The equine hoof wall has a complex, hierarchical structure that can inspire designs of impact-resistant materials. In this study, we utilized micro-computed tomography (micro-CT) and serial block-face scanning electron microscopy (SBF-SEM) to image the microstructure and nanostructure of the hoof wall. We quantified the morphology of tubular medullary cavities by measuring equivalent diameter, surface area, volume, and sphericity. Highresolution micro-CT revealed that tubules are partially or fully filled with tissue near the exterior surface and become progressively empty towards the inner part of the hoof wall. Thin bridges were detected within the medullary cavity, starting in the middle section of the hoof wall and increasing in density and thickness towards the inner part. Porosity was measured using three-dimensional (3D) micro-CT, two-dimensional (2D) micro-CT, and a helium pycnometer. The highest porosity was obtained using the helium pycnometer (8.07%), followed by 3D (3.47%) and 2D (2.98%) micro-CT. SBF-SEM captured the 3D structure of the hoof wall at the nanoscale, showing that the tubule wall is not solid, but has nano-sized pores, which explains the higher porosity obtained using the helium pycnometer. The results of this investigation provide morphological information on the hoof wall for the future development of hoof-inspired materials and offer a novel perspective on how various measurement methods can influence the quantification of porosity.
more »
« less
Equine Hoof Wall Deformation: Novel Aspects Revealed
The equine hoof wall has a unique hierarchical structure that allows it to survive high‐impact scenarios. Previous authors have explored the compressive, viscoelastic, and fracture control properties of the hoof wall and suggested that this complex structure plays a vital role in the hoof's behavior. However, the link between the structure and the behavior of the hoof wall has been made primarily with the use of post‐fracture analysis. Here, periodic microcomputed tomography scans are used to observe the temporal behavior of the hoof's meso and microstructures during compression, fracture, and relaxation. These results shed light on the structural anisotropy of the hoof wall and how its hollow tubules behave when compressed in different directions, at different hydration levels, and in various locations within the hoof wall. The behavior of tubule bridges during compression is also reported for the first time. This study elucidates several fracture phenomena, including the way cracks are deflected at tubule interfaces and tubule bridging, tubule arresting, and fiber bridging. Finally, relaxation tests are used to show how the tubule cavities can regain their shape after compression.
more »
« less
- PAR ID:
- 10419037
- Publisher / Repository:
- Wiley Blackwell (John Wiley & Sons)
- Date Published:
- Journal Name:
- Small Structures
- Volume:
- 4
- Issue:
- 10
- ISSN:
- 2688-4062
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
The equine hoof wall has a complex, hierarchical structure that can inspire designs of impactresistant materials. In this study, we utilized micro-computed tomography (µ-CT) and serial blockface scanning electron microscopy (SBF-SEM) to image the microstructure and nanostructure of the hoof wall. We quantified the morphology of tubular medullary cavities by measuring equivalent diameter, surface area, volume, and sphericity. High-resolution µ-CT revealed that tubules are partially or fully filled with tissue near the exterior surface and become progressively empty towards the inner part of the hoof wall. Thin bridges were detected within the medullary cavity, starting in the middle section of the hoof wall and increasing in density and thickness towards the inner part. Porosity was measured using three-dimensional (3D) µ-CT, twodimensional (2D) µ-CT, and a helium pycnometer, with the highest porosity obtained using the helium pycnometer (8.07%), followed by 3D (3.47%) and 2D (2.98%) µ-CT. SBF-SEM captured the 3D structure of the hoof wall at the nanoscale, showing that the tubule wall is not solid, but has nano-sized pores, which explains the higher porosity obtained using the helium pycnometer. The results of this investigation provide morphological information on the hoof wall for the future development of hoof-inspired materials and offer a novel perspective on how various measurement methods can influence the quantification of porosity.more » « less
-
