Electrospinning is a versatile approach to generate nanofibers in situ. Yet, recently, wet electrospinning has been introduced as a more efficient way to deposit isolated fibers inside bulk materials. In wet electrospinning, a liquid bath is adopted, instead of a solid collector, for fiber collection. However, despite several studies focused on wet electrospinning to yield polymer composites, few studies have investigated wet electrospinning to yield ceramic composites. In this paper, we propose a novel in-situ fabrication approach for nanofiber-reinforced ceramic composites based on an enhanced wet-electrospinning method. Our method uses electrospinning to draw polymer nanofibers directly into a reactive pre-ceramic gel, which is later activated to yield advanced nanofiber-reinforced ceramic composites. We demonstrate our method by investigating wet electrospun Polyacrylonitrile and Poly(ethylene oxide) fiber-reinforced geopolymer composites, with fiber weight fractions in the range 0.1–1.0 wt%. Wet electrospinning preserves the amorphous structure of geopolymer while changing the molecular arrangement. Wet electrospinning leads to an increase in both the fraction of mesopores and the overall porosity of geopolymer composites. The indentation modulus is in the range 6.76–8.90 GPa and the fracture toughness is in the range 0.49–0.76 MPam with a clear stiffening and toughening effect observed for Poly(ethylene oxide)-reinforced geopolymer composites. This work demonstrates the viability of wet electrospinning to fabricate multifunctional nanofiber-reinforced composites.
more »
« less
Role of Draw Rate and Molecular Weight when Electrospun Nanofibers are Post‐Drawn with Residual Solvent
Abstract The postdrawing process is poorly understood for polymer nanofibers due to the difficulty of manipulating nanofiber structures. Here, an angled track system facilitates postdrawing of individual nanofibers with control of parameters including molecular weight, draw rate, draw ratio, and solvent evaporation time. In this study, the effects of molecular weight, draw rate, and relative residual solvent content on final nanofiber properties are investigated. Molecular weight is first investigated to clarify any influence polymer chain length can have on drawing in facilitating or hindering chain extensibility. Polyacrylonitrile nanofibers with 50 and 150 kDa molecular weights behave similarly with postdrawing resulting in reduced diameters and enhanced mechanics. Since solvent quantity during drawing is a time sensitive component it is meaningful to assess the impact of draw rate on the chemical and structural makeup of postdrawn fibers. Chemical bond vibrations and chain orientation are sensitive to draw rate when polycaprolactone nanofibers are dried for 3 minutes prior to postdrawing, but this dependency to draw rate is not observed when fibers are postdrawn immediately upon collection. These findings demonstrate that the amount of retained solvent at collection is relevant to this postprocessing approach, and highlights the dynamics of solvent evaporation during postdrawing.
more »
« less
- Award ID(s):
- 1653329
- PAR ID:
- 10397201
- Publisher / Repository:
- Wiley Blackwell (John Wiley & Sons)
- Date Published:
- Journal Name:
- Macromolecular Materials and Engineering
- Volume:
- 308
- Issue:
- 2
- ISSN:
- 1438-7492
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
This paper reports the molecular organization and mechanical properties of electrospun, post-drawn polyacrylonitrile (PAN) nanofibers. Without post-drawing, the polymer chain was kinked and oriented in hexagonal crystalline structures. Immediate post-drawing in the semi-solid state disrupted the crystal structures and chain kink at maximum draw ratio. Structural re-orientation at maximum draw resulted in a 500% increase in Young's modulus and a 100% increase in ultimate tensile strength. By applying post-drawing to electrospinning it may be possible to obtain PAN fibers and PAN-derived carbon fibers with enhanced mechanical properties compared to available fabrication technologies.more » « less
-
Ultrasound acoustic waves are demonstrated to assemble poly-3-hexylthiophene (P3HT) chains into nanofibers after they are fully dissolved in what are commonly considered to be ‘good’ solvents. In the absence of ultrasound, the polymer remains fully dissolved and does not self-assemble for weeks. UV-vis spectroscopy, ultra-small angle X-ray scattering (USAXS) and small angle neutron scattering (SANS) are used to characterize the induced assembly process and to quantify the fraction of polymer that forms nanofibers. It is determined that the solvent type, insonation time, and aging periods are all important factors affecting the structure and final concentration of fibers. The effect of changing polymer regio-regularity, alkyl chain length, and side chain to thiophene ratio are also explored. High intensity focused ultrasound (HIFU) fields of variable intensity are utilized to reveal the physical mechanisms leading to nanofiber formation, which is strongly correlated to cavitation events in the solvent. This in situ HIFU cell, which is designed for simultaneous scattering analysis, is also used to probe for structural changes occurring over multiple length scales using USAXS and SANS. The proposed acoustic assembly mechanism suggests that, even when dispersed in ‘good’ solvents such as bromobenzene, dichlorobenzene and chloroform, P3HT chains are still not in a thermodynamically stable state. Instead, they are stabilized by local energy barriers that slow down and effectively prevent crystallization. Ultrasound fields are found to provide enough mechanical energy to overcome these barriers, triggering the formation of small crystalline nuclei that subsequently seed the growth of larger nanofibers.more » « less
-
In an effort to develop and design next generation high power target materials for particle physics research, the possibility of fabricating nonwoven metallic or ceramic nanofibers by electrospinning process is explored. A low-cost electrospinning unit is set up for in-house production of various ceramic nanofibers. Yttria-stabilized zirconia nanofibers are successfully fabricated by electrospinning a mixture of zirconium carbonate with high-molecular weight polyvinylpyrrolidone polymer solution. Some of the inherent weaknesses of electrospinning process like thickness of nanofiber mat and slow production rate are overcome by modifying certain parts of electrospinning system and their arrangements to get thicker nanofiber mats of millimeter order at a faster rate. Continuous long nanofibers of about hundred nanometers in diameter are produced and subsequently heat treated to get rid of polymer and allow crystallize zirconia. Specimens were prepared to meet certain minimum physical properties such as thickness, structural integrity, thermal stability, and flexibility. An easy innovative technique based on atomic force microscopy was employed for evaluating mechanical properties of single nanofiber, which were found to be comparable to bulk zirconia. Nanofibers were tested for their high-temperature resistance using an electron beam. It showed resistance to radiation damage when irradiated with 1 MeV Kr2+ ion. Some zirconia nanofibers were also tested under high-intensity pulsed proton beam and maintained their structural integrity. This study shows for the first time that a ceramic nanofiber has been tested under different beams and irradiation condition to qualify their physical properties for practical use as accelerator targets. Advantages and challenges of such nanofibers as potential future targets over bulk material targets are discussed.more » « less
-
Polymer nanofibers hold promise in a wide range of applications owing to their diverse properties, flexibility, and cost effectiveness. In this study, we introduce a polymer nanofiber drawing process in a scanning electron microscope and focused ion beam (SEM/FIB) instrument with in situ observation. We employed a nanometer-sharp tungsten needle and prepolymer microcapsules to enable nanofiber drawing in a vacuum environment. This method produces individual polymer nanofibers with diameters as small as ∼500 nm and lengths extending to millimeters, yielding nanofibers with an aspect ratio of 2000:1. The attachment to the tungsten manipulator ensures accurate transfer of the polymer nanofiber to diverse substrate types as well as fabrication of assembled structures. Our findings provide valuable insights into ultrafine polymer fiber drawing, paving the way for high-precision manipulationmore » « less
An official website of the United States government