It is shown that short metal precursor purge times result in increased carbon and nitrogen impurities and stabilization of the antipolar Pbca phase. Long purge times lead to films comprising predominantly the ferroelectric Pca21 phase.  more » « less
Award ID(s):
2149487 2132918
PAR ID:
10595188
Author(s) / Creator(s):
; ; ; ; ; ; ; ; ; ; ;
Publisher / Repository:
American Chemical Society
Date Published:
Journal Name:
ACS Omega
Volume:
10
Issue:
20
ISSN:
2470-1343
Page Range / eLocation ID:
20524 to 20535
Subject(s) / Keyword(s):
Polarization ferroelectric atomic layer deposition impurities hafnium zirconium oxide
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. We report the growth of nanoscale hafnium dioxide (HfO2) and zirconium dioxide (ZrO2) thin films using remote plasma-enhanced atomic layer deposition (PE-ALD), and the fabrication of complementary metal-oxide semiconductor (CMOS) integrated circuits using the HfO2 and ZrO2 thin films as the gate oxide. Tetrakis (dimethylamino) hafnium (Hf[N(CH3)2]4) and tetrakis (dimethylamino) zirconium (IV) (Zr[N(CH3)2]4) were used as the precursors, while O2 gas was used as the reactive gas. The PE-ALD-grown HfO2 and ZrO2 thin films were analyzed using X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), and high-resolution transmission electron microscopy (HRTEM). The XPS measurements show that the ZrO2 film has the atomic concentrations of 34% Zr, 2% C, and 64% O while the HfO2 film has the atomic concentrations of 29% Hf, 11% C, and 60% O. The HRTEM and XRD measurements show both HfO2 and ZrO2 films have polycrystalline structures. n-channel and p-channel metal-oxide semiconductor field-effect transistors (nFETs and pFETs), CMOS inverters, and CMOS ring oscillators were fabricated to test the quality of the HfO2 and ZrO2 thin films as the gate oxide. Current-voltage (IV) curves, transfer characteristics, and oscillation waveforms were measured from the fabricated transistors, inverters, and oscillators, respectively. The experimental results measured from the HfO2 and ZrO2 thin films were compared. 
    more » « less
  2. Ferroelectric hafnium-zirconium oxide (HZO) is an excellent candidate for low-power non-volatile memory applications due to its demonstrated ferroelectricity at the nanoscale and compatibility with silicon-based technologies. The interface of HZO in contact with its electrode, typically TiN in a metal–ferroelectric–metal (MFM) capacitor configuration, is of particular interest because factors, such as volume confinement, impurity concentration, interfacial layers, thermal expansion mismatch, and defect trapping, are believed to play a crucial role in the ferroelectric performance of HZO-based devices. Processing variables, such as precursor type, oxygen source, dose duration, and deposition temperature, are known to strongly affect the quality of the oxide–metal interface. However, not many studies have focused on the effect of breaking or maintaining vacuum during MFM deposition. In this study, sequential, no-atmosphere processing (SNAP) is employed to avoid atmospheric exposure, where electrode TiN and ferroelectric HZO are deposited sequentially in the atomic layer deposition chamber without breaking vacuum. The effect of breaking vacuum during the sequential deposition steps is elucidated by fabricating and characterizing MFM capacitors with and without intentional vacuum breaks prior to the deposition of the HZO and top TiN. Using x-ray photoelectron spectroscopy and time-of-flight secondary ion mass spectrometry (ToF-SIMS), we reveal that breaking vacuum after bottom TiN electrode deposition leads to interfacial oxidation and increased carbon contamination, which preferentially stabilizes the non-ferroelectric tetragonal phase and lead to diminished remanent polarization. Avoiding carbon impurities and interfacial TiOx at the HZO and TiN interface using SNAP leads to heightened remanent polarization, reduced leakage current density, and elimination of the wake-up effect. Our work highlights the effect of vacuum breaking on the processing-structure-properties of HZO-based capacitors, revealing that maintaining vacuum can significantly improve ferroelectric properties. 
