High‐entropy oxides (HEOs) are being extensively studied for various functional applications, but there is limited research into the mechanical behavior of these materials, especially at elevated temperatures. Bulk (Co, Cu, Mg, Ni, Zn)O (transition metal (TM)‐HEO) samples are formed into dome shapes at 800 °C and 70 kPa. Deformation experiments and finite element analysis (FEA) reveal that TM‐HEO has a creep stress exponent ofn = 0.6, indicating that TM‐HEO deforms through superplastic deformation and exhibits shear‐thickening behavior. Comparisons of experimental strain rates to those calculated using existing superplasticity mechanism models signify that TM‐HEO deforms through grain boundary sliding accommodated by a solution‐precipitation mechanism from a secondary phase. A Cu‐rich tenorite phase, commonly observed in the grain boundaries of TM‐HEO, is proposed as the secondary phase facilitating deformation. It is important to highlight here that the superplastic deformation behavior in TM‐HEO is active under modest temperature and pressure conditions, as noted above. Low‐temperature superplastic deformation will provide a powerful method of manufacturing HEO ceramics into net shape parts, greatly expanding their potential applications.
more »
« less
This content will become publicly available on December 1, 2026
Shear-Thickening Superplastic Transitions in High-Entropy Oxides
Despite significant interest in their functional properties, the mechanical behavior of high-entropy oxides (HEOs) is not well studied, particularly at elevated temperatures. Bulk (Co,Cu,Mg,Ni,Zn)O (transition metal (TM)-HEO) samples were deformed under compression at applied stresses and temperatures ranging from 5 to 31 MPa and 600 to 850 °C, respectively. All of the deformation conditions result in creep stress exponents of n < 3, indicating that TM-HEO exhibits superplastic deformation. A transition from structural to solution-precipitation-based superplasticity is observed during deformation above 650 °C. Additionally, TM-HEO exhibits shear-thickening behavior when deformed at stresses above 9 MPa. The formation and behavior of a Cu-rich tenorite secondary phase during deformation is identified as a key factor underpinning the deformation mechanisms. The microstructure and phase state of TM-HEO before deformation also influenced the behavior, with finer grain sizes and increasing concentrations of Cu-rich tenorite, resulting in the increased prevalence of solution-precipitation deformation. While complex, the results of this study indicate that TM-HEO deforms through known superplastic deformation mechanisms. Superplasticity is a highly efficient manufacturing method and could prove to be a valuable strategy for forming HEO ceramics into complex geometries.
more »
« less
- PAR ID:
- 10653464
- Publisher / Repository:
- MDPI, Basel, Switzerland
- Date Published:
- Journal Name:
- Ceramics
- Volume:
- 8
- Issue:
- 4
- ISSN:
- 2571-6131
- Page Range / eLocation ID:
- 136
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
Superplastic behavior is observed in metals, ceramics, and some geologic materials where fine grained materials deform to large strains (>200%) without failure. While somewhat common in metals and ceramics, superplasticity is less studied in geologic materials, and tends to be restricted to olivine deformation experiments that are used to infer mantle rheology. Here we show unequivocal evidence for the operation of DisGBS-mediated superplasticity in naturally deformed amphibole, an abundant mineral in deep continental crust, which has not been previously shown to deform by high-temperature grain size sensitive processes. We sampled hornblendites from the base of Cordilleran-style continental arc crust exposed in Fiordland, New Zealand. The samples are from the Hawes Head ultramafic complex at the base of the Misty Pluton, which is composed of a hornblende diorite emplaced at 120-115 Ma at depths of 25-40 km. The hornblendites have an anastomosing mylonitic foliation which formed within the long-lived Straight River Shear Zone at the western edge of the Misty Pluton when it was reactivated in the Cretaceous (~126-110 Ma) during a pulse of arc magmatism. We place maximum P and T estimates on mylonitic fabric development in our samples based on amphibole crystallization pressures of 8.5 -10 kbar and temperatures of 940-1000ºC derived from electron microprobe analyses of an adjacent undeformed hornblendite. We use electron backscatter diffraction to