Title: Highly Tunable Relaxors Developed from Antiferroelectrics
Abstract Highly responsive, voltage‐tunable dielectrics are essential for microwave‐telecommunication electronics. Ferroelectric/relaxor materials have been leading candidates for such functionality and have exhibited agile dielectric responses. Here, it is demonstrated that relaxor materials developed from antiferroelectrics can achieve both ultrahigh dielectric response and tunability. The system, based on alloying the archetypal antiferroelectric PbZrO3with the dielectric BaZrO3, exhibits a more complex phase evolution than that in traditional relaxors and is characterized by an unconventional multi‐phase competition between antiferroelectric, ferroelectric, and paraelectric order. This interplay of phases can greatly enhance the local heterogeneities and results in relaxor characteristics while preserving considerable polarizability. Upon studying Pb1‐xBaxZrO3forx= 0‐0.45, Pb0.65Ba0.35ZrO3is found to provide for exceptional dielectric tunability under low bias fields (≈81% at 200 kV cm−1and ≈91% at 500 kV cm−1) at 10 kHz, outcompeting most traditional relaxor ferroelectric films. This high tunability is sustained in the radio‐frequency range, resulting in a high commutation quality factor (>2000 at 1 GHz). This work highlights the phase evolution from antiferroelectrics (with lower, “positive” dielectric tunability) to relaxors (with higher, “negative” tunability), underscoring a promising approach to develop relaxors with enhanced functional capabilities and new possibilities.  more » « less
Award ID(s):
2329111
PAR ID:
10632480
Author(s) / Creator(s):
; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ; ;
Publisher / Repository:
Wiley
Date Published:
Journal Name:
Advanced Materials
Volume:
37
Issue:
32
ISSN:
0935-9648
Subject(s) / Keyword(s):
Sponsoring Org:
National Science Foundation
More Like this
  1. Abstract Li+and Bi3+(at 1:1 ratio) substitution of Pb2+in the model compound PbZrO3is investigated. It is found that [Pb1−x(Li1/2Bi1/2)x]ZrO3ceramics remain phase pure of orthorhombic perovskite atx = 0.05, are almost phase pure atx = 0.10 and 0.15, and contain minor amounts of impurity phases atx = 0.20. The substitution allows the ceramics to be sintered to a high density at reduced temperatures, and at the same time, significantly enhances the dielectric breakdown strength. At 160°C when reversible antiferroelectric (AFE)–ferroelectric (FE) phase transitions are observed in all compositions, the chemical substitution is shown to reduce the electric hysteresis, increase the energy storage density, and improve the energy efficiency. The results will help design future high‐performance ceramics for energy storage capacitors. It is further observed that the (Li1/2Bi1/2) substitution of Pb in PbZrO3weakly impacts the dielectric behavior of the ceramics: The temperature at dielectric maximum,Tm, varies within a narrow range of 232.4–237.6°C; the relaxation parameter in the paraelectric phase,γ, stays close to unity and barely changes; and the diffuseness parameter of the phase transition atTm,d, remains low. Defect dipoles of preferably along 〈1 1 0〉 directions are proposed to explain the un‐disrupted long‐range AFE order in the [Pb1−x(Li1/2Bi1/2)x]ZrO3ceramics. 
    more » « less
  2. Abstract Relaxor ferroelectrics (RFEs) are being actively investigated for energy‐storage applications due to their large electric‐field‐induced polarization with slim hysteresis and fast energy charging–discharging capability. Here, a novel nanograin engineering approach based upon high kinetic energy deposition is reported, for mechanically inducing the RFE behavior in a normal ferroelectric Pb(Zr0.52Ti0.48)O3(PZT), which results in simultaneous enhancement in the dielectric breakdown strength (EDBS) and polarization. Mechanically transformed relaxor thick films with 4 µm thickness exhibit an exceptionalEDBSof 540 MV m−1and reduced hysteresis with large unsaturated polarization (103.6 µC cm−2), resulting in a record high energy‐storage density of 124.1 J cm−3and a power density of 64.5 MW cm−3. This fundamental advancement is correlated with the generalized nanostructure design that comprises nanocrystalline phases embedded within the amorphous matrix. Microstructure‐tailored ferroelectric behavior overcomes the limitations imposed by traditional compositional design methods and provides a feasible pathway for realization of high‐performance energy‐storage materials. 