    more » « less
  3. Abstract Hf 0.5 Zr 0.5 O 2 (HZO) thin films are promising candidates for non-volatile memory and other related applications due to their demonstrated ferroelectricity at the nanoscale and compatibility with Si processing. However, one reason that HZO has not been fully scaled into industrial applications is due to its deleterious wake-up and fatigue behavior which leads to an inconsistent remanent polarization during cycling. In this study, we explore an interfacial engineering strategy in which we insert 1 nm Al 2 O 3 interlayers at either the top or bottom HZO/TiN interface of sequentially deposited metal-ferroelectric-metal capacitors. By inserting an interfacial layer while limiting exposure to the ambient environment, we successfully introduce a protective passivating layer of Al 2 O 3 that provides excess oxygen to mitigate vacancy formation at the interface. We report that TiN/HZO/TiN capacitors with a 1 nm Al 2 O 3 at the top interface demonstrate a higher remanent polarization (2P r ∼ 42 μ C cm −2 ) and endurance limit beyond 10 8 cycles at a cycling field amplitude of 3.5 MV cm −1 . We use time-of-flight secondary ion mass spectrometry, energy dispersive spectroscopy, and grazing incidence x-ray diffraction to elucidate the origin of enhanced endurance and leakage properties in capacitors with an inserted 1 nm Al 2 O 3 layer. We demonstrate that the use of Al 2 O 3 as a passivating dielectric, coupled with sequential ALD fabrication, is an effective means of interfacial engineering and enhances the performance of ferroelectric HZO devices. 
    more » « less
  4. Abstract Ferroelectric hafnium zirconium oxide (HZO) holds promise for nextgeneration memory and transistors due to its superior scalability and seamless integration with complementary metal‐oxide‐semiconductor processing. A major challenge in developing this emerging ferroelectric material is the metastable nature of the non‐centrosymmetric polar phase responsible for ferroelectricity, resulting in a coexistence of both polar and non‐polar phases with uneven grain sizes and random orientations. Due to the structural similarity between the multiple phases and the nanoscale dimensions of the thin film devices, accurate measurement of phase‐specific information remains challenging. Here, the application of 4D scanning transmission electron microscopy is demonstrated with automated electron diffraction pattern indexing to analyze multiphase polycrystalline HZO thin films, enabling the characterization of crystallographic phase and orientation across large working areas on the order of hundreds of nanometers. This approach offers a powerful characterization framework to produce a quantitative and statistically robust analysis of the intricate structure of HZO films by uncovering phase composition, polarization axis alignment, and unique phase distribution within the HZO film. This study introduces a novel approach for analyzing ferroelectric HZO, facilitating reliable characterization of process‐structure‐property relationships imperative to accelerating the growth optimization, performance, and successful implementation of ferroelectric HZO in devices. 
    more » « less
  5. Nanolayered molybdenum diselenide (MoSe2) thin films were synthesized by plasma-enhanced atomic layer deposition (PE-ALD) using molybdenum pentachloride (MoCl5) and diethyldiselenide (C4H10Se2) precursors. Scanning and transmission electron microscopy revealed horizontally stacked nanolayers near the substrate and vertically oriented nanosheets at the surface of the film. X-ray diffraction confirmed the (002), (100), and (110) reflections of crystalline MoSe2, while X-ray photoelectron spectroscopy showed relative atomic concentrations of 33.5% Mo and 66.5% Se, consistent with stoichiometric MoSe2. Raman spectra exhibited characteristic E1g, A1g, and E12g vibrational modes. Field-effect transistors incorporating PE-ALD-grown MoSe2 as the channel material displayed p-type behavior, demonstrating the potential of nanolayered MoSe2 for nanoelectronic applications. This work demonstrates the feasibility of low-temperature, stoichiometric growth of nanolayered MoSe2 by PE-ALD and its direct integration into transistor architectures. 
    more » « less