Title: Plasma enhanced atomic layer deposition of titanium nitride-molybdenum nitride solid solutions
Award ID(s):
1826251
PAR ID:
10206268
Author(s) / Creator(s):
 ;  ;  ;  ;  ;  ;  
Publisher / Repository:
American Vacuum Society
Date Published:
Journal Name:
Journal of Vacuum Science & Technology A
Volume:
39
Issue:
1
ISSN:
0734-2101
Page Range / eLocation ID:
Article No. 012407
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. Morkoç, Hadis; Fujioka, Hiroshi; Schwarz, Ulrich T (Ed.)
  2. There is a strong drive behind the quest for thin-film materials that are oxygen-free and polar. Oxygen hinders the integration of ferroelectric oxides with semiconductors, which affects efforts to develop nonvolatile memory—that is, a memory that can sustain its information without power. Ideally, one would use single-crystalline perovskite films to construct these devices so that the polarization can be maximized. However, when depositing crystalline polar perovskite oxides onto silicon or germanium, a nonpolar oxide buffer layer ( 1 ) or a native oxide layer ( 2 ) can be present at the interface, compromising device performance. A nitrogen-based perovskite may overcome this limitation ( 3 ). On page 1488 of this issue, Talley et al. ( 4 ) report the synthesis of lanthanum tungsten nitride (LaWN 3 ) thin films, which marks the first demonstration of polar nitride perovskite. This may lead to oxygen-free integration of functional perovskite on a semiconductor platform. 
    more » « less
  3. Heteroepitaxial crystallographic tilt has been investigated as a possible strain‐relief mechanism in Al‐rich (Al>50%) AlGaN heteroepitaxial layers grown on single‐crystal (0001) AlN substrates with varying miscuts from 0.05° to 4.30°. The magnitude of the elastic lattice deformation‐induced tilt increases monotonically with the miscut angle, tightly following the Nagai tilt model. Although tilt angles as high as 0.1° are recorded, reciprocal space mapping (RSM) broadening and wafer bow measurements do not show any significant changes as a function of the heteroepitaxial tilt angle. While crystallographic tilting has been shown to be effective in controlling strain in some other heteroepitaxial systems, it does not provide any appreciable strain relief of the compressive strain in AlGaN/AlN heteroepitaxy. 
    more » « less
  4. Due to its excellent chemical/thermal stability and mechanical robustness, hexagonal boron nitride (hBN) is a promising solid matrix material for ionogels. While bulk hBN ionogels have been employed in macroscopic applications such as lithium-ion batteries, hBN ionogel inks that are compatible with high-resolution printing have not yet been realized. Here, we describe aerosol jet-printable ionogels using exfoliated hBN nanoplatelets as the solid matrix. The hBN nanoplatelets are produced from bulk hBN powders by liquid-phase exfoliation, allowing printable hBN ionogel inks to be formulated following the addition of an imidazolium ionic liquid and ethyl lactate. The resulting inks are reliably printed with variable patterns and controllable thicknesses by aerosol jet printing, resulting in hBN ionogels that possess high room-temperature ionic conductivities and storage moduli of >3 mS cm −1 and >1 MPa, respectively. By integrating the hBN ionogel with printed semiconductors and electrical contacts, fully-printed thin-film transistors with operating voltages below 1 V are demonstrated on polyimide films. These devices exhibit desirable electrical performance and robust mechanical tolerance against repeated bending cycles, thus confirming the suitability of hBN ionogels for printed and flexible electronics. 
    more » « less