Titanium nitride and vanadium nitride–carbon-based composite systems, TiN/C and VN/C, were prepared using a new synthesis method based on the thermal decomposition of titanyl tetraphenyl porphyrin (TiOTPP) and vanadyl tetraphenyl porphyrin (VOTPP), respectively. The structure of the TiN/C and VN/C composite materials, as well as their precursors, were characterized using Fourier Transformed Infrared Spectroscopy, X-Ray diffraction (XRD), X-Ray energy dispersive (EDS) and X-Ray photoelectron spectroscopy (XPS). Morphologies of the TiN/C and VN/C composites were examined by means of scanning electron (SEM) and transmission electron (TEM) microscopy. The synthesis of the non-metalated tetraphenyl porphyrin, the titanium, and vanadium tetraphenyl porphyrin complexes were confirmed using FTIR. The thermal decomposition of the titanium and vanadium tetraphenyl porphyrin complexes produced the respective metal nitride encapsulated in a carbon matrix; this was confirmed by XRD, SEM, TEM, and XPS. From the XRD patterns, it was determined that the TiN and VN were presented in cubic form with expected space group FM-3M and 1:1 (metal:N) stoichiometry. The XPS results confirmed the presence of both TiN and VN in the carbon matrix without metal carbides. The SEM and TEM results showed that both TiN and VN nanoparticles formed small clusters throughout the carbon matrix; the EDS results revealed a uniform composition. The synthesis method presented in this work is novel and serves as an effective means to produce TiN and VN NPs with good structure and morphology embedded in a carbon matrix.
more »
« less
Atomic Layer Deposition of Nickel Using Ni(dmamb)2 and ZnO Adhesion Layer Without Plasma
Abstract In this study, a novel deposition technique that utilizes diethylzinc (C4H10ZnO) with H2O to form a ZnO adhesion layer was proposed. This technique was followed by the deposition of vaporized nickel(II) 1-dimethylamino-2-methyl-2-butoxide (Ni(dmamb)2) and H2gas to facilitate the deposit of uniform layers of nickel on the ZnO adhesion layer using atomic layer deposition. Deposition temperatures ranged from 220 to 300 °C. Thickness, composition, and crystallographic structure results were analyzed using spectroscopic ellipsometry, scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS), and X-ray diffraction (XRD), respectively. An average growth rate of approximately 0.0105 angstroms per cycle at 260 °C was observed via ellipsometry. Uniform deposition of ZnO with less than 1% of Ni was displayed by utilizing the elemental analysis function via SEM, thereby providing high-quality images. XPS revealed ionizations consistent with nickel and ZnO through the kinetic and binding energies of each detected electron. XRD provided supplemental information regarding the validity of ZnO by exhibiting crystalline attributes, revealing the presence of its hexagonal wurtzite structure.
more »
« less
- Award ID(s):
- 1914751
- PAR ID:
- 10618685
- Publisher / Repository:
- Springer Nature
- Date Published:
- Journal Name:
- Nanomanufacturing and Metrology
- Volume:
- 7
- Issue:
- 1
- ISSN:
- 2520-811X
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
Nickel-Fe3O4 nanoparticles supported on multi-walled carbon nanotubes (Ni-Fe3O4/MWCNTs) were synthesized by mechanical grinding of a sample of nickel salt, Fe3O4 and MWCNTs using a ball-mill mixer. The preparation method allows for bulk production of Ni-Fe3O4 nanoparticles at room temperature without the necessity of any solvent or chemical reagent. The nanoparticles prepared by this method exhibit small particles size of 5–8 nm with uniform dispersion of nickel nanoparticles on the surface of multi-walled carbon nanotubes. The Ni-Fe3O4/MWCNTs demonstrated remarkable catalytic activity for Suzuki cross coupling reactions of functionalized aryl halides and phenylboronic acids with excellent turnover number and turnover frequency (e.g., 76,000 h−1) using Monowave 50 conventional heating reactor at 120 °C within a very short reaction time of 15 min. The catalyst is air-stable and exhibits easy removal from the reaction mixture due to its magnetic properties, recyclability with no loss of activity, and significantly better performance than the other well-known commercial nickel catalyst. The Ni-Fe3O4/MWCNTs nanoparticles were fully characterized by a variety of spectroscopic techniques including X-ray Diffraction (XRD), Transmission Electron Microscopy (TEM) and X-ray Photoelectron Spectroscopy (XPS). Since nickel offers similar properties to other more expensive transition metals including the most widely used palladium counterpart in cross coupling catalysis, this work demonstrates a promising lower-cost, air-moisture stable and efficient alternative catalyst based on nickel nanoparticles for cross coupling reactions.more » « less