    more » « less
  3. Abstract Achieving substantial electrostrain alongside a large effective piezoelectric strain coefficient (d33*) in piezoelectric materials remains a formidable challenge for advanced actuator applications. Here, a straightforward approach to enhance these properties by strategically designing the domain structure and controlling the domain switching through the introduction of arrays of ordered {100}<100> dislocations is proposed. This dislocation engineering yields an intrinsic lock‐in steady–state electrostrain of 0.69% at a low field of 10 kV cm−1without external stress and an output strain energy density of 5.24 J cm−3in single‐crystal BaTiO3, outperforming the benchmark piezoceramics and relaxor ferroelectric single‐crystals. Additionally, applying a compression stress of 6 MPa fully unlocks electrostrains exceeding 1%, yielding a remarkabled33* value over 10 000 pm V−1and achieving a record‐high strain energy density of 11.67 J cm−3. Optical and transmission electron microscopy, paired with laboratory and synchrotron X‐ray diffraction, is employed to rationalize the observed electrostrain. Phase‐field simulations further elucidate the impact of charged dislocations on domain nucleation and domain switching. These findings present an effective and sustainable strategy for developing high‐performance, lead‐free piezoelectric materials without the need for additional chemical elements, offering immense potential for actuator technologies. 
    more » « less
  4. Abstract The pursuit of smaller, energy‐efficient devices drives the exploration of electromechanically active thin films (<1 µm) to enable micro‐ and nano‐electromechanical systems. While the electromechanical response of such films is limited by substrate‐induced mechanical clamping, large electromechanical responses in antiferroelectric and multilayer thin‐film heterostructures have garnered interest. Here, multilayer thin‐film heterostructures based on antiferroelectric PbHfO3and ferroelectric PbHf1‐xTixO3overcome substrate clamping to produce electromechanical strains >4.5%. By varying the chemistry of the PbHf1‐xTixO3layer (x = 0.3‐0.6) it is possible to alter the threshold field for the antiferroelectric‐to‐ferroelectric phase transition, reducing the field required to induce the onset of large electromechanical response. Furthermore, varying the interface density (from 0.008 to 3.1 nm−1) enhances the electrical‐breakdown field by >450%. Attaining the electromechanical strains does not necessitate creating a new material with unprecedented piezoelectric coefficients, but developing heterostructures capable of withstanding large fields, thus addressing traditional limitations of thin‐film piezoelectrics. 
    more » « less
  5. null (Ed.)
    A systematic study of (1− x )Pb(Fe 0.5 Nb 0.5 )O 3 – x BiFeO 3 ( x = 0–0.5) was performed by combining dielectric and electromechanical measurements with structural and microstructural characterization in order to investigate the strengthening of the relaxor properties when adding BiFeO 3 into Pb(Fe 0.5 Nb 0.5 )O 3 and forming a solid solution. Pb(Fe 0.5 Nb 0.5 )O 3 crystalizes in monoclinic symmetry exhibiting ferroelectric-like polarization versus electric field ( P–E ) hysteresis loop and sub-micron-sized ferroelectric domains. Adding BiFeO 3 to Pb(Fe 0.5 Nb 0.5 )O 3 favors a pseudocubic phase and a gradual strengthening of the relaxor behavior of the prepared ceramics. This is indicated by a broadening of the peak in temperature-dependent permittivity, narrowing of P–E hysteresis loops and decreasing size of ferroelectric domains resulting in polar nanodomains for x = 0.20 composition. The relaxor behavior was additionally confirmed by Vogel–Fulcher analysis. For the x ≥ 0.30 compositions, broad high-temperature anomalies are observed in dielectric permittivity versus temperature measurements in addition to the frequency-dispersive peak located close to room temperature. These samples also exhibit pinched P–E hysteresis loops. The observed pinching is most probably related to the reorganization of polar nanoregions under the electric field as shown by synchrotron X-ray diffraction measurements as well as by piezo-response force microscopy analysis, while in part affected by the presence of charged point defects and anti-ferroelectric order, as indicated from rapid cooling experiments and high-resolution transmission electron microscopy, respectively. 
    more » « less