Title: Temperature‐Dependent Properties of Atomic Layer Deposition‐Grown TiO 2 Thin Films
Abstract This study investigates the presence of titanium oxynitride bonds in titanium dioxide (TiO2) thin films grown by atomic layer deposition (ALD) using tetrakis dimethyl amino titanium (TDMAT) and water at temperatures between 150 and 350 °C and its effect on the films’ optical and electrical properties. Compositional analysis using X‐ray photoelectron spectroscopy (XPS) reveals increased incorporation of oxynitride bonds as the process temperature increases. Furthermore, depth profile data demonstrates an increase in the abundance of this type of bonding from the surface to the bulk of the films. Ultraviolet‐visible spectroscopy (UV‐vis) measurements correlate increased visible light absorption for the films with elevated oxynitride incorporation. The optical constants (n, k) of the films show a pronounced dependence on the process temperature that is mirrored in the film conductivity. The detection of oxynitride bonding suggests a secondary reaction pathway in this well‐established ALD process chemistry, that may impact film properties. These findings indicate that the choice of process chemistry and conditions can be used to optimize film properties for optoelectronic applications.  more » « less
Award ID(s):
1905305
PAR ID:
10625388
Author(s) / Creator(s):
;
Publisher / Repository:
Wiley
Date Published:
Journal Name:
Advanced Materials Interfaces
Volume:
12
Issue:
14
ISSN:
2196-7350
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. Typical titanium oxide (TiO2) films are transparent in the visible range, allowing for their index of refraction and thickness to be extracted by single-angle spectroscopic ellipsometry (SE) using a Cauchy model. However, TiO2 films grown by atomic layer deposition (ALD) from tetrakis(dimethylamino)titanium (IV) (TDMAT) and H2O at 350 °C absorb in the visible range due to the formation of Ti-O-N/Ti-N bonds. Single-angle SE is inadequate for extracting the optical constants of these films, as there are more unknowns (n, k, d) than measurable parameters (ψ, Δ). To overcome this limitation, we combined SE with transmission (T) measurements, a method known as SE + T. In the process, we developed an approach to prevent backside deposition on quartz substrates during ALD deposition. When applying a B-spline model to SE + T data, the film thicknesses on the quartz substrates closely matched those on companion Si samples measured via standard lithography. The resulting optical constants indicate a reduced refractive index, n, and increased extinction coefficient, k, when compared to purer TiO2 thin films deposited via a physical vapor deposition (PVD) method, reflecting the influence of nitrogen incorporation on the optical properties. 
    more » « less
  2. Abstract An extensive examination of the nanoscale, crystallographic growth dynamics of the system, which is impacted by the thermal energy given to the GaN, is carried out to derive a deeper understanding of the growth kinetics, morphology and microstructure evolution, chemical bonding, and optical properties of Ga─O─N films. Thermal annealing of GaN films is performed in the temperature range of 900–1200 °C. Crystal structure, phase formation, chemical composition, surface morphology, and microstructure evolution of Ga─O─N films are investigated as a function of temperature. Increasing temperature induces surface oxidation, which results in the formation of stable β‐Ga2O3phase in the GaN matrix, where the overall film composition evolves from nitride (GaN) to oxynitride (Ga─O─N). While GaN surfaces are smooth, planar, and featureless, oxidation induced granular‐to‐rod shaped morphology evolution is seen with increasing temperature to 1200 °C. The considerable texturing and stability of the nanocrystalline Ga─O─N on Si substrates can be attributed to the surface and interface driven modification because of thermal treatment. Corroborating with structure and chemical changes, Raman spectroscopic analyses also indicate that the chemical bonding evolution progresses from fully Ga─N bonds to Ga─O─N. While the GaN oxidation process starts with the formation of β‐Ga2O3at an annealing temperature of 1000 °C, higher annealing temperatures induce structural distortion with the potential formation of Ga─O─N bonds. The structure‐phase‐chemical composition correlation, which will be useful for nanocrystalline materials for selective optoelectronic applications, is established in Ga─O─N films made by thermal treatment of GaN. 