-
A magnetron co-sputtering system was used for producing nickel-doped Ge2Sb2Te5 (GST-Ni) thin films. The nickel content in the thin film was adjusted by the ratio of the plasma discharge power applied to the GST and nickel targets, as well as a physical shuttering technique to further control the nickel deposition rate. The doping concentration of the film was con firmed using Energy Dispersion Spectroscopy (EDS) technique. Results from a four-point probe measurement indicate that the nickel doping can reduce the resistivity of GST in the amorphous state by nearly three orders of magnitude. The dopant's influence on crystallization behavior was studied by analyzing X-Ray Diffraction (XRD) patterns of the pure GST and GST-Ni at different annealing temperatures. To examine the structural changes due to the nickel dopant, the thin films were investigated with the aid of Raman scattering. Additionally, we extracted the optical constants for both the amorphous and crystalline states of undoped-GST and GST-Ni films by ellipsometry. The results indicate that at low doping concentrations nickel does not appreciably affect the optical constants, but dramatically improves the electrical conductivity. Therefore, nickel-doping of GST a viable method for designing optical devices for lower operating voltages at higher switching speeds.more » « less
-
Abstract Ti3C2Tx(MXenes) are novel 2D nanomaterials with exceptional electrical conductivity. Their surfaces are covered with functional groups that may significantly affect material properties such as hydrophobicity, electrical conductivity, and oxidation resistance. The role of these terminations in high-temperature ceramic systems with regard to phase and microstructural evolution has not been investigated. In this study, Ti3C2Tx-SiOC 2D nanocomposites were fabricated with -F and -OH terminated MXene to evaluate the role of surface terminations in silane coupling and phase formation during the polymer-to-ceramic transformation. X-ray diffraction (XRD), scanning electron microscopy (SEM), thermogravimetric analysis (TGA), and X-ray photoelectron spectroscopy (XPS) identified self-etching mechanisms caused by F-terminated Ti3C2Txand revealed that the F surface terminations were retained in the MXene structure until evolution at ~ 550 °C. Evolved F reacted with Si–H bonds in the transforming ceramic matrix, causing additional mass loss and volumetric deformation. LiOH alkalization was shown to suppress the self-etching phenomenon through the substitution of F groups with OH on the nanosheet surface. Furthermore, F terminations were determined to only engage in hydrogen bonding with silane molecules as opposed to covalent linkages with OH terminations, which accelerated silane removal and Ti3C2Txdegradation. The study provides a fundamental understanding of the nature and behavior of MXene surface terminations in the context of high-temperature ceramic nanocomposite fabrication.more » « less
-
The present work focuses on the synthesis of a vanadium nitride (VN)/carbon nanocomposite material via the thermal decomposition of vanadyl phthalocyanine (VOPC). The morphology and chemical structure of the synthesized compounds were characterized using scanning electron microscopy (SEM), transmission electron microscopy (TEM), energy dispersive spectroscopy (EDS), Fourier transformed infrared spectroscopy (FTIR), X-ray diffraction (XRD), and X-ray photoemission spectroscopy (XPS). The successful syntheses of the VOPC and non-metalated phthalocyanine (H2PC) precursors were confirmed using FTIR and XRD. The VN particles present a needle-like morphology in the VN synthesized by the sol-gel method. The morphology of the VN/C composite material exhibited small clusters of VN particles. The XRD analysis of the thermally decomposed VOPC indicated a mixture of amorphous carbon and VN nanoparticles (VN(TD)) with a cubic structure in the space group FM-3M consistent with that of VN. The XPS results confirmed the presence of V(III)-N bonds in the resultant material, indicating the formation of a VN/C nanocomposite. The VN/C nanocomposite synthesized through thermal decomposition exhibited a high carbon content and a cluster-like distribution of VN particles. The VN/C nanocomposite was used as an anode material in LIBs, which delivered a specific capacity of 307 mAh g−1 after 100 cycles and an excellent Coulombic efficiency of 99.8 at the 100th cycle.more » « less
An official website of the United States government