We have developed a numerical model of two osculating cylindrical elastic renal tubules to investigate the impact of neighboring tubules on the stress applied to a primary cilium. We hypothesize that the stress at the base of the primary cilium will depend on the mechanical coupling of the tubules due to local constrained motion of the tubule wall. The objective of this work was to determine the in-plane stresses of a primary cilium attached to the inner wall of one renal tubule subject to the applied pulsatile flow, with a neighboring renal tube filled with stagnant fluid in close proximity to the primary tubule. We used the commercial software COMSOLⓇ to model the fluid-structure interaction of the applied flow and tubule wall, and we applied a boundary load to the face of the primary cilium during this simulation to produces a stress at its base. We confirm our hypothesis by observing that on average the in-plane stresses are greater at the base of the cilium when there is a neighboring renal tube versus if there is no neighboring tube at all. In combination with the hypothesized function of a cilium as a biological fluid flow sensor, these results indicate that flow signaling may also depend on how the tubule wall is constrained by neighboring tubules. Our results may be limited in their interpretation due to the simplified nature of our model geometry, and further improvements to the model may potentially lead to the design of future experiments.more » « less
-
The equine hoof wall has outstanding impact resistance, which enables high-velocity gallop over hard terrain with minimum damage. To better understand its viscoelastic behavior, complex moduli were de- termined using two complementary techniques: conventional ( ∼5 mm length scale) and nano ( ∼1 μm length scale) dynamic mechanical analysis (DMA). The evolution of their magnitudes was measured for two hydration conditions: fully hydrated and ambient. The storage modulus of the ambient hoof wall was approximately 400 MPa in macro-scale experiments, decreasing to ∼250 MPa with hydration. In contrast, the loss tangent decreased for both hydrated ( ∼0.1–0.07) and ambient ( ∼0.04–0.01) conditions, over the frequency range of 1–10 Hz. Nano-DMA indentation tests conducted up to 200 Hz showed little frequency dependence beyond 10 Hz. The loss tangent of tubular regions showed more hydration sensitivity than in intertubular regions, but no significant difference in storage modulus was observed. Loss tangent and effective stiffness were higher in indentations for both hydration levels. This behavior is attributed to the hoof wall’s hierarchical structure, which has porosity, functionally graded aspects, and material interfaces that are not captured at the scale of indentation. The hoof wall’s viscoelasticity characterized in this work has implications for the design of bioinspired impact-resistant materials and structures.more » « less
-
This paper describes the main findings from an experimental investigation into local and overall strength and fracture behavior of a microstructurally flexible, quadruplex, high entropy alloy (HEA), Fe42Mn28Co10Cr15Si5 (in at%). The alloy consists of metastable face-centered cubic austenite (g), stable hexagonal epsilon martensite (ε), stable body-centered cubic ferrite (a), and stable tetragonal sigma (σ) phases. The overall behavior of the alloy in compression features a great deal of plasticity and strain hardening before fracture. While the contents of diffusion created a and σ phases remain constant during deformation, the fraction of ε increases at the expanse of g due to the diffusionless strain induced γ→ε phase transformation. High-throughput nanoindentation mapping is used to assess the mechanical hardness of individual phases contributing to the plasticity and hardening of the alloy. Increasing the fraction of the dislocated ε phase during deformation due to the transformation is found to act as a secondary source of hardening because g and ε exhibit similar hardness at a given strain level. While these two phases exhibit moderate hardening during plasticity, significant softening is observed in σ owing to the phase fragmentation. While the phase transformation mechanism facilitates accommodation of the plasticity, the primary source of strain hardening in the alloy is the refinement of the structure during the transformation inducing a dynamic Hall-Petch-type barrier effect. Results pertaining to the evolution of microstructure and local behavior of the alloy under compression are presented and discussed clarifying the origins of strain hardening. While good under compression, the alloy poorly behaves under tension. Fracture surfaces after tension feature brittle micromechanisms of fracture. Such behavior is attributed to the presence of the brittle σ phase.more » « less