    more » « less
  3. Abstract This study reports a pulsed laser deposition-assisted synthesis of highly metallic titanium nitride (TiN) and a series of semiconducting titanium oxynitride (TiNxOy) compounds in thin film form with tunable plasmonic properties by carefully altering the nitrogen (N)-oxygen (O) ratio. The N/O ratio was controlled from 0.3 (highest oxygen doping of TiN) to ~ 1.0 (no oxygen doping of TiN) by growing the TiN films under nitrogen pressures of 50, 35, and 10 mTorr and high vacuum conditions of 2 × 10−6 Torr with no external gas introduced. The presence of nitrogen in the deposition chamber during the film growth affects the gas phase oxidation of TiN to TiNxOyby increasing the mean free path-dependent N and O inter-collisions per second by two to three orders of magnitudes. The evidence of increased oxidation of TiN to TiNxOywith an increase in nitrogen deposition pressure was obtained using X-ray photoelectron spectroscopy analysis. While the TiN samples deposited in high vacuum conditions had the highest reflectance, TiNxOythin films were also found to possess high reflectance at low frequency with a well-defined edge around 20,000 cm−1. Furthermore, the vacuum-deposited TiN samples showed a large negative dielectric constant of -330 and the largest frequency of zero-crossing at 25,000 cm−1; the TiNxOysamples deposited in the presence of nitrogen ambient also showed promising plasmonic applications at the near-mid infrared range. A comparison of the dielectric constant and loss function data of this research with the literature values for noble metals seems to indicate that TiN and TiNxOyhave the potential to replace gold and silver in the visible and near-infrared spectral regions. 
    more » « less
  4. Atomic layer deposition (ALD) of ruthenium (Ru) is being investigated for next generation interconnects and conducting liners for copper metallization. However, integration of ALD Ru with diffusion barrier refractory metal nitrides, such as tantalum nitride (TaN), continues to be a challenge due to its slow nucleation rates. Here, we demonstrate that an ultraviolet-ozone (UV-O3) pretreatment of TaN leads to an oxidized surface that favorably alters the deposition characteristics of ALD Ru from islandlike to layer-by-layer growth. The film morphology and properties are evaluated via spectroscopic ellipsometry, atomic force microscopy, electrical sheet resistance measurements, and thermoreflectance. We report a 1.83 nm continuous Ru film with a roughness of 0.19 nm and a sheet resistance of 10.8 KΩ/□. The interface chemistry between TaN and Ru is studied by x-ray photoelectron spectroscopy. It is shown that UV-O3 pretreatment, while oxidizing TaN, enhances Ru film nucleation and limits further oxidation of the underlying TaN during ALD. An oxygen “gettering” mechanism by TaN is proposed to explain reduced oxygen content in the Ru film and higher electrical conductivity compared to Ru deposited on native-TaN. This work provides a simple and effective approach using UV-O3 pretreatment for obtaining sub-2 nm, smooth, and conducting Ru films on TaN surfaces. 
    more » « less
  5. Abstract BaTiO3is a technologically relevant material in the perovskite oxide class with above‐room‐temperature ferroelectricity and a very large electro‐optical coefficient, making it highly suitable for emerging electronic and photonic devices. An easy, robust, straightforward, and scalable growth method is required to synthesize epitaxial BaTiO3thin films with sufficient control over the film's stoichiometry to achieve reproducible thin film properties. Here the growth of BaTiO3thin films by hybrid molecular beam epitaxy is reported. A self‐regulated growth window is identified using complementary information obtained from reflection high energy electron diffraction, the intrinsic film lattice parameter, film surface morphology, and scanning transmission electron microscopy. Subsequent optical characterization of the BaTiO3films by spectroscopic ellipsometry revealed refractive index and extinction coefficient values closely resembling those of stoichiometric bulk BaTiO3crystals for films grown inside the growth window. Even in the absence of a lattice parameter change of BaTiO3thin films, degradation of optical properties is observed, accompanied by the appearance of a wide optical absorption peak in the IR spectrum, attributed to optical transitions involving defect states present. Therefore, the optical properties of BaTiO3can be utilized as a much finer and more straightforward probe to determine the stoichiometry level present in BaTiO3films. 
    more » « less