investigate deformation mechanisms of naturally deformed amphibole in the hornblendite. Microstructural, pole figure, and misorientation data indicate that dynamic recrystallization (DRX) and grain size reduction led to the transition from dislocation creep to the onset of DisGBS-mediated superplasticity in the mylonites. Our data are consistent with a textural evolution in which easy slip on (100)[001] initially drives subgrain rotation DRX and CPO development in porphyroclasts during dislocation creep, producing dislocations that quickly climb out of the grains, leaving behind dislocations indicative of a harder slip system such as (010)[100] or {110}1/2<110>. Matrix grains show textural traits of DisGBS-mediated superplasticity including four grain junctions, aspect ratios >1.5, a paucity of subgrains, and the operation of a single hard slip system. This discovery of superplasticity in a natural example of amphibole-rich lower crust has profound implications for the ease of strain localization leading to the creation of crustal-scale shear zones that reactivate and drive plate tectonic boundary development.more » « less
-
Shearing an isotactic polypropylene melt, even above its equilibrium melting temperature (Tm° ~187°C) leads to the formation of stable flow-induced precursors. Anisotropic structures result from shearing at temperatures as high as 220°C (>30°C above Tm°), and are no longer generated at shearing temperatures exceeding 230°C. The long periods increase with deformation, accompanied by a change in structural morphology. The crystallization kinetics were strongly affected by flow at shearing temperatures near Tm°, and persist at even higher shearing temperatures, as chains continue to be aligned and stretched with large deformations, perhaps further stabilized by stretched chains adsorbing onto heterogeneous impurities from polymerization.more » « less
-
null (Ed.)Superplasticity denotes the ability of a limited number of materials to achieve exceptionally high tensile elongations of at least 400%. Experiments show that the Al-Mg-Sc alloys provide excellent capabilities for achieving superplastic flow and also they can be formed easily in biaxial superplastic forming operations. It is important, therefore, to examine the superplastic flow mechanism when the alloy is prepared using different procedures. This report examines the superplastic characteristics of these alloys after preparation without subjecting to any severe plastic deformation (SPD), after processing using the two SPD procedures of equal-channel angular pressing (ECAP) and high-pressure torsion (HPT) and after processing using the alternative procedure of friction stir processing (FSP). The results are compared using each technique and they are examined with reference to a theoretical model that was developed specifically for superplastic flow in conventional alloys.more » « less
-
Abstract The frictional velocity dependence and healing behavior of subduction fault zones play key roles in the nucleation of stick‐slip instabilities at convergent margins. Diagenetic to low‐grade metamorphic processes such as pressure solution are proposed to be responsible for the change in frictional properties of fault materials along plate interfaces; pressure solution also likely contributes to the acceleration of healing according to previous studies. Here, we report friction studies for temperatures of 20–100°C and normal stresses from 20 to 125 MPa on samples collected from ancient subduction fault zones, the Lower Mugi and Makimine mélanges of the Cretaceous Shimanto belt. The two mélanges correspond to the updip and downdip limits of the seismogenic zone and include deformation features that indicate lower and higher degrees of pressure solution. Our data show that the Lower Mugi mélange exhibits velocity‐weakening to velocity‐neutral frictional behavior under low normal stress and that the Makimine mélange sample shows velocity‐strengthening behavior under high normal stress. We suggest that mineralogical changes due to diagenesis and metamorphism influence fault slip behavior. We measure frictional healing in slide‐hold‐slide experiments for the Lower Mugi mélange sample and document the role of pressure solution in fault healing. Our results show that frictional healing increases at higher temperatures. The microstructures related to pressure solution found in the post‐experimental gouges support the idea that the enhanced healing is related to pressure solution.more » « less