Title: Influence of In Situ and Ex Situ Heat Treatments on the Mechanical Behavior of LPBF-Fabricated Fe–Mn–Al–Ni Shape Memory Alloys
Abstract This study investigates the fabrication of Fe–Mn–Al–Ni iron-based shape memory alloys (SMAs) using laser powder bed fusion (LPBF) across a range of laser powers. The influence of energy input on material properties was assessed by evaluating the resulting volumetric energy density. Samples were produced under both as-built conditions and subjected to in situ and ex situ treatments to enhance performance. Mechanical properties were characterized through macro-indentation, Profilometry-based Indentation Plastometry (PIP), and nanoindentation techniques, while room-temperature compression testing was conducted to assess superelastic behavior. Microstructural and phase variations were analyzed using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results showed that increasing the fabrication power improved the mechanical properties of the as-built SMAs, with the optimal performance achieved at 175 W. In situ/ex situ treatments led to a significant reduction in strength but enhanced ductility by up to 39%, along with a 52% reduction in microhardness for samples fabricated at 175 W. Overall, the LPBF-produced Fe–Mn–Al–Ni SMAs exhibited good strain recovery and stability, comparable to those produced by conventional methods. This work demonstrates the potential of LPBF in developing Fe–Mn–Al–Ni SMAs with properties matching traditionally manufactured counterparts. Graphical Abstract Mechanical behavior and microstructural features of LPBF-fabricated Fe–Mn–Al–Ni SMA under the effects of in situ and ex situ treatments  more » « less
Award ID(s):
2301766
PAR ID:
10617116
Author(s) / Creator(s):
; ;
Publisher / Repository:
Springer
Date Published:
Journal Name:
Shape Memory and Superelasticity
ISSN:
2199-384X
Subject(s) / Keyword(s):
Sponsoring Org:
National Science Foundation
More Like this
  1. Laser powder bed fusion (LPBF) is a metal additive manufacturing technique that enables the production of high-performance, geometrically complex parts by selectively melting and solidifying fine metal powders under a laser source. However, the LPBF process is often accompanied by the formation of internal defects such as lack-of-fusion pores, keyhole pores, gas porosity nucleation, and vapor-induced porosity, and cracks, which can significantly deteriorate the mechanical integrity and reliability of the fabricated components. Among these defects, cracks remain one of the least investigated due to the challenges associated with capturing their rapid formation and propagation during the LPBF process. To observe crack initiation and propagation in real time, in-situ synchrotron X-ray imaging was employed to capture high-speed videos of the LPBF process of aluminum (Al) alloy. The experiment was conducted at the Stanford Synchrotron Radiation Lightsource (SSRL) to observe Al-6061 alloy LPBF process melt pool and crack formation dynamics with in-situ synchrotron X-ray imaging at 20 kfps with 2 µm spatial resolution and capture the transient melt pool and crack dynamics. The captured X-ray videos were analyzed through quantitative grayscale pixel-intensity mapping to identify crack initiation sites and analyze their propagation behavior. This robust analysis visualizes (i) the timing of crack initiation, (ii) the direction of crack propagation, and (iii) the relationship between process parameters and crack formation. Two key observations were made: (i) cracks predominantly initiate within the melt pool length and propagate vertically upward along the solidification direction, and (ii) at higher laser powers, the upward-propagating cracks develop secondary side branches inclined at distinct angles to the main crack path. These findings provide critical insight into the mechanisms of crack initiation and propagation and provide foundation for developing predictive models and scan strategies to mitigate defect formation in LPBF Al alloy printing. 
    more » « less
  2. Nd-Fe-B permanent magnets are crucial for high-performance applications, yet their fabrication by laser powder bed fusion (LPBF) is limited by defects, microstructural instability, and degradation of magnetic properties. This work examines printability, microstructure evolution, and defect formation in two Nd-rich gas-atomized Nd–Fe–B powders (Alloy A and Alloy B) as a function of laser power, scan speed, and hatch spacing. X-ray computed tomography (XCT) reveals that Alloy A consistently achieves > 99% relative density but attains a maximum coercivity of 0.58 kOe, whereas a specific processing condition for Alloy B reaches ~99.99% density with a coercivity of 0.49 kOe at higher energy input. These results demonstrate that the optimal LPBF processing window is strongly composition dependent, and the resulting insights provide practical guidelines for tailoring process parameters to improve the performance and reliability of Nd-Fe-B permanent magnets. 
