skip to main content
US FlagAn official website of the United States government
dot gov icon
Official websites use .gov
A .gov website belongs to an official government organization in the United States.
https lock icon
Secure .gov websites use HTTPS
A lock ( lock ) or https:// means you've safely connected to the .gov website. Share sensitive information only on official, secure websites.

Attention:

The NSF Public Access Repository (PAR) system and access will be unavailable from 10:00 PM ET on Friday, February 6 until 10:00 AM ET on Saturday, February 7 due to maintenance. We apologize for the inconvenience.


Title: Data-driven Bayesian model-based prediction of fatigue crack nucleation in Ni-based superalloys
Abstract This paper develops a Bayesian inference-based probabilistic crack nucleation model for the Ni-based superalloy René 88DT under fatigue loading. A data-driven, machine learning approach is developed, identifying underlying mechanisms driving crack nucleation. An experimental set of fatigue-loaded microstructures is characterized near crack nucleation sites using scanning electron microscopy and electron backscatter diffraction images for correlating the grain morphology and crystallography to the location of crack nucleation sites. A concurrent multiscale model, embedding experimental polycrystalline microstructural representative volume elements (RVEs) in a homogenized material, is developed for fatigue simulations. The RVE domain is modeled by a crystal plasticity finite element model. An anisotropic continuum plasticity model, obtained by homogenization of the crystal plasticity model, is used for the exterior domain. A Bayesian classification method is introduced to optimally select informative state variable predictors of crack nucleation. From this principal set of state variables, a simple scalar crack nucleation indicator is formulated.  more » « less
Award ID(s):
1825115
PAR ID:
10379159
Author(s) / Creator(s):
; ; ; ;
Date Published:
Journal Name:
npj Computational Materials
Volume:
8
Issue:
1
ISSN:
2057-3960
Format(s):
Medium: X
Sponsoring Org:
National Science Foundation
More Like this
  1. Abstract Microstructurally small fatigue‐crack growth in polycrystalline materials is highly three‐dimensional due to sensitivity to local microstructural features (e.g., grains). One requirement for modeling microstructurally sensitive crack propagation is establishing the criteria that govern crack evolution, including crack deflection. Here, a high‐fidelity finite‐element modeling framework is used to assess the performance and validity of various crack‐growth criteria, including slip‐based metrics (e.g., fatigue‐indicator parameters), as potential criteria for predicting three‐dimensional crack paths in polycrystalline materials. The modeling framework represents cracks as geometrically explicit discontinuities and involves voxel‐based remeshing, mesh‐gradation control, and a crystal‐plasticity constitutive model. The predictions are compared to experimental measurements of WE43 magnesium samples subject to fatigue loading, for which three‐dimensional grain structures and fatigue‐crack surfaces were measured post‐mortem using near‐field high‐energy x‐ray diffraction microscopy and x‐ray computed tomography. Findings from this work are expected to improve the predictive capabilities of simulations involving microstructurally small fatigue‐crack growth in polycrystalline materials. 
    more » « less
  2. The effects of build orientation on the fatigue behavior of additively-manufactured Ti-6Al- 4V using a Laser-Based Power Bed Fusion (L-PBF) process is investigated. Ti-6Al-4V rods were manufactured in vertical, horizontal, and 45º angle orientations. The specimens were then machined and polished along the gage section in order to reduce the effects of surface roughness on fatigue behavior. Fully-reversed strain-controlled uniaxial fatigue tests were performed at various strain amplitudes with frequencies adjusted to maintain an average constant strain rate throughout testing. Results indicate slight variation in fatigue behavior of specimens fabricated in the different orientations investigated. Fractography was conducted using scanning electron microscopy after mechanical testing in order to investigate the crack initiation sites and determine the defect responsible for the failure. The experimental program utilized and results obtained will be presented and discussed. 
    more » « less
  3. Subcritical crack growth can occur under a constant applied load below the threshold value for catastrophic failure, also known as static fatigue. Here, we report how a crack grows under a combination of stress-intensity factor (K) and temperature in a model brittle glass using molecular dynamics simulations. The model glass is under dry conditions, thus avoiding the complexity of corrosion chemistry. The crack growth rate is shown to be inconsistent with the commonly used subcritical crack growth model rooted in the transition state theory (TST), in which the applied stress-intensity factor reduces the transition barrier. A new subcritical crack growth model is proposed with a constant barrier and a K-dependent prefactor in TST, representing the size of the region for potential bond breaking. The thermomechanical condition for subcritical crack growth is also mapped in the K-T domain, in between elastic deformation and catastrophic fracture regimes. Finally, we show substantial crack self-healing once the applied load is removed, under the thermodynamic driving force of surface energy reduction. Our findings provide new insights into the mechanochemical coupling during static fatigue and call for experimental investigation of whether the activation energy is K-dependent. 
    more » « less
  4. The present work investigates fracture toughness, and actuation and mechanical fatigue crack growth responses of Ni50.3Ti29.7Hf20 HTSMAs across martensitic transformation with two different microstructures, one with H-phase nanoprecipitates and one without. H-phase precipitation is known to stabilize the actuation cycling response of NiTiHf HTSMAs and notably impacts transformation-induced plasticity. The fracture toughness tests performed reveal that precipitate-free NiTiHf has a higher fracture toughness and undergoes significantly more inelastic deformation than the one with the precipitates resulting in toughness enhancement, i.e., stable crack advance during fracture toughness experiments, which is not observed in the precipitated NiTiHf for the crack configuration and loading conditions tested. Furthermore, the precipitate free NiTiHf has higher actuation and mechanical fatigue crack growth resistance than the precipitation-hardened microstructure. This is attributed to plasticity buildup, which exacerbates the manifestation of retained martensite upon repeated transformations. The fatigue crack growth rates obtained from both actuation and mechanical fatigue experiments align to a single Paris Law Curve for the precipitation-hardened NiTiHf. This work aims to determine if unified Paris Law curves can be generated from mechanical and actuation fatigue experiments, irrespective of composition and microstructure, to estimate actuation fatigue crack growth rates, laborious and challenging to measure, from easier to detect mechanical fatigue crack growth rates. 
    more » « less
  5. A novel dislocation-density-based crystal plasticity model for nanocrystalline face-centered cubic metals is developed based on the thermally-activated mechanism of dislocations depinning from grain boundaries. Dislocations nucleated from grain boundary dislocation sources are assumed to be the primary carriers of plasticity in the nanocrystals. The evolution of the dislocation density thereby involves a competition between the nucleation of dislocations from grain boundary defect structures, such as ledges, and the absorption of dislocations into the grain boundary via diffusion processes. This model facilitates the simulation of plastic deformation in nanocrystalline metals, with consideration of the initial microstructure resulting from a particular processing method, to be computed as a direct result of dislocation-mediated plasticity only. The exclusion of grain boundary-mediated plasticity mechanisms in the formulation of the crystal plasticity model allows for the exploration of the fundamental role dislocations play in nanocrystalline plasticity. The combined effect of average grain size, grain size distribution shape, and initial dislocation density on the mechanical performance and strain-rate sensitivity are explored with the model. Further, the influence of the grain boundary diffusivity on post-yielding strain-hardening behavior is investigated to discern the impact that the choice of processing route has on the resulting deformation response of the material. 
    more » « less