Wrinkle topographies have been studied as simple, versatile, and in some cases biomimetic surface functionalization strategies. To fabricate surface wrinkles, one material phenomenon employed is the mechanical-instability-driven wrinkling of thin films, which occurs when a deforming substrate produces sufficient compressive strain to buckle a surface thin film. Although thin-film wrinkling has been studied on shape-changing functional materials, including shape-memory polymers (SMPs), work to date has been primarily limited to simple geometries, such as flat, uniaxially-contracting substrates. Thus, there is a need for a strategy that would allow deformation of complex substrates or 3D parts to generate wrinkles on surfaces throughout that complex substrate or part. Here, 4D printing of SMPs is combined with polymeric and metallic thin films to develop and study an approach for fiber-level topographic functionalization suitable for use in printing of arbitrarily complex shape-changing substrates or parts. The effect of nozzle temperature, substrate architecture, and film thickness on wrinkles has been characterized, as well as wrinkle topography on nuclear alignment using scanning electron microscopy, atomic force microscopy, and fluorescent imaging. As nozzle temperature increased, wrinkle wavelength increased while strain trapping and nuclear alignment decreased. Moreover, with increasing film thickness, the wavelength increased as well.
more »
« less
Tuning the Topography of Dynamic 3D Scaffolds through Functional Protein Wrinkled Coatings
Surface wrinkling provides an approach to fabricate micron and sub-micron-level biomaterial topographies that can mimic features of the dynamic, in vivo cell environment and guide cell adhesion, alignment, and differentiation. Most wrinkling research to date has used planar, two-dimensional (2D) substrates, and wrinkling work on three-dimensional (3D) structures has been limited. To enable wrinkle formation on architecturally complex, biomimetic 3D structures, here, we report a simple, low-cost experimental wrinkling approach that combines natural silk fibroin films with a recently developed advanced manufacturing technique for programming strain in complex 3D shape–memory polymer (SMP) scaffolds. By systematically investigating the influence of SMP programmed strain magnitude, silk film thickness, and aqueous media on wrinkle morphology and stability, we reveal how to generate and tune silk wrinkles on the micron and sub-micron scale. We find that increasing SMP programmed strain magnitude increases wavelength and decreases amplitudes of silk wrinkled topographies, while increasing silk film thickness increases wavelength and amplitude. Silk wrinkles persist after 24 h in cell culture medium. Wrinkled topographies demonstrate high cell viability and attachment. These findings suggest the potential for fabricating biomimetic cellular microenvironments that can advance understanding and control of cell–material interactions in engineering tissue constructs.
more »
« less
- Award ID(s):
- 2022421
- PAR ID:
- 10559108
- Publisher / Repository:
- MDPI
- Date Published:
- Journal Name:
- Polymers
- Volume:
- 16
- Issue:
- 5
- ISSN:
- 2073-4360
- Page Range / eLocation ID:
- 609
- Format(s):
- Medium: X
- Sponsoring Org:
- National Science Foundation
More Like this
-
-
Abstract Bacterial biofilms on the surfaces of indwelling biomedical devices can cause long‐term infection and patient morbidity and mortality. Wrinkled surface topographies have previously demonstrated promising antifouling properties. Here we report a bioinspired strategy in which the actuation of silk fibroin produces tunable, wrinkled surface topographies on 2D shape memory polymer (SMP) substrates and investigate the influence of these topographies on biofilm formation. To mimic biofilm‐associated infections related to the geometries of indwelling medical devices, silk wrinkles are produced on complex, 3D SMP architectures, and biofilm formation is evaluated. Using common biofilm‐causing agents, smaller silk wrinkle wavelengths and amplitudes are found to significantly reduce biofilm formation, resulting in primarily isolated, single‐cell bacteria on the 2D wrinkled surfaces. These single‐cell bacteria are nearly completely eradicated by treatment with antibiotics, which are ineffective against control surfaces. Antibiotics are also physically incorporated into the 2D wrinkled surfaces, which resulted in a further significant reduction in bacterial adhesion. Lastly, silk wrinkled topographies are successfully applied on 3D architectures, and the wrinkled surfaces display a significant reduction in biofilm coverage compared to controls. The findings demonstrate the potential for biopolymer wrinkles on biomaterials to be used as antifouling surfaces for biofilm prevention.more » « less
-
