Abstract A highly stable phosphonate‐functionalized viologen is introduced as the redox‐active material in a negative potential electrolyte for aqueous redox flow batteries (ARFBs) operating at nearly neutral pH. The solubility is 1.23mand the reduction potential is the lowest of any substituted viologen utilized in a flow battery, reaching −0.462 V versus SHE at pH = 9. The negative charges in both the oxidized and the reduced states of 1,1′‐bis(3‐phosphonopropyl)‐[4,4′‐bipyridine]‐1,1′‐diium dibromide (BPP−Vi) effect low permeability in cation exchange membranes and suppress a bimolecular mechanism of viologen decomposition. A flow battery pairing BPP−Vi with a ferrocyanide‐based positive potential electrolyte across an inexpensive, non‐fluorinated cation exchange membrane at pH = 9 exhibits an open‐circuit voltage of 0.9 V and a capacity fade rate of 0.016% per day or 0.00069% per cycle. Overcharging leads to viologen decomposition, causing irreversible capacity fade. This work introduces extremely stable, extremely low‐permeating and low reduction potential redox active materials into near neutral ARFBs.
more »
« less
A High Potential, Low Capacity Fade Rate Iron Complex Posolyte for Aqueous Organic Flow Batteries
Abstract An iron complex, tris(4,4′‐bis(hydroxymethyl)‐2,2′‐bipyridine) iron dichloride is reported, which operates at near‐neutral pH with a redox potential of 0.985 V versus SHE. This high potential compound is employed in the posolyte of an aqueous flow battery, paired with bis(3‐trimethylammonio)propyl viologen tetrachloride in the negolyte, exhibiting an open‐circuit voltage of 1.3 V at near‐neutral pH. It demonstrates excellent cycling performance with a low temporal capacity fade rate of 0.07% per day over 35 days of cycling. The extended cycling lifetime is the result of low permeability and improved structural stability of the newly developed iron complex compared to that of the iron tris(bipyridine) complex. The combination of high redox potential and low capacity fade rate compares favorably with those of all previously demonstrated organic and organometallic aqueous posolytes. Extensive investigation into the possible degradation mechanisms, including post‐mortem chemical and electrochemical analyses, indicates that stepwise ligand dissociations of the iron complex are responsible for the reported capacity loss during cell cycling. This investigation provides unprecedented insight to guide further improvements of such metalorganic compounds for energy storage and conversion applications.
more »
« less
- Award ID(s):
- 1914543
- PAR ID:
- 10381629
- Publisher / Repository:
- Wiley Blackwell (John Wiley & Sons)
- Date Published:
- Journal Name:
- Advanced Energy Materials
- Volume:
- 12
- Issue:
- 44
- ISSN:
- 1614-6832
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
Abstract Aqueous organic redox flow batteries are promising candidates for large‐scale energy storage. However, the design of stable and inexpensive electrolytes is challenging. Here, we report a highly stable, low redox potential, and potentially inexpensive negolyte species, sodium 3,3′,3′′,3′′′‐((9,10‐anthraquinone‐2,6‐diyl)bis(azanetriyl))tetrakis(propane‐1‐sulfonate) (2,6‐N‐TSAQ), which is synthesized in a single step from inexpensive precursors. Pairing 2,6‐N‐TSAQ with potassium ferrocyanide at pH=14 yielded a battery with the highest open‐circuit voltage, 1.14 V, of any anthraquinone‐based cell with a capacity fade rate <10 %/yr. When 2,6‐N‐TSAQ was cycled at neutral pH, it exhibited two orders of magnitude higher capacity fade rate. The great difference in anthraquinone cycling stability at different pH is interpreted in terms of the thermodynamics of the anthrone formation reaction. This work shows the great potential of organic synthetic chemistry for the development of viable flow battery electrolytes and demonstrates the remarkable performance improvements achievable with an understanding of decomposition mechanisms.more » « less
-
Aqueous redox flow batteries using low-cost organic and inorganic active materials have received growing interest for sustainable energy storage. In this study, a low-cost, high redox potential (1.08 V vs. NHE) and high capacity ammonium bromide (NH 4 Br, 214.4 A h L −1 ) catholyte was coupled with an organic viologen anolyte to demonstrate 1.51 V high voltage (SPr) 2 V/Br − aqueous redox flow batteries under pH neutral conditions for the first time. Benefitting from the high water solubility of both the NH 4 Br catholyte and (SPr) 2 V anolyte, the newly designed (SPr) 2 V/Br − organic flow battery was operated at up to 1.5 M and an energy density of up to 30.4 W h L −1 . Using multiwall carbon nanotubes as an electrochemical additive for the Br 3 − /Br − redox couple, the highly energy dense (SPr) 2 V/Br − flow battery manifested outstanding current performance, up to 78% energy efficiency at 40 mA cm −2 current density and 227 mW cm −2 power density, the highest power density known for pH neutral organic flow batteries.more » « less
-
Non-aqueous organic redox flow batteries (NAORFBs) are considered emerging large-scale energy storage systems due to their larger voltage window as compared to aqueous systems and their metal-free nature. However, low solubility, sustainability, and crossover of redox materials remain major challenges for the development of NAORFBs. Here, we report the use of redox active α-helical polypeptides suitable for NAORFBs. The polypeptides exhibit less crossover than small molecule analogs for both Daramic 175 separator and FAPQ 375 PP membrane, with FAPQ 375 PP preventing crossover most effectivley. Polypeptide NAORFBs assembled with a TEMPO-based polypeptide catholyte and viologen-based polypeptide anolyte exhibit low capacity fade ( ca. 0.1% per cycle over 500 cycles) and high coulombic efficiency (>99.5%). The polypeptide NAORFBs exhibit an output voltage of 1.1 V with a maximum capacity of 0.53 A h L −1 (39% of the theoretical capacity). After 500 charge–discharge cycles, 60% of the initial capacity was retained. Post cycling analysis using spectral and electrochemical methods demonstrate that the polypeptide backbone and the ester side chain linkages are stable during electrochemical cycling. Taken together, these polypeptides offer naturally-derived, deconstructable platforms for addressing the needs of metal-free energy storage.more » « less
-
Abstract Aqueous organic redox flow batteries (AORFBs) have been recognized as a promising technology for large‐scale, long‐duration energy storage of renewables (e.g., solar and wind) by overcoming their intermittence and fluctuation. However, simultaneous demonstration of high energy densities and stable cycling are still challenging for AORFBs. Herein, asymmetrically substituted sulfonate viologen molecular designs, e.g. (1‐[3‐sulfonatopropyl]‐1′‐[4‐sulfonatobutane]‐4,4′‐bipyridinium (3,4‐S2V), as capacity dense, chemically stable anolytes for cation exchange AORFBs are presented. The robust cycling performance of 3,4‐S2V is confirmed using half‐cell and full‐cell flow battery studies at pH neutral conditions. The 3,4‐S2V based AORFB is demonstrated with a discharge capacity of 23.2 Ah L−1for 1700 cycles or 100 days without observing chemical degradation. Furthermore, a 3,4‐S2V/(NH4)4[Fe(CN)6] AORFB with a discharge capacity of 259.9 mAh is demonstrated for 50 days of authentic energy storage for the first time with a total capacity retention of 97.77% or a temporal capacity retention rate of 99.955% per day, representing the most stable, longest cycled AORFB to date.more » « less
An official website of the United States government