This content will become publicly available on November 1, 2025
- Award ID(s):
- 1809640
- PAR ID:
- 10553157
- Publisher / Repository:
- Elsevier
- Date Published:
- Journal Name:
- Scripta Materialia
- Volume:
- 252
- Issue:
- C
- ISSN:
- 1359-6462
- Page Range / eLocation ID:
- 116236
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
A robust and efficient synthesis of triisopropylsilyl (TIPS)-protected γ-substituted enoldiazoacetates with excellent Z stereocontrol by using lithium bis(trimethylsilyl)azanide (LiHMDS) as a base and TIPSOTf as a silyl transfer reagent is reported. Despite their increased size compared to previously tert-butyldimethylsilyl (TBS)-protected γ-unsubstituted enoldiazoacetates, a high product yield with exceptional stereocontrol has been achieved in copper-catalyzed [3+3] cycloaddition reaction with nitrones by using a chiral indeno bisoxazoline ligand.more » « less
-
Cataract disease is strongly associated with progressively accumulating oxidative damage to the extremely long-lived crystallin proteins of the lens. Cysteine oxidation affects crystallin folding, interactions, and light-scattering aggregation especially strongly due to the formation of disulfide bridges. Minimizing crystallin aggregation is crucial for lifelong lens transparency, so one might expect the ubiquitous lens crystallin superfamilies (α and βγ) to contain little cysteine. Yet, the Cys content of γ-crystallins is well above the average for human proteins. We review literature relevant to this longstanding puzzle and take advantage of expanding genomic databases and improved machine learning tools for protein structure prediction to investigate it further. We observe remarkably low Cys conservation in the βγ-crystallin superfamily; however, in γ-crystallin, the spatial positioning of Cys residues is clearly fine-tuned by evolution. We propose that the requirements of long-term lens transparency and high lens optical power impose competing evolutionary pressures on lens βγ-crystallins, leading to distinct adaptations: high Cys content in γ-crystallins but low in βB-crystallins. Aquatic species need more powerful lenses than terrestrial ones, which explains the high methionine content of many fish γ- (and even β-) crystallins. Finally, we discuss synergies between sulfur-containing and aromatic residues in crystallins and suggest future experimental directions.