ABSTRACT Peripheral nerve injuries (PNIs) resulting in myelin breakdown and axonal degeneration at both the proximal and distal nerve stumps are major clinical concerns that can induce functional loss and diminished quality of life. In biomaterials science, considerable attention has been given to artificial nerve guidance conduits (NGCs), since the engineered tubular structures have the potential to supply a supportive nerve microenvironment to longitudinally align the regenerating axons for bridging the injured nerve sites. Although NGCs may become promising alternatives to nerve autografts, the fabrication approaches available to incorporate directional cues for dictating neuronal behavior and nerve reconnection have been limited to conventional micro/nano‐fabrication techniques that are complex and time‐consuming due to manual processing steps. Thus, our goal here was to develop a simple manufacturing approach for introducing topographical cues onto NGCs. To achieve this goal, we used an established mechanically actuated silk wrinkling approach to create topographically functionalized surfaces as a potential NGC material platform for guided directional alignment of neurons. We 3D‐printed thermo‐responsive shape‐memory polymer (SMP)‐based NGCs that can produce silk fibroin (SF)‐wrinkled topographies on the micro and nano‐meter length scale. Since SF is a commonly used biomaterial surface coating with excellent neuro‐compatibility, we studied the ability to develop NGCs that can autonomously actuate silk wrinkles upon heat‐induced contraction of the SMP and evaluated the effects of the topographically functionalized construct on neuronal behavior. Using an immortalized dorsal root ganglion neuronal cell line, we found that the silk‐wrinkled conduits displayed high neuronal viability and adhesion compared to uncoated conduits and tissue‐culture polystyrene controls. We also found that the wrinkled conduits enabled the neurons to elongate and align parallel to the direction of the wrinkled topography. Longer neurite extension was also observed on the wrinkled conduits compared to their respective controls. These findings demonstrate the potential for functional wrinkled protein coatings to provide directional cues in the fabrication of artificial NGCs for peripheral nerve repair.more » « less
-
Congreve, Daniel; Nielsen, Christian; Musser, Andrew J. (Ed.)Inhomogeneous and three-dimensional strain engineering in two dimensional materials opens up new avenues to straintronic devices for control strain sensitive photonic properties. Here we present a method to tune strain by wrinkling monolayer WSe2 attached to a 15 nm thick ALD support layer and compressing the heterostructure on a soft substrate. The ALD film stiffens the 2D material, enabling optically resolvable micron scale wrinkling rather than nanometer scale crumpling and folding. Using photoluminescence spectroscopy, we show the wrinkling introduces periodic modulation of the bandgap by 47 meV, corresponding with strain modulation from +0.67% tensile strain at the wrinkle crest to -0.31% compressive strain at the trough. Moreover, we show that cycling the substrate strain mechanically reconfigures the magnitude and direction of wrinkling and resulting band tuning. These results pave the way towards stretchable multifuctional devices based on strained 2D materials.more » « less
-
We studied the wetting behavior of multiscale self-similar hierarchical wrinkled surfaces. The hierarchical surface was fabricated on poly(dimethylsiloxane) (PDMS) substrates by manipulating the sequential strain release and combined plasma/ultraviolet ozone (UVO) treatment. The generated structured surface shows an independently controlled dual-scale roughness with level-1 small-wavelength wrinkles (wavelength of 700–1500 nm and amplitude of 50–500 nm) resting on level-2 large-wavelength wrinkles (wavelength of 15–35 μm and amplitude of 3.5–5 μm), as well as accompanying orthogonal cracks. By tuning the aspect ratio of hierarchical wrinkles, the degree of wetting anisotropy in hierarchical wrinkled surfaces, defined as the contact angle difference between the parallel and perpendicular directions to the wrinkle grooves, is found to change between 3° and 9°. Through both experimental characterization (confocal fluorescence imaging) and theoretical analyses, we showed that the wetting state in the hierarchical wrinkled surface is in the Wenzel wetting state. We found that the measured apparent contact angle is larger than the theoretically predicted Wenzel contact angle, which is found to be attributed to the three-phase contact line pinning effect of both wrinkles and cracks that generates energetic barriers during the contact line motion. This is evidenced by the observed sudden drop of over 20° in the static contact angles along both perpendicular and parallel directions after slight vibration perturbation. Finally, we concluded that the observed small degree of wetting anisotropy in the hierarchical wrinkled surfaces mainly arises from the competition between orthogonal wrinkles and cracks in the contact line pinning.more » « less