    more » « less
  3. This study investigated the impact of low-temperature heat treatments on the mechanical and thermophysical properties of Cu-10Sn alloys fabricated by a laser powder bed fusion (LPBF) additive manufacturing (AM) process. The microstructure, phase structure, and mechanical and thermal properties of the LPBF Cu-10Sn samples were comparatively investigated under both the as-fabricated (AF) condition and after low-temperature heat treatments at 140, 180, 220, 260, and 300 °C. The results showed that the low-temperature heat treatments did not significantly affect the phase and grain structures of the Cu-10Sn alloys. Both pre- and post-treatment samples displayed consistent grain sizes, with no obvious X-ray diffraction angle shift for the α phase, indicating that atom diffusion of the Sn element is beyond the detection resolution of X-ray diffractometers (XRD). However, the 180 °C heat-treated sample exhibited the highest hardness, while the AF samples had the lowest hardness, which was most likely due to the generation of precipitates according to thermodynamics modeling. Heat-treated samples also displayed higher thermal diffusivity values than their AF counterpart. The AF sample had the longest lifetime of ~0.19 nanoseconds (ns) in the positron annihilation lifetime spectroscopy (PALS) test, indicating the presence of the most atomic-level defects. 
    more » « less
  4. Abstract Laser powder bed fusion (L-PBF) additive manufacturing (AM) is an effective method of fabricating nickel–titanium (NiTi) shape memory alloys (SMAs) with complex geometries, unique functional properties, and tailored material compositions. However, with the increase of Ni content in NiTi powder feedstock, the ability to produce high-quality parts is notably reduced due to the emergence of macroscopic defects such as warpage, elevated edge/corner, delamination, and excessive surface roughness. This study explores the printability of a nickel-rich NiTi powder, where printability refers to the ability to fabricate macro-defect-free parts. Specifically, single track experiments were first conducted to select key processing parameter settings for cubic specimen fabrication. Machine learning classification techniques were implemented to predict the printable space. The reliability of the predicted printable space was verified by further cubic specimens fabrication, and the relationship between processing parameters and potential macro-defect modes was investigated. Results indicated that laser power was critical to the printability of high Ni content NiTi powder. In the low laser power setting (P < 100 W), the printable space was relatively wider with delamination as the main macro-defect mode. In the sub-high laser power condition (100 W ≤ P ≤ 200 W), the printable space was narrowed to a low hatch spacing region with macro-defects of warpage, elevated edge/corner, and delamination happened at different scanning speeds and hatch spacing combinations. The rough surface defect emerged when further increasing the laser power (P > 200 W), leading to a further narrowed printable space. 
    more » « less
  5. null (Ed.)
    Laser powder bed fusion (LPBF) is an additive manufacturing technology with the capability of printing complex metal parts directly from digital models. Between two available emission modes employed in LPBF printing systems, pulsed wave (PW) emission provides more control over the heat input compared to continuous wave (CW) emission, which is highly beneficial for printing parts with intricate features. However, parts printed with pulsed wave LPBF (PW-LPBF) commonly contain pores, which degrade their mechanical properties. In this study, we reveal pore formation mechanisms during PW-LPBF in real time by using an in-situ high-speed synchrotron x-ray imaging technique. We found that vapor depression collapse proceeds when the laser irradiation stops within one pulse, resulting in occasional pore formation during PW-LPBF. We also revealed that the melt ejection and rapid melt pool solidification during pulsed-wave laser melting resulted in cavity formation and subsequent formation of a pore pattern in the melted track. The pore formation dynamics revealed here may provide guidance on developing pore elimination approaches. 
    more » « less