Title: The glass transition and enthalpy recovery of polystyrene nanorods using Flash differential scanning calorimetry
The glass transition (Tg) behavior and enthalpy recovery of polystyrene nanorods within an anodic aluminum oxide (AAO) template (supported nanorods) and after removal from AAO (unsupported nanorods) is studied using Flash differential scanning calorimetry. Tg is found to be depressed relative to the bulk by 20 ± 2 K for 20 nm-diameter unsupported polystyrene (PS) nanorods at the slowest cooling rate and by 9 ± 1 K for 55 nm-diameter rods. On the other hand, bulk-like behavior is observed in the case of unsupported 350 nm-diameter nanorods and for all supported rods in AAO. The size-dependent Tg behavior of the PS unsupported nanorods compares well with results for ultrathin films when scaled using the volume/surface ratio. Enthalpy recovery was also studied for the 20 and 350 nm unsupported nanorods with evolution toward equilibrium found to be linear with logarithmic time. The rate of enthalpy recovery for the 350 nm rods was similar to that for the bulk, whereas the rate of recovery was enhanced for the 20 nm rods for down-jump sizes larger than 17 K. A relaxation map summarizes the behavior of the nanorods relative to the bulk and relative to that for the 20 nm-thick ultrathin film. Interestingly, the fragility of the 20 nm-diameter nanorod and the 20 nm ultrathin film are identical within the error of measurements, and when plotted vs departure from Tg (i.e., T − Tg), the relaxation maps of the two samples are identical in spite of the fact that the Tg is depressed 8 K more in the nanorod sample.  more » « less
Award ID(s):
2141221
PAR ID:
10506280
Author(s) / Creator(s):
;
Publisher / Repository:
AIP
Date Published:
Journal Name:
The Journal of Chemical Physics
Volume:
160
Issue:
12
ISSN:
0021-9606
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. Abstract Conjugated polymers consist of complex backbone structures and side‐chain moieties to meet various optoelectronic and processing requirements. Recent work on conjugated polymers has been devoted to studying the mechanical properties and developing new conjugated polymers with low modulus and high‐crack onset strain, while the thin film mechanical stability under long‐term external tensile strain is less investigated. Here we performed direct mechanical stress relaxation tests for both free‐standing and thin film floated on water surface on both high‐Tgand low‐Tgconjugated polymers, as well as a reference nonconjugated sample, polystyrene. We measured thin films with a range of film thickness from 38 to 179 nm to study the temperature and thickness effect on thin film relaxation, where an apparent enthalpy–entropy compensation effect for glassy polymer PS and PM6 thin films was observed. We also compared relaxation times across three different conjugated polymers and showed that both crystalline morphology and higher modulus reduce the relaxation rate besides higher glass transition temperature. Our work provides insights into the mechanical creep behavior of conjugated polymers, which will have an impact on the future design of stable functional organic electronics. 
    more » « less
  2. The self-assembly of gold nanorods (AuNRs) of different sizes with a block copolymer (BCP) is studied. Polystyrene- block -poly(2-vinylpyridine) (PS- b -P2VP) films containing P2VP functionalized AuNRs are solvent annealed resulting in a BCP morphology of vertical P2VP cylinders in a PS matrix. At the surface of the PS- b -P2VP films long AuNRs are found in the bridging and vertical states. The bridging state is where the long axis of the AuNR is parallel to the film surface, the AuNR is embedded in the film, and each end of the AuNR is at the top of nearest neighbor P2VP cylinders. The vertical state is where the AuNR is localized within a vertical P2VP cylinder, the AuNR long axis is perpendicular to the film surface and the upper tip of the AuNR is at the film surface. Short AuNRs were found in the bridging and vertical states as well as in a state not observed for the long AuNRs, the centered state. The centered state is where an AuNR has its long axis parallel to the film surface, is embedded in the film, and is centered over a vertical P2VP cylinder. Hybrid particle-field theory (HPFT) simulations modeling the experimental system predict that for the long AuNRs only the bridging state should be observed while for the short AuNRs only the bridging and centered states should be observed. Possible explanations for why the vertical state is observed in experiments despite being thermodynamically unfavorable in simulations are discussed. HPFT simulations also show that when a nanorod is in the bridging state the two cylinders it bridges remain intact and extend from the nanorod to the substrate. Further, the minority block of the BCP is shown to wet the bottom of the bridging nanorod. The bridging state is very promising for the future development of self-assembled nanoscale devices. 
    more » « less
  3. In the present work, we use ellipsometry to extract the physical aging response of thin glassy polystyrene (PS) layers from rubbery–glassy bilayer films of poly(n-butyl methacrylate) (PnBMA) atop PS. How the soft interface between rubbery and glassy polymer domains can impact the physical aging response of glassy domains is unclear. Measurements in the literature have shown that the local glass transition temperature Tg of PS is strongly reduced near a PnBMA/PS interface with a magnitude twice as large compared to that imparted by a free surface. As the free surface is known to reduce physical aging, we anticipated large changes in the physical aging response of PS within PnBMA/PS bilayer films. However, surprisingly the aging response remained equivalent to bulk down to 75 nm PS layer thicknesses that were the thinnest we found could be accurately measured given the optical limits of dispersion. With complementary fluorescence measurements, we show that the average Tg(hPS) of such PS layers within 150 nm PnBMA/75 nm PS bilayer films are also still bulk. These findings demonstrate that films with finite domain sizes have interfacial dynamical gradients that are significantly altered from those previously measured in systems with semi-infinite domain sizes. 
    more » « less
  4. The work demonstrates a three-fold increase in photoelectrochemical efficiency of hematite nanorods as a result of the combination of Hafnium surface doping and the incorporation of a ZrO2 underlayer on FTO. While the ZrO2 layer reduced the electron loss from the back-injection into the FTO contact support, Hafnium surface doping did not significantly alter the hematite lattice structure. But rather, Hafnium induced nanorod diameter reduction from 32 ± 2 and 26 ± 2 nm, with a consequent increase in the active surface area. The linear sweep voltammetry measurements with 100 mW cm−2 illumination in a 500 nm photoanode thickness showed a photocurrent density of 2.07 mA cm−2 at 1.23 V in a reversible hydrogen electrode (RHE). The value contrasts with the bare hematite rods (0.75 mA cm−2), highlighting the photoanode design's role in improving solar power hydrogen production. 
    more » « less
  5. Glassy films of methyl-m-toluate have been vapor deposited onto a substrate equipped with interdigitated electrodes, facilitating in situ dielectric relaxation measurements during and after deposition. Samples of 200 nm thickness have been deposited at rates of 0.1 nm/s at a variety of deposition temperatures between 40 K and Tg = 170 K. With increasing depth below the surface, the dielectric loss changes gradually from a value reflecting a mobile surface layer to that of the kinetically stable glass. The thickness of this more mobile layer varies from below 1 to beyond 10 nm as the deposition temperature is increased, and its average fictive temperature is near Tg for all deposition temperatures. Judged by the dielectric loss, the liquid-like portion of the surface layer exceeds a thickness of 1 nm only for deposition temperatures above 0.8Tg, where near-equilibrium glassy states are obtained. After deposition, the dielectric loss of the material positioned about 5–30 nm below the surface decreases for thousands of seconds of annealing time, whereas the bulk of the film remains unchanged. 
    more » « less